Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTA Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
Alphabetical Index
0.0021C-0.25Nb Steel
0.0021C-0.75Nb Steel
0.003C-0.004Si-0.51Mn-0.002Cr-0.001Mo-0.017Ni Steel
0.005C Steel
0.010C-0.011N-0.11Ti Steel
0.01C-0.15Mn Steel
0.01C-0.30Si Steel
0.01C-0.50Mn Steel
0.01C-0.60Si Steel
0.01C-0.90Mn Steel
0.01C-1.0Si Steel
0.01C-1.35Mn Steel
0.01C-1.75Mn Steel
0.01C-1.75Mn Steel
0.025C Steel
0.02C-3.5Ni-3.6Mo Steel
0.032C-2.02Mn-7.23Ni Steel
0.032C-7.23Ni-2.02Mn Steel
0.037C-0.61Si-0.68Nb Steel
0.038C-0.25Si-1.43Mn-17.50Cr-12.81Ni-4.60Mo-0.55Nb Steel
0.03C-0.10Mn-29.50Co-17.76W Steel
0.03C-0.15Mn Steel
0.03C-0.17Si-1.49Mn-0.1Nb-0.26Cu-0.15Ni Steel
0.03C-1.78Mn-0.26Cu-0.17Ni-0.29Cr Steel
0.03C-2Mn-7Ni Weld Steel
0.041V-0.0074N Steel
0.043C-0.24Si-1.57Mn-17.44Cr-12.89Ni-4.55Mo-2.05Nb Steel
0.044C-0.18Si-1.66Mn-16.67Cr-12.67Ni-2.50Mo Steel
0.044C-0.38Si-1.65Mn-16.55Cr-12.86Ni-2.00Mo-0.86Nb Steel
0.049C-0.795Si-1.235Mn Steel
0.04C-0.026Si-0.31Mn-0.02Cr-0.01Mo-0.02Ni-0.005V Steel
0.04C-0.2Si-2.94Mn Steel I
0.04C-0.2Si-2.94Mn Steel II
0.04C-0.2Si-2.95Mn Steel III
0.04C-V-Mo Steel
0.04C-V-Mo Steel
0.04C-V-Mo Steel
0.04C-V-Mo Steel
0.04C-Vanadium Steel
0.05-0.10Mn Steel
0.053Cr-2.32Si-0.23Mn-0.32Cr Steel
0.054C-0.14Si-1.51Mn-0.16Cr-0.87Ni-0.99Cu Steel
0.054C-1.27Si-0.23Mn-9.05Cr Steel
0.056Nb, 0.057Nb + 0.23 Mo Steels
0.059C-1.96Si-2.88Mn Steel
0.059C-1.96Si-2.88Mn Steel
0.05Al-550 TRIP Steel
0.05Al-550 TRIP Steel
0.05C, 0.10C, 0.15C Boron Steels
0.05C-0.04Nb Steel
0.05C-0.05Si-1.56Mn-0.06Nb Steel
0.05C-0.13Si-0.17Mn-1.85Cr-29.30Co-17.21W Steel
0.05C-0.13Si-0.17Mn-2.76Cr-29.10Co-17.33W Steel
0.05C-0.25Si-1.92Mn-0.067(Nb+Ti) Steel
0.05C-0.3Si-1.5Mn Steel
0.05C-0.50Mn Steel
0.05C-0.90Mn-1.20Si-0.40Mo Steel
0.05C-1.5Mn-0.25Mo-0.1Cr Steel
0.05C-1.70Mn-0.10Nb-0.10Mo-0.25Cr Steel
0.05C-1.7Mn-0.10Nb-0.10Mo-0.25Cr Steel
0.05C-17Cr-13Ni-5Mo Alloy
0.05C-17Cr-13Ni-5Mo with 0.039% N Steel
0.05C-17Cr-13Ni-5Mo with 0.145% N Steel
0.05C-17Cr-13Ni-5Mo-0.039N Steel
0.05C-2Mn Steel
0.05C-V-Ti Steel
0.05C-Vanadium Steel
0.06%C-1.20Mn-0.0062-Nb-0.053V Steel
0.0637C-0.747Si-1.30Mn Steel
0.0657C-0.66Si-1.36Mn Steel
0.065C-0.559Si-1.144Mn Steel
0.065C-0.87Si-1.19Mn-0.61Cr-0.38Mo Steel
0.069C-0.64Si-1.61Mn Steel
0.069C-0.64Si-1.61Mn Steel
0.06C Steel
0.06C Steel
0.06C-0.04Ti-0.10Nb Steel
0.06C-0.27Si-1.53Mn-0.28Mo-0.018Ti-0.064V-0.0144N-0.0012B Steel
0.06C-0.27Si-1.84Mn-0.02Mo Steel
0.06C-0.30Si-0.39Mn-0.61Mo-0.03Cu-0.01N Steel
0.06C-0.45V Steel
0.06C-0.45V Steel
0.06C-1.45Mn-1.25Cu-0.97Ni-0.72Cr-0.42Mo Steel
0.06C-Mn-Cu-Ni-Mo-Nb-Ti Steel
0.06C-V Steel
0.06C-V Steel
0.06C-V Steel
0.06C-V-Mo Steel
0.06C-V-Mo Steel
0.06C-V-Mo Steel Steel
0.06C-V-Nb-Mo Steel
0.06C-V-Nb-Mo Steel
0.06C-V-Ti Steel
0.06C-Vanadium-Niobium Steel
0.06C-Vanadium-Niobium Steel
0.072C-0.15Si-1.00Mn-0.40Cr-0.029Al Steel
0.072C-0.21Si-0.42Mn-2.38Cr-0.12Ni-0.20Mo-1.50W-0.20V Steel
0.074C-0.16Si-1.00Mn-0.40Cr-0.85Al Steel
0.076C Steel
0.076C-1.17Si-1.86Mn Steel
0.0774C-0.666Si-1.21Mn Steel
0.077V - 0.01N Steel
0.079C-1.39Mn-0.20Si-0.002Al-0.012Ti Steel
0.079V-0.0076N Steel
0.07C-0.25Si-1.75Mn-0.03Cr-1.00Mo-0.18Mo-0.02Cu Steel
0.07C-0.26Si-1.39Mn-0.019Al-0.021Ti Steel
0.07C-0.45V Steel
0.07C-0.45V Steel
0.07C-1.08Mn-0.09Si-0.19Mo-0.040Nb-0.014Ti Steel
0.07C-1.61Mn-0.32Si-0.22Mo-0.052Nb-0.012Ti Steel
0.07C-V-Mo Steel
0.07C-V-Mo Steel
0.07C-V-N Steel
0.07C-V-Nb-Mo Steel
0.07C-Vanadium Steel
0.07C-Vanadium-Niobium Steel
0.07N Steel
0.080C-0.04Si-1.46Mn-0.25V Steel
0.080C-0.40Si-1.42Mn Steel
0.081C-0.10Si-1.74Mn-0.18Ti Steel
0.081C-0.22Si-0.98Mn Steel
0.081V-0.014N Steel
0.085C-0.72Si-1.219Mn Steel
0.086C-0.22Si-1.01Mn Steel
0.08C-0.13Si-0.26Mn-2.93Cr Steel
0.08C-0.16Si-0.38Mn-11.94Cr-0.53Mo-0.44Ni-0.0035B Steel
0.08C-0.21Si-0.53Mn-2.44Cr-0.95Mo Steel
0.08C-0.40Si-0.80Mn-0.30Cr-0.20Ni-0.10Ti-0.20Cu Steel
0.08C-0.40Si-1.50Mn-0.30Cr-0.20Ni-0.10Ti-0.20Cu Steel
0.08C-0.60Si-1.70Mn Steel
0.08C-0.60Si-1.70Mn Steel
0.08C-0.65Si-1.93Mn Steel
0.08C-0.70Si-1.92Mn Steel
0.08C-0.81Si-1.47Mn-0.03Al Steel
0.08C-1.0Mn-0.2Si-0.8Al Steel
0.08C-1.0Mn-0.8Si-0.8Al Steel
0.08C-1.0Ni-12.0Cr-2.0Mo-0.3V Steel
0.08C-1.0Ni-12.0Cr-2.0Mo-0.3V Steel
0.08C-1.46Mn-0.25V-0.018N Steel
0.08C-1.55Mn-0.41Si-0.18Mo-0.031Nb-0.013Ti Steel
0.08C-1.55Mn-0.51Si-0.18Mo-0.031Nb-0.013Ti Steel
0.08C-2.44Cr-0.95Mo-0.26V Steel
0.08C-2.9Cr Steel
0.08C-9Ni Steel
0.08C-V Steel
0.08C-Vanadium-Niobium Steel
0.091C-0.40Si-1.36Mn Steel
0.092C-1.18Si-1.81Mn Steel
0.094C-0.30Si-1.32Mn Steel
0.094C-0.30Si-1.32Mn Steel
0.096C-0.66Si-1.90Mn Steel
0.09C-0.26Si-0.44Mn-2.25Cr-0.99Mo Steel
0.09C-0.31Si-0.95Mn-1.72Ni Steel
0.09C-0.32Si-0.92Mn-0.85Cr-0.35Mo-2.09Ni Steel
0.09C-0.45Si-0.87Mn Steel
0.09C-0.60Si-0.47Mn-1.14Cr-0.57Mo Steel
0.09C-0.60Si-0.47Mn-1.14Cr-0.57Mo Steel
0.09C-0.60Si-0.47Mn-1.14Cr-0.57Mo Steel
0.09C-0.68Si-1.90Mn Steel
0.09C-0.73Si-2.08Mn Steel
0.09C-V Steel
0.09C-V Steel
0.09C-V Steel
0.09C-V Steel
0.09C-V-Nb-Mo Steel
0.09C-Vanadium Steel
0.09C-1.48Mn-0.25Si-0.01Cr-0.01Ni-0.01Mo Steel
0.105C-0.0035Si Steel
0.10C-0.06Si-1.97Mn Steel
0.10C-0.06Si-1.97Mn-0.014Al-0.0011N Steel
0.10C-0.30Si Steel
0.10C-0.3Si-1.45Mn-0.028Nb Steel
0.10C-0.40Si-0.65Mn-0.60Cr-0.30Mo Steel
0.10C-0.54Si-1.42Mn Steel
0.10C-0.65Si-1.17Mn Steel
0.10C-0.68Si-1.24Mn-1.87Cr Steel
0.10C-0.70Mn-0.30Si Steel
0.10C-0.70Mn-0.30Si-0.28Mo Steel
0.10C-0.70Mn-0.30Si-0.30Mo-B Steel
0.10C-0.70Mn-0.30Si-0.30Ni-0.24Mo-B Steel
0.10C-0.70Mn-0.30Si-0.30Ni-0.53Mo-B Steel
0.10C-0.70Mn-0.30Si-0.30Ni-B Steel
0.10C-0.70Mn-0.30Si-0.50Mo-B Steel
0.10C-0.70Mn-0.30Si-0.54Mo Steel
0.10C-0.70Mn-0.30Si-1.40Ni-0.26Mo-B Steel
0.10C-0.70Mn-0.30Si-1.40Ni-0.51Mo-B Steel
0.10C-0.70Mn-0.30Si-1.40Ni-B Steel
0.10C-0.70Mn-0.30Si-3.00Ni-0.24Mo-B Steel
0.10C-0.70Mn-0.30Si-3.00Ni-0.55Mo-B Steel
0.10C-0.70Mn-0.30Si-3.00Ni-B Steel
0.10C-0.70Mn-0.30Si-B Steel
0.10C-0.72Si-2.02Mn Steel
0.10C-0.7Mn-0.3Si-0.3Cr-0.25Mo-B Steel
0.10C-0.7Mn-0.3Si-0.3Cr-0.50Mo-B Steel
0.10C-0.7Mn-0.3Si-0.3Cr-B Steel
0.10C-0.7Mn-0.3Si-0.7Cr-0.22Mo-B Steel
0.10C-0.7Mn-0.3Si-0.7Cr-0.51Mo-B Steel
0.10C-0.7Mn-0.3Si-0.7Cr-B Steel
0.10C-0.7Mn-0.3Si-1.4Cr-0.25Mo-B Steel
0.10C-0.7Mn-0.3Si-1.4Cr-0.56Mo-B Steel
0.10C-0.7Mn-0.3Si-1.4Cr-1.03Mo-B Steel
0.10C-0.7Mn-0.3Si-1.4Cr-B Steel
0.10C-1.0Si Steel
