Ferromanganese, manganese silicate and Mn-Si-Cr alloys - Chemical etching

Material Name: Ferromanganese, manganese silicate and Mn-Si-Cr alloys
Recipe No.: 10747
Primary Chemical Element in Material: Mn
Sample Type: Bulk
Uses: General microstructure
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 90-95 ml distilled water, 5-10 ml HF.
Procedure (Condition): Etch up to a few minutes.
Note: No data
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 660.