Silver Bromide - AgBr

Classification: Bromide
Atomic numbers: 47 & 35
Atomic weight: 187.8
Melting point (C): 434
Boiling point (C): 700
Density (g/cm3): 5.8-6
Refractive index (n=): 2.25
Hardness (Mosh-scratch): 1-1.5
Crystal structure: Isometric-normal: (100) cube
Color (solid): Yellow/greenish
Cleavage: Cubic-perfect: (001)