Platinum Antimonide - PtSb2

Classification: Antimonide
Atomic numbers: 78 & 51
Atomic weight: 447.6
Melting point (C): >1200
Boiling point (C):
Density (g/cm3):
Refractive index (n=):
Hardness (Mosh-scratch): 6-7
Crystal structure: Isometric-pyritohedral: (100) pyrithohedron
Color (solid): Grey-white metal
Cleavage: Cubic: (001)