Niobium Carbide - NbC

Classification: Carbide
Atomic numbers: 41 & 6
Atomic weight: 104.92
Melting point (C): 2750
Boiling point (C):
Density (g/cm3): 15.77
Refractive index (n=):
Hardness (Mosh-scratch): 9+
Hardness (Vickers-kgf/mm2): 2800
Crystal structure: Hexagonal-normal: (10T0) prism, Isometric-normal: (100) cube
Color (solid): Grey-white
Cleavage: Basal/cubic: (0001)/(001)