Named Etchants

1 + 2 Tucker’s etchant - All except high Si castings - Chemical etching - General macrostructure
100 etchant - Ge (100) wafers - Chemical etching
111 etchant - Ge (111) and Si (111) wafers - Chemical polishing/etching
6.6.1 etchant - For etch pits on InP, InPAs, GeInPAs
92.5.3 etchant - Steel for high temperatures
A etchant
A/B etchant - Al2O3 clear fused sapphire blanks and (0001) single crystal oriented blanks
A/B etchant - GaAs (111) wafers with zinc diffusion - Chemical etching
A/B etchant - GaSb (100) wafers Te-doped - Chemical etching
A/B etchant - InAs (111), (110) and (100) wafers - Chemical etching
A/B etchant - InP (TTT)B wafers - Chemical etching
AB etchant (RCA) - Glass-thin film deposition and growth - Chemical cleaning
AB etchant, diluted - Alminium gallium arsenide (Al(x) Ga(1-x) As) - Dislocation etching
AB etchant, modified - Gallium arsenide
AB etchant, modified - Indium phosphide (InP) - Chemical etching - General microstructure
AG-21's etchant for superalloy - Chemical etching
AHA etchant - For GaAs
AI-7 etchant - For macro etching ferrous cast alloys - Chemical etching
ASTM dislocation etchant - Dislocation etching
ASTM etchant No. 1 - For Al base alloys
ASTM etchant No. 10 - Beryllium - Chemical etching
ASTM etchant No. 10 - For Be
ASTM etchant No. 10 - Ni superalloys - Chemical etching
ASTM etchant No. 100 - Fe + 12-20 Cr + 4-10 Ni + <7% steels - Chemical etching
ASTM etchant No. 100 - Ferric chloride - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No. 100 - Non stainless maraging steels - Chemical etching
ASTM etchant No. 101 - Chrome regia - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No. 101 - Fe + 15-30 Cr + 6-40 Ni + <5% steels - Chemical etching
ASTM etchant No. 102 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No. 102 - Fe + 15-30 Cr + 6-40 Ni + <5% steels - Electrolytic etching
ASTM etchant No. 103 - Fe + 16-25 Cr + 3-6 Ni + 5-1C
ASTM etchant No. 103 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 103 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 104 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 104 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 104 - Frank's etchant - Fe + 16-25 Cr + 3-6 Ni + 5-1C
ASTM etchant No. 105 -2-5-3 etchant - Steel for high temperatures
ASTM etchant No. 105 - High temperature steels - Chemical etching
ASTM etchant No. 105 - Ni superalloys - Chemical etching
ASTM etchant No. 106 - High temperature steels - Chemical etching
ASTM etchant No. 106 - Steel for high temperatures
ASTM etchant No. 107 - E-etchant (EI-IR etchant) - Steel for high temperatures
ASTM etchant No. 107 - High temperature steels - Electrolytic etching
ASTM etchant No. 107 - Ni superalloys - Electrolytic etching
ASTM etchant No. 107 - Ni superalloys - Electrolytic etching
ASTM etchant No. 107 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 108 - High temperature steels - Electrolytic etching
ASTM etchant No. 108 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 108 - Steel for high temperatures
ASTM etchant No. 109 - HCl-HNO3-CuCl2 x H2O - Non stainless maraging steels
ASTM etchant No. 109 - Non stainless maraging steels - Chemical etching
ASTM etchant No. 11 - Beryllium - Chemical etching
ASTM etchant No. 11 - For Be allloys
ASTM etchant No. 11 - Ti alloys - Chemical etching
ASTM etchant No. 110 - Tool steels
ASTM etchant No. 110 - Tool steels - Chemical etching
ASTM etchant No. 111 - Fe superalloys - Electrolytic etching
ASTM etchant No. 111 - Iron
ASTM etchant No. 111 - Ni superalloys - Chemical etching
ASTM etchant No. 112 - Pb + Ca alloys - Chemical etching
ASTM etchant No. 112 - Pb+Ca alloys
ASTM etchant No. 113 - Pb + Ca alloys - Chemical etching
ASTM etchant No. 113 - Acetic/nitric - Pb + <2 Sb alloys
ASTM etchant No. 113 - Pb + >2 Sb alloys - Chemical etching
ASTM etchant No. 114 - Acetic/nitric - Pb + <2 Sb alloys
ASTM etchant No. 114 - Pb + >2 Sb alloys - Chemical etching
ASTM etchant No. 114Pb + <2 Sb alloys - Chemical etching
ASTM etchant No. 115 - Pb + <2 Sb alloys
ASTM etchant No. 115 - Pb + <2 Sb alloys - Chemical etching
ASTM etchant No. 116 - Pb alloys
ASTM etchant No. 116 - Pb alloys - Chemical etching
ASTM etchant No. 116 - Sn-Pb alloys - Chemical etching
ASTM etchant No. 117 - Sn-Fe
ASTM etchant No. 117a - Sn-Fe alloys - Chemical etching
ASTM etchant No. 117b - Pb alloys - Chemical etching
ASTM etchant No. 118 - Glycol - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 118 - Magnesium - Chemical etching
ASTM etchant No. 118 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 118 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 118 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 119 - Acetic glycol - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 119 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 119 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 119 - Mg-Mn alloys - Chemical etching
ASTM etchant No. 119 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 119 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 119 - Pure magnesium - Chemical etching
ASTM etchant No. 12 - Aqua regia - For chromium base alloys
ASTM etchant No. 12 - Chromium - Chemical etching
ASTM etchant No. 12 - Ni superalloys - Chemical etching
ASTM etchant No. 120 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 120 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 120 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 120 - Mg-Rare Earth-Zr alloys - Chemical etching
ASTM etchant No. 120 - Mg-Zn-Th-Zr alloys - Chemical etching
ASTM etchant No. 120 - Pure magnesium - Chemical etching
ASTM etchant No. 121 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 121 - Mg-Rare Earth-Zr alloys - Chemical etching
ASTM etchant No. 121 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 121 - Mg-Zn-Th-Zr alloys - Chemical etching
ASTM etchant No. 121 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 121 - Phospho picral - Mg-Al, Mg-Al-Zn (Al + Zn >5%
ASTM etchant No. 121 - Pure magnesium - Chemical etching
ASTM etchant No. 122 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 122 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 122 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 122 - Mg-Mn alloys - Chemical etching
ASTM etchant No. 122 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 122 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 122 - Pure magnesium - Chemical etching
ASTM etchant No. 123 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 123 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Electrolytic etching
ASTM etchant No. 123 - Pure magnesium - Electrolytic etching
ASTM etchant No. 124 - Acetic-picral - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 124 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 124 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 124 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 124 - Mg-Mn alloys - Chemical etching
ASTM etchant No. 124 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 124 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 127 - Acetic-picral - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 127 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 127 - Mg-Al, Mg-Al-Zn (Al + Zn 5% alloys - Chemical etching
ASTM etchant No. 127 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 127 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 127 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 128 - Mg-Zn-Zr
ASTM etchant No. 128 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 129 - Molybdenum
ASTM etchant No. 129 - Molybdenum - Chemical etching
ASTM etchant No. 129 - Molybdenum - Chemical etching
ASTM etchant No. 129 - Molybdenum - Chemical etching
ASTM etchant No. 129 - Niobium - Chemical etching
ASTM etchant No. 129 - Niobium - Chemical etching
ASTM etchant No. 13 - Oxalic acid - For Cr base alloys
ASTM etchant No. 130 - Molybdenum
ASTM etchant No. 130 - Molybdenum - Chemical etching
ASTM etchant No. 130 - Molybdenum - Electrolytic etching
ASTM etchant No. 131 - Molybdenum
ASTM etchant No. 131 - Molybdenum - Electrolytic etching
ASTM etchant No. 131 - Molybdenum - Electrolytic etching
ASTM etchant No. 131 - Tungsten - Electrolytic etching
ASTM etchant No. 131 - Tungsten - Electrolytic etching
ASTM etchant No. 132 - Molybdenum
ASTM etchant No. 132a - As cast molybdenum - Chemical etching
ASTM etchant No. 132a - As cast tungsten - Chemical etching
ASTM etchant No. 133 - Ni superalloys - Chemical etching
ASTM etchant No. 133 - Ni-Ti
ASTM etchant No. 133 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 133 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 134 - Ni-Cr
ASTM etchant No. 134 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 134 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 134 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 135 - Pure Ni and high Ni alloys
ASTM etchant No. 135 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 136 - Pure Ni and high Ni alloys
ASTM etchant No. 136 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 137 - Pure Ni and high Ni alloys
ASTM etchant No. 137 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 138 - Carapella's etchant - Ni-Ag
ASTM etchant No. 138 - Ni superalloys - Chemical etching
ASTM etchant No. 138 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 139 - Ni-Ag
ASTM etchant No. 139 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 13a - Fe + 15-30 Cr + 6-40 Ni + <5% - Electrolytic etching
ASTM etchant No. 13a - Ni superalloys - Electrolytic etching
ASTM etchant No. 13a - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 13b - Fe + 15-30 Cr + 6-40 Ni + <5% steels - Electrolytic etching
ASTM etchant No. 13b - Rhenium - Electrolytic etching
ASTM etchant No. 13c - Chromium - Electrolytic etching
ASTM etchant No. 14 - For Co
ASTM etchant No. 14 - Tool steels - Chemical etching
ASTM etchant No. 140 - Ni-Al
ASTM etchant No. 140 - Ni-Al alloys - Chemical etching
ASTM etchant No. 140 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 141 - Contrast etchant - Ni-Al
ASTM etchant No. 141 - Ni-Al alloys - Chemical etching
ASTM etchant No. 141 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 142 - Ni-Al
ASTM etchant No. 142 - Ni-Al alloys - Electrolytic etching
ASTM etchant No. 143 - Ni-Al
ASTM etchant No. 143 - Ni-Al alloys - Chemical etching
ASTM etchant No. 143 - Ni-Mo alloys - Chemical etching
ASTM etchant No. 143 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 144 - Ni-Cr
ASTM etchant No. 144 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 145 - Ni-Cr
ASTM etchant No. 145 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 146 - Ni-Cr
ASTM etchant No. 146 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 147 - Ni-Cr
ASTM etchant No. 147 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 148 - Ni-Fe
ASTM etchant No. 148 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 149 - Ni-Fe
ASTM etchant No. 149 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 15 - For Co
ASTM etchant No. 150 - Ni-Fe
ASTM etchant No. 150 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 151 - Ni-Ti
ASTM etchant No. 151 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 152 - Ni-Zn
ASTM etchant No. 152 - Ni-Zn alloys - Chemical etching
ASTM etchant No. 153 - Ni superalloys
ASTM etchant No. 153 - Ni superalloys - Chemical etching
ASTM etchant No. 154 - Ni superalloys
ASTM etchant No. 154 - Ni superalloys - Chemical etching
ASTM etchant No. 154 - Ni superalloys - Chemical etching
ASTM etchant No. 155 - Beraha's E etchant - Ni superalloys
ASTM etchant No. 155 - Ni superalloys - Chemical etching
ASTM etchant No. 156 - Ni superalloys
ASTM etchant No. 156 - Ni superalloys - Electrolytic etching
ASTM etchant No. 157 - Hastelloy-W - Chemical etching
ASTM etchant No. 157 - Ni Hastelloy-W
ASTM etchant No. 158 - Niobium
ASTM etchant No. 158 - Niobium - Chemical etching
ASTM etchant No. 158 - Niobium - Chemical etching
ASTM etchant No. 158 - Ta alloys - Chemical etching
ASTM etchant No. 158 - Tantalum - Chemical etching
ASTM etchant No. 158 - Ti alloys - Chemical etching
ASTM etchant No. 159 - Niobium
ASTM etchant No. 159 - Niobium - Chemical etching
ASTM etchant No. 159 - Niobium - Chemical etching
ASTM etchant No. 159 - Ta alloys - Chemical etching
ASTM etchant No. 159 - Tantalum - Chemical etching
ASTM etchant No. 16 - Co high temperature alloys - Electrolytic etching
ASTM etchant No. 16 - Hydrochloric acid - For Co, high temperature alloys
ASTM etchant No. 16 - Fe as residual metal in vacuum systems - Chemical cleaning
ASTM etchant No. 160 - Niobium
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 161 - Niobium
ASTM etchant No. 161 - Niobium - Chemical etching
ASTM etchant No. 161 - Niobium - Chemical etching
ASTM etchant No. 161 - Ta alloys - Chemical etching
ASTM etchant No. 161 - TaN thin films - Chemical etching - General microstructure
ASTM etchant No. 161 - Tantalum - Chemical etching
ASTM etchant No. 162 - Niobium
ASTM etchant No. 162 - Niobium - Chemical etching
ASTM etchant No. 162B - Niobium - Chemical etching
ASTM etchant No. 163 - Niobium
ASTM etchant No. 163 - Niobium - Chemical etching
ASTM etchant No. 163 - Niobium - Chemical etching
ASTM etchant No. 163 - Ta alloys - Chemical etching
ASTM etchant No. 163 - Tantalum - Chemical etching
ASTM etchant No. 164 - Niobium
ASTM etchant No. 164 - Niobium - Chemical etching