0.10C-1.40Mn-0.30Si-0.26Mo-B Steel
0.10C-1.40Mn-0.30Si-0.52Mo-B Steel
0.10C-1.40Mn-0.30Si-B Steel
0.10C-1.63Mn-0.41Mo Weld Metal Steel
0.10C-V Steel
0.10C-V Steel
0.10C-V-Nb-Ti Steel
0.10C-V-Ti Steel
0.10C-Vanadium-Niobium Steel
0.10C-Vanadium-Niobium Steel
0.11C-0.01Ti-0.05Nb Steel
0.11C-0.25Si-0.59Mn-0.74Mo Steel
0.11C-0.31Si-0.62Mn-13.24Cr-0.15Ni Steel
0.11C-0.34Si-1.21Mn-0.20Cr-0.15Mo-0.45Ni Steel
0.11C-0.34Si-1.21Mn-0.45Ni-0.20Cr-0.15Mo Steel
0.11C-0.40Si-1.60Mn-0.13Ti Steel
0.11C-0.44Si-0.38Mn-5.46Cr-0.42Mo Steel
0.11C-0.68Si-1.24Mn Steel
0.11C-0.70Si-1.27Mn Steel
0.11C-0.70Si-1.27Mn Steel
0.11C-0.74Mo Steel
0.11C-0.85Mn-0.4Si-1.4Ni-0.7Cr-0.21Mo-B Steel
0.11C-0.85Mn-0.4Si-1.4Ni-0.7Cr-0.54Mo-B Steel
0.11C-0.85Mn-0.4Si-1.4Ni-0.7Cr-B Steel
0.11C-5.00Ni-0.55Cr-0.47Mo-0.075V Steel
0.11C-V Steel
0.11C-V Steel
0.11C-V Steel
0.11C-V Steel
0.11C-Vanadium Steel
0.11C-Vanadium Steel
0.11C-Vanadium Steel
0.11C-Vanadium-Niobium Steel
0.11C-0.45Mn Steel
0.12C Steel
0.12C-0.13Mo Steel
0.12C-0.16Si-0.70Mn-0.60Cr-0.65Mo Steel
0.12C-0.22Si-0.60Mn-0.49Mo Steel
0.12C-0.25Si-0.63Mn-0.31Mo Steel
0.12C-0.26Si-0.65Mn Steel
0.12C-0.27Si-0.61Mn-0.13Mo Steel
0.12C-0.30Si-0.83Mn-0.53Cr-0.49Mo-1.11Ni Steel
0.12C-0.30Si-0.83Mn-0.53Cr-0.49Mo-1.11Ni Steel
0.12C-0.30Si-0.83Mn-0.53Cr-1.11Ni-0.49Mo-0.03V Steel
0.12C-0.30Si-0.83Mn-0.53Cr-1.11Ni-0.49Mo-0.03V Steel
0.12C-0.30Si-0.84Mn-0.53Cr-1.11Ni-0.47Mo Steel
0.12C-0.34Si-0.80Mn-0.44Cr-0.32Mo-1.20Ni Steel
0.12C-0.34Si-0.80Mn-1.20Ni-0.44Cr-0.32Mo Steel
0.12C-0.39Mn-1.87Ni-1.05Cu Steel
0.12C-0.3Mo Steel
0.12C-0.5Mo Steel
0.12C-0.6Cr-0.65Mo Steel
0.12C-0.74Si-0.79Mn-0.18S-12.82Cr-0.05Mo-0.25Ni Steel
0.12C-0.85Mn-0.3Si-1.4Ni-0.7Cr Steel
0.12C-0.85Mn-0.3Si-1.4Ni-0.7Cr-0.19Mo Steel
0.12C-0.85Mn-0.3Si-1.4Ni-0.7Cr-0.45Mo Steel
0.12C-1.9Ni-1Cu Steel
0.12C-13Cr Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V Steel
0.12C-V-Mo Steel
0.12C-V-Nb-Mo Steel
0.12C-2.03Si-2.96Mn Steel
0.12C-9Cr-2W ODS Martensitic Steel
0.12V-0.0082N Steel
0.13C-0.16Mn-1.76Cr-0.49Mo-3.08Ni Steel
0.13C-0.41Si-1.06Mn-0.26Cr-1.22Ni-0.33Mo-0.02Nb Steel
0.13C-0.78Mn Steel
0.13C-1.5Cr-1.55Ni Steel
0.13C-1.5Cr-1.55Ni Steel
0.13C-2.99Cr Steel
0.13C-3Ni-1.76Cr-0.5Mo Steel
0.13C-V Steel
0.13C-V Steel
0.13C-V Steel
0.13C-V Steel
0.142C-1.577Mn-0.011Nb Steel
0.142C-1.577Mn-0.011Nb Steel
0.143C-1.599Mn-0.001Nb Steel
0.149C-1.607Mn-0.001Nb Steel
0.149C-1.607Mn-0.026Nb Steel
0.149C-1.607Mn-0.026Nb Steel
0.14C-0.26Mn-1.05Cr-0.26Mo-2.21Ni Steel
0.14C-0.3Cr-1.2Mn-0.5Si-0.002B Steel
0.14C-0.43Si-1.13Mn-0.18Cr Steel
0.14C-04Si-0.84Mn-0.048Nb Steel
0.14C-2.2Ni-1Cr-0.26Mo Steel
0.14C-2.43Cr-1.07Mo Steel
0.14C-V Steel
0.14C-V Steel
0.14C-V Steel
0.14C-V-Nb-Mo Steel
0.14C-Vanadium Steel
0.14C-Vanadium Steel
0.14C-0.74Mn Steel
0.14C-1.0Mn Steel
0.154C-0.022Si-1.10Mn-0.050Cr Steel
0.15C Steel
0.15C Steel
0.15C Steel
0.15C-0.10Mn Steel
0.15C-0.12Si-0.24Mn-2.91Cr Steel
0.15C-0.25Si-1.6Mn-0.2Mo Steel
0.15C-0.40Mn Steel
0.15C-0.40Mn Steel
0.15C-0.45Si-1.27Mn Steel
0.15C-0.45Si-1.27Mn-0.07Ni-0.05Cr-0.02Mo Steel
0.15C-0.5Mn Steel
0.15C-0.60Si-0.80Mn Steel
0.15C-1.0Si-2.0Mn Steel
0.15C-1.2Cr-0.25Ni-0.3V Steel
0.15C-1.50Si-0.50Mo-2.00Ni Steel
0.15C-1.50Si-2.00Ni Steel
0.15C-1Cr-0.9Mo-0.2V Steel
0.15C-2.0Mn Steel
0.15C-2.9Cr Steel
0.15C-4Ni-1.5Cr Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V Steel
0.15C-V-Mo Steel
0.15C-V-Ni Steel
0.15C-Vanadium Steel
0.15C-Vanadium Steel
0.16C-0.24Si-0.90Mn-0.31Cr-0.40Mo-0.27Nb Steel
0.16C-0.34Si-1.50Mn-0.035Nb-0.004V-0.015Ti Steel
0.16C-0.34Si-1.50Mn-0.035Nb-0.015Ti-0.037Al Steel
0.16C-0.57Si-2.14Mn-0.12Cr-0.06Mo-0.02Al Steel
0.16C-0.92Ni, 0.12C-1.86Ni Steels
0.16C-0.92Ni, 0.12C-1.86Ni Steels
0.16C-1.45Mn-1.48Cr-0.81Ni-0.41Mo Steel
0.16C-1.45Mn-1.48Cr-0.81Ni-0.41Mo-0.017B Steel
0.16C-1.45Mn-1.48Mo-0.81Ni-0.41Mo with B Steel
0.16C-1.45Mn-1.48Mo-0.81Ni-0.41Mo without B Steel
0.16C-V Steel
0.16C-V Steel
0.16C-V-N Steel
0.16C-Vanadium Steel
0.16C-Vanadium Steel
0.16C-Vanadium Steel
0.17C-0.03Cr-0.03Nb Steel
0.17C-0.20Si-1.81Mn-0.15(Nb+V+Ti) Steel
0.17C-0.21Si-1.35Mn-0.019Nb-0.50Ni-0.001B Steel
0.17C-0.24Si-1.19Mn-0.10Ni Steel
0.17C-0.24Si-1.46Mn-0.04Cr-0.76Ni-0.53Mo Steel
0.17C-0.27Si-1.21Mn-0.13Ni Steel
0.17C-0.33Si-1.37Mn-0.66Cr-0.77Ni Steel
0.17C-0.33Si-1.37Mn-0.77Ni-0.66Cr Steel
0.17C-1.00Si-1.87Mn-0.22Mo-0.031Ti-0.022V Steel
0.17C-1.37Mn-0.66Cr Steel
0.17C-1.46Mn-0.15Si Steel
0.17C-1.65Mn-1.0Ni Steel
0.17C-1.6Mn-0.2Mo Steel
0.17C-V Steel
0.17C-V Steel
0.17C-V-Mo Steel
0.17C-V-N Steel
0.17C-V-N Steel
0.18C Carbon Steel
0.18C-0.036Si-1.21Mn Steel
0.18C-0.34Si-0.87Mn-0.28Cr-0.38Mo Steel
0.18C-0.34Si-0.87Mn-0.28Cr-0.38Mo-0.93Cu Steel
0.18C-0.35Si-1.6Mn-0.01P-0.008S-0.006N Steel
0.18C-1.1Ni-0.26Mo Steel
0.18C-1.80Mn-0.33Si-0.43Cr-0.015Mo Steel
0.18C-1Ni Steel
0.18C-V Steel
0.18C-V-Cr-Mo-Ni Steel
0.18C-V-Nb-Mo Steel
0.19C-0.71Mn-1.80Ni-0.97Cu Steel
0.19C-1.37Mn-0.56Ni-0.2Cr-0.31Mo Steel
0.19C-1.46Si-2.96Mn Steel
0.19C-1.50Mn-1.20Cr-2.50Ni-0.35Mo Steel
0.19C-1.64Mn Steel
0.19C-1.81Mo Steel
0.19C-2.146Si-2.96Mn-0.04Al Steel
0.19C-V-N Steel
0.19C-Vanadium Steel
0.1C-0.19Si-1.1Mn, 0.14C-0.22Si-1.81Mn Steels
0.1C-0.1C-Mo-0.1C-Cr-0.1C-Mo-Cr Steels
0.1C-0.24Mn-B Steel
0.1C-0.24Mn-B Steel
0.1C-0.39Mo-B Steel
0.1C-0.39Mo-B Steel
0.1C-0.66Mo-B Steel
0.1C-0.66Mo-B Steel
0.1C-13.0Cr Steel
0.1C-13.0Cr Steel
0.1C-13.0Cr Steel
0.1C-13.0Cr Steel
0.1C-13.0Cr Steel
0.1C-13.0Cr Steel
0.1C-13.0Cr Steel
0.1C-5.5Cr-0.4Mo Steel
0.2% C Carbon Steel
0.20C-0.04Si-4.49Mn-1.30Al Steel
0.20C-0.17Si-0.25Mn-3.02Cr Steel
0.20C-0.28Si-1.25Mn-0.15Cr Steel
0.20C-0.28Si-1.25Mn-25 ppm B Steel
0.20C-0.30Si-0.70Mn Steel
0.20C-0.30Si-1.75Mn Steel
0.20C-0.36Si-1.60Mn-0.025Cr-0.056V-0.064Nb Steel
0.20C-0.6Mn-0.3Si-3.0Ni-0.004Mo Steel
0.20C-0.6Mn-0.3Si-3.0Ni-0.25Mo Steel
0.20C-0.6Mn-0.3Si-3.0Ni-0.51Mo Steel
0.20C-0.78Mn-0.60Cr-0.16Mo-0.52Ni Steel
0.20C-0.78Mn-0.60Cr-0.52Ni-0.16Mo Steel
0.20C-1.0Si-0.05Mn Steel
0.20C-1.0Si-0.70Mn Steel
0.20C-1.0Si-1.60Mn Steel
0.20C-1.44Mn-0.49Ni-0.16V Steel
0.20C-1.50Si-3.50Mn Steel
0.20C-V Steel
0.20C-V Steel
0.20C-V Steel
0.20C-V Steel
0.20C-Vanadium Steel
0.20C-Vanadium Steel
0.20C-1.65Mn-1.40Si-1.50Al-1.30Cu-1.05Ni-1.07Co Steel
0.21C-1.80Si-1.40Mn-0.07Ni-0.02Mo-0.002Nb Steel
0.21C-V Steel
0.21C-V-N Steel
0.22C Steel
0.22C Steel
0.22C Steel
0.22C-0.24Si-0.83Mn-0.54Cr-0.51Mo-1.06Ni Steel
