Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTA Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
Wr.Nr. (Mat.No.) Steels
080M46 Steel
1.0037 Steel
1.0045 Steel
1.0461 Steel
1.0481 Steel
1.0482 Steel
1.0482 Steel
1.0501 Steel
1.0501 Steel
1.0503 Steel
1.0503 Steel
1.0505 Steel
1.0528 Steel
1.0528 Steel
1.0535 Steel
1.0535 Steel
1.0540 Steel
1.0562 Steel
1.0601 Steel
1.0601 Steel
1.0603 Steel
1.0605 Steel
1.0614 Steel
1.0615 Steel
1.0615 Steel
1.0915 Steel
1.0987 Steel
1.1106 Steel
1.1127 Steel
1.1132 Steel
1.1133 Steel
1.1140 Steel
1.1144 Steel
1.1157 Steel
1.1157 Steel
1.1160 Steel
1.1165 Steel
1.1165 Steel
1.1167 Steel
1.1170 Steel
1.1172 Steel
1.1172 Steel
1.1174 Steel
1.1174 Steel
1.1178 Steel
1.1178 Steel
1.1179 Steel
1.1179 Steel
1.1180 Steel
1.1180 Steel
1.1181 Steel
1.1181 Steel
1.1183 Steel
1.1183 Steel
1.1191 Steel
1.1191 Steel
1.1191 Steel
1.1192 Steel
1.1192 Steel
1.1193 Steel
1.1193 Steel
1.1194 Steel
1.1194 Steel
1.1199 Steel
1.1201 Steel
1.1201 Steel
1.1203 Steel
1.1203 Steel
1.1204 Steel
1.1204 Steel
1.1206 Steel
1.1209 Steel
1.1209 Steel
1.1211 Steel
1.1211 Steel
1.1217 Steel
1.1219 Steel
1.1219 Steel
1.1219 Steel
1.1221 Steel
1.1221 Steel
1.1223 Steel
1.1223 Steel
1.1231 Steel
1.1237 Steel
1.1237 Steel
1.1237 Steel
1.1240 Steel
1.1241 Steel
1.1248 Steel
1.1248 Steel
1.1248 Steel
1.1249 Steel
1.1249 Steel
1.1249 Steel
1.1251 Steel
1.1251 Steel
1.1251 Steel
1.1253 Steel
1.1253 Steel
1.1253 Steel
1.1269 Steel
1.1269 Steel
1.1273 Steel
1.1520 Steel
1.1520 Steel
1.1520 Steel
1.1520 Steel
1.1525 Steel
1.1545 Steel
1.1620 Steel
1.1620 Steel
1.1620 Steel
1.1625 Steel
1.1645 Steel
1.1730 Steel
1.1730 Steel
1.1740 Steel
1.1740 Steel
1.1744 Steel
1.1750 Steel
1.1820 Steel
1.1820 Steel
1.1830 Steel
1.2002 Steel
1.2002 Steel
1.2003 Steel
1.2003 Steel
1.2004 Steel
1.2056 Steel
1.2056 Steel
1.2057 Steel
1.2058 Steel
1.2058 Steel
1.2063 Steel
1.2067 Steel
1.2067 Steel
1.2067, 1.2601, 1.2080, 1.2379 Steels
1.2080 Steel
1.2080 Steel
1.2080 Steel
1.2082 Steel
1.2083 Steel
1.2083 Steel
1.2083 Steel
1.2085 (~1.2316+S) Steel
1.2086 Steel
1.2101 Steel
1.2103 Steel
1.2103 Steel
1.2109 Steel
1.2109 Steel
1.2127 Steel
1.2162 Steel
1.2162 Steel
1.2208 Steel
1.2210 Steel
1.2210 Steel
1.2210 Steel
1.2241 Steel
1.2242 Steel
1.2242 Steel
1.2243 Steel
1.2249 Steel
1.2304 Steel
1.2311 Steel
1.2311 Steel
1.2311 Steel
1.2311 Steel
1.2311, 1.2738, 1.2738 mod. Steels
1.2312 Steel
1.2312 Steel
1.2312 Steel
1.2313 Steel
1.2316 Steel
1.2316 Steel
1.2316 Steel
1.2316 Steel
1.2322 Steel
1.2323 Steel
1.2323 Steel
1.2323 Steel
1.2327 Steel
1.2334 Steel
1.2341 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 VICTORY ES /EFS Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2345 Steel
1.2345 Steel
1.2347 Steel
1.2347 Steel
1.2358 Steel
1.2358 Steel
1.2360 Steel
1.2361 Steel
1.2362 Steel
1.2363 Steel
1.2363 Steel
1.2363 Steel
1.2365 Steel
1.2365 Steel
1.2365 Steel
1.2365 Steel
1.2365 mod. Steel
1.2365 mod. Steel
1.2367 Steel
1.2367 Steel
1.2367 Steel
1.2378 Steel
1.2378 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2380 Steel
1.2381 Steel
1.2390 Steel
1.2414 Steel
1.2419 Steel
1.2419 Steel
1.2436 Steel
1.2436 Steel
1.2510 Steel
1.2510 Steel
1.2516 Steel
1.2516 Steel
1.2541 Steel
1.2541 Steel
1.2542 Steel
1.2542 Steel
1.2542 Steel
1.2550 Steel
1.2550 Steel
1.2550 Steel
1.2550 Steel
1.2550 Steel
1.2552 Steel
1.2564 Steel
1.2564 Steel
1.2567 Steel
1.2567 Steel
1.2581 Steel
1.2581 Steel
1.2581 Steel
1.2601 Steel
1.2601 Steel
1.2603 Steel
1.2603 Steel
1.2603 Steel
1.2606 Steel
1.2606 Steel
1.2606 Steel
1.2622 Steel
1.2622 Steel
1.2622 Steel
1.2631 Steel
1.2662 Steel
1.2662 Steel
1.2678 Steel
1.2705 Steel
1.2709 Steel
1.2710 Steel
1.2711 Steel
1.2713 Steel
1.2713 Steel
1.2714 Steel
1.2714 Steel
1.2714 Steel
1.2714 Steel
1.2714 Steel
1.2718 Steel
1.2721 Steel
1.2721 Steel
1.2721 Steel
1.2726 Steel
1.2738 Steel
1.2738 Steel
1.2738TS Steel
1.2740 Steel
1.2743 Steel
1.2743 Steel
1.2744 Steel
1.2744 Steel
1.2745 Steel
1.2746 Steel
1.2762 Steel
1.2764 Steel
1.2764 Steel
1.2765 Steel
1.2766 Steel
1.2766 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2770 Steel
1.2787 Steel
1.2787 Steel
1.2790 Steel
1.2791 Steel
1.2823 Steel
1.2826 Steel
1.2826 Steel
1.2833 Steel
1.2834 Steel
1.2838 Steel
1.2838 Steel
1.2842 Steel
1.2842 Steel
1.2842 Steel
1.2880 Steel
1.2880 Steel
1.2885 Steel
1.2885 Steel
1.2888 Steel
1.3202 Steel
1.3207 Steel
1.3207 Steel
1.3243 Steel
1.3243 Steel
1.3247 Steel
1.3247 Steel
1.3247 Steel
1.3255 Steel
1.3265 Steel
1.3302 Steel
1.3333 Steel
1.3333 Steel
1.3333 Steel
1.3343 Steel
1.3343 Steel
1.3343 Steel
1.3343 Steel
1.3345 Steel
1.3346 Steel
1.3348 Steel
1.3355 Steel
1.3501 Steel
1.3503 Steel
1.3505 Steel
1.3505 Steel
1.3505 Steel
1.3514 Steel
1.3514 Steel
1.3520 Steel
1.3520 Steel
1.3521 Steel
1.3521 Steel
1.3523 Steel
1.3523 Steel
1.3531 Steel
1.3531 Steel
1.3533 Steel
1.3533 Steel
1.3536 Steel
1.3536 Steel
1.3541 Steel
1.3551 Steel
1.3553 Steel
1.3554 Steel
1.3561 Steel
1.3563 Steel
1.3563 Steel
1.3565 Steel
1.3565 Steel
1.4000 Steel
1.4000 Steel
1.4000 Steel
1.4003 Steel
1.4003 Steel
1.4005 Steel
1.4005 Steel
1.4005 Steel
1.4005 Steel
1.4006 Steel
1.4016 Steel
1.4016 Steel
1.4016 Steel
1.4021 Steel
1.4021 Steel
1.4021 Steel
1.4021 Steel
1.4021 Steel
1.4024 Steel
1.4024 Steel
1.4028 Steel
1.4029 Steel
1.4031 Steel
1.4034 Steel
1.4034 Steel
1.4034 Steel
1.4037 Steel
1.4057 Steel
1.4057 Steel
1.4057 Steel
1.4057 Steel
1.4104 Steel
1.4104 Steel
1.4104 Steel
1.4106 Steel
1.4108 Steel
1.4108 Steel
1.4112 Steel
1.4113 Steel
1.4120 Steel