ASTM etchant No. 164 - Niobium - Chemical etching
ASTM etchant No. 164 - Ta alloys - Chemical etching
ASTM etchant No. 164 - Tantalum - Chemical etching
ASTM etchant No. 164 - Tantalum - Chemical etching
ASTM etchant No. 165 - Vanadium
ASTM etchant No. 165a - Osmium - Electrolytic etching
ASTM etchant No. 165a - Osmium - Electrolytic etching
ASTM etchant No. 165a - Pd alloys - Electrolytic etching
ASTM etchant No. 165a - Pure palladium - Electrolytic etching
ASTM etchant No. 165b - Pure vanadium - Electrolytic etching
ASTM etchant No. 166 - Pd alloys
ASTM etchant No. 166 - Pd alloys - Chemical etching
ASTM etchant No. 166 - Pure palladium - Chemical etching
ASTM etchant No. 167 - Pt alloys
ASTM etchant No. 167 - Pt alloys - Chemical etching
ASTM etchant No. 167 - Pure platinum - Chemical etching
ASTM etchant No. 168 - Pt-10% Rh
ASTM etchant No. 168 - Pt-10% Rh alloy - Chemical etching
ASTM etchant No. 169 - Plutonium
ASTM etchant No. 169 - Plutonium - Electrolytic etching
ASTM etchant No. 17 - For Co
ASTM etchant No. 170 - Rhenium
ASTM etchant No. 170a - Rhenium - Chemical etching
ASTM etchant No. 170a - Ti alloys - Chemical etching
ASTM etchant No. 170a - U Beryllides - Chemical etching
ASTM etchant No. 170b - Pure vanadium - Chemical etching
ASTM etchant No. 171 - Hydrochloric acid - Rhodium
ASTM etchant No. 171 - Rhodium - Electrolytic etching
ASTM etchant No. 172 - Pure Ag
ASTM etchant No. 172 - Pure silver - Chemical etching
ASTM etchant No. 173 - Ag solders
ASTM etchant No. 173 - Ag solders - Chemical etching
ASTM etchant No. 173 - Ag-Pd alloys - Chemical etching
ASTM etchant No. 173 - Pure Ag - Chemical etching
ASTM etchant No. 174 - Ag alloys
ASTM etchant No. 174 - Ag alloys - Chemical etching
ASTM etchant No. 175 - Ag alloys
ASTM etchant No. 175 - Ag alloys - Chemical etching
ASTM etchant No. 176 - Ag solders
ASTM etchant No. 176 - Ag solders - Chemical etching
ASTM etchant No. 177 - Pure tantalum - Chemical etching
ASTM etchant No. 177 - Tantalum
ASTM etchant No. 177 - Tantalum - Chemical etching
ASTM etchant No. 177 - Zn-Co alloys - Chemical etching
ASTM etchant No. 178 - Ta alloys
ASTM etchant No. 178 - Ta alloys - Chemical etching
ASTM etchant No. 178 - Tantalum - Chemical etching
ASTM etchant No. 178 - Ti alloys - Chemical etching
ASTM etchant No. 179 - Ta alloys
ASTM etchant No. 179 - Ta alloys - Chemical etching
ASTM etchant No. 18 - Chromic acid - For Co alloys, high temperature alloys
ASTM etchant No. 18 - Hard-Facing and tool metals - Electrolytic etching
ASTM etchant No. 18 - High temperature alloys - Electrolytic etching
ASTM etchant No. 18 - Ni superalloys - Electrolytic etching
ASTM etchant No. 18 - Pure titanium - Electrolytic etching
ASTM etchant No. 180 - Pure tin - Chemical etching
ASTM etchant No. 180 - Tin
ASTM etchant No. 181 - Pure tin
ASTM etchant No. 181 - Pure tin - Chemical etching
ASTM etchant No. 182 - Sn-Pb
ASTM etchant No. 182 - Sn-Pb alloys - Chemical etching
ASTM etchant No. 183 - Sn coatings (on steel)
ASTM etchant No. 183 - Sn coatings (on steel) - Chemical etching
ASTM etchant No. 183 - Sn-Pb alloys - Chemical etching
ASTM etchant No. 184 - Babbitts
ASTM etchant No. 184 - Sn babbitts - Chemical etching
ASTM etchant No. 185
ASTM etchant No. 186 - Pure titanium
ASTM etchant No. 186 - Pure titanium - Chemical etching
ASTM etchant No. 186 - Ti alloys - Chemical etching
ASTM etchant No. 187 - Kroll's etchant - Ti alloys
ASTM etchant No. 187 - Ti alloys - Chemical etching
ASTM etchant No. 188 - Mg-Al, Mg-Al-Zn (Al + Zn <5 alloys - Chemical etching
ASTM etchant No. 188 - Pure titanium
ASTM etchant No. 188 - Pure titanium - Chemical etching
ASTM etchant No. 188 - Ti alloys - Chemical etching
ASTM etchant No. 189 - Ti-5 Al-2.5 Sn
ASTM etchant No. 189 - Ti-5 Al-2.5 Sn alloys - Chemical etching
ASTM etchant No. 19 - Co Hard-Facing and tool metals - Chemical etching
ASTM etchant No. 19 - Co high temperature alloys - Chemical etching
ASTM etchant No. 19 - Groesbeck's etchant - For Co alloys, high temperature alloys
ASTM etchant No. 190 - Ti-6 Al-6V-2 Sn
ASTM etchant No. 190 - Ti-6 Al-6V-2 Sn alloys - Chemical etching
ASTM etchant No. 191 - Ti-Al-Zr
ASTM etchant No. 191 - Ti-Al-Zr alloys - Chemical etching
ASTM etchant No. 192 - Kroll's etchant - Ti alloys
ASTM etchant No. 192 - Ti alloys - Chemical etching
ASTM etchant No. 192 - Ti alloys - Chemical etching
ASTM etchant No. 192 - Ti-13V-11Cr3 Al (aged) alloys - Chemical etching
ASTM etchant No. 192 - Ti-8Mn alloys - Chemical etching
ASTM etchant No. 193 - Ti-Si
ASTM etchant No. 193 - Ti-Si alloys - Chemical etching
ASTM etchant No. 194 - Ti alloys
ASTM etchant No. 194 - Ti alloys - Chemical etching
ASTM etchant No. 195 - Pure uranium
ASTM etchant No. 195 - Pure uranium - Electrolytic etching
ASTM etchant No. 195 - U alloys - Electrolytic etching
ASTM etchant No. 196 - Pure uranium
ASTM etchant No. 196 - Pure uranium - Chemical etching
ASTM etchant No. 196 - U alloys - Chemical etching
ASTM etchant No. 197 - Pure vanadium
ASTM etchant No. 197 - Pure vanadium - Electrolytic etching
ASTM etchant No. 198 - Pure vanadium
ASTM etchant No. 198 - Pure vanadium - Chemical etching
ASTM etchant No. 198 - V alloys - Chemical etching
ASTM etchant No. 199 - V alloys
ASTM etchant No. 199 - V alloys - Chemical etching
ASTM etchant No. 19b - Ni superalloys - Chemical etching
ASTM etchant No. 1a - Aluminum 1000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 2000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 3000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 4000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 5000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 6000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 7000 series - Chemical etching
ASTM etchant No. 1a - Pure aluminum - Chemical etching
ASTM etchant No. 1b - Pure aluminum - Chemical etching
ASTM etchant No. 1c - Ti alloys - Chemical etching
ASTM etchant No. 1c - Ti alloys - Chemical etching
ASTM etchant No. 1d - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 1d - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 2 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 5000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 7000 series - Chemical etching
ASTM etchant No. 2 - NaOH (Hatch's etchant) - Al alloys
ASTM etchant No. 2 - Pure aluminum - Chemical etching
ASTM etchant No. 20 - Co Hard-Facing and tool metals - Chemical etching
ASTM etchant No. 20 - Co high temperature alloys - Chemical etching
ASTM etchant No. 20 - For Co alloys, high temperature alloys
ASTM etchant No. 200 - Potassium etchant - Pure zinc
ASTM etchant No. 200 - Pure zinc - Chemical etching
ASTM etchant No. 201 - Zn-Cu
ASTM etchant No. 201 - Zn-Cu alloys - Chemical etching
ASTM etchant No. 202 - Zinc die castings
ASTM etchant No. 202 - Zn Die castings - Chemical etching
ASTM etchant No. 203 - Zn-Cu
ASTM etchant No. 203 - Zn-Cu alloys - Electrolytic etching
ASTM etchant No. 204 - Zirconium
ASTM etchant No. 204 - Zirconium - Chemical etching
ASTM etchant No. 205 - Zirconium
ASTM etchant No. 205 - Zirconium - Chemical etching
ASTM etchant No. 206 - Zirconium
ASTM etchant No. 206 - Zirconium - Chemical etching
ASTM etchant No. 207 - U alloys
ASTM etchant No. 207 - U alloys - Chemical etching
ASTM etchant No. 208
ASTM etchant No. 209 - Molybdenum - Chemical etching
ASTM etchant No. 209 - Tungsten - Chemical etching
ASTM etchant No. 209 - W-Th
ASTM etchant No. 209 - W-Th alloys - Chemical etching
ASTM etchant No. 21 - Co high temperature alloys - Chemical etching
ASTM etchant No. 21 - For high temperature alloys
ASTM etchant No. 22 - HCl+H2O2 - For high temperature alloys
ASTM etchant No. 220 - Stainless steels - Chemical etching
ASTM etchant No. 22a - Ni superalloys - Chemical etching
ASTM etchant No. 22b - Co high temperature alloys - Chemical etching
ASTM etchant No. 23 - HCl-methanol
ASTM etchant No. 24 - Co high temperature alloys - Chemical etching
ASTM etchant No. 24 - HCl-HNO3-FeCl3 - For high temperature alloys
ASTM etchant No. 25 - Co high temperature alloys - Chemical etching
ASTM etchant No. 25 - High temperature steels - Chemical etching
ASTM etchant No. 25 - Marble's etchant - For high temperature alloys
ASTM etchant No. 25 - Ni superalloys - Chemical etching
ASTM etchant No. 25 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 25 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 26 - Cu alloys - Chemical etching
ASTM etchant No. 26 - For Cu and alloys
ASTM etchant No. 26 - Pure copper - Chemical etching
ASTM etchant No. 27 - Cu alloys - Chemical etching
ASTM etchant No. 27 - For Cu and alloys
ASTM etchant No. 27 - Pure copper - Chemical etching
ASTM etchant No. 28 - Cu alloys - Chemical etching
ASTM etchant No. 28 - Cu alloys - Chemical etching
ASTM etchant No. 28 - Ferric nitrate - For Cu and alloys
ASTM etchant No. 28 - Pure copper - Chemical etching
ASTM etchant No. 28 - Pure copper - Chemical etching
ASTM etchant No. 29 - Cu alloys - Chemical etching
ASTM etchant No. 29 - Potassium dichromate - For Cu and alloys
ASTM etchant No. 29 - Pure copper - Chemical etching
ASTM etchant No. 3 - Aluminum 000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 4000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 5000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 7000 series - Chemical etching
ASTM etchant No. 3 - Keller's etchant - For Al and alloys
ASTM etchant No. 3 - Pure aluminum - Chemical etching
ASTM etchant No. 30 - Ag-Cu alloys - Chemical etching
ASTM etchant No. 30 - Cu alloys - Chemical etching
ASTM etchant No. 30 - NH4OH+H2O - For Cu and alloys
ASTM etchant No. 30 - Pure copper - Chemical etching
ASTM etchant No. 31 - Amonium persulphate - For Cu, Cu-Al, Cu-Ni-Zr, Cu alloys
ASTM etchant No. 31a - Fe + C - Chemical etching
ASTM etchant No. 31b - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No. 31c - Fe + 12-20 Cr + 4-10 Ni + <7% - Electrolytic etching
ASTM etchant No. 31c - Fe + 12-20 Cr + 4-10 Ni + 7% - Electrolytic etching
ASTM etchant No. 31c - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 31d - Pure copper - Chemical etching
ASTM etchant No. 31d - Cu alloys - Chemical etching
ASTM etchant No. 31d - Cu-Al (aluminum bronze) - Chemical etching
ASTM etchant No. 31d - Nickel silver - Chemical etching
ASTM etchant No. 32 - Chromic acid - For Cu, Cu-Ni-Zn, Cu alloys
ASTM etchant No. 32 - Cu alloys - Chemical etching
ASTM etchant No. 32 - Nickel silver - Chemical etching
ASTM etchant No. 32 - Pure copper - Chemical etching
ASTM etchant No. 33 - Chromic/hydrochloric - For Cu, Cu-Al, Cu-Ni, Cu alloys
ASTM etchant No. 33 - Cu alloys - Chemical etching
ASTM etchant No. 33 - Nickel silver - Chemical etching
ASTM etchant No. 33 - Pure copper - Chemical etching
ASTM etchant No. 34 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 34 - For Cu, Cu-Al, Cu-Ni, Cu alloys
ASTM etchant No. 34b - Cu alloys - Chemical etching
ASTM etchant No. 34b - Cu-Al (aluminum bronze) - Chemical etching
ASTM etchant No. 34b - Pure copper - Chemical etching
ASTM etchant No. 35 - Cu alloys - Chemical etching
ASTM etchant No. 35 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 35 - Grard's No.1 etch - For Cu, Cu-Al, Cu alloy
ASTM etchant No. 35 - Pure copper - Chemical etching
ASTM etchant No. 36 - Cu alloys - Chemical etching
ASTM etchant No. 36 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 36 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 36 - Pure copper - Chemical etching
ASTM etchant No. 37 - Cu alloys - Chemical etching
ASTM etchant No. 37 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 37 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 37 - Pure copper - Chemical etching
ASTM etchant No. 38 - Cu alloys - Chemical etching
ASTM etchant No. 38 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 38 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 38 - Pure copper - Chemical etching
ASTM etchant No. 38- For Cu, Cu-Al, Cu alloys
ASTM etchant No. 39 - Cu alloys - Chemical etching
ASTM etchant No. 39 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 39 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 39 - Pure copper - Chemical etching
ASTM etchant No. 3a - Ti alloys - Chemical etching
ASTM etchant No. 3b - Aluminum 7000 series - Chemical etching
ASTM etchant No. 4 - For Al and Al base alloys
ASTM etchant No. 4 - Pure aluminium - Electrolytic etching
ASTM etchant No. 40 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 40 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 40 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 40 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 40 - Pure copper - Chemical etching
ASTM etchant No. 41 - Cu alloys - Chemical etching
ASTM etchant No. 41 - Cu-Be alloys - Chemical etching
ASTM etchant No. 41 - Cu-Cr alloys - Chemical etching
ASTM etchant No. 41 - Cu-Mn alloys - Chemical etching
ASTM etchant No. 41 - Cu-Si alloys - Chemical etching
ASTM etchant No. 41 - For Cu, Cu-Be, Cu-Cr, Cu-Mn, Cu-Si, Cu-Ni-Zn, Cu alloys
ASTM etchant No. 41 - Nickel silver - Chemical etching
ASTM etchant No. 41 - Pure copper - Chemical etching
ASTM etchant No. 42 - Cu alloys - Chemical etching
ASTM etchant No. 42 - For Cu, Cu-Ni-Zn, beta-brass
ASTM etchant No. 42 - Nickel silver - Chemical etching
ASTM etchant No. 42 - Pure copper - Chemical etching
ASTM etchant No. 43 - Cu alloys - Chemical etching
ASTM etchant No. 43 - For Cu and alloys
