Tellurium Dioxide - TeO2

Classification: Oxide
Atomic numbers: 52 & 8
Atomic weight: 159.61
Melting point (C): 800
Boiling point (C):
Density (g/cm3): 5.9
Refractive index (n=): 2.0-2.35
Hardness (Mosh-scratch): 2
Crystal structure: Orthorhombic-normal: (100) a-pinacoid
Color (solid): Yellow-white
Cleavage: Pismatic-perfect: (010)