1.4122 Steel
1.4122 Steel
1.4122 Steel
1.4122 Steel
1.4125 Steel
1.4125 Steel
1.4310 Steel
1.4313 Steel
1.4418 Steel
1.4418 Steel
1.4460 Steel
1.4460 Steel
1.4462 Steel
1.4462 Steel
1.4535 Steel
1.4704 Steel
1.4713 Steel
1.4713 Steel
1.4718 Steel
1.4718 Steel
1.4731 Steel
1.4747 Steel
1.4748 Steel
1.4903 Steel
1.4913 Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 Steel
1.4914 with 10% Cr Steel
1.4914 with 11% Cr Steel
1.4914 with 12% Cr Steel
1.4914 with 13% Cr Steel
1.4914 with 14% Cr Steel
1.4914 with 9% Cr Steel
1.4920 Steel
1.4921 Steel
1.4921 Steel
1.4922 Steel
1.4922 Steel
1.4923 Steel
1.4923 Steel
1.4926 Steel
1.4926 Steel
1.4935 Steel
1.4935 Steel
1.4935 Steel
1.4970 Steel
1.5024 Steel
1.5026 Steel
1.5028 Steel
1.5029 Steel
1.5029 Steel
1.5120 Steel
1.5121 Steel
1.5122 Steel
1.5122 Steel
1.5141 Steel
1.5223 Steel
1.5223 Steel
1.5231 Steel
1.5232 Steel
1.5232 Steel
1.5233 Steel
1.5402 Steel
1.5403 Steel
1.5404 Steel
1.5404 Steel
1.5404 Steel
1.5406 Steel
1.5415 Steel
1.5415 Steel
1.5415 Steel
1.5419 Steel
1.5423 Steel
1.5510 Steel
1.5523 Steel
1.5523 Steel
1.5523 Steel
1.5525 Steel
1.5525 Steel
1.5527 Steel
1.5531 Steel
1.5532 Steel
1.5622 Steel
1.5633 Steel
1.5637 Steel
1.5639 Steel
1.5662 Steel
1.5662 Steel
1.5680 Steel
1.5680 Steel
1.5680 Steel
1.5710 Steel
1.5710 Steel
1.5710 Steel
1.5710 Steel
1.5713 Steel
1.5713 Steel
1.5732 Steel
1.5732 Steel
1.5732 Steel
1.5736 Steel
1.5737 Steel
1.5737 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5755 Steel
1.5755 Steel
1.5805 Steel
1.5805 Steel
1.5807 Steel
1.5807 Steel
1.5808 Steel
1.5808 Steel
1.5815 Steel
1.5815 Steel
1.5860 Steel
1.5860 Steel
1.5860 Steel
1.5864 Steel
1.5864 Steel
1.5918 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5920 Steel
1.5920 Steel
1.5920 Steel
1.5924 Steel
1.5924 Steel
1.5934 Steel
1.5934 Steel
1.6210 Steel
1.6211 Steel
1.6213 Steel
1.6217 Steel
1.6310 Steel
1.6310 Steel
1.6310 Steel
1.6311 Steel
1.6347 Steel
1.6349 Steel
1.6359 Steel
1.6368 Steel
1.6368 Steel
1.6368 Steel
1.6511 Steel
1.6511 Steel
1.6511 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6526 Steel
1.6541 Steel
1.6545 Steel
1.6545 Steel
1.6546 Steel
1.6546 Steel
1.6546 Steel
1.6562 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6582 Steel
1.6582 Steel
1.6582 Steel
1.6587 Steel
1.6587 Steel
1.6587 Steel
1.6604 Steel
1.6604 Steel
1.6738 Steel
1.6738 Steel
1.6742 Steel
1.6746 Steel
1.6749 Steel
1.6751 Steel
1.6751 Steel
1.6753 Steel
1.6757 Steel
1.6780 Steel
1.6782 Steel
1.6926 Steel
1.6926 Steel
1.6926 Steel
1.6946 Steel
1.6946 Steel
1.6949 Steel
1.6956 Steel
1.6957 Steel
1.6959 Steel
1.6959 Steel
1.6985 Steel
1.6985 Steel
1.7003 Steel
1.7005 Steel
1.7006 Steel
1.7014 Steel
1.7015 Steel
1.7015 Steel
1.7016 Steel
1.7023 Steel
1.7025 Steel
1.7033 Steel
1.7033 Steel
1.7034 Steel
1.7034 Steel
1.7035 Steel
1.7035 Steel
1.7037 Steel
1.7037 Steel
1.7038 Steel
1.7038 Steel
1.7039 Steel
1.7039 Steel
1.7045 Steel
1.7045 Steel
1.7108 Steel
1.7131 Steel
1.7131 Steel
1.7131 Steel
1.7138 Steel
1.7139 Steel
1.7139 Steel
1.7147 Steel
1.7147 Steel
1.7149 Steel
1.7149 Steel
1.7160 Steel
1.7168 Steel
1.7176 Steel
1.7182 Steel
1.7214 Steel
1.7214 Steel
1.7218 Steel
1.7218 Steel
1.7218 Steel
1.7218 Steel
1.7219 Steel
1.7219 Steel
1.7220 Steel
1.7220 Steel
1.7223 Steel
1.7223 Steel
1.7225 Steel
1.7225 Steel
1.7225 Steel
1.7226 Steel
1.7226 Steel
1.7227 Steel
1.7227 Steel
1.7228 Steel
1.7228 Steel
1.7238 Steel
1.7238 Steel
1.7242 Steel
1.7242 Steel
1.7243 Steel
1.7243 Steel
1.7244 Steel
1.7244 Steel
1.7255 Steel
1.7255 Steel
1.7258 Steel
1.7258 Steel
1.7271 Steel
1.7273 Steel
1.7311 Steel
1.7311 Steel
1.7320 Steel
1.7323 Steel
1.7323 Steel
1.7325 Steel
1.7326 Steel
1.7335 Steel
1.7335 Steel
1.7361 Steel
1.7362 Steel
1.7362 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7561 Steel
1.7701 Steel
1.7701 Steel
1.7701 Steel
1.7701 Steel
1.7703 Steel
1.7707 Steel
1.7707 Steel
1.7707 Steel
1.7715 Steel
1.7733 Steel
1.7733 Steel
1.7734 Steel
1.7734 Steel
1.7734 Steel
1.7734 Steel
1.7735 Steel
1.7735 Steel
1.7765 Steel
1.7767 Steel
1.7779 Steel
1.7783 Steel
1.8070 Steel
1.8154 Steel
1.8154 Steel
1.8159 Steel
1.8159 Steel
1.8159 Steel
1.8159 Steel
1.8159 Steel
1.8161 Steel
1.8161 Steel
1.8506 Steel
1.8507 Steel
1.8509 Steel
1.8515 Steel
1.8515 Steel
1.8519 Steel
1.8519 Steel
1.8521 Steel
1.8521 Steel
1.8523 Steel
1.8550 Steel
1.8550 Steel
1.8807 Steel
1.8814 Steel
1.8903 Steel
1.8905 Steel
1.8905 Steel
1.8905 Steel
1.8905 Steel
1.8918 Steel
1.8918 Steel
1.8918 Steel
1.8928 Steel
1.8931 Steel
1.8940 Steel
1.8983 Steel
10 NC 12 Steel
10 NC 6 Steel
10 NC 6 Steel
100 C 6 Steel
100 C 6 Steel
100 CD 7 Steel
100 CD 7 Steel
100Cr2 Steel
100Cr2 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel - Dry Grind-Hardening Process
100Cr6 Steel - Wet Grind-Hardening Process
100CrMn6 Steel
100CrMn6 Steel
100CrMn6 Steel
100CrMnSi6-4 (100CrMn6) Steel
100CrMnSi6-4 (100CrMn6) Steel
100CrMo6 Steel
100CrMo7 Steel
100CrMo7-3 Steel
100CrMo7-3 Steel
100CrMo7-3 Steel
100CrMo7-3 Steel
102Cr6 Steel
102Cr6 Steel
1034 Steel
105Cr2 Steel
105Cr4 Steel
1090 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrSiMoV-7 Steel
10Ni14 Steel
10NiCr6 Steel
10NiCr6 Steel
12 NC 15 Steel
12CrMo19-5 Steel
12CrMo4 Steel
12Ni19 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13NiCr6 Steel
13NiCr6 Steel
13NiCr6, 16NiCrS4 Steels
13NiCr6, 16NiCrS4 Steels
14 NC 11 Steel
14 NC 11 Steel
14 NC 12 Steel
145Cr6 Steel
145Cr6 Steel
145V33 Steel
14CrMoV6-9 Steel
14CrMoV6-9 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14Ni6 Steel