ASTM etchant No. 43 - Pure copper - Chemical etching
ASTM etchant No. 44 - Ammonium/peroxide - For Cu-Al, Cu alloys
ASTM etchant No. 44 - Cu alloys - Chemical etching
ASTM etchant No. 44 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 45 - Cu-Al (Aluminum bronze) - Electrolytic etching
ASTM etchant No. 45 - Cu-Be alloys - Electrolytic etching
ASTM etchant No. 45 - For Cu-Al, Cu-Be
ASTM etchant No. 46 - Cu-Be
ASTM etchant No. 46 - Cu-Be alloys - Chemical etching
ASTM etchant No. 47 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 47 - Cyanide/persulphate - For Cu-Ni
ASTM etchant No. 47 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 48 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 48 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No. 48 - For Cu-Ni
ASTM etchant No. 49 - Cu alloys - Electrolytic etching
ASTM etchant No. 49 - Cu alloys - Electrolytic etching
ASTM etchant No. 49 - Cu-Ni alloys - Electrolytic etching
ASTM etchant No. 49 - For Cu-Ni, Cu-Ni-Zn, Cu alloys, beta-brass
ASTM etchant No. 49 - Nickel silver - Electrolytic etching
ASTM etchant No. 5 - Aluminum 1000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 3000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 5000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 6000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 7000 series - Electrolytic etching
ASTM etchant No. 5 - Barker's etchant - For Al base alloys and brass
ASTM etchant No. 5 - Pure aluminum - Electrolytic etching
ASTM etchant No. 50 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 50 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 50 - Ni-Al alloys - Chemical etching
ASTM etchant No. 50 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 50 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 50 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 50 - Nitric/acetic - For Cu-Ni
ASTM etchant No. 51 - Cu-Sn (Tin bronze) - Chemical etching
ASTM etchant No. 51 - For Cu-Sn
ASTM etchant No. 51 - Pure tin - Chemical etching
ASTM etchant No. 52 - Cu-Sn (Tin bronze) - Chemical etching
ASTM etchant No. 52 - Cu-Sn (tin bronze)
ASTM etchant No. 53 - Cu alloys - Chemical etching
ASTM etchant No. 53 - For Cu alloys (polish)
ASTM etchant No. 54 - Cu alloys - Electrolytic etching
ASTM etchant No. 54 - For brass
ASTM etchant No. 55 - Dysprosium - Chemical etching
ASTM etchant No. 55 - Erbium - Chemical etching
ASTM etchant No. 55 - For Dy, Er, Gd, Ho
ASTM etchant No. 55 - Gadolinium - Chemical etching
ASTM etchant No. 55 - Holmium - Chemical etching
ASTM etchant No. 56 - Dysprosium - Chemical etching
ASTM etchant No. 56 - Erbium - Chemical etching
ASTM etchant No. 56 - For Dy, Er, Gd, Ho
ASTM etchant No. 56 - Gadolinium - Chemical etching
ASTM etchant No. 56 - Holmium - Chemical etching
ASTM etchant No. 57 - Acetic acid/peroxide - For Gd
ASTM etchant No. 57 - Gadolinium - Chemical etching
ASTM etchant No. 57 - Pb + <2 Sb - Chemical etching
ASTM etchant No. 57 - Pure lead - Chemical etching
ASTM etchant No. 58 - For Ge
ASTM etchant No. 58 - Germanium - Chemical etching
ASTM etchant No. 59 - For Ge
ASTM etchant No. 59 - Germanium - Chemical etching
ASTM etchant No. 6 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 3000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 5000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 7000 series - Chemical etching
ASTM etchant No. 6 - For Al base alloys
ASTM etchant No. 60 - CP4 etchant - For Ge
ASTM etchant No. 60 - Germanium - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - Ag alloys - Chemical etching
ASTM etchant No. 61 - For Au and noble metals (>0%)
ASTM etchant No. 61 - Pure gold - Chemical etching
ASTM etchant No. 61 - Pure palladium - Chemical etching
ASTM etchant No. 62 - Ag alloys - Chemical etching
ASTM etchant No. 62 - Au alloys - Chemical etching
ASTM etchant No. 62 - For Au and alloys
ASTM etchant No. 62 - Pd alloys - Chemical etching
ASTM etchant No. 62 - Pure Ag - Chemical etching
ASTM etchant No. 62 - Pure gold - Chemical etching
ASTM etchant No. 62 - Pure palladium - Chemical etching
ASTM etchant No. 63 - Au alloys - Chemical etching
ASTM etchant No. 63 - For Au (polish) and Au alloys
ASTM etchant No. 63 - Pure gold - Chemical etching
ASTM etchant No. 64 - For Au alloys
ASTM etchant No. 64a - Pd alloys - Chemical etching
ASTM etchant No. 64a - Pure platinum - Chemical etching
ASTM etchant No. 64b - Au alloys - Chemical etching
ASTM etchant No. 64b - Pt alloys - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
ASTM etchant No. 65 - Ag alloys - Chemical etching
ASTM etchant No. 65 - For noble metals (<0%)
ASTM etchant No. 66 - For Hf alloys
ASTM etchant No. 66 - Hafnium - Chemical etching
ASTM etchant No. 66 - Niobium - Chemical etching
ASTM etchant No. 66 - Niobium - Chemical etching
ASTM etchant No. 66 - Ta alloys - Chemical etching
ASTM etchant No. 66 - Tantalum - Chemical etching
ASTM etchant No. 66 - Zirconium - Chemical etching
ASTM etchant No. 67 - For Hf base alloys
ASTM etchant No. 67 - Hafnium - Chemical etching
ASTM etchant No. 67 - Pure titanium - Chemical etching
ASTM etchant No. 67 - Pure uranium - Chemical etching
ASTM etchant No. 67 - Ti alloys - Chemical etching
ASTM etchant No. 67 - U alloys - Chemical etching
ASTM etchant No. 67 - Zirconium - Chemical etching
ASTM etchant No. 68 - For Hf base alloys
ASTM etchant No. 68 - Hafnium - Electrolytic etching
ASTM etchant No. 68 - Pure titanium - Electrolytic etching
ASTM etchant No. 68 - Ti alloys - Electrolytic etching
ASTM etchant No. 68 - U + Zr alloys - Electrolytic etching
ASTM etchant No. 68 - Zirconium - Electrolytic etching
ASTM etchant No. 69 - For Hf base alloys
ASTM etchant No. 69 - For Hf base alloys
ASTM etchant No. 69 - Hafnium - Electrolytic etching
ASTM etchant No. 69 - Pure titanium - Electrolytic etching
ASTM etchant No. 69 - Pure uranium - Electrolytic etching
ASTM etchant No. 69 - Ti alloys - Electrolytic etching
ASTM etchant No. 69 - U alloys - Electrolytic etching
ASTM etchant No. 69 - Zirconium - Electrolytic etching
ASTM etchant No. 7 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 7 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 7 - Aluminum 3000 series - Chemical etching
ASTM etchant No. 7 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 7 - For Al base alloys
ASTM etchant No. 70 - For Hf base alloys
ASTM etchant No. 70 - Hafnium - Chemical etching
ASTM etchant No. 71 - For Hf base alloys
ASTM etchant No. 71 - Hafnium - Chemical etching
ASTM etchant No. 71 - Zirconium - Chemical etching
ASTM etchant No. 72 - For Hf base alloys
ASTM etchant No. 73 - For Ir base alloys
ASTM etchant No. 73a - Pt alloys - Electrolytic etching
ASTM etchant No. 73a - Pure platinum - Electrolytic etching
ASTM etchant No. 73b - Ruthenium - Electrolytic etching
ASTM etchant No. 73b - Ruthenium - Electrolytic etching
ASTM etchant No. 73c - Iridium - Electrolytic etching
ASTM etchant No. 74 - Nital - For steels
ASTM etchant No. 74a - Fe + C - Chemical etching
ASTM etchant No. 74a - Fe + C - Chemical etching
ASTM etchant No. 74a - Mg-Al, Mg-Al-Zn (Al + Zn <5% - Chemical etching
ASTM etchant No. 74a - Mg-Al, Mg-Al-Zn (Al + Zn >5% - Chemical etching
ASTM etchant No. 74a - Mg-Mn alloys - Chemical etching
ASTM etchant No. 74a - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 74a - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 74a - Pure iron - Chemical etching
ASTM etchant No. 74a - Pure magnesium - Chemical etching
ASTM etchant No. 74a - Tool steels - Chemical etching
ASTM etchant No. 74a - Zn-Fe alloys - Chemical etching
ASTM etchant No. 74b - Pb + <2 Sb - Chemical etching
ASTM etchant No. 74b - Pb + >2 Sb - Chemical etching
ASTM etchant No. 74b - Pb Babbitt - Chemical etching
ASTM etchant No. 74b - Sn-Pb alloys - Chemical etching
ASTM etchant No. 74d - Pure tin - Chemical etching
ASTM etchant No. 74d - Sn-Cd alloys - Chemical etching
ASTM etchant No. 74d - Sn-Fe alloys - Chemical etching
ASTM etchant No. 74e - Ni-Fe alloys - Chemical etching
ASTM etchant No. 74e - Ni-Mn alloys - Chemical etching
ASTM etchant No. 75 - Gorsuch's etchant - Iron
ASTM etchant No. 75 - Pure iron - Chemical etching
ASTM etchant No. 76 - Fe + C - Chemical etching
ASTM etchant No. 76 - Picral - Fe + C
ASTM etchant No. 77 - Fe + C - Chemical etching
ASTM etchant No. 77 - Fe + C - Chemical etching
ASTM etchant No. 77 - Super picral - Fe + C
ASTM etchant No. 78 - Fe + <1C + <4% additions
ASTM etchant No. 78 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No. 78 - Fe + 1C + <4% additions - Chemical etching
ASTM etchant No. 78 - Fe + C - Chemical etching
ASTM etchant No. 79 - Fe + C - Chemical etching
ASTM etchant No. 79 - Fry's etchant - Fe + C
ASTM etchant No. - For Al-Cu, Al-Mg, Al-Si, Cu
ASTM etchant No.0 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.0 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.0 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.0 - Tool steels - Chemical etching
ASTM etchant No.0 - Vilella - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.1 - Fe + <1C + <4% additions
ASTM etchant No.1 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.1 - Steels, carbon and alloy types - Chemical etching
ASTM etchant No.2 - Acid ferric chloride - Fe + <1C + <4% additions
ASTM etchant No.2 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.3 - Fe + <1C + <4% additions
ASTM etchant No.3 - Fe + <1C + <4% additions - Electrolytic etching
ASTM etchant No.3 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No.3 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No.3a - Fe + 15-30 Cr + 6-40 Ni + <5% - Electrolytic etching
ASTM etchant No.3b - Non-stainless maraging steels - Electrolytic etching
ASTM etchant No.4 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.4 - Howarth's etchant - Fe + <1C + <4% additions
ASTM etchant No.5 - Alkaline sodium picrate - Fe + <1C + <4% additions
ASTM etchant No.5 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.6 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.6 - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.6 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.6 - Fe + 16-25 Cr + 3-6 Ni + 5-1C - Chemical etching
ASTM etchant No.6 - High temperature steel - Chemical etching
ASTM etchant No.6 - Non-stainless maraging steels - Chemical etching
ASTM etchant No.6 - Tool steels - Chemical etching
ASTM etchant No.7 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.7 - Glyceregia - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.9 - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.9 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.9 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.9 - High temperature steels - Chemical etching
ASTM etchant No.9 - Ni-Al alloys - Chemical etching
ASTM etchant No.9 - Non-stainless maraging steels - Chemical etching
ASTM etchant No.a - Aluminum 2000 series - Chemical etching
ASTM etchant No.a - Aluminum 3000 series - Chemical etching
ASTM etchant No.a - Aluminum 5000 series - Chemical etching
ASTM etchant No.a - Aluminum 6000 series - Chemical etching
ASTM etchant No.a - Aluminum 6000 series - Chemical etching
ASTM etchant No.b - Admiralty metal - Electrolytic etching
ASTM etchant No.b - Pure copper - Electrolytic etching
ASTM etchant No. - Beryllium - Chemical etching
ASTM etchant No. - For Be
ASTM etchant No. - Pure cobalt - Chemical etching
ASTM etchant No.0 - HNO3-HF in glycerol - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.1 - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.1 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.1 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.2
ASTM etchant No.3
ASTM etchant No.4 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.4 - Kalling's etchant No. 2 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.4 - Ni superalloys - Chemical etching
ASTM etchant No.5 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.5 - Kalling's etchant No. 1 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.6 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.6 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.7 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.7 - High temperature steels - Chemical etching
ASTM etchant No.7 - Potassium hydroxide - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.8 - Murakami's etchant - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Ni-Cr alloys - Chemical etching
ASTM etchant No.8c - Molybdenum - Chemical etching
ASTM etchant No.8c - Pure tungsten - Chemical etching
ASTM etchant No.8c - Rhenium - Chemical etching
ASTM etchant No.9 - Beraha's etchant - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.9 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.9 - Fe + 16-25 Cr + 3-6 Ni + 5-1C - Chemical etching
ASTM etchant No.9 - Non-stainless maraging steels - Chemical etching
ASTM etchant No.57 - Pb + >2 Sb - Chemical etching
Abraham's AB etchant - - Gallium arsenide
Accary etchant - U-C alloys - Electrolytic etching
Accary etchant - Uranium - Chemical etching
Accary etchant - Uranium - For etching U carbide
Acetic glycol etchant - Magnesium - Chemical etching
Acetic glycol etchant - Rare earth - Chemical etching
Acetic-glycol etchant - Mg and alloys - Chemical etching
Acetic-picral etchant - Magnesium - Chemical etching
Acetic-picral etchant - Magnesium - Chemical etching