0.22C-0.24Si-0.83Mn-0.54Cr-0.51Mo-1.06Ni Steel
0.22C-0.24Si-0.83Mn-0.54Cr-1.05Ni-0.51Mo-0.02V Steel
0.22C-0.24Si-0.83Mn-0.54Cr-1.05Ni-0.51Mo-0.02V Steel
0.22C-0.24Si-0.83Mn-0.54Cr-1.06Ni-0.51Mo Steel
0.22C-0.24Si-0.83Mn-0.54Cr-1.06Ni-0.51Mo Steel
0.22C-0.24Si-0.83Mn-0.54Cr-1.06Ni-0.51Mo Steel
0.22C-0.24Si-0.85Mn-0.54Cr-0.51Mo-1.05Ni Steel
0.22C-0.24Si-0.85Mn-0.54Cr-0.51Mo-1.05Ni Steel
0.22C-0.25Si-0.64Mn-0.97Cr-0.33Ni-0.23Mo Steel
0.22C-0.28Si-1.17Mn-0.0022B Steel
0.22C-0.28Si-1.17Mn-0.0022B Steel
0.22C-0.35Si-0.86Mn-0.02Nb-0.072Ti Steel
0.22C-0.35Si-0.86Mn-0.072Ti Steel
0.22C-0.35Si-1.54Mn-0.014P-0.036S-0.11Mo-0.11V-0.011N Steel
0.22C-0.47Si-2.50Mn-0.41Cr-0.020Nb Steel
0.22C-0.5Mo Steel
0.22C-0.79Mn-0.50Mo Steel
0.22C-0.79Mn-0.50Mo Steel
0.22C-0.79Mn-0.50Mo Steel
0.22C-0.79Mn-0.50Mo Steel
0.22C-0.97Cr-0.33Ni Steel
0.22C-0.97Cr-0.33Ni Steel
0.22C-0.98Cr-0.23Mo Steel
0.22C-0.98Cr-0.23Mo Steel
0.22C-1.20Mn-0.15Cr-0.002B Steel
0.22C-1.20Mn-1.50Si-0.23Cr-0.0027B Steel
0.22C-1.80Si-2.0Mn-1.0Cr-0.25V-0.50Al Steel I
0.22C-1.80Si-2.0Mn-1.0Cr-0.25V-0.50Al Steel II
0.22C-2Mn Steel
0.22C-2Mn Steel
0.22C-V Steel
0.22C-V Steel
0.22C-1.80Si-2.00Mn-1.00Cr-0.25Mo-0.50Al Steel
0.23C-0.0021B Steel
0.23C-0.24Si-0.35Mn-1.46Cr-4.15Ni-0.88W Steel
0.23C-0.82Mn-1.22Cr-0.53Mo-0.22V Steel
0.23C-1.2Cr-0.5Mo-0.22V Steel
0.23C-V Steel
0.23C-V Steel
0.23C-V-Cr Steel
0.24C-0.22Si-1.14Mn-0.17Cr-0.003B Steel
0.24C-0.69Mn-0.50Mo-3.35Ni-0.09V Steel
0.24C-0.79Cr-0.18Ni Steel
0.24C-0.79Cr-0.18Ni Steel
0.24C-1.55Mn-0.87Si-0.40Al Steel
0.24C-1.67Mn-0.22Mo Steel
0.24C-1.67Mn-0.22Mo Steel
0.24C-2.0Si-1.6Mn-0.5Cr-0.2Mo-0.2V-0.0003B Steel
0.24C-2.0Si-1.6Mn-0.5Cr-0.2Mo-0.2V-0.0003B Steel
0.24C-Mn-Mo-V Steel
0.24C-V Steel
0.24C-V-Cr-Mo-Ni Steel
0.24C-V-Cr-Mo-Ni Steel
0.24C-V-Cr-Mo-Ni Steel
0.24C-V-Cr-Mo-Ni Steel
0.24C-V-Cr-Mo-Ni Steel
0.25C, 0.32C, 0.40C, 0.74C Steels
0.25C-0.25Si-1.55Mn-0.009Cr-0.002Ni-0.004Ti-0.027W Steel
0.25C-0.40Mn Steel
0.25C-0.6Ni-0.7Cr-0.9Mo-0.23V Steel
0.25C-0.88Mn-0.73Cr-0.88Mo-0.59Ni-0.23V Steel
0.25C-1.0Si-1.5Mn-0.6Cr-0.0005B Steel
0.25C-1.0Si-1.5Mn-0.6Cr-0.0005B Steel
0.25C-1.2Si-2.0Mn-0.2Cr (+Nb, B, Ti) Steel
0.25C-1.2Si-2.0Mn-0.2Cr-0.08Mo (+Nb, B, Ti) Steel
0.25C-1.5Mn-1.2Si-1.5Ni-0.05Nb Steel
0.25C-1.5Mn-1.2Si-1.5Ni-0.05Nb Steel
0.25C-1.5Si-3Mn Steel
0.25C-1.80Ni-1.50Si-0.40Mo Steel
0.25C-1.8Ni-0.4Mo Steel
0.25C-3.3Ni-1.1Cr-0.65Mo-0.16V Steel
0.25C-6.60Ni Weld Steel
0.25C-6.60Ni Weld Steel
0.26% C-V-Cr-Mo-Ni Steel
0.26C-0.23Si-0.31Mn-3.11Cr Steel
0.26C-0.3Ni-5Cr-0.5Mo Steel
0.26C-0.42Si-1.51Mn-0.45Cr-0.50Mo Steel
0.26C-0.57Mn-0.48Mo-2.20Ni-0.09V Steel
0.26C-0.62Mn-5.17Cr-0.46Mo-0.32Ni Steel
0.26C-0.62Mn-5.17Cr-0.46Mo-0.32Ni Steel
0.26C-0.94Si-1.14Mn-1.76Cr-2.15Ni-0.37Mo Steel
0.26C-1.5Mn-0.45Cr-0.5Mo Steel
0.26C-2.2Ni-0.5Mo-0.09V Steel
0.26C-3.34Cr-0.54Mo Steel
0.26C-3Cr Steel
0.26C-V Steel
0.26C-V Steel
0.27C Steel
0.27C-0.25Si-0.86Mn-0.71Mo Steel
0.27C-0.26Si-0.53Mn-0.71Cr-0.18Mo-3.38Ni Steel
0.27C-0.6Ni-0.7Cr-0.9Mo-0.11V Steel
0.27C-0.84Mn-0.73Cr-0.90Mo-0.60Ni-0.11V Steel
0.27C-1.17Mn-0.31Si-0.48Cr-0.0012B Steel
0.27C-1.17Mn-0.31Si-0.48Cr-0.0012B Steel
0.27C-1.17Mn-0.31Si-0.48Cr-0.0012B Steel
0.27C-1.17Mn-0.31Si-0.48Cr-0.0012B Steel
0.27C-1.67Si-0.80Mn Steel
0.27C-1Cr Steel
0.27C-1Cr Steel
0.27C-1Cr Steel
0.27C-2.0Si-0.9Mn-0.7Cr-0.0015B Steel
0.27C-2.0Si-0.9Mn-0.7Cr-0.0015B Steel
0.27C-2.0Si-0.9Mn-0.7Cr-0.0015B Steel
0.27C-2.20Si-2.80Mn-0.75Cr-0.50Al-0.001B Steel
0.27C-3.4Ni-0.7Cr-0.18Mo Steel
0.27C-V Steel
0.27C-V Steel
0.27C-V-Cr-Mo-Ni Steel
0.28C-0.29Si-1.40Mn-0.26Cr-0.003B Steel
0.28C-0.41Si-0.49Mn-1.00Cr-0.41Mo Steel
0.28C-0.47Si-0.70Mn-5.25Cr-0.62Mo Steel
0.28C-1.0Cr-0.4Mo Steel
0.28C-1.41Mn-0.29Si-0.26Cr-0.11Ni-0.22Mo-0.027Nb Steel
0.28C-1.41Mn-0.29Si-0.26Cr-0.22Mo Steel
0.28C-3.3Ni Steel
0.28C-3.3Ni Steel
0.28C-3.8Ni Steel
0.28C-5Cr-0.6Mo Steel
0.28C-V Steel
0.28C-V-Cr Steel
0.28C-1.4Si-0.67Mn-1.49Cr-0.56Mo Steel
0.29C-0.13Si-0.15Mn-7.61Ni Steel
0.29C-0.21Mn-1.45Cr-3.25Ni Steel
0.29C-0.24Si-1.64Mn-0.45Mo Steel
0.29C-0.34Si-0.50Mn-2.40Cr-0.34Mo Steel
0.29C-0.40Si-0.49Mn-1.49Cr-0.41Mo Steel
0.29C-1.11Si-1.70Mn-0.13Mo-0.10Ni Steel
0.29C-1.28Mn-0.34Si-0.09V-0.019Ti Steel
0.29C-1.34Mn-0.26Si-0.10V-0.003Ti Steel
0.29C-1.5Cr-0.4Mo Steel
0.29C-1.64Mn-0.45Mo Steel
0.29C-1.67Mn Steel
0.2C Steel
0.2C-0.38Mo-B Steel
0.2C-0.38Mo-B Steel
0.2C-0.83Mn, 0.2C-2Mn Steels
0.2C-0.8Mn-0.5Mo Steel
0.2C-1.0Mn-0.1Mn Steel
0.2C-1.2Mn-1Cu-0.6Ni Steel
0.2C-1.5Mn-0.5Ni-0.16V Steel
0.2C-1.60/2.82/3.92Mn-1.6Si Steel
0.2C-1.8Ni-1Cu Steel
0.2C-12Cr-1Mo Steel
0.2C-1Mn-1Cu-0.25Mo-0.8Ni Steel
0.2C-1Mn-1Cu-0.25Mo-0.8Ni Steel
0.2C-1V Steel
0.2C-3.35Ni-0.5Mo-0.09V Steel
0.2C-3Cr Steel
0.2C-5Cr Steel
0.2C-1.5Si-1.5Mn Steel
0.2C-Si-Mn-Nb Steel
0.30C-0.30Mn-3.64Ni-l.63Cr-0.49Mo Steel
0.30C-0.40Mn Steel
0.30C-0.41Si-0.49Mn-0.51Cr-0.41Mo Steel
0.30C-0.48Si-1.53Cr-0.20Ni-0.12V Steel
0.30C-0.49Si-1.63Mn-0.44Cr-0.33Mo Steel
0.30C-0.55Mn-3.34Ni Steel
0.30C-0.7Mn-0.4Si-Ni-Cr-0.24Mo Steel
0.30C-0.7Mn-0.4Si-Ni-Cr-0.43Mo Steel
0.30C-0.7Mn-0.4Si-Ni-Cr-0.57Mo Steel
0.30C-0.80Mn Steel
0.30C-0.95Cr-0.20Mo Steel
0.30C-1.4Si-1.9Mn-0.5Cr Steel
0.30C-1.4Si-1.9Mn-0.5Cr Steel
0.30C-1.52Mn-0.66Cr-0.55Mo-1.11Ni Steel
0.30C-1.54Mn-2.05Cr-0.43Mo-0.97Ni Steel
0.30C-2.02Mn-0.66Cr-0.55Mo-1.11Ni Steel
0.30C-2.0Mn Steel
0.30C-2.50Mn-2.05Cr-0.43Mo-0.97Ni Steel
0.30C-O.30Mn-3.64Ni-1.63Cr-O.49Mo Steel
0.30C-O.30Mn-3.64Ni-1.63Cr-O.49Mo Steel
0.30C-V-Mo Steel
0.30Cu-0.36Si-0.60Mn-2.04Cr-0.33Mo Steel
0.31C-0.20Si-0.44Mn-1.26Cr-0.47Mo-3.40Ni Steel
0.31C-0.26Si-0.46Mn-2.08Cr-0.48Mo-0.26Ni Steel
0.31C-1.22Mn-0.10Ni-0.25Si Steel
0.31C-2.02Mn-0.66Cr-0.55Mo-1.11Ni Steel
0.31C-2.02Mn-0.66Cr-0.55Mo-1.80Ni Steel
0.31C-2.6Ni-0.64Cr-0.58Mo Steel
0.31C-3.4Ni-1.26Cr-0.47Mo Steel
0.31C-V-Mo Steel
0.322C-2.52Si-0.43Mn-0.020Sn-0.045Mg Cast Iron
0.32C-0.20Si-0.30Mn-0.69Cr-2.95Ni-0.10Mo-0.31Cu Steel
0.32C-0.22Si-0.57Mn-0.65Cr-0.26Mo-3.38Ni Steel
0.32C-0.64Mn-0.10Ni-1.14Cu Steel
0.32C-0.95Si-0.35Mn-4.86Cr-1.45Mo-1.29W Steel
0.32C-1.1Cu Steel
0.32C-1.39Mn-0.33Si-0.129V-0.039Ti Steel
0.32C-2.37Ni-0.74Cr-0.51Mo Steel
0.32C-3.2Ni-0.63Cr-0.22Mo Steel
0.32C-3.38Ni-0.65Cr-0.26Mo Steel
0.32C-3Ni-1.4Cr-0.5Mo-0.18V Steel
0.32C-4.13Ni-1.2Cr-0.3Mo Steel
0.32C-V Steel
0.32C-V-Cr-Mo Steel
0.32C-V-Cr-Mo-Ni Steel
0.32C-V-Cr-Mo-Ni Steel