14NiCr10 Steel
14NiCr10 Steel
14NiCr14 Steel
14NiCr14 Steel
14NiCr14 Steel
14NiCr18 Steel
14NiCr18 Steel
14NiCrMo13-4 Steel
14NiCrMo13-4 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15NiCr13 Steel
15NiCuMoNb5 Steel
15NiCuMoNb5 Steel
16 MC 5 Steel
16 MC 5 Steel
16 NC 6 Steel
16 NC 6 Steel
16 NCD 13 Steel
16 NCD 13 Steel
16CD4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrNi4 Steel
16CrNi4 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5, 16MnCrS5 Steels
16MnCr5, 16MnCrS5 Steels
16MnCrB5 Steel
16MnCrB5 Steel
16MnCrB5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16NiCr11 Steel
16NiCr4 Steel
16NiCr4 Steel
16NiCrMo12 Steel
16NiCrMo12 Steel
16NiCrS4 Steel
17-7 PH Steel
17Cr3 Steel
17Cr3 Steel
17Cr3 Steel
17CrMoV10 Steel
17CrMoV10 Steel
17CrNi6-6 Steel
17CrNi6-6 Steel
17CrNi6-6, 15CrNi6 Steels
17CrNi6-6, 15CrNi6 Steels
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrS3 Steel
17Mn4 Steel
17Mn4 Steel
17MnB4 - 20MnB4 - 22MnB4 - 23MnB4 Steels
17MoV8-4 Steel
17MoV8-4 Steel
17NiCrMo6-4 Steel
17NiCrMo6-4 Steel
17NiCrMoS6-4 Steel
17NiCrMoS6-4 Steel
18 C 3 Steel
18 CD 4 Steel
18 CD 4 Steel
18 NCD 6 Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMoS4 Steel
18CrMoS4 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel Steel
18MnCr4 Steel
18MnCr4 Steel
18NiCr5-4 Steel
18NiCr5-4 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo7 Steel
18NiCrMo7 Steel
19Mn5 Steel
19Mn5 Steel
19Mn5 Steel
19Mn5 Steel
20 NC 6 Steel
20 NC 6 Steel
20 NCD 2 Steel
20 NCD 2 Steel
20 NCD 7 Steel
20 NCD 7 Steel
2083/2083 SUPRA ESR Steel
20CrMo2 Steel
20CrMo2 Steel
20CrMo5 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrNi4 Steel
20Mn5 Steel
20MnB4 Steel
20MnB4 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5, 20MnCrS5 Steels
20MnCrB5 Steel
20MnCrB5 Steel
20MnCrS5 Steel
20MnCrS5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr5 Steel
20MoCrS4 Steel
20MoCrS4 Steel
20NiCr6 Steel
20NiCr6 Steel
20NiCrMo14-6 Steel
20NiCrMo14-6 Steel
20NiCrMo2 Steel
20NiCrMo2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2, 20NiCrMoS2-2 Steels
20NiCrMo2-2, 20NiCrMoS2-2 Steels
20NiCrMo3 Steel
20NiCrMo3 Steel
20NiMoCr6 Steel
20NiMoCr6 Steel
20NiMoCr6-5 Steel
20NiMoCr6-5 Steel
20NiMoCrS6 Steel
2162 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
22 N 8 Steel
2205 Duplex Stainless Steel
2210 Steel
22MnB4 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
2311 Steel
2312 Steel
2316/4122 Steel
2343 EFS/EFS SUPRA ESR Steel
2344 EFS/EFS SUPRA ESR Steel
2361/4112 EFS/EFS SUPRA ESR Steel
2363 Steel
2365 EFS Steel
2367 EFS/EFS SUPRA ESR Steel
23CrMoB3-3 Steel
23CrMoB3-3 Steel
23MnB4 Steel
23MnNiCrMo5-3 Steel
2436 Steel
24CrMo5 Steel
24CrMo5 Steel
24CrMo5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
25 CD 4 Steel
25 CD 4 Steel
2507 Steel
2510 Steel
2550 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMoS4 Steel
25CrMoS4 Steel
25MoCr4 Steel
25MoCr4 Steel
25MoCr4 Steel
26CrMo4 Steel
26NiCr6-4 Steel
26NiCr6-4 Steel
2714 Steel
2738/2738 HH Steel
2764 Steel
2767/2767 SUPRA ESR Steel
27MnCrB5 Steel
27MnCrB5-2 Steel
27MnCrB5-2 Steel
27MnCrV4 Steel
27MnCrV4 Steel
2826 Steel
2842 Steel
28CrMoNiV4-9 Steel
28CrMoNiV4-9 Steel
28Mn6 Steel
28Mn6 Steel
28Mn6 Steel
2990 Steel
2Mn Steel
2Mn Steel
30 CD 12 Steel
30 CD 12 Steel
30 CND 8 Steel
30 CND 8 Steel
30 NC 11 Steel
30 NC 11 Steel
30 NC 12 Steel
30 NCD 12 Steel
30 NCD 12 Steel
30 NCD 12 Steel
30 NCD 2 Steel
30 NCD 2 Steel
30 NCD 8 Steel
301LN Steel
30CrMo4 Steel
30CrMo4 Steel
30CrMoNiV5-11 Steel
30CrMoNiV5-11 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30MiCrMo12 Steel
30Mn5 Steel
30Mn5 Steel
30Mn5 Steel
30MnB5 Steel
30MnVS6 (27MnSiVS6) Steel
30NiCr-11 Steel
30NiCr-11 Steel
30NiCrMo2-2 Steel
30NiCrMo2-2 Steel
31CrMo12 Steel
31CrMo12 Steel
31CrMo12 Steel
31CrMoV9 Steel
31CrMoV9 Steel
31CrMoV9 Steel
31CrMoV9 Steel
31CrV2 Steel
31CrV3 Steel
31CrV3 Steel
31CrV3 Steel
32 C 4 Steel
32 C 4 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMoV12-10 Steel
32MnCrMo6-4-3 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4, 34CrS4 Steels
34Cr4, 34CrS4 Steels
34CrAl6 Steel
34CrAlMo5 Steel
34CrAlMo5 Steel
34CrAlMo5 Steel
34CrAlNi7 Steel
34CrAlNi7 Steel
34CrAlNi7 Steel
34CrAlNi7-10 Steel
34CrAlNi7-10 Steel
34CrAlS5 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4, 34CrMoS4 Steels
34CrMo4, 34CrMoS4 Steels
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrS4 Steel
34CrS4 Steel
35 CD 4 Steel
35 CD 4 Steel
35 M 5 Steel
35 M 5 Steel
35 NC 11 Steel
35 NC 6 Steel
35 NC 6 Steel
35 NCD 16 Steel
35 NCD 16 Steel
35 NCD 16 Steel
36CrMn5 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36Mn5 Steel
36NiCr6-4 Steel
36NiCr6-4 Steel
36NiCrMo16 Steel
36NiCrMo16 Steel
37Cr4 Steel
37Cr4 Steel
37Cr4 Steel
37Cr4, 37CrS4 Steels
37Cr4, 37CrS4 Steels
37CrS4 Steel
37MnB4 Steel
37MnB5 (40MnB4) Steel
37MnB5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37Mo2 Steel
38 C 4 Steel
38 C 4 Steel
38Cr2 Steel
38Cr2 Steel
38MnB5 Steel
38Si6 Steel
38Si6 Steel
38Si7 Steel
39NiCrMo4 Steel
39NiCrMo4 Steel
40 NCD 3 Steel
40 NCD 3 Steel
40CrMnMo7 Steel
40CrMnNiMo8-6-4 Steel
40Mn4 Steel
40Mn4 Steel
40MnSiCrMoB4 Steel
40MnSiCrMoB4 Steel
40NiCrMo18-6 Steel
40NiCrMo18-6 Steel
40NiCrMo2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo3 Steel
40NiCrMo7 Steel
40NiCrMo8-4 Steel
41 S 7 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4, 41CrS4 Steels
41Cr4, 41CrS4 Steels
41CrAlMo7-10 Steel
41CrAlMo7-10 Steel
41CrMo4 Steel
41CrMo4 Steel
41CrS4 Steel
41CrS4 Steel
41NiCrMo7-3-2 Steel
42 C 4 Steel
42 C 4 Steel