Acetic-picral etchant - Magnesium - Chemical etching
Adcock etchant - Lead - Electrolytic etching
Adcock etchant - Pb-Sb alloys - Electrolytic etching
Adler's etchant - Stainless steel - Chemical etching
Adler's etchant - Co and Co-Al alloys - Chemical etching - General microstructure
Adler's etchant - For iron and steels - General macrostructure
Adler's etchant - For the investigation of the cast structure and the heat-affected zone in welds in steels
Adler's etchant - High-alloy, corrosion-resistant steels, Co and Ni alloys
Adler's etchant - Ni alloys - General macrostructure
Adler's etchant - Ni brazing alloys when brazed to steels - Galvanic Ni coatings - Chemical etching
Adler's etchant - Ni-base foundary alloys - Chemical etching - General microstructure
Adler's etchant - Pd-Ga alloy (Pd5Ga2) - Chemical etching
Adler's etchant - Stainless steel
Adler's etchant - Stainless steel
Adler's etchant - Steel for turbine blades - Chemical etching
Adler's etchant - Welded steel - Chemical etching
Aqua regia - Au-Al alloys - Chemical etching - General microstructure
Aqua regia - Austenitic stainless steels
Aqua regia - Austenitic stainless steels - Chemical etching
Aqua regia - Austenitic stainless steels - Chemical etching
Aqua regia - Aluminium - Chemical etching - Electrolytic polishing
Agua regia - Au thin films and specimens - Chemical etching
Agua regia - AuSn (20%) alloy as an evaporated thin film - Chemical etching
Aqua regia - Chromium - Chemical etching
Aqua regia 6% - Cemented carbides (Co) - Electrolytic etching - General microstructure
Aqua regia 5% - 73 J (Co-20Cr-6Mo) alloy - Chemical etching - General microstructure
Agua regia - Cr and Cr alloys - Chemical etching
Agua regia - Ir crystalline specimens as wire, rod, sheet - Chemical etching
Agua regia - Ir thin films deposited on silicon (100), n-type - Chemical etching
Agua regia - IrPt as alloy mixtures - Chemical etching
Agua regia - IrV and Ir80V20 thin films - Chemical etching
Aqua regia - Fe-Ni-Cr heat resistant casting alloys - Etchant for delineating general structure
Aqua regia - Gold - Chemical etching
Aqua regia - Heat resistant alloys - Chemical etching
Aqua regia - Lead sulphide (PbS) - Chemical polishing
Aqua regia - Lead sulphide-selenide (PbS(1-x) x Se(x)) - Chemical etching
Aqua regia - Molybdenum - Chemical etching
Aqua regia - Ni and Ni alloys
Aqua regia - Ni-Cr-Fe alloys (Inconel) - Chemical etching - General microstructure
Agua regia - Mo specimens - Chemical polishing
Agua regia - Ni alloys - General macrostructure
Agua regia - Ni superalloys, Ni-Cr alloys - Chemical etching
Agua regia - Ni-Cr thin films evaporated on (111) and (100) oriented Si - Chemical etching
Aqua regia - Pd thin film - Chemical cleaning
Aqua regia - PdAu deposited as a 11 mixture on glass, quartz, and aapphire substrates - Chemical etching
Aqua regia - Platinum - Chemical etching
Aqua regia - Pt and alloys - Chemical etching
Aqua regia - Pt-Tb alloys (20-35 at.% Tb) - Etch for TbPt3
Aqua regia - Pure Au and alloys
Aqua regia - Pure gold - Chemical etching
Agua regia - Pd-H as powdered "Palladium Black" with absorbed hydrogen
Agua regia - PdAg alloy - Chemical etching
Agua regia - PdNiP, PtNiP, and PtCuP metallic glasses - Chemical etching
Agua regia - Pt and Au evaporated on silicon (111) - Chemical etching
Agua regia - PtRh (2-15%) as thermocouple wires - Chemical cleaning
Agua regia - Pure Au, Au-Pt and Au-Ag alloys with more than0% Au - Chemical etching
Aqua regia - Refactaly steel - Chemical etching - General microstructure
Aqua regia - Rh alloys - Chemical etching
Aqua regia - Rh specimens as wire, rods, sheets, and plated coatings - Chemical etching
Aqua regia - Rhodium - Chemical etching
Aqua regia - Ru specimens - Chemical etching - General microstructure
Agua regia - Rare earth nickelides - Chemical etching
Aqua regia - Se Chemical etching
Aqua regia - Selenium - Chemical etching
Aqua regia - SnGe (1%) thin films - Chemical etching - General microstructure
Aqua regia - Stainless steel - Chemical etching
Aqua regia - Stainless steel - Chemical etching
Aqua regia - Si (111) and (100) wafers - Chemical cleaning
Agua regia - Si3N4, oxynitrides, SiO2 as thin films or glass and quartzware - Chemical cleaning
Agua regia - SiO2 as single crystal natural quartz, artificial quartz, and vitreous silica (fused glass)
Agua regia - Sn (100) single crystal - Chemical etching - General microstructure
Agua regia - Te (10T0) cleaved wafers - Chemical polishing/etching
Agua regia - Th specimen - Chemical polishing
Aqua regia - Ti0.3W0.7Si2 thin films - Chemical polishing
Agua regia - Ti3W7Si2 thin films on silicon wafers, (111), (110) and (100) - Chemical etching - General microstructure
Agua regia - TiO2 single crystal natural rutile crystals - Chemical cleaning
Agua regia - TiW (1% Ti) thin films - Chemical etching - General microstructure
Agua regia - TlBiTe2 single crystal n-type - Chemical polishing/etching
Agua regia - V specimens - Chemical ething
Agua regia - W specimens - Chemical etching - General microstructure
Aqua regia - Wrought heat-resistant steels - Chemical etching
Aqua regia - ZnTe thin film deposits - Chemical etching - General microstructure
Agua regia - Zr specimens - Chemical etching - General microstructure
Agua regia - a-Zr2Pd thin films - Chemical polishing/etching
Agua regia - a-Zr3Rh amorphous thin films - Chemical polishing/etching
Agua regia, dilute - Pd thin films - Chemical cleaning
Agua regia, modified - Ni specimens - Chemical etching
Aqua regia plus acetic acid etchant - Ferritic stainless steels - Chemical etching
Aqua regia, dilute - Alloy steels - General macrostructure
Aqua regia, dilute - Austenitic stainless steels - Chemical etching
Aqua regia, dilute - High speed steels - General microstructure
Aqua regia, dilute - Pb-Te-Co system - Lead telluride-Cobalt section
Aqua regia, modified - GaP (111) wafers - Chemical etching
Alcoholic ferric chloride etchant - Cu and Cu alloys
Aldridge's etchant - Chemical etching
Alexander's etchant - Chemical etching
Alkaline sodium picrate etchant - Chemical etching
Alkaline sodium picrate etchant - High carbon steels - Electrolytic etching
Alkaline sodium picrate etchant - Tool steels - Chemical etching
Alkaline sodium picrate etchant - Tool steels - Electrolytic etching
Alkaline sodium picrate etchant - Tool steels - Electrolytic etching
Alkaline sodium picrate etchant - Tool steels - Electrolytic etching
Alkaline sodium picrate etchant - W-Co eutectic alloys - Chemical etching
Allen's etchant - InSb (111) wafers - Chemical polishing
Amberg's etchant - High speed steels - Chemical etching
Amberg's etchant - Martensitic stainless steels - Chemical etching
Ambler and Slattery's etchant - UO2 - Chemical etching
Ambler and Slattery's etchant - Uranium - Electrolytic etching
Ambler's etchant - Zr3Al alloys - Chemical etching
Ambler's etchant - Zr3Al-based alloys - Chemical etching
Amine Gallate etching of silicon wafers I - Chemical etching
Ammonium persulphate etchant - Steels - Chemical etching
Amyl nital - Iron and steels - Chemical etching
Amyl nital etchant - Steels - etching
Anderson's etchant - For etching pure Mn and lean alloys - Chemical etching
Anderson's etchant - Manganese - Chemical etching
B etchant - For Ti
B etchant - Silicon - Chemical etching
BCK-111 etchant - InP (100) wafers - Chemical etching
BF3 etchant - Si single crystal spheres - Chemical ecthing
BHF etchant - NxSiO2 thin films - Chemical etching - General microstructure
BHF etchant - Si (100), p-type, 2 Ohm cm resistivity wafers - Chemical etching
BHF etchant - Si thin film epitaxy grown on (100) silicon wafer substrates
BHF etchant - Si3N4 thin film amorphous deposits - Chemical etching
BHF etchant - Si3N4 thin films RF plasma grown on silicon - Chemical etching
BHF etchant - Si3N4 thin films deposited on (100) silicon wafers - Chemical cleaning
BHF etchant - SiO2 thin films thermally evaporated - Chemical etching
BHF etchant - Ta (111) and (100) wafers - Chemical etching
BHF etchant - TiN thin films - Chemical etching - General microstructure
BHF etchant - TiN thin films deposited on poly-Si epitaxy layers - Chemical etching - General microstructure
BHF etchant - Zr specimens used for electroplating
BHF etchant, modified - Si3N4 and Si3NxOy thin films - Chemical etching
BHF etchant, modified - Si3N4 thin films - Chemical etching
BJ etchant - Ge (111) wafers - Chemical polishing
BPK-221 etchant - InP (100) wafers - Chemical etching
BRM etchant - InP (100) n-type wafers - Chemical polishing
BRM etchant - WS2 single crystal specimens - Chemical polishing
BRM etchant - WSe2 single crystal specimens - Chemical polishing
BRM etchant - p-GaSb (111) wafers - Chemical etching
BSG as borosilicate glass on silicon - Metal diffusion
BSG etchant - SiO22 as a BSG glassy layer on silicon - Chemical etching
Bain-Vilella's etchant - Steel specimens - To reveal the prexisting austenite grain boundaries and tempered steels
Baker's etchant - Pure Al, Al-Zn, Al-Mn, Al-Mg-Si, Al-Zn-Mg and Al-Mn-Mg alloys - Electrolytic etching
Barber's etchant - NaCl (100) wafers - Chemical etching
Barker's anodizing solution for grain structure - Al and Al alloys - Chemical etching
Barker's etchant - 1000 series aluminium
Barker's etchant - Aluminium alloys - 1xxx, 3xxx, 5xxx, 6xxx series alloys, most casting alloy
Baumann print - Sulfur print, unalloyed steels, sulfide inclusions
Beaujard and Tordeux's tint etchant - Tint etchant for steels
Beaujard and Tordeux`s tint etchant - Reveals grain boundaries and ferrite orientations
Beaujard's tint etchant - Tint etchant for steels
Beaujard's tint etchant - Tint etchant for steels
Bechet and Beaujard's etchant - Martensitic and bainitic steels - Chemical etching
Beck's solution - Aluminium
Beck's solution - Aluminium - Dislocation etching
Beraha's E etchant - Ni superalloys
Beraha's I etchant - Unalloyed and low alloy steels
Beraha's II etchant - Austenitic CrNi steels - Chemical etching - General microstructure
Beraha's II etchant - High-alloy steels
Beraha's III I etchant - Ni-base alloys, Hastelloy X, Hastelloy
Beraha's III etchant - Ni base casting alloys - Chemical etching
Beraha's III etchant - Ni-base alloys with more thanMo, Hastelloy X, Hastelloy C - Chemical etching
Beraha's III etchant - Ni-base and Co-base alloys
Beraha's cadmium sulfide tint etchant - For Fe, steel, and ferritic and martensitic stainless steel - Chemical etching
Beraha's etchant - Al and Al alloys - Chemical etching
Beraha's etchant - Cu alloys, cast irons, ferritic and martensitic stainless steels
Beraha's etchant - Iron, steels, cast irons - Tint etchant for pure iron and carbon steels, cast iron, and alloyed steels
Beraha's etchant - Martensitic chromium steels - Tint etching
Beraha's etchant - Martensitic chromium steels - Tint etching
Beraha's etchant - Steels specimen - Sulfides are colored yelow and matrix dark
Beraha's lead sulfide tint etchant - Iron and steels - Chemical etching
Beraha's martensite etchant - Color etching for ADI iron
Beraha's selenic acid etchant for copper - General microstructure
Beraha's selenic acid etchant for steels and superalloys - General microstructure
Beraha's sodium molybdate etchant - For steels - General microstructure
Beraha's tint etchant - For Al alloys - Chemical etching - General microstructure
Beraha's tint etchant - Al and Al alloys - Tint etching
Beraha's tint etchant - Austenitic stainless steels, maraging steels, PH gredes
Beraha's tint etchant - Brass and Cu-Be alloys - Tint etching
Beraha's tint etchant - Cast Ti alloys - Tint etching
Beraha's tint etchant - Co-based alloys - Tint etching
Beraha's tint etchant - Cu and Cu alloys - Tint etching
Beraha's tint etchant - Cu, brass, bronze alloys - Tint etching
Beraha's tint etchant - Ferritic and martensitic stainless steels, Mn steels, tool steels
Beraha's tint etchant - For cast irons, steels, tool steels, Mn steels, and ferritic and martensitic stainless steels - Chemical etching
Beraha's tint etchant - For ferrite - Chemical etching
Beraha's tint etchant - For irons, steels, tool steels - General microstructure
Beraha's tint etchant - For pearlitic steels and and cast irons - Chemical etching
Beraha's tint etchant - For stainless steels
Beraha's tint etchant - For stainless steels
Beraha's tint etchant - Ni superalloys - Tint etching
Beraha's tint etchant - Ni-base alloys
Beraha`s lead sulfide tint etchant - Chemical etching - General macrostructure
Beraha`s tint etchant - For iron and steels - General microstructure
Beraha`s tint etchant - For stainless steels - General microstructure
Beraha`s tint etchant - For Fe, Ni, or Co base heat resistant alloys
Beraha`s tint etchant - For cast iron and steels - General microstructure
Beraha`s tint etchant - For stainless steels - General microstructure
Bichromate finish dip etchant - Brass (70Cu-30Zn), bronze, and copper parts - Chemical etching
Billig's etchant - For Ge, Si
Bish's etchant - For iron and steels - General macrostructure
Blackburn and William's solution - A286 stainless steel - Standard and modified
Blackburn and William's solution - Ti-Mo alloy - Alloy with 11.6% Mo
Blackburn and William's solution - Ti-Mo-Al-Sn-Zr alloy - Titanium 6246-6Al-2Sn-4Zr-6 Mo
Blackburn and Williams's solution - Ti-Mo alloys
Blackburn-William's electrolyte - Ti-Al-Nb alloy - Ti3Al-Nb
Boss's etchant - Al and Al alloys - Chemical etching
Bossert's etchant - Al and Al alloys - Chemical etching
