Mn-Sn system - Quoted for non-stoichometric Mn-Sn alloys

Material Name: Mn-Sn system
Recipe No.: 4192
Primary Chemical Element in Material: Mn
Sample Type: Bulk
Uses: Chemical polishing
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical polishing
Etchant (Electrolyte) Composition: 1 part 50% hydrofluoric acid, 1 part 30% hydrogen peroxide.
Procedure (Condition): No data
Note: Quoted for non-stoichometric Mn-Sn alloys.
Reference: S.Takevchi, et al., Acta Met., Vol.24, No.4, April 1974, p. 429.