42Cr4 Steel
42Cr4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4, 42CrMoS4 Steels
42CrMo4, 42CrMoS4 Steels
42CrV6 Steel
42CrV6 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
4340 Steel
45 SCD 6 Steel
45 SCD 6 Steel
45 SCD 6 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrVMoW5-8 Steel
45CrVMoW5-8 Steel
45WCrV7-7 Steel
45WCrV7-7 Steel
46Cr2 Steel
46Cr2 Steel
46CrS2 Steel
46Si7 Steel
46Si7 Steel
46Si7 Steel
46Si7 Steel
46SiCrMo6-3 Steel
46SiCrMo6-3 Steel
48Si7 Steel
49CrMo4 Steel
49CrMo4 Steel
50 CD 4 Steel
50 CD 4 Steel
50 CV 4 Steel
50 CV 4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50MnV7 Steel
50MnV7 Steel
50SiCrMo6 Steel
5140 Steel
5140 Steel
5140 Steel
51CrMoV4 Steel
51CrMoV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51Si7 Steel
51Si7 Steel
51Si7 Steel
51Si7 Steel
52CrMo4V Steel
52CrMo4V Steel
52CrMoV4 (51CrMoV4) Steel
52CrMoV4 (51CrMoV4) Steel
52CrMoV4 Steel
52CrMoV4 Steel
52MnCrB3 Steel
52MnCrB3 Steel
52SiCrNi5 Steel
52SiCrNi5 Steel
54SiCr6 Steel
54SiCr6 Steel
54SiCrV6 Steel
54SiCrV6 Steel
55 NCDV 7 Steel
55 S 7 Steel
55 S 7 Steel
55Cr3 Steel
55Cr3 Steel
55Cr3 Steel
55Cr3 Steel
55NiCrMoV6 Steel
55NiCrMoV6 Steel
55Si7 Steel
55Si7 Steel
55SiMo8 Steel
56NiCrMoV7 Steel
56NiCrMoV7 Steel
56NiCrMoV7 Steel
56Si7 (55Si7) Steel
56Si7 Steel
56Si7 Steel
56SiCr7 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
60Cr3 Steel
60Si7 Steel
60SiCr7 Steel
60SiCr7 Steel
60SiCr8 Steel
60SiCrV7 Steel
60SiCrV7 Steel
60SiCrV7 Steel
61CrSiV5 Steel
61CrSiV5 Steel
61CrSiV5 Steel
61CrSiV5 Steel
61SiCr7 Steel
61SiCr7 Steel
65Si7 Steel
65Si7 Steel
65Si7 Steel
65Si7 Steel
65SiCr7 Steel
65SiCr7 Steel
71Si7 Steel
71Si7 Steel
80MoCrV42-16 Steel
80MoCrV42-16 Steel
80MoCrV42-16 Steel
819B Steel
8630 Steel
86CrMoV7 Steel
86CrMoV7 Steel
86CrMoV7 Steel
86CrMoV7 Steel
8MnCrB3 Steel
8MnMoNi5-5 Steel
90MnCrV8 Steel
90MnCrV8 Steel
90MnCrV8 Steel
90MnV8 Steel
90MnV8 Steel
90MnV8 Steel
A2 Steel
ABC III Steel
ADC3 Steel
ADS-4 Steel
AISI 01 Steel
AISI 1020 Steel
AISI 1025 Steel
AISI 1025 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1055 Steel
AISI 304 Steel
AISI 304 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 410 Steel
AISI 410 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4137 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 420C Steel
AISI 420C Steel
AISI 431 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 8630 mod. Steel
AISI A2 (A2, A2F) Steel
AISI A2 Steel
AISI D2 (D2, D2F) Steel
AISI H13 EFS Steel
AISI H13 Steel
AISI H13 Steel
AISI P20 Steel
AISI S1 Steel
AISI W210 Steel
ARMAD Steel
ASP 2023 Steel
ASP 2023 Steel
ASP 2060 Steel
ASSAB 8407 2M Steel
ASSAB 8407 SUPREME Steel
ASSAB 8407 Steel
ASSAB PM 23 SuperClean Steel
Alloy 625 Steel
Ausa 42CrMo4 Steel
Avesta Sheffield 2205 Steel
B18 Steel
B30 Steel
B30H Steel
BOHLER K100 Steel
BOHLER K100 Steel
BOHLER K105 Steel
BOHLER K105 Steel
BOHLER K105 Steel
BOHLER K107 Steel
BOHLER K107 Steel
BOHLER K110 Steel
BOHLER K110 Steel
BOHLER K110 Steel
BOHLER K190 MICROCLEAN Steel
BOHLER K245 Steel
BOHLER K305 Steel
BOHLER K305 Steel
BOHLER K306 Steel
BOHLER K455 Steel
BOHLER K455 Steel
BOHLER K460 Steel
BOHLER K460 Steel
BOHLER K600 Steel
BOHLER K600 Steel
BOHLER K605 Steel
BOHLER K605 Steel
BOHLER K700 Steel
BOHLER K720 Steel
BOHLER K720 Steel
BOHLER K990 Steel
BOHLER M200 Steel
BOHLER M238 VMR/VAR Steel
BOHLER M300 ISOPLAST Steel
BOHLER M303 EXTRA Steel
BOHLER M310 ISOPLAST Steel
BOHLER M330 VMR Steel
BOHLER N360 ISOEXTRA Steel
BOHLER S500 Steel
BOHLER S500 Steel
BOHLER S590 MICROCLEAN Steel
BOHLER S600 Steel
BOHLER S600 Steel
BOHLER S690 MICROCLEAN Steel
BOHLER S705 Steel
BOHLER S705 Steel
BOHLER S790 MICROCLEAN Steel
BOHLER W100 Steel
BOHLER W100 Steel
BOHLER W300 Steel
BOHLER W300 Steel
BOHLER W302 ISOBLOC Steel
BOHLER W302 Steel
BOHLER W303 Steel
BOHLER W320 Steel
BOHLER W320 Steel
BOHLER W321 Steel
BOHLER W321 Steel
BOHLER W400 VMR Steel
BOHLER W400 VMR Steel
BOHLER W403 VMR Steel
BOHLER W500 Steel
BOHLER W500 Steel
BR1500HS Steel
BR1500HS Steel
BR885 Steel
BR885 Steel
BRM1 Steel
BRM2 Steel
BRM2 Steel
BRU Steel
BRW1 Steel
BRW1 Steel
BeyLos 2329 Steel
BeyLos 2340 Steel
BeyLos 2343 Steel
BeyLos 2344 Steel
BeyLos 2365M Steel
BeyLos 2367 Steel
BeyLos 2711 Steel
BeyLos 2714 Steel
Bohler 25CrMo4 Steel
Bohler CM193 Steel
Bohler CM193 Steel
Bohler D114 Steel
Bohler D114 Steel
Bohler D118 Steel
Bohler D118 Steel
Bohler D122 Steel
Bohler D122 Steel
Bohler D204 Steel
Bohler D204 Steel
Bohler D206 Steel
Bohler D206 Steel
Bohler D220 Steel
Bohler D220 Steel
Bohler D221 Steel
Bohler D221 Steel
Bohler D230 Steel
Bohler D230 Steel
Bohler D240 Steel
Bohler D240 Steel
Bohler D320 Steel
Bohler D320 Steel
Bohler D402 Steel
Bohler D402 Steel
Bohler D500 Steel
Bohler D500 Steel
Bohler D608 Steel
Bohler D608 Steel
Bohler D612-SO Steel
Bohler D612-SO Steel
Bohler D612-SO Steel
Bohler D612-SO Steel
Bohler E200 Steel
Bohler E200 Steel
Bohler E230 Steel
Bohler E230 Steel
Bohler E410 Steel
Bohler E410 Steel
Bohler F550 Steel
Bohler F550 Steel
Bohler H700 SD Steel
Bohler H700 SD Steel
Bohler H700 Steel
Bohler H700 Steel
Bohler H700 Steel
Bohler H700 Steel
Bohler H710 Steel
Bohler H710 Steel
Bohler H730 Steel
Bohler H730 Steel
Bohler H732 Steel
Bohler H732 Steel
Bohler K100 Steel
Bohler K100 Steel
Bohler K103 Steel
Bohler K103 Steel
Bohler K105 Steel
Bohler K105 Steel
Bohler K105 Steel
Bohler K105 Steel
Bohler K107 So Steel
Bohler K107 So Steel
Bohler K110 Steel
Bohler K110 Steel
Bohler K200 Steel
Bohler K200 Steel
Bohler K243 Steel
Bohler K243 Steel
Bohler K243 Steel
Bohler K243 Steel