Bright dip etchant - Brass, bronze, and copper alloy
Bright-field etchant for U - Electrolytic etching
Brilliant's etchant - Cu and Cu alloys
Brilliant's etchant - Cu and Cu alloys - Chemical etching
Brite dip etchant - Aluminium and alloys
Bromine etchant - As (111) specimens - Dislocation etching
CP4 etchant - LiF - Dislocation etching
CP4 etchant - Antimonium - Dislocation etching
CP4 etchant - For Si, Ge, Sb, TiC, InSb, InAs
CP4 etchant - InSb (111) wafers - Chemical polishing
CP4 etchant - LiF (10O) cleaved wafers - Dislocation etching
CP4 etchant - Si wafers - Chemical etching - General microstructure
CP4 etchant - Si-Ge single crystal ingots - Chemical etching
CP4 etchant - Silicon - Chemical polishing
CP4 etchant - Te (0001) cleaved wafers - Chemical etching - General microstructure
CP4 etchant - ZnO thin film deposit - ZnO thin film deposit formed by oxidation of ZnSe
CP4 etchant, modified - InAs (111) wafers used in a polarity study - Chemical etching
CP4 etchant, modified - Silicon specimens - Chemical etching
CP4 etchants, dilute CP4, modified - Ge (111), (100), (110), and (211) wafers - Chemical etching
CP4, variety CP4A etchant - InSb (111) wafers and other orientation - Chemical polishing
CP4A etchant - FeGe2 (100) and (110) wafers - Chemical etching
CP4A etchant - InSb (111) wafers - Chemical etching - General microstructure
CP4A etchant - Si (111) wafers and other orientations - Chemical polishing
CP4A or CP8 etchants - Silicon - Final chemical polishing
Cain's B etchant - For Hf
Cain's etchant - Hf, Zr and allloys - Chemical etching
Cain's etchant - Hf-W eutectoid alloys - Chemical etching
Camp No. 2 (Superoxol) etchant - Si (111) n-type wafers and p-doped with 60Co - Chemical etching
Camp No. 2 (Superoxol, CP2) etchant - Ge (111) wafers - Chemical etching
Camp No. 3 (CP3) etchant - Ge (111) wafers - Chemical etching
Camp No. 4 (CP4) etchant - Ge (100) wafers and other orientations - Chemical polishing/etching
Camp No. (CP8) etchant - Si (111) wafers - Chemical etching
Canada's etchant - Nickel superalloy 718 - Chemical etching - General microstructure
Canfield's etchant - For iron and steels - General macrostructure
Carapella's etchant - Fe-Ni, Ni-Cu, and Ag alloys, Ni-base superalloys, Monel metal
Carapella's etchant - Ni and Ni-Cu (Monel) alloys - Chemical etching
Caro's etch, modified - Si (111) p-type wafers used for diffusion of antimony from glass
Caro's etchant - GaAs (100) n-type wafers grown by LEC as ingots - Chemical etching
Caro's etchant - Si (111) wafers and other orientations - Chemical cleaning
Caro's etchant, modified - Si (111) wafers used in a study of ion bombardment cleaning - Chemical polishing
Carpella's etchant - Ni-B alloys - Chemical etching - General microstructure
Carpenter special #4 etchant - AerMet 310/340, AerMet 100 steels - Chemical etching
Carpenter special #5 etchant - Co-Ni alloys - Chemical etching
Caustic etchant - Al and Al alloys - General macrostructure
Chase's etchant - Ag-30% Zn alloy - Chemical polishing
Chen-Hendrickson's etchant - For Ag
Chrome etchant - Au thin films and specimens - Chemical etching
Chrome etchant - Au-Cr thin films - Chemical etching
Chrome etchant - Cr thin films - Chemical etching
Chrome etchant - Cr2O3 amorphous thin films - Chemical etching
Chrome etchant - For Cr thin films
Chrome etchants, modified - Cr thin film deposits on glass substrates
Chrome regia etchant - Fe + 15-30 Cr + 6-40 Ni + <5%
Chrome regia etchant - Si wafers both float zone ingot material and epitaxy thin film deposit
Chrome regia etchant - Si3N4 oxynitrides and SiO2 thin films - Chemical cleaning
Chrome regia etchant - Stainless steels - Chemical etching
Coates's etchant - Pb-Sn-Te alloys
Coates's etchant - Pb-Sn-Te alloys (Pb(1-x)Sn(x)Te, x <= 0.03) - Chemical polishing and etching
Comstock's etchant - For iron and steels - General macrostructure
Contrast etchant - Ni-Al alloys
Cook's etchant - NaCl (100) wafers - Chemical etching
Coon's electrolytic etchant - Bi alloy and 5% Sb
Copper britte dip etchant - Cu specimens and parts - Chemical polishing
Copper dislocation etchant - Si single crystal wafers of different orientations - Chemical etching
Copper etchant - Si (111) wafers and other orientations - Chemical etching
Corke and Amelincky's electropolish solution - Cu-Pt alloy - Electrolytic etch
Crowell's etchant - Ag-Sn-Zn-Cu alloys, Cu-Sn-Ag dental alloys
Crowell's etchant - Ag-Sn-Zn-Cu dental amalgam alloys - Chemical etching
Crowell's etchant - Cu-Sn-Ag dental alloys - Chemical etching
Crowell's etchant - Cu-Sn-Ag dental alloys - Chemical etching - General microstructure
Curan's etchant - Stainless steels - Chemical etching
Czochralski's - Antimony specimens - Grain contrast etch
Czochralski's etchant - Antimony - Chemical etching
Czochralski's etchant - Sb alloys
DE-100 etchant - SiO2 thin films deposited by Silox system method on (100) silicon and GaAs-Cr (SI) wafers - Ionized gas etching
Dash etchant - Sb (0001) specimen
Dash etchant - Sb (0001) specimen cleaved in LN2
Dash etchant - Sb (0001) specimen cleaved in LN2
Dash etchant - Sb (OOO1) specimen
Dash etchant, modified - Sb (0001) specimen cleaved in LN2
Dash etchant, modified - Sb (0001) specimen cleaved in LN2
Dash's copper decoration etchant - Si (111) wafers - Metal difusion
Dash's etchant - Si (111) wafers and other orientations, both n- and p-type of different resistivity levels
Dash's etchant, modified - Si (100), (111), (110) and (112) wafers
Dash's etchant, modified - Si (111) wafers - Chemical etching
DeSy's etchant - For iron and steels - General macrostructure
Dickenson's etchant - Fe-As alloys - For alloys with 0.6 - 4.6 at.% As - General microstructure
Dickenson's etchant - For cast steels
Dickenson's etchant - For iron and steels - General macrostructure
Dix and Keller etchant - Al, Al-Cu alloys, Al-Si alloys - Chemical etching
Dix-Keller's etchant - Foamed Al, Al alloys, Al-Zr-Ti alloys
Dix-Keller's etchant - For most Al types and alloys except for Al alloys with high Si content, Al foils - Chemical etching
Dix-Keller's etchant - Pure Al and Al alloys
Doped ZnO-ZnO-0.5 mole % each of Bi2O3, CaO, MnO, SnO2
Dow's etchant
DuPont Nb etchant - Nb-Hf and Nb alloys - Chemical etching
Dual phase steel etchants - Chemical etching - General microstructure
E etchant - Ni superalloys
E etchant - Zn (0001) wafers - Chemical etching
EAg1 etchant - CdTe (100), (111) and (110) wafers - Chemical etching
EAg2 etchant - CdTe (100), (111), and (110) wafers - Chemical etching
EDTA etchant - CaCO3 r(1011) cleaved wafers - Acid cleaning
EDTA etchant - Li-alumina-silica glass - Li2O x Al2O3 x SiO2
EI-IR etchant - Steels for high temperatures
EPW etchant - Si (111) and (100), p-type 1 - 10 Ohm cm and n-type wafers - Chemical etching
Ellis's No. 1 etchant - Ge spheres and hemispheres - Chemical etching
Ellis's No. 5 etchant - Ge spheres and hemispheres - Chemical etching
Ellis's No. 7 etchant - Ge spheres and hemispheres - Ge spheres and hemispheres
Emanuel's etchant - Cast steels - Chemical etching
Emanuel's etchant - Fe-Ni-Cr heat resistant casting alloy - Attacks sigma phase with little or no effect on carbide particles
Ence and Margolin's etching solution (H-etch) - Ti alloys - Electrolytic etching
Erhard's etchant - Si (111) wafers - Dislocation etching
Etch pits etchant - Nickel oxide (NiO)
Etch pits etchant - Selenium
Etchant No. 2 - InSb (100) and (110) wafers - Chemical etching
Evans etchant - Inconel 617 - Chemical etching
F (Fast) etchant - Silicon - Chemical etching
F etchant - LiF - Dislocation etching
Ferric cyanide etchant - Ge hemispheres - Chemical etching
Finlay's A etchant (Remington's A etchant) - For Ti and Ti/Zr
Finlays B etchant - For Ti
Fisher-Marcinkowski's electropolish solution
Flat's etchant - Ni-Ti alloys
Flick's etchant - Al, cast alloys
Flick's etchant - Aluminium - Pure Al, Cu-Al alloys - General macrostructure
Flick's etchant - Aluminium and its alloys - For 2xxx Al alloys, high Cu aloys
Flick's etchant - Pure Al and Al alloys
Flick’s etchant - 2XXX, high Cu alloys - Chemical etching - General macrostructure
Flinn's etchant - For iron and steels - General macrostructure
Flint glass - Etching for revealing recrystallization effects
Fluor regia - Silicon - Chemical etching
Fluor regia etchant - Cr and Cr alloy - Chemical etching
Fluor regia etchant - Nb and alloys - Chemical etching
Fluor regia, modified - Beryllium - Chemical etching
Franchini's color etchant - Al-Si-Cu-Ni cast alloys - Chemical etching
Frank's etchant - Fe + 16-25 Cr + 3-6 Ni + 5-1C
Frey's etchant - Flow lines in low carbon N2 steels, convertor steels - Chemical etching - General microstructure
Fry's No. 1 etchant - For iron and steels - General macrostructure
Fry's No. 2 etchant - For iron and steels - General macrostructure - General macrostructure
Fry's No. 4 etchant - For iron and steels - General macrostructure
Fry's etchant (1) - Flow lines in low carbon N2 steels, Thomas steels
Fry's etchant (2)
Fry's etchant - Fe pure metal samples - Chemical etching
Fry's etchant - Fe-Si specimens and other iron alloys - Chemical etching
Fry's etchant - Iron - Dislocation etching
Fry's etchant - Iron and steel specimens - Mild steel specimens, Bessemer and high N2 steel specimens
Fry's etchant - Iron and steels - Chemical etching
Fry's etchant - Iron, steel specimens, cast irons - Flow lines in low carbon N2 steel specimens
Fry's etchant - Iron, steels, cast irons - Normalized steels
Fry's etchant - Ni-Ge alloys - Chemical etching - General microstructure
Fry's etchant - Ni-Pd-Ga alloys - Chemical etching - General microstructure
Fry's etchant - Ni-Pt-Ga alloys - Chemical etching
Fry's etchant - Nimonic alloys - Nimonic alloys PE7, PE11, and PE16, Nimonic Pk 31
Fry's etchant - Stainless steels - Chemical etching
Fry's etchant - Wrought stainless steels - General structure
Fry's etchant, modified - Fe, mild steel - Dislocation etching
Fry's etchant, modified - Iron and steel specimens - Plain and alloy steel specimens
Fry’s etchant - Steels
Fuss's etchant - Wrought aluminium alloy - Chemical etching
G etchant - For Fe/Ni
G etchant - Steels for high temperatures
GE Turbo-chrome etchant - Martensitic stainless steel and high-alloy steels - Chemical etching
GE Turbo-chrome etchant - P91 (X10CrMoV91) steel - Chemical etching
GE Turbo-chrome etchant - Stainless steels - Chemical etching
Gilman's etchant - Zinc - Chemical polishing and etching
Gilman's etchant I - For Cd
Gilman's etchant II - For Zn
Giometto and Capella's etchant - Martensitic chromium steels - Chemical etching
Glyceregia (1) - Austenitic stainless steels
Glyceregia (2) - Fe + 15-30 Cr + 6-40 Ni + <5%
Glyceregia - Austenitic stainless steels - Chemical etching
Glyceregia - Cr and Cr alloys - Chemical etching
Glyceregia - Fe-Ni-Cr heat resistant casting alloys - Etchant for delineating general structure
Glyceregia - High alloy steels, austenitic Mn steels, stainless steels - Chemical etching
Glyceregia - Ni superalloys and Ni-Cr alloys - Chemical etching
Glyceregia - Steel and SST vacuum system parts - Chemical cleaning
Glyceregia - Wrought stainless steels - General structure
Glyceregia etchant - Stainless steel castings - General structure
Glycol - Mg and alloys - Chemical etching
Goeren's amyl picral - Iron and steels - Chemical etching
Gorsuch's etchant - Pure iron
Graff and Sargent's etchant - 2XXX, 3XXX, 6XXX, 7XXX Al alloys - Chemical etching
Grard's No. 1 etchant - Cu alloys
Gray cast irons - Color etchant - General microstructure
Green's contrast etchant - Fe + 15-30 Cr + 6-40 Ni + <5%
Griffis and Spretnak's etchant - For iron and steels - General macrostructure
Groesbeck etchant - Alloys with Cr and or Co
Groesbeck's etchant - High alloy steels and castings - Chemical etching - General microstructure
Groesbeck's etchant - High-alloy steels, cast steels
Groesbeck's etchant - Iron and steels - Chemical etching
Groesbeck's etchant - Stainless steels - Chemical etching
Groesbeck's etchant - Stainless steels - Color etchant - General microstructure
H etchant - Ti alloys
H100 etchant - InSb (111) wafers - Chemical etching
Hasson's etchant - For Mo - General microstructure
Hasson's etchant - Molybdenum, color etchant - Chemical etching - General microstructure
Hasson's etchant - Pure Mo
Heppenstall etchant - Ni-based superalloys - General macrostructure
Heppenstall's etchant - Inconel 625 alloy - Chemical etching - General microstructure
Heyn's etchant - For iron and steels - General macrostructure
Heyn's etchant - Iron, steel specimens, cast irons - Phosphorus segregation in low carbon steel specimens
Heyn's etchant - Low-carbon steels
Heyn's etchant - Steel specimens and cast iron - To reveal phosphorus segregations
Hone and Pearson's anodizing solution - Pure Al - Chemical etching
Hone and Pearson's anodizing solution - Pure Al - Chemical etching
Hordon's etchant - Al-Cu alloy - Alloy with 7.5 at.% Al
Howarth's etchant - Carbon and alloy steels - For detection of overheating and burning
Howarth's etchant - Carbon and alloy steels with medium carbon content - Detection of overheating and burning
Howarth's etchant - Fe + <1C + <4% additions
Huber and Linh's H etchant - For etch pits on InP
Hume-Rothery's etchant - Al-Si alloys
Humfrey's etchant - For iron and steels - General macrostructure
Humphrey’s etchant - Cast steels
Hydal's etchant - For InBiSn
Hypo etchant - AgCl (100) oriented material - Chemical etching