0.32C-V-Cr-Mo-Ni Steel
0.33C Steel
0.33C-0.03Si-0.06Mn-0.17Cr-2.27Ni-3.40Mo-1.09W Steel
0.33C-0.06Si-0.23Mn-1.79Cr-3.78Ni Steel I
0.33C-0.06Si-0.23Mn-1.79Cr-3.78Ni Steel II
0.33C-0.06Si-0.23Mn-1.79Cr-3.78Ni Steel III
0.33C-0.23Mn-1.79Cr-3.78Ni Steel
0.33C-0.41Mn-1.96Mo Steel
0.33C-0.45Mn-1.97Cr Steel
0.33C-0.45Mn-1.97Cr Steel
0.33C-0.51Mn-2.32Cr-0.36Mo-0.82Ni Steel
0.33C-0.84Mn-1.05Cr-1.07Mo-0.26V Steel
0.33C-0.8Ni-2.3Cr-0.36Mo Steel
0.33C-0.9Ni Steel
0.33C-1.49Mn-0.67Cr-0.50Mo-2.07Ni Steel
0.33C-1.49Mn-0.67Cr-0.95Mo-2.07Ni Steel
0.33C-1.4Ni-0.72Cr-0.28Mo Steel
0.33C-1.4Ni-0.7Cr-0.3Mo Steel
0.33C-1.5Mn-0.27Mo Steel
0.33C-1Cr-1Mo-0.26V Steel
0.33C-2Cr Steel
0.33C-2Mo Steel
0.33C-2Ni-0.67Cr-0.5Mo Steel
0.33C-3.26Ni-0.85Cr Steel
0.33C-V Steel
0.33C-V-Cr-Mo-Ni Steel
0.33C-V-Cr-Mo-Ni Steel
0.33C-V-Mo Steel
0.34C-0.75Ni Steel
0.34C-1.07Cr-0.17Mo Steel
0.34C-V Steel
0.34C-V Steel
0.34C-V Steel
0.34C-V-Cr-Mo-Ni Steel
0.34C-V-Cr-Mo-Ni Steel
0.35%C-0.23Si-0.65Mn-1.11Cr-0.05Mo-0.23Ni-0.11Cu Steel
0.35C Steel
0.35C, 0.45C, 0.75C Steels
0.35C-0.24Si-1.19Mn-0.20Cr-0.0027B Steel
0.35C-0.25Si-0.43Mn-1.55Cr-0.53Mo-2.52Ni Steel
0.35C-0.37Mn Hypoeutectoid Steel
0.35C-0.37Mn Steel
0.35C-0.40Mn Steel
0.35C-0.41Si-0.89Mn-1.86Cr-0.53Mo Steel I
0.35C-0.41Si-0.89Mn-1.86Cr-0.53Mo Steel II
0.35C-0.41Si-0.99Mn-1.86Cr-0.50Ni-0.53Mo Steel
0.35C-0.85Mn-0.005Si-0.032Al-0.07Nb-0.0006Ti Steel
0.35C-0.8Mn-0.3Si-0.3Cr-0.01Mo Steel
0.35C-0.8Mn-0.3Si-0.3Cr-0.24Mo Steel
0.35C-0.8Mn-0.3Si-0.3Cr-0.51Mo Steel
0.35C-0.8Mn-0.3Si-0.3Cr-0.78Mo Steel
0.35C-1.40Mn-0.19Mo Steel
0.35C-1.40Mn-0.19Mo Steel
0.35C-1.4Mn-0.76Si-0.06Ni-0.16V Steel
0.35C-1.80Ni-0.80Cr-0.35Mo-0.20V Steel
0.35C-12.00Cr Steel
0.35C-13Cr Steel
0.35C-2.5Ni-1.55Cr-0.53Mo Steel
0.35C-4.23Ni-1.43Cr Steel
0.35C-Mn-Mo-V Steel
0.35C-V Steel
0.35C-V Steel
0.35C-V Steel
0.35C-V-Mo Steel
0.368C-1.44Mn-0.62Si-0.16Mo-0.10V Steel I
0.368C-1.44Mn-0.62Si-0.16Mo-0.10V Steel II
0.36C-0.17Mn-0.82Mo Steel
0.36C-0.22Si-0.53Mn Steel
0.36C-0.22Si-0.53Mn Steel
0.36C-0.26Si-0.45Mn-4.95Cr-1.60Ni-1.70Mo-0.67V Steel
0.36C-0.30Si-0.98Mn-1.97Al-0.48Cu Steel
0.36C-0.31Si-0.56Mn-0.16Cr-3.28Ni Steel
0.36C-0.49Si-0.43Mn-13.50Cr-0.24Ni Steel
0.36C-0.8Mn-0.3Si-0.7Ni-0.02Mo Steel
0.36C-0.8Mn-0.3Si-0.7Ni-0.24Mo Steel
0.36C-0.8Mn-0.3Si-0.7Ni-0.49Mo Steel
0.36C-0.8Mn-0.3Si-0.7Ni-0.82Mo Steel
0.36C-0.8Mn-0.3Si-1.5Cr-0.01Mo Steel
0.36C-0.8Mn-0.3Si-1.5Cr-0.26Mo Steel
0.36C-0.8Mn-0.3Si-1.5Cr-0.50Mo Steel
0.36C-0.8Mn-0.3Si-1.5Cr-0.84Mo Steel
0.36C-0.8Mn-0.3Si-2.6Ni-0.02Mo Steel
0.36C-0.8Mn-0.3Si-2.6Ni-0.24Mo Steel
0.36C-0.8Mn-0.3Si-2.6Ni-0.49Mo Steel
0.36C-0.8Mn-0.3Si-2.6Ni-0.78Mo Mo Steel
0.36C-0.8Mo Steel
0.36C-1.44Mn-0.63Si-0.17Cr-0.13Ni-0.02Mo Steel I
0.36C-1.44Mn-0.63Si-0.17Cr-0.13Ni-0.02Mo Steel II
0.36C-V-Cr-Mo Steel
0.36VC-0.17Mn-0.82Mo Steel
0.37C-0.37Mn-0.57Cr Steel
0.37C-0.50Mn-0.30Si-0.0033Mo Steel
0.37C-0.50Mn-0.30Si-0.0077Mo Steel
0.37C-0.50Mn-0.30Si-0.19Mo Steel
0.37C-0.56Si-1.45Mn-0.11V Steel
0.37C-0.8Mn-0.3Si-0.7Cr-0.02Mo Steel
0.37C-0.8Mn-0.3Si-0.7Cr-0.26Mo Steel
0.37C-0.8Mn-0.3Si-0.7Cr-0.50Mo Steel
0.37C-0.8Mn-0.3Si-0.7Cr-0.76Mo Steel
0.37C-0.8Mn-0.3Si-1.4Ni-0.02Mo Steel
0.37C-0.8Mn-0.3Si-1.4Ni-0.24Mo Steel
0.37C-0.8Mn-0.3Si-1.4Ni-0.4Mo Steel
0.37C-0.8Mn-0.3Si-1.4Ni-0.74Mo Steel
0.37C-1.5Mn-0.3Si-0.8Cr-0.02Mo Steel
0.37C-1.5Mn-0.3Si-0.8Cr-0.25Mo Steel
0.37C-1.5Mn-0.3Si-0.8Cr-0.50Mo Steel
0.37C-1.5Mn-0.3Si-0.8Cr-0.78Mo Steel
0.37C-1Cr and 0.46C-1Cr Steels
0.37C-V Steel
0.37C-V-Cr-Mo-Ni Steel
0.37C-0.25Si-1.45Mn Steel
0.38C--0.25Si-0.46Mn-0.91Cr-3.03Mo-0.25Mo Steel
0.38C--0.37Mn-0.57Cr Steel
0.38C-0.18Si-0.20Mn-2.98Cr Steel
0.38C-0.18Si-0.20Mn-2.98Cr Steel
0.38C-0.20Si-0.70Mn Steel
0.38C-0.26Si-1.51Mn-0.99Cr-0.40Ni Steel
0.38C-0.28Si-0.90Mn-1.01Cr-0.20Mo-0.12V Steel
0.38C-0.62Si-1.44Mn-0.16Mo-0.10V Steel
0.38C-0.64Mn-0.23Si-0.99Cr Steel
0.38C-0.64Mn-0.23Si-0.99Cr Steel
0.38C-0.6Cr Steel
0.38C-0.73Si-0.63Mn-0.99Cr-0.16Mo Steel
0.38C-0.8Mn-0.3Si-1.4Ni-0.7Cr-0.01Mo Steel
0.38C-0.8Mn-0.3Si-1.4Ni-0.7Cr-0.24Mo Steel
0.38C-0.8Mn-0.3Si-1.4Ni-0.7Cr-0.48Mo Steel
0.38C-0.8Mn-0.3Si-1.4Ni-0.7Cr-0.78Mo Steel
0.38C-0.99Cr-0.16Mo Steel
0.38C-1.5Mn-0.4Mo Steel
0.38C-1.5Mn-0.4Ni-1Cr Steel
0.38C-1.6Ni-1Cr-0.26Mo Steel
0.38C-2.4Ni-0.74Cr-0.46Mo Steel
0.38C-V Steel
0.38C-V-Cr-Mo Steel
0.38C-V-Cr-Mo Steel
0.38C-V-Cr-Mo Steel
0.38C-V-Cr-Mo Steel
0.38C-V-Cr-Mo-Ni Steel
0.38C-V-Cr-Mo-Ni-Ti Steel
0.39C-0.26Si-0.67Mn-0.49Mo Steel
0.39C-0.27Si-0.68Mn-0.08Mo-3.01Ni Steel III
0.39C-0.27Si-1.58Mn-0.16Cr-0.44Mo Steel
0.39C-0.45Mn-0.74Mo-3.53Ni Steel
0.39C-0.56Mn-0.74Mn-0.74Mo-3.53Ni Steel
0.39C-0.62Si-1.30Mn-0.11V Steel
0.39C-0.71Si-1.10Mn-0.46Mo Steel
0.39C-0.80Mn-1.50Si-0.02Mo Steel
0.39C-0.80Mn-1.50Si-0.26Mo Steel
0.39C-0.80Mn-1.50Si-0.52Mo Steel
0.39C-0.80Mn-1.50Si-0.79Mo Steel
0.39C-0.86Mn-0.72Cr-0.97Ni Steel
0.39C-0.8Mn-0.3Si-3.5Ni-0.02Mo Steel
0.39C-0.8Mn-0.3Si-3.5Ni-0.24Mo Steel
0.39C-0.8Mn-0.3Si-3.5Ni-0.48Mo Steel
0.39C-0.8Mn-1.5Si-0.7Cr-0.02Mo Steel
0.39C-0.8Mn-1.5Si-0.7Cr-0.26Mo Steel
0.39C-0.8Mn-1.5Si-0.7Cr-0.73Mo Steel
0.39C-0.8Mn-1.5Si-0.7Cr-0.77Mo Steel
0.39C-1.10Mn-1.00Cr-0.56Mo-0.12V Steel
0.39C-1.40Mn-0.30Si-0.03Mo Steel
0.39C-1.40Mn-0.30Si-0.26Mo Steel
0.39C-1.40Mn-0.30Si-0.49Mo Steel
0.39C-1.40Mn-0.30Si-0.76Mo Steel
0.39C-1.44Ni-1.1Cr-0.18Mo Steel
0.39C-1.67Mn-0.10Ni Steel
0.39C-V Steel
0.39C-V-Cr-Mo Steel
0.39C-V-Cr-Mo-Ni Steel
0.39C-V-Cr-Mo-Ni Steel
0.39C-V-Cr-Mo-Ni-Ti Steel
0.3C-0.5Cr-0.4Mo Steel
0.3C-0.75Cr-0.27Mo Steel
0.3C-0.9Cr (Normal P) Steel
0.3C-1.1Ni-0.66Cr-0.55Mo Steel
0.3C-1.63Mn-0.44Cr-0.33Mo Steel
0.3C-1.7Mn-1.1Si-0.13Mo Steel
0.3C-1.8Ni-0.66Cr-0.55Mo Steel
0.3C-1Cr- (Low P) Steel
0.3C-1Mn-4Cr-0.3V-1Mn Steel
0.3C-1Ni-2Cr-0.43Mo Steel
0.3C-2.1Cr-0.48Mo Steel
0.3C-2.4Cr-0.34Mo Steel
0.3C-2Cr-0.33Mo Steel
0.3C-2Mn-1Ni-0.66Cr-0.55Mo Steel
0.3C-3.3Ni Steel
0.3C-3.5Ni (Low P) Steel
0.3C-3.65Ni (Normal P) Steel
0.3C-3Ni Steel
0.3C-5Mn-1.5Si Steel
0.40C Carbon Steel
0.40C-0.32Si-0.69Mn-0.18Mo-2.99Ni Steel I
0.40C-0.32Si-0.69Mn-0.18Mo-2.99Ni Steel II
0.40C-0.3Mn-0.2Si-4Co-0.01Mo Steel
0.40C-0.3Mn-0.2Si-4Co-0.48Mo Steel
0.40C-0.3Mn-0.2Si-4Co-0.95Mo Steel
0.40C-0.3Mn-0.2Si-8.0Ni-4.0Co Steel
0.40C-0.3Mn-0.2Si-8.0Ni-4.0Co-0.44Mo Steel
0.40C-0.3Mn-0.2Si-8.0Ni-4.0Co-1.00Mo Steel
0.40C-0.40Mn Steel
0.40C-0.42Mn-0.59Mo Steel
0.40C-0.42Mo-0.52Mo Steel
