Titanium Nitride - TiN

Classification: Nitride
Atomic numbers: 22 & 7
Atomic weight: 61.9
Melting point (C): 3220
Boiling point (C):
Density (g/cm3): 5.3
Refractive index (n=):
Hardness (Mosh-scratch): 5-7
Crystal structure: Isometric-normal: (100) cube
Color (solid): Bronze-red/gold
Cleavage: Cubic: (001)