Iodate etchant- PbTe (100) wafers - Chemical etching
Iodine A etchant - Ba2TiO3 (111) and (100) wafers, single crystals - Chemical etching
Iodine etchant - Si (111) wafers, boron doped - Chemical etching
Jacquet's etchant - Al, single crystal
Jacquet's etchant - Aluminium - Etching for etch pits
Jacquet's solution - For Al - Electrolytic polishing
Jewitt-Wise's etchant - Ni specimens - Chemical etching
Jin's etchant - For iron and steels - General macrostructure
Jodid (high-purity, iodide-process) Ti - Chemical etching - General macrostructure
Jong's color etchant - OFHC copper - Tint etching
KKI etchant - InP (100) wafers - Chemical etching
Kalling's 1 etchant - Martensitic stainless steels
Kalling's 1 etchant - Martensitic, stainless steels - Chemical etching - General microstructure
Kalling's 2 etchant - Ni-Cu alloys and Ni-base superalloys - Chemical etching
Kalling's 2 etchant - Stainless steel castings - General structure
Kalling's 2 etchant - Stainless steels - Chemical etching
Kalling's 2 etchant - Stainless steels - Chemical etching - General microstructure
Kalling's 2 etchant - Stainless steels, Ni-Cu alloys, Ni-base superalloys
Kalling's I etchant - Stainless steels - Chemical etching
Kalling's etchant - Cr stainless steels - Chemical etching
Kalling's etchant - Ho2Fe17 and Ho2Co14Fe3 specimens - Chemical etching
Kalling's etchant - Nickel specimens T.D. grade - Chemical etching
Kalling's etchant - SST 400 series - Chemical etching
Kalling's etchant - UCe2 specimen - Chemical polishing
Kalling's etchant - UCo2 specimen - Chemical polishing
Kalling's etchant - UNi2 specimen - Chemical polishing
Kalling's etchant - UPt3 specimen - Chemical polishing
Kalling's etchant - Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - General structure
Kalling's etchant - Wrought heat-resistant steels
Kalling's etchant - Y2(CoM)17 single crystal ingots - Chemical polishing
Kallings 2 etchant - Ni-Cu alloys and superalloys - Chemical etching
Kallings's etchant - Wrought stainless steels - General structure
Kallings's etchant - Wrought stainless steels - General structure
Keller and Geisler's anodizing solution - Al and Al alloys - Chemical etching
Keller' etchant, modified - Ni-Cr-Th alloy - Ni-20Cr-2ThO2
Keller's etchant - Al and Al alloys - Chemical etching
Keller's etchant - Al-Cu-Ag-Mg-Ti alloy - 4.7% Cu, 0.6% Ag, 0.3% Mg, 0.3% Al, 0.2% Ti
Keller's etchant - Al-Cu-Ti alloy - Alloy with 4% Cu, and 0.1% Ti
Keller's etchant - Al-Ni system - Al-Al3Ni eutectic
Keller's etchant - Al-Si alloys - Chemical etching
Keller's etchant - Al-Zn-Mg alloy
Keller's etchant - Al-Zn-Mg alloy - Chemical etching - General microstructure
Keller's etchant - Al-Zn-Mg-Cu alloy - 7075 alloy 5-3% Zn, 2-7% Mg, 1.6 Cu
Keller's etchant - Al-Zn-Mg-Cu alloys (+Cr, Ti) - Chemical etching
Keller's etchant - Aluminium (99.945%) - Dislocation etching
Keller's etchant - Aluminium - General microstructure
Keller's etchant - Deep-etching of Al-Si - For most aluminum and aluminum alloys
Keller's etchant - Determining grain structure in A356 aluminum
Keller's etchant - RE-Al alloys - Chemical etching - General microstructure
Keller's etchant - Sleeve bearing materials (Pb, Al)-Pb-Sn-Cu overlay on Al-Cd alloy
Keller's etchant - Ti alloys - Chemical etching
Keller's etchant - Ti alloys - Chemical etching - General microstructure
Keller's etchant - Ti, Ti-Al alloys - Dislocation etching
Keller's etchant - Ti-6% Al-4% V alloy, Ti-5% Al-2.75% Cr-1.25% Fe alloy, Ti-2.55% Al-3.75% Mn alloy - General macrostructure
Keller's etchant - Ti-Al-Mn, Ti-Al-V, and Ti-Al-Cr-Fe alloys, flow lines - Chemical etching
Keller's etchant 1 - Pure Al and Al alloys, Ti alloys, RE-Al alloys
Keller's etchant 2 - For Al and Al alloys
Keller's etchant, conc. - Al-Cu-Si alloys
Keller's etchant, concentrated - and Al alloys
Keller's etchant, diluted - Aluminium 7075, 7475 alloy - Al-5.1/5.7 Zn-2.1/2.3 Mg-1.5 Cu-0.2 Cr
Keller's etchant, modified - Al and Al alloys - Chemical etching
Keller's etchant, modified - Al and Al alloys - Chemical etching
Keller's etchant, modified - Al and Al alloys - Chemical etching
Keller's etchant, modified - Aluminium alloys - Alloy 7075, recrystalliyed
Keller’s etchant - Al and Al alloys - Chemical etching
Klemm's I etchant - Alpha and beta brass - Tint etching
Klemm's I etchant - Iron and steels - Chemical etching
Klemm's I etchant - Iron and steels - Chemical etching
Klemm's I etchant - Pure Zn and low-alloy Zn - Chemical etching
Klemm's I etchant - Tint etchant for steels
Klemm's I etchant - Zn and lean alloys - Chemical etching
Klemm's I tint etchant - Brass, bronze
Klemm's II etchant - Alpha brass - Tint etching
Klemm's II etchant - Tin - Chemical etching
Klemm's II etchant - Tint etchant for steels
Klemm's II tint etchant - Steels, alpha brass, tin alloys
Klemm's III etchant - Bronze alloys - Tint etching
Klemm's III etchant - Ni alloys - Tint etching
Klemm's III tint etchant - General microstructure
Klemm's etchant
Klemm's etchant - Iron, steel specimens, cast irons - Phosphorus distribution in cast steel specimens and cast iron
Klemm's etchant - Temper embrittlement in steels - Chemical etching
Klemm's etchant I - Etches segregations in unalloyed and low alloy steels - Chemical etching - General microstructure
Klemm's etchant I - Unalloyed and low-alloy steels, cast irons, Mn steels, pure Zn and low-alloy Zn
Klemm's etchant II - Cu and Cu alloys and soft solders
Klemm's etchant II - Cu and Cu alloys with soft solders - Chemical etching - General microstructure
Klemm's etchant III - Pure Cu and Cu alloys
Klemm's etchant III - Pure Cu, leaded bronze, bronzes, alpha/beta brasses, Al bronze, Be bronze - Chemical etching - General microstructure
Kodak's EB-5 etchant - Cr thin films - Chemical etching
Kroll's etchant - For most Ti materials, especially for Ti-Al-V-(Sn) alloys - Chemical etching
Kroll's etchant - Suited especially for Al-Cu alloys - Chemical etching
Kroll's etchant - Ti alloys - Chemical etching
Kroll's etchant - Ti and alloy - Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si
Kroll's etchant - Ti-Al-Mo alloy - 5.8-9.7% Al, 0.5-8.2% Mo
Kroll's etchant - Ti-Al-O alloy - Ti-6-10% Al-0.04-0.12% O
Kroll's etchant - Ti-Al-V alloy (6Al-4V) - Chemical etching - General microstructure
Kroll's etchant - Ti-Mo alloy - Ti-26Mo
Kroll's etchant - Ti-Mo-V-Al-Fe alloy - Ti-8Mn-8V-3Al-2Fe - General microstructure
Kroll's etchant - Ti-Mo-Zr-Sn alloy - Ti-11Mo-6.6Zr-4.6Sn
Kroll's etchant - Ti-Ni alloys - Chemical etching
Kroll's etchant - Ti-V-Cr-Zr-Mo-Al alloy - Ti-8V-6Cr-4Zr-4Mo-3Al
Kroll's etchant - Titanium - For many Ti raw materials, especially for Ti-Al-V alloys
Kroll's etchant - Titanium and titanium alloy
Kroll's etchant - Titanium and titanium alloys - General purpose etch - For most titanium alloys
Kroll's etchant 1 - Al-Cu alloys, Ti alloys, mainly Ti-Al-V (Sn) alloys
Kroll's etchant 2 - For Ti/Al
Krumm's etchant - Al thin films evaporated on GaAs, (100) wafer substrates
LBH etchant, modified - Steels - Chemical etching
LaPera's etchant - For steels
LaPera's etchant - Low alloy dual-phase and TRIP steels - Chemical etching
LaPera's etchant - TRIP steel - Chemical etching
Lacombe and Beaujard's etchant - Al and Al alloys - Chemical etching
Landyren's etchant - Si (111) wafers and other orientations - Chemical etching
LeChatelier's No. 1 etchant - For iron and steels - General macrostructure
LeChatelier's No. 2 etchant - For iron and steels - General macrostructure
Lenoir's etchant - Al-Zn-Mg alloy
Lenoir's etchant, modified - Cu-Al-Mn alloy - Alloys with 3-4% Cu, 0.5 Mn
Lenoir's solution - Ag-Al alloy - Alloy with 5% Ag
Lenoir's solution - Al-Zn-Mg alloy - Alloy with 6.86 wt.% Zn, 2.5 wt.% Mg
Lenoir's solution - For Al and U
Lenoir's solution - Nimonic PE16 alloy
Lenoir's solution, modified - Ag-Al-Cd alloy - 4.8 at.% Ag, 0.15 at.% Cd
Lenoir's solution, modified - Ag-Al-Cu alloy - 4.8 at.% Ag, 0.2 at.% Cu
Lenoir's solution, modified - Al-Cu alloy - Alloys with 1-5% Cu
Lenoir's solution, modified - Al-Cu-Mg alloy - Alloys with 1-5% Cu, 0.5-1.5% Mg
Lepito's No. 1 etchant - Austenitic stainless steels, Ni-based alloys - General macrostructure
Lepito's No. I etchant - Ni alloys - General macrostructure
Lepito's No. II etchant - Ni-Cr-Fe alloys - General macrostructure
Lepito's etchant
Lepito's etchant - General microstructure
Lepito's etchant - Ni and its alloys - Alloys containing Cr, Fe and other elements - Etchant for nickel welds
Lepito's etchant - Stainless and high temperature ateel specimens - Austenitic stainless steel specimens and Ni base alloys
Lepito's etchant - Stainless steel
Lepito’s etchant I - Austenitic stainless steels and nickel base alloys - Chemical etching
Lepito’s etchant II - Alloys containing Cr, Fe, and other elements II - Chemical etching
Levenstein-Robinson's etchant (and (Hen-Hen) Rickson's modification) - For Ag
Levenstein-Robinson's etchant - Silver single crystal - Chemical polishing and etching
Levinstein and Robinson's etchant - Silver - Chemical polishing
Livingstone's etchant - Al-Cu alloys - Electrolytic polishing and chemical etching
Livingstone's etchant - Chemical etching - General microstructure
Livingstone's etchant - For Al/Cu
Livingstone's etchant, Young's etchant - Copper single crystal - Etching for etch pits
Livingstone's solution - For Ni - Electrolytic polishing
M (Medium) etchant - Silicon - Chemical etching
Malette's etchant - Iron and steels - Chemical etching
Marble's etchant - Austenitic and high-temperature-resistant steels, Co superalloys
Marble's etchant - Austenitic stainless steels - General macrostructure
Marble's etchant - Co high-temeprature alloys - Chemical etching
Marble's etchant - Co superalloys - Chemical etching - General microstructure
Marble's etchant - Co-Cr-Mo-Si alloy - Tribaloy 400, Tribaloy00
Marble's etchant - Co-Mo-Si alloy - 55Co-35Mo-10Si
Marble's etchant - Etchant of M-type ferrites - Chemical etching
Marble's etchant - Fe-Ni and Fe-Co magnetic alloys - Chemical etching
Marble's etchant - Fe-Ni and Fe-Co magnetic alloys - Grain size
Marble's etchant - For iron-nickel and cobalt-base superalloys
Marble's etchant - Hard facing alloys - Chemical etching - General microstructure
Marble's etchant - In-Ni eutectoid (30% Ni) - Chemical ecthing
Marble's etchant - Iron and steel specimens - Austenitic stainless steel specimens
Marble's etchant - Ni and its alloys - Nickel - For grain structure
Marble's etchant - Ni, Ni-Cu and Ni-Fe alloys and superalloys - Chemical etching
Marble's etchant - Ni-Cr alloys - Chemical etching - General microstructure
Marble's etchant - Ni-Cr-Th alloy - Etch for TD Ni-Cr
Marble's etchant - Ni-Mo-Cr-Si alloy - 50Ni-31Mo-15Cr-3Si
Marble's etchant - Nickel - Attack polishing
Marble's etchant - Nickel - General macrostructure
Marble's etchant - Nickel superalloy 718 - Chemical etching - General microstructure
Marble's etchant - Nickel superalloys - Production of thin foils for electron microscopy
Marble's etchant - Stainless and high temperature Steel specimens - Austenitic stainless steel specimens and high temperature alloys
Marble's etchant - Stainless steels - Chemical etching
Marble's etchant - Stainless steels - General etchant - General microstructure
Marble's etchant - Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - Good for contrast
Marble's etchant, modified - For Ni-Nb alloys
Marble's etchant, modified - Ni alloys - General macrostructure
Marble's etchant, modified - Ni and its alloys - Alloys containing Cr, Fe and other elements
Marble's etchant, modified - Stainless steels - Chemical etching
Marble’s etchant - Austenitic stainless steels and high-temperature alloys - Chemical etching
Marble’s etchant - Nickel - Chemical etching - General macrostructure
Marshall's etchant -9.999% pure iron - For etching of all grain boundaries
Marshall's etchant - Galvannealed sample - Chemical etching
Marshall's etchant - Iron and steels - Chemical etching
Marshall's solution - Fe specimens - Chemical polishing
Marts and Capes's etchant - For iron and steels - General macrostructure
Matte's dip etchant - Cu and Cu alloy parts
Methanolic aqua regia - Austenitic stainless steels - Chemical etching
Meyer and Eichholz's No. 1 etchant - For iron and steels - General macrostructure
Meyer and Eichholz's No. 2 etchant - For etching nitrided layer in steel
Meyer and Eichholz's No. 2 etchant - For iron and steels - General macrostructure
Meyer and Eichholz's No. 2 etchant - Nitrided DIN 1.8550(34CrAlNi7) steel specimens - Macro etching for segregation
Modification of Lacombe and Beaujard's etchant - Aluminium (HP) - Dislocation etching
Moly's etchant - Mo discs - Chemical cleaning
Moran's etchant - NaCl (100) wafers, NaCl single crystal whiskers - Chemical etching
Morris's electrolytic polishing solution - Dislocation etching
Morris's electrolytic polishing solution - Fe-3% Si alloy - Dislocation etching
Murakami's etchant - W and W alloys - Chemical etching
Murakami's etchant - Alumina (Al2O3) - Aluminia with additives
Murakami's etchant - Cast irons - 30% chromium irons
Murakami's etchant - Cast irons - High phosphorus irons
Murakami's etchant - Co-Cr-Mo-Ni-Fe-Si-C-Mn-Al-Ti alloy
Murakami's etchant - Co-Cr-Ni alloys - For identification of sigma phase
Murakami's etchant - Co-Sn0Sb alloys - For carbides
Murakami's etchant - Copper-Tungsten (Cu-W) - Electric contact material
