Titanium Carbide - TiC

Classification: Carbide
Atomic numbers: 22 & 6
Atomic weight: 60
Melting point (C): 3140
Boiling point (C): 4300
Density (g/cm3): 6.5
Refractive index (n=):
Hardness (Mosh-scratch): 9+
Crystal structure: Isometric-normal: (100) cubic
Color (solid): Grey-white
Cleavage: Cubic: (001)