Germanium Oxide - Ge2O3

Classification: Oxide
Atomic numbers: 32 & 8
Atomic weight: 104.60
Melting point (C): 1086
Boiling point (C):
Density (g/cm3): 6.24
Refractive index (n=):
Hardness (Mosh-scratch): 6-7
Crystal structure: Tetragonal-normal: (110) prism
Color (solid): Clear/grayish
Cleavage: None