Bohler K245 Steel
Bohler K245 Steel
Bohler K305 Steel
Bohler K305 Steel
Bohler K306 Steel
Bohler K306 Steel
Bohler K306 Steel
Bohler K306 Steel
Bohler K450 Steel
Bohler K450 Steel
Bohler K455 ISODUR Steel
Bohler K455 ISODUR Steel
Bohler K455 Steel
Bohler K455 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K463 Steel
Bohler K463 Steel
Bohler K510 Steel
Bohler K510 Steel
Bohler K600 Steel
Bohler K600 Steel
Bohler K600 Steel
Bohler K603 Steel
Bohler K603 Steel
Bohler K605 Steel
Bohler K605 Steel
Bohler K605 Steel
Bohler K710 So Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K990 Steel
Bohler K990 Steel
Bohler M200 Steel
Bohler M200 Steel
Bohler M200 Steel
Bohler M200-So Steel
Bohler M200-So Steel
Bohler M210 Steel
Bohler M210 Steel
Bohler M210 Steel
Bohler M210 Steel
Bohler M238 Steel
Bohler M238 Steel
Bohler M303 EXTRA Steel
Bohler M310 ISOPLAST Steel
Bohler N310 Steel
Bohler N310 Steel
Bohler N320 Steel
Bohler N320 Steel
Bohler N320 Steel
Bohler N335 Steel
Bohler N335 Steel
Bohler N335 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N351 SB Steel
Bohler N351 SB Steel
Bohler N352 Steel
Bohler N352 Steel
Bohler N400 Steel
Bohler N530 Steel
Bohler N530 Steel
Bohler N540 Steel
Bohler N540 Steel
Bohler N540 Steel
Bohler N545 Steel
Bohler N545 Steel
Bohler N555 Steel
Bohler N555 Steel
Bohler N685 EXTRA
Bohler N685 Steel
Bohler N685 Steel
Bohler N690 Steel
Bohler N690 Steel
Bohler N700 Steel
Bohler S200 Steel
Bohler S200 Steel
Bohler S200 Steel
Bohler S200 Steel
Bohler S300 Steel
Bohler S300 Steel
Bohler S305 Steel
Bohler S305 Steel
Bohler S400 Steel
Bohler S400 Steel
Bohler S400 Steel
Bohler S400 Steel
Bohler S401 Steel
Bohler S500 Steel
Bohler S500 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S601 Steel
Bohler S601 Steel
Bohler S604 Steel
Bohler S604 Steel
Bohler S607 Steel
Bohler S607 Steel
Bohler S607 Steel
Bohler S607 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S705 Steel
Bohler S705 Steel
Bohler T502 Steel
Bohler T502 Steel
Bohler T550 Steel
Bohler T550 Steel
Bohler T550 Steel
Bohler T550 Steel
Bohler T552 Steel
Bohler T552 Steel
Bohler T560 Steel
Bohler T560 Steel
Bohler T560 Steel
Bohler T560 Steel
Bohler T562 Steel
Bohler T562 Steel
Bohler T651 Steel
Bohler T651 Steel
Bohler V-V118 Steel
Bohler V-V118 Steel
Bohler V117 Steel
Bohler V117 Steel
Bohler V124 Steel
Bohler V124 Steel
Bohler V126 Steel
Bohler V126 Steel
Bohler V129 Steel
Bohler V129 Steel
Bohler V130 Steel
Bohler V130 Steel
Bohler V130 Steel
Bohler V130 Steel
Bohler V131 So Steel
Bohler V131 So Steel
Bohler V131 So Steel
Bohler V131 So Steel
Bohler V131 Steel
Bohler V131 Steel
Bohler V145 Steel
Bohler V145 Steel
Bohler V145 Steel
Bohler V145 Steel
Bohler V147 Steel
Bohler V147 Steel
Bohler V155 Steel
Bohler V155 Steel
Bohler V155 Steel
Bohler V155 Steel
Bohler V162 Steel
Bohler V162 Steel
Bohler V163 Steel
Bohler V163 Steel
Bohler V164 Steel
Bohler V164 Steel
Bohler V165 Steel
Bohler V165 Steel
Bohler V304 Steel
Bohler V304 Steel
Bohler V310 Steel
Bohler V310 Steel
Bohler V320 SX Steel
Bohler V320 SX Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V330SH Steel
Bohler V340 Steel
Bohler V340 Steel
Bohler V350 Steel
Bohler V350 Steel
Bohler V359 Steel
Bohler V359 Steel
Bohler V913 Steel
Bohler V913 Steel
Bohler V930 Steel
Bohler V930 Steel
Bohler V945 Steel
Bohler V945 Steel
Bohler W100 Steel
Bohler W100 Steel
Bohler W104 Steel
Bohler W104 Steel
Bohler W108 Steel
Bohler W108 Steel
Bohler W2773 Steel
Bohler W2773 Steel
Bohler W300 Steel
Bohler W300 Steel
Bohler W300 Steel
Bohler W300 Steel
Bohler W302 ISOBLOC Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W303 ISODISC Steel
Bohler W303 Steel
Bohler W304 Steel
Bohler W304 Steel
Bohler W304 Steel
Bohler W320 ISODISC Steel
Bohler W320 Steel
Bohler W320 Steel
Bohler W320 Steel
Bohler W320 Steel
Bohler W3202 Steel
Bohler W321 Steel
Bohler W326 Steel
Bohler W326 Steel
Bohler W329 Steel
Bohler W329 Steel
Bohler W338 Steel
Bohler W338 Steel
Bohler W400 WMR Steel
Bohler W403 WMR Steel
Bohler W500 Steel
Bohler W500 Steel
Bohler W501 Steel
Bohler W501 Steel
Bohler W503 Steel
Bohler W503 Steel
Bohler W6735 Steel
Bohler W6735 Steel
Bohler W6735 Steel
Bohler W6735 Steel
Bohler W705 Steel
Bohler W705 Steel
Bohler W705 Steel
Buderis 1730 Steel
Buderus 1730 Steel
Buderus 2067 Steel
Buderus 2080 Steel
Buderus 2085 Steel
Buderus 2085 Steel
Buderus 2311 ISO-BM Steel
Buderus 2312 Steel
Buderus 2313 Steel
Buderus 2316 ISO-B MOD Steel
Buderus 2323 ISO-B Steel
Buderus 2343 ISO-B MOD Steel
Buderus 2343 ISO-B MOD Steel
Buderus 2343 ISO-B Steel
Buderus 2344 ISO-B Steel
Buderus 2344 ISO-B Steel
Buderus 2360 ISO-B Steel
Buderus 2360 ISO-B Steel
Buderus 2365 ISO-B Steel
Buderus 2365 ISO-B Steel
Buderus 2367 ISO-B Steel
Buderus 2367 ISO-B Steel
Buderus 2436 ISO-B Steel
Buderus 2436 ISO-B Steel
Buderus 2510 Steel
Buderus 2550 Steel
Buderus 2601 Steel
Buderus 2606 ISO-B Steel
Buderus 2606 ISO-B Steel
Buderus 2678 Steel
Buderus 2711 ISO-B MOD Steel
Buderus 2711 ISO-B Steel
Buderus 2711 ISO-B Steel
Buderus 2711 Steel
Buderus 2714 ISO-B MOD Steel
Buderus 2714 ISO-B MoD Steel
Buderus 2714 ISO-B Steel
Buderus 2714 ISO-B Steel
Buderus 2738 ISO-BM Steel
Buderus 2738 Steel
Buderus 2739 ISO-B Steel
Buderus 2744 ISO-B Steel
Buderus 2744 ISO-B Steel
Buderus 2766 Steel
Buderus 2767 ISO-B Steel
Buderus 2767 ISO-B Steel
Buderus 2842 Steel
Buderus 7220 Steel
Buderus Thruhard Supreme 2738mod.TS(HHH) Steel
C10 Steel
C10 Steel
C100S Steel
C100S Steel
C100W1 Steel
C10E2C Steel
C10E2C Steel
C125S Steel
C15E2C (Cq15) Steel
C15R Steel
