Tin Telluride - SnTe

Classification: Telluride
Atomic numbers: 50 & 52
Atomic weight: 246.31
Melting point (C): 780
Boiling point (C):
Density (g/cm3): 6.47
Refractive index (n=):
Hardness (Mosh-scratch): 6-7
Crystal structure: Hexagonal-normal: (10T0) prism
Color (solid): Grey/black
Cleavage: Basal: (0001)