AgInSe2 single crystals - Chemical etching

Material Name: AgInSe2 single crystals
Recipe No.: 8234
Primary Chemical Element in Material: Ag
Sample Type: Single crystal
Uses: Etching
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Wet (chemical) etching
Etchant (Electrolyte) Composition: 1.) x...x % Br2, x...MeOH. 2.) x...HNO3. Note: The volume/quantity was not shown in the referenced article and is therefore designated as an "x".
Procedure (Condition): No data
Note: AgInSe2 single crystals used to evaluate the cohesive energy features of tetrahedral semiconductors. Forty materials were studied.
Reference: Aresti, A et al. - J Phys Chem Solids, 45,361(1984).