C16 Steel
C17E2C Steel
C20 Steel
C22.8 Steel
C35 Steel
C35 Steel
C35E Steel
C35E Steel
C35EC Steel
C35EC Steel
C35EC Steel
C35EC Steel
C35R Steel
C35R Steel
C35R Steel
C35R Steel
C35RC Steel
C35RC Steel
C36 Steel
C36 Steel
C40E Steel
C40R Steel
C43 Steel
C43 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45E Steel
C45E Steel
C45E Steel
C45E Steel
C45E, C45R Steels
C45E, C45R Steels
C45EC (Cq45) Steel
C45EC (Cq45) Steel
C45EC Steel
C45EC Steel
C45R Steel
C45R Steel
C45RC Steel
C45RC Steel
C46 Steel
C46 Steel
C50E Steel
C50E Steel
C50R Steel
C53 Steel
C55E Steel
C55E Steel
C55R (Cm55) Steel
C55R (Cm55) Steel
C55R Steel
C55R Steel
C55R Steel
C55S Steel
C60 Steel
C60 Steel
C60 Steel
C60 Steel
C60 Steel
C60E Steel
C60R Steel
C60R Steel
C60R Steel
C60R Steel
C60S Steel
C60S Steel
C67S Steel
C70W1 Steel
C70W1 Steel
C75S Steel
C75S Steel
C75S Steel
C80U Steel
C80U Steel
C80U Steel
C80U Steel
C90S Steel
CALMAX Steel
CARBODUR 15NiCr13 Steel
CARBODUR 16MnCr5/16MnCrS5 Steel
CARBODUR 17Cr3 Steel
CARBODUR 17CrNi6-6 Steel
CARBODUR 18CrNi8 Steel
CARBODUR 18CrNiMo7-6 Steel
CARBODUR 20MnCr4/20MnCrS4 Steel
CARBODUR 20MnCr5/20MnCrS5 Steel
CARBODUR 20NiCrMo2-2/20NiCrMoS2-2 Steel
CARBODUR 20NiMoCrS6-5 Steel
CH16V Steel
CH5M Steel
CLC 1.2312 Steel
CLC 1.2312 Steel
CLC 1.2316 S Steel
CLC 1.2316 Steel
CLI-SAF 2507 Steel
CM167 Steel
CMR Steel
CRONIDUR 30 Steel
CRONIDUR 30 Steel
CRV1 Steel
CRV3 Steel
CRV3 Steel
CT781 Steel
CT781 Steel
Calmax Steel
Carbodur 6587 Steel
Carbodur 6758 Steel
Carbodur 7131/Carbodur 7139 Steel
Carmo Steel
Carpenter 440-XH Steel
Carpenter Micro-Melt M42 Steel
Carpenter No. 158 Steel
Carpenter No. 345 Steel
Carpenter No. 484 Steel
Carpenter No. 484 Steel
Carpenter No. 610 Steel
Carpenter No. 882 Steel
Carpenter No. 883 Steel
Carpenter O1 Steel
Carpenter VIM-VAR M-50 Steel
Cf35 Steel
Cf35 Steel
Cf45 Steel
Cf45 Steel
Cf53 Steel
Cf53 Steel
Cf70 Steel
Cf70 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck30 Steel
Ck30 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck50 Steel
Ck55 Steel
Ck55 Steel
Ck55 Steel
Ck55 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck75 Steel
Ck75 Steel
Ck85 Steel
Ck85 Steel
Ck85 Steel
Ck85 Steel
Corrodur 4418 Mod Steel
Cr26Ni6Mo3Cu3 Steel
Cronidur 30 Steel
Cronidur 30 Steel
Cronifer1925 hMo - alloy 926
Cryodur 2242 Steel
Cryodur 2767 Steel
D Steel
D2 Steel
D3 Steel
DC04 Steel
DIMO 2311 Steel
DIMO 2312 Steel
DIMO 2312 Steel
DIMO 2738 XH Steel
DIMO 2738 XH Steel
DMo5 Steel
Docol Boron 02 Steel
Dominial BA Steel
Dominial C H W Steel
Dominial CH 16 V Steel
Dominial CH 160 W Steel
Dominial CH 16V Steel
Dominial CH 2 V Steel
Dominial CH 5 M Steel
Dominial CH Steel
Dominial CM 167 Steel
Dominial DSW, PK Steels
Dominial Extra E, Extra Mo, C 2 Mo Steels
Dominial HMoD Steel
Dominial HWD Steel
Dominial KL Steel
Dominial KS 60, KS 80 Steels
Dominial KTW/KTW-Ni Steel
Dominial MA Steel
Dominial MAK Steel
Dominial MKSt Steel
Dominial N400 Steel
Dominial PD Steel
Dominial PWM Steel
Dominial RP Mo H Steel
Dominial RP Steel
Dominial RPU Steel
Dominial SN Steel
Dominial SP und RS Steels
Dominial SS 50, SS 60 Steels
Dominial UNI Steel
Dominial US Steel
Dominial USD Steel
Dominial USN Steel
Dominial W44 Steel
Dorrenberg P5M Steel
Dorrenberg R65 Steel
Dorrenberg WP5 Steel
Dorrenberg 1.2379 PLUS Steel
Dorrenberg 1.2379PLUS Steel
Dorrenberg 1.3343PLUS Steel
Dorrenberg A50 Steel
Dorrenberg AMO Steel
Dorrenberg AMO Steel
Dorrenberg CP10V Steel
Dorrenberg CPPK Steel
Dorrenberg CPPU Steel
Dorrenberg CPPU Steel
Dorrenberg CPW Steel
Dorrenberg DM05 Steel
Dorrenberg DM3 Steel
Dorrenberg DM3X Steel
Dorrenberg DM3X Steel
Dorrenberg DM51 Steel
Dorrenberg DMO5 Steel
Dorrenberg ECN4M Steel
Dorrenberg EMo5Co5 Steel
Dorrenberg EMo5Co5 Steel
Dorrenberg EMo9CoH Steel
Dorrenberg EPM2 Steel
Dorrenberg Extra Nr. 45 Steel
Dorrenberg GX155CrVMo12-1 Steel
Dorrenberg HC16S Steel
Dorrenberg HC17M Steel
Dorrenberg HC17M Steel
Dorrenberg HC50 Steel
Dorrenberg HC50 Steel
Dorrenberg Hidalgo I Steel
Dorrenberg KHD Steel
Dorrenberg KHD Steel
Dorrenberg KHD Steel
Dorrenberg KHD Steel
Dorrenberg M4S Steel
Dorrenberg M4S Steel
Dorrenberg M4S Steel
Dorrenberg M4S Steel
Dorrenberg MCM Steel
Dorrenberg MCMN Steel
Dorrenberg MCMS Steel
Dorrenberg MS Steel
Dorrenberg NC50E Steel
Dorrenberg NCM Steel
Dorrenberg NCM Steel
Dorrenberg NCM Steel
Dorrenberg NCM Steel
Dorrenberg NCV Steel
Dorrenberg NCV Steel
Dorrenberg NCV Steel
Dorrenberg NCV Steel
Dorrenberg Ni50 Steel
Dorrenberg Ni50 Steel
Dorrenberg Ni50 Steel
Dorrenberg Ni50 Steel
Dorrenberg PV4 Steel
Dorrenberg PV6 Steel
Dorrenberg R118 Steel
Dorrenberg R17WS Steel
Dorrenberg R17X Steel
Dorrenberg R18 Steel
Dorrenberg R18So Steel
Dorrenberg R45 Steel
Dorrenberg VNC4 Steel
Dorrenberg WP5V Steel
Dorrenberg WR Special Steel
Dorrenberg Z1B Steel
Dorrenberg Z3C Steel
Durapur 1219 Steel
Durapur 3505 Steel
Durapur 3520 Steel
E355 Steel
EC100 Steel
EC100 Steel
EC60 Steel
ECMO100 Steel
ECMO100 Steel
ECN150 Steel
ECN200 Steel
ECN35 Steel
ECN35 Steel
ECN35 Steel
ECN35 Steel
ES 100 K Steel
ES 106 K Steel
ES 120 K ESR Steel
ES 120 K Steel
ES 235 W Steel
ES 245 W ESR Steel
ES 245 W Steel
ES 265 W ESR Steel
ES 265 W Steel
ES 275 ESR Steel
ES 275 K ESR Steel
ES 370 G Steel
ES 4122 Steel
ES 50 S Steel
ES 50 SW Steel
ES 60 S Steel
ES 65 S Steel
ES 70 S Steel
ES Aktuell 1000 Steel
ES Aktuell S Steel
ES Aktuell Steel
ES Antikor S Steel
ES Antikor Steel
ES Maximum 500 Steel
ES ULW 65 Steel
EUROFER-97 Steel
EUROFER-97 Steel
EUROFER-97 Steel
EskyLos 2083 Steel
EskyLos 2083 Steel
EskyLos 2083 Steel
EskyLos 2340 DC Steel