0.40C-0.57Mn-0.01Mo-3.49Ni Steel
0.40C-0.57Mn-3.49Ni Steel
0.40C-0.78Mn-1.25Cr-0.53Mo-0.22V Steel
0.40C-0.7Mn-0.3Si-4.5Ni-0.7Cr-0.03Mo Steel
0.40C-0.7Mn-0.3Si-4.5Ni-0.7Cr-0.26Mo Steel
0.40C-0.7Mn-0.3Si-4.5Ni-0.7Cr-0.50Mo Steel
0.40C-0.7Mn-0.4Si-0.8Ni-0.7Cr-0.03Mo Steel
0.40C-0.7Mn-0.4Si-0.8Ni-0.7Cr-0.27Mo Steel
0.40C-0.7Mn-0.4Si-0.8Ni-0.7Cr-0.50Mo Steel
0.40C-0.7Mn-0.4Si-2.5Ni-0.7Cr-0.03Mo Steel
0.40C-0.7Mn-0.4Si-2.5Ni-0.7Cr-0.24Mo Steel
0.40C-0.7Mn-0.4Si-2.5Ni-0.7Cr-0.49Mo Steel
0.40C-0.80Mn-0.30Si-0.01Mo Steel
0.40C-0.80Mn-0.30Si-0.26Mo Steel
0.40C-0.80Mn-0.30Si-0.53Mo Steel
0.40C-0.80Mn-0.30Si-0.79Mo Steel
0.40C-0.8Mn-0.3Si-0.3Cr-0.01Mo Steel
0.40C-0.8Mn-0.3Si-0.3Cr-0.25Mo Steel
0.40C-0.8Mn-0.3Si-0.3Cr-0.49Mo Steel
0.40C-0.8Mn-0.3Si-0.3Cr-0.77Mo Steel
0.40C-0.8Mn-0.3Si-3.5Ni-0.8Cr-0.03Mo Steel
0.40C-0.8Mn-0.3Si-3.5Ni-0.8Cr-0.25Mo Steel
0.40C-0.8Mn-0.3Si-3.5Ni-0.8Cr-0.50Mo Steel
0.40C-0.8Mn-0.3Si-4.5Ni-0.01Mo Steel
0.40C-0.8Mn-0.3Si-4.5Ni-0.25Mo Steel
0.40C-0.8Mn-0.3Si-4.5Ni-0.47Mo Steel
0.40C-1.20Cr-1.50Ni-0.30Mo Steel
0.40C-1.32Mn-0.33Si-0.004Mo-B Steel
0.40C-1.32Mn-0.33Si-0.08Mo-B Steel
0.40C-1.32Mn-0.33Si-0.18Mo-B Steel
0.40C-1.4Mn-1.4Si-1.4Ni-0.8Cr-0.03Mo Steel
0.40C-1.4Mn-1.4Si-1.4Ni-0.8Cr-0.26Mo Steel
0.40C-1.4Mn-1.4Si-1.4Ni-0.8Cr-0.52Mo Steel
0.40C-1.4Mn-1.4Si-1.4Ni-0.8Cr-0.73Mo Steel
0.40C-1.4Mn-1.5Si-0.02Mo Steel
0.40C-1.4Mn-1.5Si-0.27Mo Steel
0.40C-1.4Mn-1.5Si-0.53Mo Steel
0.40C-1.4Mn-1.5Si-0.7Cr-0.01Mo Steel
0.40C-1.4Mn-1.5Si-0.7Cr-0.26Mo Steel
0.40C-1.4Mn-1.5Si-0.7Cr-0.51Mo Steel
0.40C-1.4Mn-1.5Si-0.7Cr-0.77Mo Steel
0.40C-1.4Mn-1.5Si-0.80Mo Steel
0.40C-1.80Ni-0.80Cr-0.25Mo Steel
0.40C-5.00Cr-1.30Mo-0.50V Steel
0.40C-V-Cr-Mo Steel
0.40C-V-Cr-Mo Steel
0.40C-V-Cr-Mo-Ni Steel
0.40C-V-Cr-Mo-Ni Steel
0.40C-V-Cr-Mo-Ni-Ti Steel
0.41C-0.21Si-0.69Mn-0.95Cr-0.08Mo Steel
0.41C-0.23Si-0.69Mn-0.29Mo Steel
0.41C-0.27Si-0.68Mn-0.95Cr-0.05Ni Steel
0.41C-0.28Si-0.70Mn-3.02Ni Steel
0.41C-0.60Mn-0.21Mo-3.51Ni Steel
0.41C-0.60Mn-0.21Mo-3.51Ni Steel
0.41C-1.75Ni-0.17Cr-0.22Mo Steel
0.41C-2.05Mn-1.78Si-0.42Cr Steel
0.41C-3Ni Steel
0.42C (A-4) Alloy and S50C Steel
0.42C Steel
0.42C-0.20Mn-0.20Mo Steel
0.42C-0.20Mn-0.21Mo Steel
0.42C-0.20Mn-0.21Mo Steel
0.42C-0.20Si-0.65Mn-0.94Cr-0.32Mo Steel
0.42C-0.23Si-0.69Mn-0.94Cr-0.18Mo Steel
0.42C-0.25Si-0.55Mn-0.71Mo Steel
0.42C-0.31Si-0.67Mn-0.72Cr-0.48Mo-2.53Ni Steel
0.42C-0.31Si-0.67Mn-1.00Cr-0.48Mo-2.71Ni Steel
0.42C-0.72Mn-0.99Cr-0.42Mo Steel
0.42C-0.7Mo Steel
0.42C-0.8Cr-O.3Mo-1.5Ni Steel
0.42C-1.10Cr Steel
0.42C-1.10Cr Steel
0.42C-1.10Cr Steel
0.42C-2.53Ni-0.72Cr-0.48Mo Steel
0.43C-0.19Si-0.25Mn-0.70Mo Steel
0.43C-0.23Si-1.57Mn-0.12Cr-0.20Ni Steel
0.43C-0.27Si-0.76Mn-0.67Mo Steel
0.43C-0.28Si-1.70Mn-0.17Mo Steel
0.43C-1.45Mn-0.98Si-1.00Al Steel
0.43C-1.7Mn-0.17Mo Steel
0.43C-V Steel
0.43C-V-Cr Steel
0.43C-V-Cr-Mo Steel
0.43C-V-Cr-Mo Steel
0.43C-V-Cr-Mo Steel
0.43C-V-Cr-Mo Steel
0.43C-V-Cr-Mo Steel
0.43C-V-Cr-Mo Steel
0.43Mn-1.6Mn Steel
0.44 C Steel
0.44C Steel
0.44C Steel
0.44C-0.06Si-1.64Mn-1.64Mn-1.64Cr-0.40Mo-1.84Ni Steel
0.44C-0.06Si-1.64Mn-1.64Mn-1.64Cr-0.40Mo-1.84Ni Steel
0.44C-0.06Si-1.64Mn-1.64Mn-1.64Cr-0.40Mo-1.84Ni Steel
0.44C-0.15Mo Steel
0.44C-0.24Mo Steel
0.44C-0.28Si-0.65Mn-0.15Mo Steel
0.44C-0.28Si-0.77Mn-0.98Cr-0.18Ni Steel
0.44C-1.04Cr-0.26Ni Steel
0.44C-1.04Cr-0.26Ni Steel
0.44C-1.4Ni-1.26Cr-0.11Mo Steel
0.44C-1.64Mn-1.64Cr-0.40Mo-1.84Ni-0.15V Steel
0.44C-1.8Ni-1.6Cr-0.4Mo-0.15V Steel
0.44C-V Steel
0.44C-V-Cr-Mo Steel
0.44C-V-Cr-Mo Steel
0.44C-V-Cr-Mo Steel
0.44C-V-Cr-Mo Steel
0.44C-0.22Si-0.66Mn-0.15Cr, 0.38C-1.05Si-1.14Mn Steels
0.44Mn, 0.87Mn, 2.02Mn Cast Irons
0.45C-0.05Si Steel
0.45C-0.26Si-0.67Mn Steel
0.45C-0.40Mn Steel
0.45C-0.60Si Steel
0.45C-2Mn Steel
0.45C-3.5Cr Steel
0.45C-3.5Cr Steel
0.45C-5Ni Steel
0.45C-V Steel
0.45C-V-Cr-Mo Steel
0.46C-0.19Si-0.80Mn-0.13Cr-0.17Ni Steel
0.46C-1.00Cr-1.00Mo-0.55Ni Steel
0.46C-1.85Ni-1.59Si-0.75Cr-0.43Mo Steel
0.47C-1.37Mn-0.36Si-0.15Cr Steel
0.47C-V-Cr-Mo Steel
0.47C-V-Cr-Mo Steel
0.47C-V-Cr-Mo Steel
0.47C-V-Cr-Mo Steel
0.48C-0.16Si-0.33Mn-7.61Ni Steel
0.48C-0.94Mn-0.25Mo Steel
0.49C-0.33Si-0.41Mn-1.87Cr-2.97Ni Steel
0.49C-V-Cr-Mo-Ni Steel
0.4C Steel
0.4C-0.53Mo Steel
0.4C-0.5Mo Steel
0.4C-0.65Mn-0.08Al-V-Cr Steel
0.4C-0.74Ni-0.5Cr-0.16Mo Steel
0.4C-1.0Mn-0.1Mo Steel
0.4C-1.15Mn-1.23Al-V Steel
0.4C-1.1Ni Steel
0.4C-1.25Cr-0.5Mo-0.22V Steel
0.4C-1.34Mn-1.0Ni-0.53Cr-0.22Mo Steel Steel
0.4C-1.49Mn-0.08Al-V Steel
0.4C-1.50Mn-2.10Al-V Steel
0.4C-1.6Cr-0.36Mo-1.26Al Steel
0.4C-1.6Mn-0.44Mo Steel
0.4C-1.8Mn Steel
0.4C-1Cr-0.42Mo Steel
0.4C-3.5Ni-0.21Mo Steel
0.4C-3.5Ni-0.7Mo Steel
0.4C-3Cr Steel
0.4C-3Ni-0.08Mo Steel
0.4C-3Ni-0.18Mo Steel
0.4C-3Ni-0.32Mo Steel
0.4C-1.4Mn-0.2Mo-0.1V Steel
0.4C-1.4Mn-0.2Mo-0.1V Steel
0.50C Steel
0.50C-0.131Si-0.91Mn Steel
0.50C-0.17Si-1.50Mn-0.20Cr-0.45Mo-0.10V Steel
0.50C-0.40Mn Steel
0.50C-0.53Si-0.23Mn-0.05Cr Steel
0.50C-0.53Si-0.23Mn-0.05Cr Steel
0.50C-0.73Mn-3.92Ni Steel
0.50C-0.91Mn Steel
0.50Mn Cast Iron
0.51C-0.16Si-0.21Mn-10.11Ni Steel
0.51C-0.17Si-0.23Mn-5.26Ni Steel
0.51C-0.35Mo-3.69Ni Steel
0.51C-0.73Mn-0.99Cr-0.45Mo-2.74Ni Steel
0.51C-1Cr-0.2V Steel
0.51C-3.80Si-0.25Mn-0.32Cr Steel
0.51C-V Steel
0.52C-0.25Si-0.30Mn-4.80Cr-3.0Mo-0.60Ni-0.60W Steel
0.52C-0.30Si-1.18Mn-0.13Cr-0.30Mo-0.16Ni Steel
0.52C-1.09Cr-1.72Ni Steel
0.52C-1.09Cr-1.72Ni Steel
0.52C-1.18Mn-0.3Mo Steel
0.52C-2.11Ni Steel
0.52C-V-Cr-Mo-Ni Steel
0.53C-0.24Mn-0.32Cr-2.32Ni Steel
0.54C Steel
0.54C-0.46Mn Steel
0.54C-0.46Mn Steel
0.54C-0.66Mn-0.20U Steel
0.54C-0.93Si-0.62Mn-7.83Cr-6.90W Steel
0.54C-1.27Si-0.23Mn-0.05Cr Steel
0.54C-1.3Si Steel
0.55C-0.30Si-0.67Mn-0.83Cr-0.28Mo-1.15Ni Steel
0.55C-0.30Si-0.67Mn-0.83Cr-0.28Mo-1.51Ni Steel
0.55C-0.33Mn-3.88Ni Steel
0.55C-0.34Mo-2.13Ni Steel
0.55C-0.35Mo Steel
0.55C-0.83Mn-1.01Cr-0.48Mo-1.15Ni Steel
0.55C-0.85Si-0.30Mn-8.50Cr-1.60Mo-0.25V-1.10W Steel
0.55C-1.04Mn Steel
0.55C-1.15Ni-1Cr-0.5Mo Steel
0.55C-1.62Si-0.78Mn-0.77Cr Steel
0.55C-1.6Si-0.77Cr Steel
0.55C-1.9Mn Steel
0.55C-1Cr-3Ni-0.3Mo Steel
0.55C-2W Steel
0.55C-3.78Ni Steel
0.55C-3.9Cr-0.45Mo-0.9V Steel
0.55C-V Steel
0.55C-V Steel
0.55C-V Steel
0.55C-V-Cr-Mo Steel
0.55C-V-Cr-Mo Steel
0.55C-V-Cr-Mo Steel
0.56% C Carbon Steel
0.56C-0.26Mn-1.97Ni
0.56C-0.47Mn-0.35Si-0.10Mo-0.10Ni Steel
0.56C-4.89Ni Steel
0.56C-V-Cr-Mo-Ni Steel
0.57C-0.24Mn-1.94Ni Steel