Murakami's etchant - Cr and Cr alloys - Chemical etching
Murakami's etchant - Fe-Ni-Cr heat resistant casting alloys - Etchant for staining or film forming
Murakami's etchant - Gold-Plated Nickel-Iron (Au-Ni-Fe) - Electric contact material
Murakami's etchant - Iron - Selective carbides
Murakami's etchant - Iron and steels - Chemical etching
Murakami's etchant - Martensitic chromium steels - Chemical etching
Murakami's etchant - Mo and alloys - Chemical etching
Murakami's etchant - Mo specimens - Chemical etching
Murakami's etchant - Mo-C alloys - Chemical etching
Murakami's etchant - Mo-C alloys - Chemical etching
Murakami's etchant - Molybdenum - Chemical etching
Murakami's etchant - Molybdenum - Electric contact material
Murakami's etchant - Molybdenum-Silver (Mo-Ag) - Electric contact material
Murakami's etchant - Ni-Cu alloys and superalloys - Chemical etching
Murakami's etchant - Rhenium - Chemical etching
Murakami's etchant - Rhenium - Chemical etching
Murakami's etchant - Sb telluride - Chemical etching
Murakami's etchant - SiC alloy with 1% B4C - Chemical etching
Murakami's etchant - Silicon carbide (SiC) - For SiSiC
Murakami's etchant - Silver - Molybdenum (Ag-Mo) - Electric contact material
Murakami's etchant - Silver-Tungsten (Ag-W) - Electric contact material
Murakami's etchant - Silver-Tungsten carbide (Ag-WC) - Electric contact material
Murakami's etchant - Sn-Cd-Sb alloys - Chemical etching
Murakami's etchant - Stainless steel castings - General structure
Murakami's etchant - Stainless steel castings - General structure
Murakami's etchant - Stainless steels - Chemical etching
Murakami's etchant - Stainless steels - Color etchant - General microstructure
Murakami's etchant - Steels and other alloys
Murakami's etchant - Ta-Mo alloys - Chemical etching
Murakami's etchant - TiC coated steel - Chemical etching
Murakami's etchant - Tungsten - Electric contact material
Murakami's etchant - Tungsten - Mo, W and their alloys
Murakami's etchant - Tungsten-Copper (W-Cu) - Electric contact material
Murakami's etchant - Tungsten-Nickel (W-Ni) - Electric contact material
Murakami's etchant - Tungsten-rhenium-thoria system (O-Re-Th-W)-W - 3% Re-2% ThO2
Murakami's etchant - U-Zr alloys - Chemical etching
Murakami's etchant - U-Zr alloys, U-Fe-Co alloys, U-Al2-U3Si3 alloys - Chemical etching
Murakami's etchant - V and V-O alloys - Chemical etching
Murakami's etchant - Vanadium specimens - Chemical etching
Murakami's etchant - Vanadium-nitrogen system (V-N) - Electrolyticlytic and chemical polishing
Murakami's etchant - W-Hf alloys (< 3% Hf) - Chemical etching
Murakami's etchant - W-Hf-N alloys alloy - < 3% Hf, nitrided
Murakami's etchant - W-Hf-Re alloys - Chemical etching
Murakami's etchant - W-Hf-Re-N alloys alloy - < 2% Hf, < 25% Re, nitrided
Murakami's etchant - W-Mo-Hf-Re alloy - < 20% Mo, < 2% Hf, < 30% Re
Murakami's etchant - W-Mo-Hf-Re-N alloy - < 20% Mo, < 2% Hf, < 30% Re, nitrided
Murakami's etchant - WC specimens - Chemical cleaning
Murakami's etchant - WC-Co, Eta phase appears multicolored; Co is white, WC-TiC-TaC-Co, WC-NbC-Co
Murakami's etchant - Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718, carbide particles
Murakami's etchant - Wrought stainless steels - General structure, sigma phase
Murakami's etchant, boiling - Aluminium nitride (AlN) - Chemical etching - General microstructure
Murakami's etchant, boiling - SiC-AlN specimens - SiC-10/80% AlN
Murakami's etchant, modified (Klemm) - Al-Si aloys - Chemical etching
Murakami's etchant, modified - AlN-Al2O3 - Chemical etching - General microstructure
Murakami's etchant, modified - Aluminium nitride (AlN) - AlN with Al2O3 - General microstructure
Murakami's etchant, modified - Iron and steels - Chemical etching
Murakami's etchant, modified - Molybdenum - Mo, W and their alloys
Murakami's etchant, modified - Silicon carbide (SiC) - For RSiC - Reveals alpha/beta grain boundaries
Murakami's etchant, modified - Silicon carbide (SiC) - For alpha-SiC - Reveals alpha/alpha and alpha/beta grain boundaries
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Ti-V-Mo alloys - Chemical etching
Murakami's etchant, modified - Tungsten - Mo, W and their alloys
Murakami's etchant, modified - W and lean alloys - Chemical etching
Murakmi's etchant - Austenitic and ferritic-Austenitic stainless steels - Chemical etching
Murkami's etchant - Steel specimens - Carbide etching
Murkami's etchant - TiC specimens - Chemical cleaning
Nital (0.5-10%) - Yb-Zn system - Chemical etching
Nital (1%) - Co-Ce-Fe alloy - Co5CeFe02
Nital (1%) - Co-Dy-Mn alloy - Co5DyMn0.2 - General microstructure
Nital (1%) - Co-Dy-Ni alloy - Co5DyNi0.2 - General microstructure
Nital (1%) - Co-Dy-Pb alloy - Co5DyPb0.2 - General microstructure
Nital (1%) - Co-Dy-Pd alloy - Co5DyPd0.2 - General microstructure
Nital (1%) - Co-Dy-Pt alloy - Co5DyPt0.2- General microstructure
Nital (1%) - Co-Dy-Si alloy - Co5DySi0.2- General microstructure
Nital (1%) - Co-Er alloys - Chemical etching - General microstructure
Nital (1%) - Co-Er-Fe alloy - Co5ErFe0.2- General microstructure
Nital (1%) - Co-Fe-Y alloy - Y-Co(1-x)-Fe(x)- General microstructure
Nital (1%) - Co-Gd-Fe alloy - Co5GdFe0.2 - General microstructure
Nital (1%) - Co-Ho system - Approx. HoCo5
Nital (1%) - Co-Ho-Fe alloy - Co5HoFe0.2 - General microstructure
Nital (1%) - Co-La-Fe alloy - Co5LaFe0.2 - General microstructure
Nital (1%) - Co-Lu alloy - Approx. LuCo5
Nital (1%) - Co-Nd-Fe alloy - Co5NdFe0.2 - General microstructure
Nital (1%) - Co-Pr-Fe alloy - Co5PrFe0.2 - General microstructure
Nital (1%) - Co-Sm-Al alloy - Co5SmAl0.2 - General microstructure
Nital (1%) - Co-Sm-Fe alloy - Co5SmFe0.2 - General microstructure
Nital (1%) - Co-Tb alloy - Approx. TbCo5
Nital (1%) - Co-Tb-Al alloy - Co5TbAl0.2 - General microstructure
Nital (1%) - Co-Tb-Fe alloy - Co5TbFe0.2 - General microstructure
Nital (1%) - Co-Tm alloy - Approx. Co5Tm
Nital (1%) - Co-Yb alloy - Aprox. YbCo5
Nital (1%) - Fe-Ni-Co alloy - Iron rich alloys
Nital (1%) - La-Cd alloys - Chemical etching
Nital (1%) - La-Ni alloys - Chemical etching
Nital (1%) - Mn-C alloys - Chemical etching
Nital (10%) - Magnesium - Chemical polishing
Nital (10%) - Nickel superalloy 718 - Electrolytic etching - General microstructure
Nital (10%) - Steels
Nital (2%) - Ce-Zn alloys - Chemical etching
Nital (2%) - Fe-Mo-Co alloy - Chemical etching
Nital (2%) - Mg-Li alloys - Chemical etching
Nital (2-10%) - Pr-Zn alloys - Chemical etching
Nital (3/4%) - Y-Mn alloys - Chemical etching
Nital - AISI 4340 annealed steel - Chemical etching - General microstructure
Nital - Carbon and alloy steels - Develops ferrite grain boundaries in low carbon steels
Nital - Carbon and alloy steels with medium carbon content - General structure (most used etchant for routine work)
Nital - Cast irons - Used to reveal macrostructure in white irons
Nital - Cd-Sc alloy - Alloy with 3% Sc
Nital - Co-Ce-Al alloy - Ce(1-x) Al (x) Co5, 0< x < 0.6
Nital - Co-Pr-Al alloy - Co5Pr(x)Al(1-x) - General microstructure
Nital - Dual-phase steel
Nital - Fe pure metal samples - Chemical etching
Nital - Fe-Ni (5%)-O (15%) specimens - Chemical etching
Nital - Iron and steels - Chemical etching
Nital - Iron, steels, cast irons - Most common etchant - General microstructure
Nital - Mg and alloys - Chemical etching
Nital - Permanent magnet materials - Rare earth (Co3Cu1.6Fe0.5Ce)
Nital - Pure Gd, RE-Co alloys, grain bounday etchant - Chemical ecthing
Nital - Pure iron, carbon steels, low-alloy steels, and gray cast irons and other alloys
Nital - Steel, carbon type - Chemical etching - General microstructure
Nital - Wrought Fe-Ni-Cr heat resisting alloys - Incoloy00, general structure; grain boundaries
Nital - Wrought Fe-Ni-Cr heat resisting alloys - Incoloy25, general structure; grain boundaries
Nital - Zn-Cd alloys - Chemical etching - General microstructure
Nital - Zn-Sn alloy - Zn-Sn alloys processed in a study of solidification in lamellar eutectic systems
Nital 1% - CaCO3 - Dislocation etching
Nital 1% - Co-Dy alloy - DyCo5 alloy
Nital 2% - Cast irons - Observation of ferrite grains boundaries at higher magnification
Nital etch procedures - Low alloy steels - Chemical etching
Nitrosulfuric (Wesley Austin's) etchant - Iron and steels - Chemical etching
Nitrosulfuric acid etchant - Fe and most steels - General microstructure
Noren's etchant - Steel weld - Chemical etching
Oberhoffer's etchant - For iron and steels - General macrostructure
Oberhoffer's etchant - For macro etching of steel specimens
Oberhoffer's etchant - Iron, steel specimens, cast irons - Blowhole segregation, primary structure, fiber orientation
Oberhoffer's etchant - Steel specimens and cast irons - Etching to reveal sgregations
Oberhoffer's etchant - Unalloyed and low-alloy steels
Osmond's etchant - Fe and most steels - General macrostructure
Oxygen sensing etchant for steels - This etchants is claimed as good for detection of oxygen penetration into steels
P etchant - SiO2 thin films deposited on (100) silicon wafers - Chemical etching
P-1 etchant - Zn (0001) wafers - Chemical etching
P-2 etchant - Zn (0001) wafers and cylinders - Chemical etching
P-3 etchant - Zn (0001) wafers and cylinders - Chemical etching
P-ED (EPW) etchant - Si (100) wafers within +/-1° of the plane - Chemical etching
P-Etchant - Chemical etching
PBr etchant - CdTe (111), (100), and (110) wafers - Chemical etching
Palmerton's etchant - Pure Zn and alloys - Chemical etching
Palmerton's etchant - Zinc specimens - Chemical etching
Palmerton's etchant - Zn alloys (with Cu) - General macrostructure
Palmerton's etchant 1 - Cu-containing Zn alloys
Palmerton's etchant 2 - Pure Zn and Zn alloys
Palmerton's etchant, modified - All Zn alloys, for pressure die-casting, Zn coatings - Chemical etching
Palmerton's etchant, modified - Zn die-casting alloys - Chemical etching
Palmerton's etchant, modified - Zn-Cu alloys - Chemical etching
Panseri's etchant - Al and Al alloys - Chemical etching
Pelleg's electrolytic polishing solution - Niobium - Dislocation etching
Phillip's anodizing solution - Pure Al and Al-Mg alloys - Chemical etching
Phoschromic etchant - Fe superalloys - Electrolytic etching
Phospho-picral etchant - Mg and alloys - Chemical etching
Picklesimer's anodizing solution - Nb and alloys - Electrolytic etching
Picklesimer's anodizing solution - Ta and alloys - Electrolytic etching
Picklesimer's anodizing solution - U alloys - Electrolytic etching
Picklesimer's anodizing solution - Zr and alloys - Electrolytic etching
Picklesimer's solution - For Zr, Nb/Sn, Nb/Ti
Picklesimer's solution - Nb-Ti alloy - Anodising
Picklesimer's solution - Nb-Ti alloys
Pickling's anodizing solution - Brass, bronze, and copper alloys - Chemical cleaning
Picral (4%) etchant - Cast irons - Used to reveal macrostructure in white irons
Picral etchant - Carbon and alloy steels - For general structure
Picral etchant - Carbon and alloy steels with medium carbon content - General structure
Picral etchant - Cast iron - General microstructure
Picral etchant - Cast irons - General purpose etching of all pearlitic gray, melleable and ductile cast irons
Picral etchant - Fe, single crystal iron whiskers - Dislocation etching
Picral etchant - Fe-Cr alloys - Chemical etching - General microstructure
Picral etchant - Iron and steels - Chemical etching
Picral etchant - Iron, steels, cast irons - Generally used for iron and heat treated steels
Picral etchant - Pure iron, carbon steels, low-alloy steels, and cast iron
Picral etchant - Steels - Chemical etching - General microstructure
Picral etchant - Steels, high carbon and high alloy types - Chemical etching - General microstructure
Picral etchant - Tin and tin alloys - For etching tin-coated steel and tin-coated cast iron
Polisar's etchant - For etch pits on CdTe, CdHgTe, HgTe
Pondo's etchant - Copper
Pondo's etchant - Cu and Cu alloys - Chemical etching
Pondo's etchant - Cu-Sn alloys - Chemical etching - General microstructure
Pondo's etchant - For Cu alloys
Poulton's etchant - 6005, 6063 and 6061 Al-Mg-Si alloys - Chemical and electrolytic etching
Poulton's etchant - Al alloys - General macrostructure
Poulton's etchant - Aluminium alloys - High purity Al, commercial purity Al, Al-Mn alloys, Al-Si alloys, Al-Mg alloys, Al-Mg-Si alloys
Poulton's etchant - High purity Al, commercial purity Al, Al-Mn alloys, Al-Si alloys
Precision No. 1 etchant - Ni alloys - Chemical etching
Precision No. 2 etchant - Ni alloys - Chemical etching
R etchant - For Ti/Al, Ti/Zr
R or A etchant - Ti-Zr alloys - Chemical etching
R-etchant - Ti-Al and Ti-Al-Zr alloys - Chemical etching
R.C. etchant
R.R.E. etchant - For InP, InPAs, GeInPAs
RC-1 etchant - GaAs (111) wafers - Dislocation etching
RCA etchant (AB) - SiO2 alpha-quartz frequency crystals - Chemical cleaning
RCA etchant - Si wafers of all major plane orientations - Chemical cleaning
RIE etchant - TiW thin films - Ionized gas etching
Ralph’s etchant - Stainless steel - Chemical etching
Reinhardt's etchant - Fe and most steels - General macrostructure
Remington A etchant - Ti alloys - Chemical etching
Remington B etchant - Titanium - Chemical etching
Remington's A etchant (Finlay's A etchant) - For Ti alloys
Retained austenite etchant I - Steels - Chemical etching
Retained austenite etchant II - Steels - Chemical etching
Retained austenite etchant III - Steels - Chemical etching
Retained austenite etchant IV - Steels - Chemical etching