EskyLos 2340 HDC Steel
EskyLos 2340 Steel
EskyLos 2343 DC Steel
EskyLos 2343 HDC Steel
EskyLos 2343 Steel
EskyLos 2344 HDC Steel
EskyLos 2344 Steel
EskyLos 2344 Steel
EskyLos 2367 Steel
EskyLos 4542 Steel
EskyLos HiMo Steel
EskyLos HiMo Steel
EskyLos OptiMo Steel
EskyLosS 6959 Steel
Eskylos 2365M Steel
F82H (8Cr-2WVTa) Steel
F82H mod. Steel
F82H mod. Steel
FAM Steel
FDG (W) Steel
Feroxy 1.2311 Steel
Feroxy 1.2311 Steel
Feroxy 1.2738 Steel
Firmodur 1213 Steel
Firmodur 1249 Steel
Firmodur 6582 Steel
Firmodur 7220/Firmodur 7226 Steel
Firmodur 7225/Firmodur 7227 Steel
GKH (W - YW) Steel
GS-22CrMo5 Steel
H13 Steel
H13 Steel
H21 Steel
HFX 6926 Steel
HFX 6926 Steel
HFX 6928 Steel
HFX 6928 Steel
HFX 7783 Steel
HFX 7783 Steel
HMoD Steel
HS18-0-1 Steel
HS6-5-2 Steel
Hasco 1.2436 Steel
Inconel 625 Steel
Industeel 1.2312 Steel
Industeel 1.2316S Steel
Industeel D2 Steel
Industeel D2 Steel
Influence of the Austenitizing Temperature (8 Diagrams)
KATO2 Steel
KATO2 Steel
KATO2 Steel
KATO3 Steel
KATO3 Steel
KATO3 Steel
KATO3 Steel
KL Steel
KSV Steel
KeyLos 1730 Steel
KeyLos 1730M Steel
KeyLos 2083 Steel
KeyLos 2085 Steel
KeyLos 2311 Steel
KeyLos 2311 Steel
KeyLos 2312 Steel
KeyLos 2316 Steel
KeyLos 2738 Steel
KeyLos 6959 Steel
KeyLos 7225 Steel
LA 13Ta Steel
LA-Steel with Ce+Ta
LA-Steel with Ta+Hf
M2 Steel
M268 Steel
MA Steel
MD Steel
MD Xtra Steel
MEK3 Steel
MEK4 Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MFR Steel
MLQ Xtra Steel
Magnadie-RF Steel
Marker DCM, DCM-ESR Steel
Marker PHM Steel
Marker WM 28 Steel
Mf temperature of 1.2080, 1.2345, 1.2363, 1.2376, 1.2379, 1.2436, 1.2550, 1.2601, 1.2631, 1.2714, 1.4116, 1.5028, 1.6511, 1.6580, 1.6582, 1.6773, 1.7225 Steels
N400 Steel
NITRODUR 15CrMoV5-9 Steel
NITRODUR 15CrMoV5-9 Steel
NITRODUR 31CrMoV9 Steel
NITRODUR 34CrAlMo5 Steel
NITRODUR 34CrAlNi7 Steel
NITRODUR 41CrAlMo7 Steel
NOVONOX FT 13 Steel
NVONOX F 17a Steel
NVONOX M 131 Steel
NVONOX M 171 H Steel
NVONOX T 13 Steel
NVONOX T 131 Steel
NVONOX T 17 Steel
NVONOX T 171 Steel
NVONOX TT 13 Steel
NVONOX TT 131 Steel
NZ3 Steel
New TAF Steel
Nicrofer 3127 hMo - alloy 31
Nicrofer 4823 hMo - alloy G-3
Nicrofer3033 - alloy 33
Nicrofer4221 - alloy 825
Nicrofer4320 Ti Alloy
Nicrofer5120 CoTi - alloy C-263
Nicrofer5621 hMoW - alloy 22
Nicrofer5716 hMoW - alloy C-276
Nicrofer5923 hMo - alloy 59
Nicrofer6020 hMo - alloy 625
Nicrofer6616 hMo - alloy C-4
Nitrodur 8515 Steel
Nitrodur 8523 Steel
Nitrodur 8524 Steel
Nitrodur 8550 Steel
O1 Steel
OA2 Steel
OA2 Steel
OC100 Steel
OC100 Steel
OC80 Steel
OCR12 Steel
OCR12 Steel
OCR12 Steel
OCR12 Steel
OCR12EX Steel
OCR12EX Steel
OCR12EXL Steel
OCR12EXL Steel
OCR12EXL Steel
OCR12EXL Steel
OCR12SP Steel
OCR12SP Steel
OCR12VM Steel
OCR12VM Steel
OCR12VM Steel
OCR12VM Steel
OCR12VMS Steel
OCR12VMS Steel
OCR12VMS Steel
OCR6 Steel
OCR6 Steel
OH239 Steel
OH239 Steel
OH239 Steel
OH239 Steel
OH239 Steel
OH246 Steel
OH246 Steel
OH248 Steel
OH248 Steel
OH252 Steel
OH252 Steel
OH253 Steel
OH253 Steel
OH257 Steel
OH257 Steel
OH260 Steel
OH842 Steel
OH842 Steel
OHV4 Steel
OHV4 Steel
OHV4 Steel
OHV5 Steel
OPTIFER II (GeCe) Steel
OPTIFER III (TaCe) Steel
OPTIFER Ib (WTaY) Steel
OPTIFER-V (W,Ce) Steel
OPTIFER-VI (Ge,Ce) Steel
OPTIFER-VII (8.5 Cr, W) Steel
OPTIFER-X (W) Steel
OPTIMAR Steel
OPTIMAR-W Steel
ORVAR 2 Microdized Steel
ORVAR SUPREME Steel
OSIKROSP Steel
OSIKROSP Steel
OSIKROSP Steel
OSIKROSP Steel
OSIKROSP Steel
OW1 Steel
OW4 Steel
OW4 Steel
OW4 Steel
OW4 Steel
OW4 Steel
Ovako 280T Steel
Ovako 5450 Steel
P20 MOULD Steel
P20 Steel
P20+Ni Steel
P295GH Steel
P91 Steel
P91 Steel
PD Steel
PER1 Steel
PER1 Steel
PK Steel
PK324 Steel
PK330 Steel
PK335 Steel
PK335 Steel
PK335 Steel
PK339 Steel
PK339 Steel
PK348 Steel
PK348 Steel
PK348 Steel
PK4 Steel
PK4EX Steel
PK4EX Steel
PK8 Steel
PO209 Steel
PO209 Steel
PO731 Steel
PO731 Steel
PO731 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO735 Steel
PO735 Steel
PO766 Steel
PO768 Steel
PO768 Steel
PO768 Steel
PO795 Steel
PO795 Steel
PT181 Steel
PT181 Steel
PT759 Steel
PT759 Steel
PT759 Steel
PWM Steel
PWU Steel
R6110 Steel
RA4W Steel
RAVNE23 Steel
RAVNE30 Steel
RAVNEX Steel
RF Steel
RIGOR Steel
RM161a Steel
RM189 Steel
RM200 Steel
RNO-D Steel
RNO-D Steel
RNO-D Steel
RNO-MoV Steel
RNO-MoV Steel
RP Steel
RPCo Steel
RR ALTAIR 1.2340 MOD. Steel
RR ALTAIR 1.2340 MOD. Steel
RR ANTARES 1.2344 MOD. Steel
RR ANTARES 1.2344 MOD. Steel
RR ASTRO 1.2343 MOD. Steel
RR ASTRO 1.2343 MOD. Steel
RR SIRIO 1.2367 MOD. Steel
RR SIRIO 1.2367 MOD. Steel
RR VEGA 1.2738 MOD. Steel
RR VEGA 1.2738 MOD. Steel
Rodacciai 16MnCr5, 16MnCrS5 Steels
Rodacciai 16MnCr5, 16MnCrS5 Steels
Rodacciai 16NiCr4, 16NiCrS4 Steels
Rodacciai 16NiCr4, 16NiCrS4 Steels
Rodacciai 17NiCrMo6-4, 17NiCrMoS6-4 Steels
Rodacciai 17NiCrMo6-4, 17NiCrMoS6-4 Steels
Rodacciai 20MnCr5, 20MnCrS5 Steels
Rodacciai 20NiCrMo2-2, 20NiCrMoS2-2 Steels
Rodacciai 20NiCrMo2-2, 20NiCrMoS2-2 Steels
Rodacciai 50CrMo4 Steel
Rodacciai 50CrMo4 Steel
Rodacciai C35R Steel
Rodacciai C35R Steel
Rodacciai C50E Steel
Rodacciai C50E Steel
Rohling-RT6 Steel
Rohling-RTW 2H Steel
S1 Steel
S235 Steel
S235JR Steel
S32760 and UR52N,SAF2507,29Cr-6Ni-2Mo-O.38N Steels
S355J2G3 Steel
S960Q Steel
SAE 1513 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SANCY2 Steel
SKD61 Steel
SKD61 Steel
SLM 4340 Steel
SM - 2738 Steel
SM - 2738 Steel
SMR Steel
SMV3 Steel
SN Steel
SUJ2 Steel
SUPERPLAST 350 Steel
SW538H Steel
SW538H Steel
SW718H Steel
SWG 2083 VICTORY ESR Steel
SWG 2085 Steel
SWG 2311 Steel
SWG 2312 Steel
SWG 2316 Steel
SWG 2316 VICTORY ESR Steel
SWG 2343 (SWG EX3) Steel