0.57C-0.24Si-0.76Mn-1.07Cr-0.45Mo-0.19V Steel
0.58C-V-Cr-Mo Steel
0.58C-V-Mo Steel
0.59C Steel
0.59C Steel
0.59C-0.20Mn Steel
0.59C-0.25Mn-3.90Ni Steel
0.59C-0.28Si-0.96Mn-1.06Cr-0.54Mo-0.12V Steel
0.59C-0.28Si-0.96Mn-1.06Cr-0.54Mo-0.12V Steel
0.59C-0.30Mn Steel
0.59C-0.30Mn Steel
0.59C-0.35Mo-5.31Ni Steel
0.59C-3.90Ni Steel
0.5C-0.5Cu Steel
0.5C-0.5Si Steel
0.5C-0.65Cr-0.18Mo Steel
0.5C-0.77Mn-1.90Al-V-Cr Steel
0.5C-1.5Cu Steel
0.5C-1.5Mn-0.45Mo Steel
0.5C-2.3Si-0.3Cr Steel
0.5C-2.7Ni-1Cr-0.45Mo Steel
0.5C-3.8Si-0.3Cr Steel
0.5C-3.9Ni Steel
0.5C-3Ni-1.9Cr Steel
0.5C-5Ni Steel
0.5Cr Cast Iron
0.5Cr and 1Cr Cast Irons
0.5Cr0.5Mo Steel
0.5Cr0.5Mo Steel
0.5Mo Cast Iron
0.6%, 0.8%, 1.2% and 1.6% C Steels
0.60C-0.30Si-0.60Mn-1.25Cr-0.50Mo-2.75Ni-0.12V Steel
0.61C Steel
0.61C-0.26Mn-0.94Ni Steel
0.61C-1Cr and 0.86C-0.5Mo Steels
0.63C-0.20Si-0.28Mn-1.93Cr-0.08Ni-2.90Mo-0.88V-1.00W Steel
0.63C-0.87Mn-0.0025B Steel
0.63C-0.87Mn-0.0025B With and Without B Steel
0.63C-O.87Mn-O.22Si Steel
0.63Mn-0.87Mn Steel
0.64C-0.22Si-0.68Mn Steel
0.64Mn-1.13Mn Steel
0.65C Steel
0.65C-0.16Si-0.45Mn Steel
0.65C-0.19Si-0.39Mn-0.16Cr-0.19Ni Steel
0.65C-0.1Mo Steel
0.65C-0.23Si-0.68Mn-0.10Mo Steel
0.65C-0.23Si-1.32Mn Steel
0.65C-0.40Mn Steel
0.65C-0.40Mn Steel
0.65C-1.32Mn Steel
0.65C-17Cr Steel
0.65C-V Steel
0.65Mn-0.25Si-1Cr-0.1Ni-0.15Mo Steels
0.66C-1.33Si-0.61Mn-0.50Cr-0.31Mo-1.54Ni-0.11V Steel
0.67C-V Steel
0.68C-0.87Mn-0.24Mo Steel
0.68C-7.40Co Steel
0.69C-0.19Si-0.31Mn-12.7Cr Steel
0.69C-V Steel
0.69Cr-0.12Si-0.22Mn-3.00Cr Steel
0.6C-1Cr-0.5Mo-0.12V Steel
0.6C-1Ni Steel
0.6C-2Mn-B Steel
0.6C-2Ni Steel
0.6C-3.9Ni Steel
0.6CCr, 0.6Mo, 1CSi Steels
0.6CCr, 0.6Mo, and 1CSi Steels
0.70C-0.29Si-0.43Mn-4.20Co Steel
0.70C-1.01Si-1.01Mn-11 ppm B Steel
0.70C-1.01Si-1.0Mn-0.013Ti-34 ppm N-11 ppm B Steel
0.71C-1.83Si-0.52Mn-0.5Cr-0.19Mo Steel
0.71C-1.95Co Steel
0.72C-0.19Si-0.32Mn-0.45Mo Steel
0.72C-0.32Si-0.96Mn Rail Steel
0.72C-0.32Si-0.96Mn-0.06Cr Steel
0.72c-0.31Si-0.78Mn-0.020Nb Steel
0.73C-V Steel
0.74C-0.25Si-0.34Mn-1.43Cr-0.23Mo-0.21Ni Steel
0.75C-0.27Si-0.50Mn Steel
0.75C-0.40Mn Steel
0.75C-0.5Cr Steel
0.75C-1.00Cr-1.75Ni Steel
0.75C-1.63Si-1.95Mn-1.48Cr-0.28Mo Steel
0.75C-V Steel
0.75C-V Steel
0.75C-1.02Mn-0.28Si-0.11Cr-0.05Ni-0.08Cu-0.01S-0.009P Steel
0.76C-0.20Si-0.41Mn-0.13Cr-2.50Ni Steel
0.76C-0.26Si-0.42Mn Steel
0.76C-0.27Mn-2.06Cr-0.25Mo Steel
0.76C-2.5Ni Steel
0.76C-2Cr-0.25Mo Steel
0.76C-V Steel
0.77C-0.15Mo Steel
0.77C-0.22Si-0.20Mn-10.01Ni Steel
0.77C-0.28Si-0.72Mn-0.52Mo Steel
0.77C-0.29Si-0.70Mn-0.15Mo Steel
0.77C-0.29Si-0.71Mn-0.017Mo Steel
0.77C-0.5Mo Steel
0.78C-0.28Si-0.73Mn-0.32Mo Steel
0.78C-0.96Mn-0.32Si-0.06Cr Steel I
0.78C-0.96Mn-0.32Si-0.06Cr Steel II
0.78C-V Steel
0.79C-0.21Si-0.76Mn Steel
0.79C-0.22Si-0.21Mn-7.53Ni Steel
0.79C-0.22Si-0.23Mn-5.25Ni Steel
0.79C-0.27Si-0.76Mn-0.77Mo Steel
0.79C-0.65Mn-0.24Si Steel
0.79C-0.76Mn Steel
0.7C-0.25Ni-0.28Cr-0.94Mo Steel
0.7C-3Cr Steel
0.7Si, 1.6Si, 2.6Si, 3.5Si, 4.5Si Cast Irons
0.80C-0.27Si-0.61Mn Steel
0.80C-0.30Si-0.90Mn-0.44Mo-0.16Ni Steel
0.80C-0.43Si-0.63Mn-3.14Cr-0.50Mo-0.12Ni-0.12V Steel
0.80C-0.7Mn-0.5Si-6Cr-0.035Mo Steel
0.80C-0.7Mn-0.5Si-6Cr-1.05Mo Steel
0.80C-02.7Si-0.23Mn-4.07Cr-6.09Mo-1.65V-5.70W Steel
0.80C-2.76Cr Steel
0.80C-V Steel
0.81C-0.75Si-0.30Mn-2.95Cr-0.19Ni-0.54Mo-0.01V Steel
0.81C-V Steel
0.82C Steel
0.83C-0.28Si-0.82Mn-1.13Cr-0.05Mo-0.34Ni Steel
0.83C-0.34Ni-1.1Cr-0.05Mo Steel
0.83C-0.77Si-0.34Mn-3.94Cr-0.16Ni-0.49Mo-0.04V Steel
0.84C-0.22Si-0.53Mn-0.09Cr-0.12Ni Steel
0.84C-0.22Si-0.53Mn-0.09Cr-0.12Ni Steel
0.84C-0.22Si-0.53Mn-0.09Cr-0.12Ni Steel
0.85 C Tool Steel
0.85C-0.18Si-0.23Mn-0.05Ni Steel
0.85C-0.26Si-1.18Mn-0.50Cr-0.44W Steel
0.85C-0.40Mn Steel
0.85C-0.7Mn-0.5Si-12Cr-0.068Mo Steel
0.85C-0.7Mn-0.5Si-12Cr-1.05Mo Steel
0.85C-0.7Mn-0.5Si-12Cr-3.07Mo Steel
0.85C-V Steel
0.85C-V Steel
0.86C-0.38Si-0.66Mn-1.21Cr-0.50Mo-2.47Ni Steel
0.86C-0.38Si-0.66Mn-1.21Cr-0.50Mo-2.47Ni Steel
0.86C-2.5Ni-1.2Cr-0.5Mo Steel
0.87C-0.30Mn-0.27V Steel
0.87C-0.30Mn-0.27V Steel
0.87C-V Steel
0.88C Steel
0.88C-0.41Si-0.41Mn Steel
0.89C-0.15Si-0.29Mn Steel
0.89C-0.29Mn Steel
0.89Cr-4Ni-1.58Cr Steel
0.8C-0.3Mo Steel
0.8C-0.77Mo Steel
0.8C-5Ni Steel
0.8C-8Cr-2Mo-0.5V Steel
0.90C-0.25Si-0.25Mn Steel
0.90C-0.30Si-0.38Mn-7.95Cr-0.25Ni-1.48Mo-2.10V Steel
0.90C-0.47Mn-0.20V Steel
0.92C-V Steel
0.95C-.48Mn-0.95Co Steel
0.95C-0.19Si-0.45Mn Steel
0.95C-0.20Si-0.25Mn Steel
0.95C-0.25Si-0.48Mn-0.95Co Steel
0.95C-0.36Mn-0.28Si-1.84Cr Steel
0.95C-0.40Mn Steel
0.95C-0.44Mn-0.21Si-1.42Cr Steel
0.95C-0.45Mn Steel
0.95C-0.44Mn-0.21Si-1.42Cr Steel
0.96C Steel
0.97C-0.14Ni-0.14Cr-O.13Cu-0.13Si-0.16Mn Steel
0.97C-0.40Si-0.48Mn04.58Cr-1.04Mo-0.25V Steel
0.97C-1.04Mn-0.32Mo Steel
0.97C-1.04Mn-0.32Mo Steel
0.97C-1.04Mn-0.32Mo Steel
0.97C-1.04Mn-0.32Mo Steel
0.97C-V Steel
0.99C (A-9) Alloy and SK3 Steel
0.99C-1.07Si-0.27Mn-7.93Cr-0.16Ni-2.27Mo-0.30V Steel
004 Steel
005 Steel
006 Steel
007 Steel
032 Steel
034 Steel
038 Steel
041 Steel
045 Steel
05Mn2MoNbTiB Steel
06C Steel
06CCr Steel
06CMo Steel
06CNb Steel
06Cr15Ni4CuMo Steel
080M46 Steel
081 Steel
082 Steel
085 Steel
08C Steel
08G2AMNb Steel
08Mn2MoNbTi Steel
09 G 2/Ch.1 Steel
09 G 2/Ch.2 Steel
09 G 2/Ch.3 Steel
09 G 2/Ch.4 Steel
09 G 2/Ch.5 Steel
09 G 2S Steel
091 Steel
092 Steel
095 + 0.25V Steel
09CrNi2MoCu Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09CuPCrNi Steel
09G2 Steel
0B, 10B, 20B, 05Mo0B, 05Mo10B, 05Mo20B, 15Mo0B, 15Mo10B, 15Mo20B Steels
0Mo Cast Iron
0Mo-0.07Mo-0.15Mo Mo Steels
0V, 200 V Steels
1 1/2 Ni Cr Mo Steel
1 1/2 Ni Cr Mo Steel
1 Cr Al Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo Steel
1 Cr Mo V Steel
1 Cr Steel
1 Cr Steel
1 Cr Steel
1 Cr Steel
1 Cr V Steel
1 Mn+S Steel
1 Mn+S Steel
1 Ni Cr Mo Steel
1 Ni Cr Steel
1 Ni Steel
1 Ni Steel
1-1/2 Cr Al Mo Steel
1-1/2 Cr Al Mo Steel
1-1/2 Cr Al Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Mo Steel
1-1/2 Mn Ni Cr Mo Steel
1-1/2 Mn Ni Cr Mo Steel
1-1/2 Mn Ni Cr Mo Steel
1-1/2 Mn Ni Cr Mo Steel
1-1/2 Mn Ni Cr Mo Steel
1-1/2 Mn Ni Steel
1-1/2 Mn Steel
1-1/2 Mn Steel
1-1/2 Mn Steel
1-1/2 Mn Steel
1-1/2 Mn+S Steel
1-1/2 Ni Cr Mo Steel
1-1/2 Ni Cr Mo Steel
1-1/2 Ni Cr Mo Steel
1-1/2 Ni Cr Steel
1-1/2 Ni Cr Steel
1-1/2 Ni Mn Steel
1-1/2 Ni Steel
1-1/2 Si Cr Steel
1-1/4 Cr Mo Steel
