Cobalt - Chemical polishing

Material Name: Cobalt
Recipe No.: 9808
Primary Chemical Element in Material: Co
Sample Type: Bulk
Uses: Polishing
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical polishing
Etchant (Electrolyte) Composition: 1 part acetic acid, 1 part HNO3.
Procedure (Condition): No data
Note: Morral
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 554.