SWG 2343 VICTORY ESR (EX3 ESR) Steel
SWG 2344 (EX4) Steel
SWG 2344 VICTORY ESR (EX4 ESR) Steel
SWG 2347 Steel
SWG 2357 (AISI S7) Steel
SWG 2367 VICTORY ESR (EX7 ESR) Steel
SWG 2379 Steel
SWG 2711 Steel
SWG 2711mod Steel
SWG 2711mod Steel
SWG 2714 Steel
SWG 2738 / 2738H / 2738HH Steel
SWG 2767 Steel
SWG 738HH Steel
SWG CPM50 VICTORY ESR Steel
SWG CRMHP VICTORY ESR Steel
SWG EX1 VICTORY ESR Steel
SWG EX2 Steel
SWG OPTI N+ Steel
SWG - 2080 Steel
SWG - 2083 Steel
SWG - 2311 Steel
SWG - 2312 Steel
SWG - 2343 Steel
SWG - 2344 Steel
SWG - 2379 Steel
SWG - 2714 Steel
SWG - 2738 Steel
SWG - 2738 mod. Steel
SWG - 2767 Steel
Sandvik 253 MA Steel
Sanicro 69 Steel
St52-3 Steel
St52-3 Steel
StE 690 Steel
Superplast 300 Steel
T/P91 Steel
TA2 Steel
TD2 Steel
TD2 Steel
THYRAPID 2990 Steel
THYRODUR 2381 Steel
THYRODUR 1520 Steel
THYRODUR 2002 Steel
THYRODUR 2067 Steel
THYRODUR 2080 Steel
THYRODUR 2101 Steel
THYRODUR 2235 Steel
THYRODUR 2242 Steel
THYRODUR 2243 Steel
THYRODUR 2249 Steel
THYRODUR 2363 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2436 Steel
THYRODUR 2510 Steel
THYRODUR 2516 Steel
THYRODUR 2550 Steel
THYRODUR 2550 Steel
THYRODUR 2721 Steel
THYRODUR 2766 Steel
THYRODUR 2767 Steel
THYRODUR 2826 Steel
THYRODUR 2833 Steel
THYRODUR 2842 Steel
THYRODUR2067 Steel
THYRODUR2210 Steel
THYROFORT 25CrMo4/25CrMoS4 Steel
THYROFORT 28Mn6 Steel
THYROFORT 30CrNiMo8 Steel
THYROFORT 34Cr4/34CrS Steel
THYROFORT 34CrMo4/34CrMoS4 Steel
THYROFORT 34CrNiMo6 Steel
THYROFORT 36CrNiMo4 Steel
THYROFORT 36NiCrMo16 Steel
THYROFORT 37Cr4/37CrS4 Steel
THYROFORT 37Cr4/37CrS4 Steel
THYROFORT 41Cr4/41CrS4 Steel
THYROFORT 42CrMo4/42CrMoS4 Steel
THYROFORT 46Cr2/46CrS2 Steel
THYROFORT 50CrMo4 Steel
THYROFORT C22E Steel
THYROFORT C45E Steel
THYROFORT C55E/C55R Steel
THYROFORT C60E/C60R Steel
THYROFORT Cf53 Steel
THYROFORT CrMoV9 Steel
THYROLL 2327 Steel
THYROLL 2362 Steel
THYROPLAST 2312 Steel
THYROPLAST 2764 Steel
THYROTHERM 2343 EFS/2343 EFS SUPRA Steel
THYROTHERM 2343 Steel
THYROTHERM 2344 Steel
TV4 Steel
Thermodur 2343 Superclean/Thermodur 2343 EFS Steel
Thermodur 2343 Superclean/Thermodur 2343 EFS Steel
Thermodur 2365 Superclean/Thermodur 2365 EFS Steel
Thermodur 2367 Superclean Steel
Thermodur 2367 Superclean/Thermodur 2367 EFS Steel
Thyrapid 3207 Steel
Thyrapid 3247 Steel
Thyrodur 2101 Steel
Thyrodur 2362 Steel
Thyrodur 2379 Steel
Thyrodur 2379 Steel
Thyrodur 2379 Steel
Thyrodur 2379 Steel
Thyrodur 2690 Steel
Thyrodur 2842 Steel
Thyroplast 2162 Steel
Thyroplast 2312 Steel
Thyroplast 2316 Steel
Thyrotherm 2343 Steel
Thyrotherm 2343 Steel
Thyrotherm 2343 Steel
Thyrotherm 2344 ESR Magnum Steel
Thyrotherm 2344 Steel
Thyrotherm 2344 Steel
Thyrotherm 2365 Steel
Thyrotherm 2365 Steel
Thyrotherm 2367 Steel
Thyrotherm 2367 Steel
Tyrapid 3343 Steel
Tyrapid 3343 Steel
Tyrodur 2762 Steel
Tyrodur 2762 Steel
Tyrodur 2762 Steel
Tyrotherm 2343 Steel
Tyrotherm 2344 Steel
UGINOX MA2 Steel
UGINOX MA3 Steel
UGINOX MA3 Steel
UGINOX MA4 Steel
UGINOX MA5M Steel
UK15 Steel
UR 2205 Steel
UR 2205Mo Steel
UR52N Steel
URANUS 45N Mo Steel
URANUS 52N
US Steel
USD-H Steel
UTOP2 Steel
UTOPMO1 Steel
UTOPMO2 Steel
UTOPMO4 Steel
UTOPMO4 Steel
UTOPMO7 Steel
UTOPMO7 Steel
UTOPN Steel
UTOPN Steel
UTOPN Steel
UTOPN Steel
UTOPN Steel
UTOPNIN Steel
Ugitech 2205 Steel
V-N Steel
VANADIS 30 Steel
VC140 Steel
VC140 Steel
VC140 Steel
VCMO125 Steel
VCMO125 Steel
VCMO135 Steel
VCMO135 Steel
VCMO140 Steel
VCMO150 Steel
VCMO150 Steel
VCMO150 Steel
VCMO150 Steel
VCMO230 Steel
VCMO230 Steel
VCMO230 Steel
VCNMO100 Steel
VCNMO100 Steel
VCNMO150 Steel
VCNMO150 Steel
VCV150 Steel
VCV150 Steel
VCV150 Steel
VCV150 Steel
VIDAR SUPERIOR Steel
VIDAR 1 ESR Steel
VIDAR SUPREME Steel
VM100 Steel
VM12-SHC Steel
VMB Steel
VMS135 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
Vanadis 23 SuperClean Steel
Vanadis 30 SuperClean Steel
Vanadis 60 SuperClean Steel
W1.2311 Steel
W1.2311 Steel
W1.2714 Steel
W1.2714 Steel
W1.2738 Steel
W44 Steel
Wrought 4340 Steel
X102CrMo17 Steel
X102CrMo17 Steel
X105CrMo17 Steel
X10CrAl7 Steel
X10CrAl7 Steel
X10CrMoVNb9-1 Steel
X10CrMoVNb91 (9% Cr-mod, P91/T91) Steel
X10CrNiNb18-9 Steel
X10CrWMoVNb9-2 Steel
X11CrMoWVNb9-1-1 Steel
X12CrMo7 Steel
X12CrMo9-1 Steel
X12CrMo9-1 Steel
X13T6 Steel
X153CrMoV12 Steel
X15TN Steel
X18CrNiMoVNb121 Steel
X20Cr13 Steel
X20CrMoV11-1 Steel
X20CrMoV12-1 Steel
X20CrMoV12-1 Steel
X20CrMoV12-1 Steel
X20CrMoWV12-1 Steel
X20CrMoWV12-1 Steel
X210Cr12 Steel
X210Cr12 Steel
X210Cr12 Steel
X210Cr12 Steel
X210CrW12 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X2CrNiMoN22-5-3 Steel
X30WCrV9-3 Steel
X30WCrV9-3 Steel
X32CrMoV33 Steel
X37CrMoV5-1 Steel
X37CrMoV5-1 Steel
X37CrMoV5-1/BH11 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X40Cr13 Steel
X40Cr13 Steel
X40Cr13 Steel
X40Cr13 Steel
X40CrMoV5-1 Steel
X40CrMoV5-1 Steel
X40CrSiMo10-2 Steel
X45Cr13 Steel
X45CrSi9-3 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X5CrNi18-9 Steel
X5CrNiCuNb16-4 Steel
X5CrNiCuNb16-4 Steel
X5CrNiMo17-13 Steel
X5CrNiMo17-13 Steel
X5CrNiMo17-13 Steel
X5CrNiMoCuNb14-5 Steel
X82WMoCrV6-5-4 Steel
X82WMoCrV6-5-4 Steel
X8Ni9 Steel
X90CrMoV18 Steel
XC 32 Steel
XC 38 Steel
XC 38 Steel
XC 38 Steel
XC 42 Steel
XC 42 Steel
XC 48 Steel
XC 55 Steel
XC 55 Steel
XC 70 Steel
XC 70 Steel
XD15NW Steel
Xl2CrMo7 Steel
Y1 90 Steel
Z 100 CDV 5 Steel
Z 12 C 13 Steel
Z 120 M 12 Steel
Z 130 WDCV 06-05-04-04 Steel
Z 160 CDV 12 Steel
Z 20 CDNbV 11 Steel
Z 200 C 12 Steel
Z 30 WCV 9 Steel
Z 38 CDV 5 Steel
Z 38 CDV 5 Steel
Z 40 C 14 Steel
Z 40 C 14 Steel
Z 40 CSD 10 Steel
Z 85 WDKCV 06-05-05-04-02 Steel
Zeron100 Alloy