1-1/4 Cr Mo Steel
1-1/4 Cr Mo Steel
1-1/4 Cr Mo Steel
1-1/4 Cr Mo V Steel
1-1/4 Mn Cr Steel
1-1/4 Mn Cr Steel
1-1/4 Mn Cr Steel
1-1/4 Mn Steel
1-1/4 Mn Steel
1-1/4 Mn Steel
1-1/4 Ni Cr Steel
1-1/4 Ni Cr Steel
1-1/4Cr-1/2Mo Steel Plate
1-1/4Cr-1/2Mo Steel Plate
1-3/4 Mn Steel
1-3/4 Mn Steel
1-3/4 Mn Steel
1-3/4 Mn+S Steel
1-3/4 Ni Cr Mo Steel
1-3/4 Ni Cr Mo Steel
1-3/4 Ni Mo Steel
1-3/4 Ni Mo Steel
1-3/4 Ni Mo Steel
1.00% C Steel
1.0037 Steel
1.0045 Steel
1.00C-1.45Cr Steel
1.00Cr Cast Iron
1.00Mn Cast Iron
1.00Ni, 1.96Ni Cast Irons
1.01C-0.30Si-0.50Mn-1.21Cr Steel
1.01C-0.30Si-0.50Mn-1.21Cr Steel
1.01C-0.49Co, 1.15C-0.98Co Steels
1.02C-0.35Si-0.33Mn-2.90Cr Steel
1.0461 Steel
1.0481 Steel
1.0482 Steel
1.0482 Steel
1.04C-0.32Mn-0.19Si-1.35Cr Steel
1.04C-0.35Si-0.18Mn-4.00Cr Steel
1.0501 Steel
1.0501 Steel
1.0503 Steel
1.0503 Steel
1.0505 Steel
1.0528 Steel
1.0528 Steel
1.0535 Steel
1.0535 Steel
1.0540 Steel
1.0562 Steel
1.0601 Steel
1.0601 Steel
1.0603 Steel
1.0605 Steel
1.0614 Steel
1.0615 Steel
1.0615 Steel
1.06C-0.32Si-0.33Mn-1.44Cr-0.11Ni-0.03Mo Steel
1.06C-V Steel
1.0915 Steel
1.0987 Steel
1.09C Steel
1.0Al-550 TRIP Steel
1.0Al-550 TRIP Steel
1.0C High-Chromium Steel
1.0C High-Chromium Steel
1.0C High-Chromium Steel
1.0C High-Chromium Steel
1.0C Steel
1.0C-0.7Mn-0.5Si-6.0Cr-0.038Mo Steel
1.0C-0.7Mn-0.5Si-6.0Cr-1.03Mo Steel
1.0C-2.4Mn Steel
1.0Cr-0.5Mo Steel
1.0Cr-0.5Mo-B Steel
1.0Cu, 1.5Cu, 2.0Cu Steels
1.0Mo Cast Iron
1.10C-1.02Si-0.28Mn-7.74Cr-0.15Ni-1.49Ni-2.33V-0.15W Steel
1.1106 Steel
1.1127 Steel
1.1132 Steel
1.1133 Steel
1.1140 Steel
1.1144 Steel
1.1157 Steel
1.1157 Steel
1.1160 Steel
1.1165 Steel
1.1165 Steel
1.1167 Steel
1.1170 Steel
1.1172 Steel
1.1172 Steel
1.1174 Steel
1.1174 Steel
1.1178 Steel
1.1178 Steel
1.1179 Steel
1.1179 Steel
1.1180 Steel
1.1180 Steel
1.1181 Steel
1.1181 Steel
1.1183 Steel
1.1183 Steel
1.1191 Steel
1.1191 Steel
1.1191 Steel
1.1192 Steel
1.1192 Steel
1.1193 Steel
1.1193 Steel
1.1194 Steel
1.1194 Steel
1.1199 Steel
1.11C-V Steel
1.1201 Steel
1.1201 Steel
1.1203 Steel
1.1203 Steel
1.1204 Steel
1.1204 Steel
1.1206 Steel
1.1209 Steel
1.1209 Steel
1.1211 Steel
1.1211 Steel
1.1217 Steel
1.1219 Steel
1.1219 Steel
1.1219 Steel
1.1221 Steel
1.1221 Steel
1.1223 Steel
1.1223 Steel
1.1231 Steel
1.1237 Steel
1.1237 Steel
1.1237 Steel
1.1240 Steel
1.1241 Steel
1.1248 Steel
1.1248 Steel
1.1248 Steel
1.1249 Steel
1.1249 Steel
1.1249 Steel
1.1251 Steel
1.1251 Steel
1.1251 Steel
1.1253 Steel
1.1253 Steel
1.1253 Steel
1.1269 Steel
1.1269 Steel
1.1273 Steel
1.12C-0.24Si-0.51Mn-5.36Ni Steel
1.12C-V Steel
1.13C Steel
1.13C-0.24Si-0.59Mn Steel
1.13C-0.30Mn Steel
1.13C-0.30Mn Steel
1.13C-V Steel
1.14TC Steel
1.1520 Steel
1.1520 Steel
1.1520 Steel
1.1520 Steel
1.1525 Steel
1.1545 Steel
1.15C-0.28Si-0.76Mn-0.53Mo Steel
1.15C-0.53Mo Steel
1.1620 Steel
1.1620 Steel
1.1620 Steel
1.1625 Steel
1.1645 Steel
1.16C Steel
1.16C Steel
1.16C-0.15Mo Steel
1.16C-0.21Si-0.27Mn-0.11Cr-0.08Ni Steel
1.16C-0.29Si-0.75Mn-0.15Mo Steel
1.1730 Steel
1.1730 Steel
1.1740 Steel
1.1740 Steel
1.1744 Steel
1.1750 Steel
1.17C-0.22Si-0.21Mn-10.30Ni Steel
1.1820 Steel
1.1820 Steel
1.1830 Steel
1.18C Steel
1.18C-0.22Si-0.22Mn-7.64Ni Steel
1.18C-0.28Si-0.75Mn-0.28Mo Steel
1.18C-0.29Si-0.76Mn-0.009Mo Steel
1.18C-0.8Mo Steel
1.19C-0.28Si-0.77Mn-0.33Mo Steel
1.19C-0.33Mo Steel
1.1C Steel
1.1C-3.6Ni Steel
1.1C-5Ni Steel
1.2002 Steel
1.2002 Steel
1.2003 Steel
1.2003 Steel
1.2004 Steel
1.2056 Steel
1.2056 Steel
1.2057 Steel
1.2058 Steel
1.2058 Steel
1.2063 Steel
1.2067 Steel
1.2067 Steel
1.2067, 1.2601, 1.2080, 1.2379 Steels
1.2080 Steel
1.2080 Steel
1.2080 Steel
1.2082 Steel
1.2083 Steel
1.2083 Steel
1.2083 Steel
1.2085 (~1.2316+S) Steel
1.2086 Steel
1.2101 Steel
1.2103 Steel
1.2103 Steel
1.2109 Steel
1.2109 Steel
1.2127 Steel
1.2162 Steel
1.2162 Steel
1.2208 Steel
1.2210 Steel
1.2210 Steel
1.2210 Steel
1.2241 Steel
1.2242 Steel
1.2242 Steel
1.2243 Steel
1.2249 Steel
1.22C-0.19Si-1.93Mn-1.52Cr-0.36Mo-0.17V Steel
1.22C-0.28Si-0.55Mn-2.56Ni Steel
1.2304 Steel
1.2311 Steel
1.2311 Steel
1.2311 Steel
1.2311 Steel
1.2311, 1.2738, 1.2738 mod. Steels
1.2312 Steel
1.2312 Steel
1.2312 Steel
1.2313 Steel
1.2316 Steel
1.2316 Steel
1.2316 Steel
1.2316 Steel
1.2316 Steel
1.2322 Steel
1.2323 Steel
1.2323 Steel
1.2323 Steel
1.2327 Steel
1.2334 Steel
1.2341 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 Steel
1.2343 VICTORY ES /EFS Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2344 Steel
1.2345 Steel
1.2345 Steel
1.2347 Steel
1.2347 Steel
1.2358 Steel
1.2358 Steel
1.2360 Steel
1.2361 Steel
1.2362 Steel
1.2363 Steel
1.2363 Steel
1.2363 Steel
1.2365 Steel
1.2365 Steel
1.2365 Steel
1.2365 Steel
1.2365 mod. Steel
1.2365 mod. Steel
1.2367 Steel
1.2367 Steel
1.2367 Steel
1.2378 Steel
1.2378 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2379 Steel
1.2380 Steel
1.2381 Steel
1.2390 Steel
1.2414 Steel
1.2419 Steel
1.2419 Steel
1.2436 Steel
1.2436 Steel
1.2510 Steel
1.2510 Steel
1.2516 Steel
1.2516 Steel
1.2541 Steel
1.2541 Steel
1.2542 Steel
1.2542 Steel
1.2542 Steel
1.2550 Steel
1.2550 Steel
1.2550 Steel
1.2550 Steel
1.2550 Steel
1.2552 Steel
1.2564 Steel
1.2564 Steel
1.2567 Steel
1.2567 Steel
1.2581 Steel
1.2581 Steel
1.2581 Steel
1.25C-0.39Si-0.45Mn-9.80Cr-0.19Ni-0.81Mo-0.43V-0.30Ti Steel
1.25Cr0.5Mo Steel
1.25Cr0.5Mo Steel
1.2601 Steel
1.2601 Steel
1.2603 Steel
1.2603 Steel
1.2603 Steel
1.2606 Steel
1.2606 Steel
1.2606 Steel
1.2622 Steel
1.2622 Steel
1.2622 Steel
1.2631 Steel
1.2662 Steel
1.2662 Steel
1.2678 Steel
1.26C-0.23Si-0.21Mn-5.30Ni Steel
1.26C-5Ni Steel
1.2705 Steel
1.2709 Steel
1.2710 Steel
1.2711 Steel
1.2713 Steel
1.2713 Steel
1.2714 Steel
1.2714 Steel
1.2714 Steel
1.2714 Steel
1.2714 Steel
1.2718 Steel
1.2721 Steel
1.2721 Steel
1.2721 Steel
1.2726 Steel
1.2738 Steel
1.2738 Steel
1.2738TS Steel
1.2740 Steel
1.2743 Steel
1.2743 Steel
1.2744 Steel
1.2744 Steel
1.2745 Steel
1.2746 Steel
1.2762 Steel
1.2764 Steel
1.2764 Steel
1.2765 Steel
1.2766 Steel
1.2766 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2767 Steel
1.2770 Steel
1.2787 Steel
1.2787 Steel
1.2790 Steel
1.2791 Steel
1.2823 Steel
1.2826 Steel
1.2826 Steel
1.2833 Steel
1.2834 Steel
1.2838 Steel
1.2838 Steel
1.2842 Steel
1.2842 Steel
1.2842 Steel
1.2842 Steel
1.2880 Steel
1.2880 Steel