Retained austenite in the steels V
Richard-Crocker's RC etchant - Gallium phosphide (GaP) - Chemical polishing
Richard-Crocker's etchant
Rolls Royce's etchant - Stainless steel - Chemical etching
Roman's etchant - Er, Dy, Gd, Ho, La - Chemical polishing
Roman's etchant - For R.E. alloys
Roman's etchant - Pr-Au alloy - Chemical etching - General microstructure
Roman's etchant - Pr-Ba alloys - Chemical etching - General microstructure
Roman's etchant - Pr-Bi alloys - Chemical etching - General microstructure
Roman's etchant - Pr-Cs alloys - Chemical etching - General microstructure
Roman's etchant - Pr-Hf alloys - Chemical etching - General microstructure
Roman's etchant - Pr-Hg alloys - Chemical etching - General microstructure
Roman's etchant - Pr-Ir alloy
Roman's etchant - Pr-Ir alloy - Chemical etching
Roman's etchant - Pr-Pt alloys - Chemical etching
Roman's etchant - Pr-Re alloys - Chemical etching
Roman's etchant - Pr-Ta alloys - Chemical etching
Roman's etchant - Pr-Tl alloys - Chemical etching
Roman's etchant - Pr-W alloys - Chemical etching
Romans's etchant - Praseodymium-lead alloys (Pr-Pb) - Chemical etching
Romans's etchant - Praseodymium-osmium alloys (Pr-Os) - Chemical etching
Rosenhain and Haighton's etchant - For iron and steels - General macrostructure
Rosenhain's etchant - Co-Sn alloys - Chemical etching
Rowland's etchant - Etchants for galvannealed steels
Russell's etchant - Pb-Sb alloys - General macrostructure
Russell’s etchant - Pb and Pb alloys
SR4 etchant - Ge (111) wafers - Chemical polishing/etching
SR4 etchant - Si (111) wafers used in a study of the variations in surface conductivity of silicon and Germanium
SSA etchant - GaAs wafers - Electrolytic etching
Scale dip etchant - Cu and Cu alloys - Chemical cleaning
Schell's etchant
Schell's etchant - GaAs (111) wafers - Chemical etching
Schimmel's etch technique - Chemical etching
Schimmel's etchant
Schimmel's etchant - Si (111) and (100) wafers used as substrates for silicon epitaxy growth - Chemical etching
Schimmel's etchant - Silicon - Chemical etching
Schrader's etchant - For iron and steels - General macrostructure
Schrader's modification of Vilella's etchant - High alloy steels - Chemical etching
Schramm's etchant - Zn-Cu, Zn-Fe, Zn-Mg, Zn-Ni, and Zn-Pb alloys
Schumann's etchant
Schumann's etchant - Fe-Mn alloys - Chemical etching - General microstructure
Schumann's etchant - Mn-Ti-Fe system - Fe-19-27% Mn - up to 1.45% Ti - General microstructure
Scimmel's etchant - Silicon - Defects in epi layers on <100> silicon
Secco's etchant - Dislocation etching
Secco's etchant - For etch pits on Si (100)
Secco's etchant - Si (111) and (100), p-type, 1-10,000 Ohm cm resistivity wafers - Chemical etching
Seeco's etchant - SiO2 thin films grown on silicon, (100), n-type substrates - Chemical etching
Sirtl's etchant - Dislocation etching
Sirtl's etchant - For Ge
Sirtl's etchant - Si (111) wafers and other orientations - Chemical etching
Sirtl's etchant - SiC (0001) wafers - Chemical polishing
Sirtl's etchant - Silicon
Sirtl's etchant - Silicon specimens - Chemical etching - General microstructure
Sirtl's etchant, modified - Si (111), (110) and (211) wafers, ingots - Chemical etching
Sopori's etchant - Si (111) wafers and other orientations - Chemical etching
Stead No. 1 etchant - For iron and steels - General macrostructure
Stead's No. I etchant - For P in steel
Stead's No. I etchant - Steel specimens and cast irons - The etching solutions reveals phosphorus segregations
Stead's No. II etchant - For P in steel
Stead's No. II etchant - For iron and steels - General macrostructure
Stead's No. II etchant - Steel specimens and cast irons - To reveal phosphorus segregations and cell structures in cast iron
Stead's etchant - Iron and steel specimens - Plain and alloy steel specimens
Stead's etchant - Used to reveal the eutectic cell number in gray cast irons
Stead’s etchant - Steels
Struer's D-2 etchant - Copper and copper alloys - Electrolytic etching
Struers A2 electrolyte - Al and Al alloys - Electrolytic polishing
Struers electrolyte A2 - For Al, Fe, Ni, Ag, stainless steel, steel, Sn, Ti - Dislocation etching
Struers electrolyte A2-I - For Al, Fe, Ni, Ag, stainless steel, steel, Sn, Ti - Dislocation etching
Struers electrolyte A2-II - For Al, Fe, Ni, Ag, stainless steel, steel, Sn, Ti - Dislocation etching
Struers electrolyte A3-I - Martensitic steel, Mo, stainless steel, Ti, V, Zr - Dislocation etching
Struers electrolyte A3-II - Martensitic steel, Mo, stainless steel, Ti, V, Zr - Dislocation etching
Struers electrolyte A8-I - Cr, Hf, Ni, Ti - Dislocation etching
Struers electrolyte A8-II - Cr, Hf, Ni, Ti - Dislocation etching
Struers electrolyte AC2-I - Cast iron, Mg, Ni, stainless steel, steels - Dislocation etching
Struers electrolyte AC2-II - Cast iron, Mg, Ni, stainless steel, steels - Dislocation etching
Struers electrolyte AC2-III - Cast iron, Mg, Ni, stainless steel, steels - Dislocation etching
Struers electrolyte D2 - Brass, Cu, Au - Dislocation etching
Struers electrolyte E5-I - Brass, bronze, carbon steel, cast iron - Dislocation etching
Struers electrolyte E5-II - Brass, bronze, carbon steel, cast iron - Dislocation etching
Struers electrolyte E5-III - Brass, bronze, carbon steel, cast iron - Dislocation etching
Sulfide etchant of Kunkele - Iron and steels - Chemical etching
Sulphur printing - Steels
Super picral - Carbon and alloy steels with medium carbon content - General structure
Super picral - Iron and steels - Chemical etching
Super picral - Steels - Chemical etching
Superoxal etchant - Germanium - Etch pits etching
Superoxol - InP (100) Zn doped p-type wafers - Chemical polishing
Superoxol No. 2 etchant - Ge hemispheres - Chemical etching
Superoxol No. 2 etchant, dilute - Ge hemispheres - Chemical etching
Superoxol etchant - Antimonium - Dislocation etching
Superoxol etchant - For Ge - Chemical etching
Superoxol etchant - Ge (111) wafers - Chemical etching
Superoxol etchant - Ge (111) wafers lithium diffused - Chemical etching
Superoxol etchant - Ge specimens - Chemical etching
Superoxol etchant - Germanium - Dislocation etching
Superoxol etchant - InAs (111) wafers - Chemical etching
Superoxol etchant - InSb (111) wafers - Chemical etching
Superoxol etchant, modified - Germanium - Chemical etching - General microstructure
Superoxol etchant, varity - Ge hemispheres - Chemical etching
Taff's etchant - For Sn-Bi
Taff's etchant - Pure Sn and Sn-Bi alloys - Chemical etching
Taff's etchant - Sn-Bi alloy (12% Bi) - Chemical etching - General microstructure
Taub's etchant - For iron and steels - General macrostructure
Tri-iodide etchant - Au specimens and thin films - Chemical etching
Tri-iodine etchant - Au thin film deposits as a multilayer Au/Ni/Au/TiW/Si(100) substrate - Chemical etching
Tri-iodine etchant - AuGe (13%) alloy ribbon - Chemical etching
Tucker's etchant - 5052 Al alloy - Chemical etching - General microstructure
Tucker's etchant - Al and Al alloys
Tucker's etchant - Aluminium alloys - Commercial-purity alloys 1xxx series, Al-Mn alloys, Al-Si alloys, Al-Mg-Si alloys
Tucker's etchant - Aluminium and its alloys - For Al alloys except high Si castings
Tucker's etchant - Aluminium and its alloys - For high purity Al, 1xxx, 3xxx, 4xxx, 5xxx, 6 xxx Al alloys
Tucker's etchant - Determining grain structure in A356 aluminum
Tucker's etchant I - Pure Al, Mn-Al, Si-Al, Mg-Al, Mg-Si-Al alloys
Tucker's etchant II - For Al alloys
Tucker's etchant, dilute - Al alloys (except high Si-castings)
Tucker's etchant, modified - Al-3% Ag alloy, Al alloys
Tucker’s etchant - Al and Al alloys - Chemical etching
Tucker’s etchant - High purity A1, 1XXX, 3XXX, 4XXX, 5XXX, 6XXX alloys - Chemical etching
Uddeholm etchant - Fe and most steels - General macrostructure
V2A etchant
Vegesack's etchant - Steel specimens - To reveal lead inclusions
Velguth's etchant - X40 or No. 31 alloys - Chemical etching - General microstructure
Vermilyea's anodizing solution for Ta - Electrolytic etching
Vilella and Beregekoff's etchant - Pb and most Pb alloys - General macrostructure
Vilella and Beregekoff's etchant - Pb-Sn alloys
Vilella etchant - Stainless steel castings - General structure
Vilella's and Beregekoff's etchant - Pb-Sb alloys, grain boundary etchant - Chemical etching
Vilella's etchant - Al and Al alloys - Chemical etching
Vilella's etchant - Carbon and alloy steels - For contrast etching
Vilella's etchant - Carbon and alloy steels with medium carbon content - For austenite grain boundaries
Vilella's etchant - Cast irons - High chromium irons
Vilella's etchant - Cu-Pb alloys - Chemical etching
Vilella's etchant - Duplex stainless steel - Sigma phase
Vilella's etchant - Fe, most steels, stainless steels - General macrostructure
Vilella's etchant - Ferritic Cr steels, austenitic CrNi steels, austenitic cast alloys, Pd and its alloys
Vilella's etchant - High alloy steels
Vilella's etchant - High-alloy steels - General macrostructure
Vilella's etchant - In and lean alloys - Chemical etching
Vilella's etchant - In-Cd alloys - Chemical ecthing
Vilella's etchant - Indium specimens - Chemical etching - General microstructure
Vilella's etchant - Iron and steel specimens - Stainless and high Cr steel specimens
Vilella's etchant - Iron and steels - Chemical etching
Vilella's etchant - Iron and steels - Chemical etching
Vilella's etchant - Nickel superalloys - Production of thin foils for electron microscopy
Vilella's etchant - Pd dental alloys, Pd alloys with Al, Os, In, Sn, Fe, and Cu - Chemical etching
Vilella's etchant - Stainless steels - Chemical etching
Vilella's etchant - Stainless steels - General microstructure
Vilella's etchant - Steels, high carbon and alloys types - Chemical etching
Vilella's etchant - Wrought Fe-Ni-Cr heat resisting alloys - Incoloy25, general structure
Vilella's etchant - Wrought stainless steels - General structure
Vilella's etchant - Zirconium specimens - Chemical etching
Vilella's etchant, modified - N-155 alloy - Chemical etching - General microstructure
Vilella’s etchant - Stainless and high-Cr steels - Chemical etching - General macrostructure
Vitallium alloy - Vitallium is a pure cobalt chromium alloy free of nickel and beryllium
Vitallium alloys - Electrolytic etching - General microstructure
Voce's etchant - Pb-Sb alloys - General macrostructure
Vogel's etchant - Si (111) and other oriented wafers - Dislocation etching
WAg etchant - Ge (111) wafers - Chemical etching
WAg etchant - Ge hemispheres - Chemical etching
Walker's etchant
Walker's etchant - Ni alloys
Walker's etchant - Rene5 alloy
Walker's etchant - Rene5 alloy - Chemical ecthing
Walker's etchant - Rene5 alloy - Chemical etching
Wallner's etchant - Corrosion-resistant CrNi steels
Warekois etchant - ZnTe (111) wafers - Chemical etching
Warke amd McCall's etchant - For iron and steels - General macrostructure
Wassermann's etchant - For Mg-Al
Wassermann's etchant - Mg-7.5% Al-2.5% Zn alloy - Chemical etching
Wassermann's etchant - Mg-Al alloys
Waterbury's etchant
Waterbury's etchant - Silver-Cadmium (Ag-Cd) - Electric contact material
Waterbury's etchant - Silver-Cadmium (Ag-Cd) brazed to brass - Electric contact material
Waterbury's etchant - Silver-Copper (Ag-Cu) - Electric contact material
Waterbury's etchant - Silver-Graphite (Ag-C) - Electric contact material
Waterless Kallings's etchant - Nickel superalloy 718 - Chemical etching - General microstructure
Watertoen Arsenal's etchant - Fe and most steels - General macrostructure
Wazau's etchant - For iron and steels - General macrostructure
Weck's color etchant - Etchant/procedure to examine for overheated titanium - Chemical etching
Weck's etchant - Pure Ti and Ti alloys
Weck's etchant - Pure Ti and Ti alloys - Chemical etching
Weck's tint etch for alpha Ti - Chemical etching - General microstructure
Weck's tint etch for alpha Ti alloys - Chemical etching - General microstructure
Weck's tint etchant - Ti and alloys - Tint etching
Weck's tint etchant - Ti and alloys - Tint etching
Westinghouse W Ag etchant - Ge and Ge alloys - Chemical etching
Westinghouse silver etchant - Germanium - Dislocation etching
Westinghouse silver etchant WAG - Ge
Westinghouse's silver etchant WAG - Germanium - Etch pits etching
White cast irons - Color etchant - General microstructure
White's etchant - Ge (111) wafers - Chemical etching
White's etchant - Si (100) cleaved wafers - Chemical polishing
White's etchant - Si (111) wafers, n- and p-type - Chemical thinning
White's etchant - Si (111) wafers, n-type, 130 Ohm cm resistivity - Chemical sphere polishing
Whiteley's etchant - For iron and steels - General macrostructure
Whiteley's etchant - Method for coloring sulfides - Iron and steels - Chemical etching
Wiliams-Blackburn's etchant - Ti-Mo-Al-Cr alloy - Ti-4.5Al-5Mo-1.5Cr
Williams's solution - For Ti and alloys - Electrolytic polishing
Worner and Worner's etchant - Pb-Sb alloys - General macrostructure
Worner and Worner's etchant - Th
Worner and Worner's etchant - Thallium specimens - Chemical polishing
Wright's etchant - For Si stacking faults dislocations
Wright's etchant - Si (100), (111), p- and n-type, 0.2-20 Ohm cm resistivity wafers - Dislocation etching
Wright-Jenkins etchant - Dislocation etching
Young's etchant - For etch pits on Al
ZIP's etchant - Inconel 617 - Chemical etching
Zeerleder's etchant - Al-Cu-Mg-Ni alloys

Copyright © 2017 by Steel Data. All Rights Reserved.