1.2885 Steel
1.2885 Steel
1.2888 Steel
1.28C-0.37Si-0.29Cr-2.90Cr Steel
1.2Mn Steel
1.2Mn-0.5C Steel
1.3202 Steel
1.3207 Steel
1.3207 Steel
1.3243 Steel
1.3243 Steel
1.3247 Steel
1.3247 Steel
1.3247 Steel
1.3255 Steel
1.3265 Steel
1.32C-0.50Si-0.28Mn-0.22Cr-3.51W Steel
1.3302 Steel
1.3333 Steel
1.3333 Steel
1.3333 Steel
1.3343 Steel
1.3343 Steel
1.3343 Steel
1.3343 Steel
1.3345 Steel
1.3346 Steel
1.3348 Steel
1.3355 Steel
1.3501 Steel
1.3503 Steel
1.3505 Steel
1.3505 Steel
1.3505 Steel
1.3514 Steel
1.3514 Steel
1.3520 Steel
1.3520 Steel
1.3521 Steel
1.3521 Steel
1.3523 Steel
1.3523 Steel
1.3531 Steel
1.3531 Steel
1.3533 Steel
1.3533 Steel
1.3536 Steel
1.3536 Steel
1.3541 Steel
1.3551 Steel
1.3553 Steel
1.3554 Steel
1.3561 Steel
1.3563 Steel
1.3563 Steel
1.3565 Steel
1.3565 Steel
1.35C Steel
1.35C-0.28Si-0.52Mn Steel
1.35C-0.7Mn-0.5Si-12.0Cr-0.078Mo Steel
1.35C-0.7Mn-0.5Si-12.0Cr-1.00Mo Steel
1.35C-0.7Mn-0.5Si-12.0Cr-3.06Mo Steel
1.35C-0.7Mn-0.5Si-6.0Cr-0.041Mo Steel
1.35C-0.7Mn-0.5Si-6.0Cr-0.98Mo Steel
1.3C-2.9Cr Steel
1.4000 Steel
1.4000 Steel
1.4000 Steel
1.4003 Steel
1.4003 Steel
1.4005 Steel
1.4005 Steel
1.4005 Steel
1.4005 Steel
1.4006 Steel
1.4016 Steel
1.4016 Steel
1.4016 Steel
1.4021 Steel
1.4021 Steel
1.4021 Steel
1.4021 Steel
1.4021 Steel
1.4024 Steel
1.4024 Steel
1.4028 Steel
1.4029 Steel
1.4031 Steel
1.4034 Steel
1.4034 Steel
1.4034 Steel
1.4037 Steel
1.4057 Steel
1.4057 Steel
1.4057 Steel
1.4057 Steel
1.4104 Steel
1.4104 Steel
1.4104 Steel
1.4106 Steel
1.4108 Steel
1.4108 Steel
1.4112 Steel
1.4113 Steel
1.4120 Steel
1.4122 Steel
1.4122 Steel
1.4122 Steel
1.4122 Steel
1.4125 Steel
1.4125 Steel
1.4310 Steel
1.4313 Steel
1.4418 Steel
1.4418 Steel
1.4460 Steel
1.4460 Steel
1.4462 Steel
1.4462 Steel
1.44C-0.38Mn-0.17Cr-0.02Ni Steel
1.44Si Melleable Iron
1.4535 Steel
1.4704 Steel
1.4713 Steel
1.4713 Steel
1.4718 Steel
1.4718 Steel
1.4731 Steel
1.4747 Steel
1.4748 Steel
1.4903 Steel
1.4913 Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 (C/N) Steel
1.4914 Steel
1.4914 with 10% Cr Steel
1.4914 with 11% Cr Steel
1.4914 with 12% Cr Steel
1.4914 with 13% Cr Steel
1.4914 with 14% Cr Steel
1.4914 with 9% Cr Steel
1.4920 Steel
1.4921 Steel
1.4921 Steel
1.4922 Steel
1.4922 Steel
1.4923 Steel
1.4923 Steel
1.4926 Steel
1.4926 Steel
1.4935 Steel
1.4935 Steel
1.4935 Steel
1.4970 Steel
1.4970 Steel
1.5024 Steel
1.5026 Steel
1.5028 Steel
1.5029 Steel
1.5029 Steel
1.50Mn Cast Iron
1.5120 Steel
1.5121 Steel
1.5122 Steel
1.5122 Steel
1.5141 Steel
1.5223 Steel
1.5223 Steel
1.5231 Steel
1.5232 Steel
1.5232 Steel
1.5233 Steel
1.5402 Steel
1.5403 Steel
1.5404 Steel
1.5404 Steel
1.5404 Steel
1.5406 Steel
1.5415 Steel
1.5415 Steel
1.5415 Steel
1.5419 Steel
1.5423 Steel
1.5510 Steel
1.5523 Steel
1.5523 Steel
1.5523 Steel
1.5525 Steel
1.5525 Steel
1.5527 Steel
1.5531 Steel
1.5532 Steel
1.55C-0.45Si-0.27Mn-11.34Cr-0.53Mo-0.24V Steel
1.5622 Steel
1.5633 Steel
1.5637 Steel
1.5639 Steel
1.5662 Steel
1.5662 Steel
1.5680 Steel
1.5680 Steel
1.5680 Steel
1.5710 Steel
1.5710 Steel
1.5710 Steel
1.5710 Steel
1.5713 Steel
1.5713 Steel
1.5732 Steel
1.5732 Steel
1.5732 Steel
1.5736 Steel
1.5737 Steel
1.5737 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5752 Steel
1.5755 Steel
1.5755 Steel
1.5805 Steel
1.5805 Steel
1.5807 Steel
1.5807 Steel
1.5808 Steel
1.5808 Steel
1.5815 Steel
1.5815 Steel
1.5860 Steel
1.5860 Steel
1.5860 Steel
1.5864 Steel
1.5864 Steel
1.5918 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5919 Steel
1.5920 Steel
1.5920 Steel
1.5920 Steel
1.5924 Steel
1.5924 Steel
1.5934 Steel
1.5934 Steel
1.59C-0.74Si-0.67Mn-11.76Cr-1.45Mo-0.53Ni Steel
1.5Mn, 3Mn, 5Mn Steels
1.5Mn-0.5Mo-B Mo Steel
1.5Mo Cast Iron
1.5Ni-Cr-Mo Steel
1.5Ni-Cr-Mo Steel
1.5Si Steel
1.5Si Steel
1.61C-0.68Si-0.75Mn-5.30Cr-1.14Ni-2.84Mo-4.69V-0.02W Steel
1.61C-0.89Si-0.81Mn-3.43Cr-1.05Ni-1.94Mo-5.77V-0.05W Steel
1.6210 Steel
1.6211 Steel
1.6213 Steel
1.6217 Steel
1.6310 Steel
1.6310 Steel
1.6310 Steel
1.6311 Steel
1.6347 Steel
1.6349 Steel
1.6359 Steel
1.6368 Steel
1.6368 Steel
1.6368 Steel
1.6511 Steel
1.6511 Steel
1.6511 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6522 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6523 Steel
1.6526 Steel
1.6541 Steel
1.6545 Steel
1.6545 Steel
1.6546 Steel
1.6546 Steel
1.6546 Steel
1.6562 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6580 Steel
1.6582 Steel
1.6582 Steel
1.6582 Steel
1.6587 Steel
1.6587 Steel
1.6587 Steel
1.6604 Steel
1.6604 Steel
1.6738 Steel
1.6738 Steel
1.6742 Steel
1.6746 Steel
1.6749 Steel
1.6751 Steel
1.6751 Steel
1.6753 Steel
1.6757 Steel
1.6780 Steel
1.6782 Steel
1.6926 Steel
1.6926 Steel
1.6926 Steel
1.6946 Steel
1.6946 Steel
1.6949 Steel
1.6956 Steel
1.6957 Steel
1.6959 Steel
1.6959 Steel
1.6985 Steel
1.6985 Steel
1.6Si Cast Iron
1.6Si Steel, 1.9Al Steel
1.6Si Steel, 1.9Al Steels
1.7003 Steel
1.7005 Steel
1.7006 Steel
1.7014 Steel
1.7015 Steel
1.7015 Steel
1.7016 Steel
1.7023 Steel
1.7025 Steel
1.7033 Steel
1.7033 Steel
1.7034 Steel
1.7034 Steel
1.7035 Steel
1.7035 Steel
1.7037 Steel
1.7037 Steel
1.7038 Steel
1.7038 Steel
1.7039 Steel
1.7039 Steel
1.7045 Steel
1.7045 Steel
1.7108 Steel
1.7131 Steel
1.7131 Steel
1.7131 Steel
1.7138 Steel
1.7139 Steel
1.7139 Steel
1.7147 Steel
1.7147 Steel
1.7149 Steel
1.7149 Steel
1.7160 Steel
1.7168 Steel
1.7176 Steel
1.7182 Steel
1.7214 Steel
1.7214 Steel
1.7218 Steel
1.7218 Steel
1.7218 Steel
1.7218 Steel
1.7219 Steel
1.7219 Steel
1.7220 Steel
1.7220 Steel
1.7223 Steel
1.7223 Steel
1.7225 Steel
1.7225 Steel
1.7225 Steel
1.7226 Steel
1.7226 Steel
1.7227 Steel
1.7227 Steel
1.7228 Steel
1.7228 Steel
1.7238 Steel
1.7238 Steel
1.7242 Steel
1.7242 Steel
1.7243 Steel
1.7243 Steel
1.7244 Steel
1.7244 Steel
1.7255 Steel
1.7255 Steel
1.7258 Steel
1.7258 Steel
1.7271 Steel
1.7273 Steel
1.7311 Steel
1.7311 Steel
1.7320 Steel
1.7323 Steel
1.7323 Steel
1.7325 Steel
1.7326 Steel
1.7335 Steel
1.7335 Steel
1.7361 Steel
1.7362 Steel
1.7362 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7380 Steel
1.7561 Steel
1.7701 Steel
1.7701 Steel
1.7701 Steel
1.7701 Steel
1.7703 Steel
1.7707 Steel
1.7707 Steel
1.7707 Steel
1.7715 Steel
1.7733 Steel
1.7733 Steel
1.7734 Steel
1.7734 Steel
1.7734 Steel
1.7734 Steel
1.7735 Steel
1.7735 Steel
1.7765 Steel
1.7767 Steel
1.7779 Steel
1.7783 Steel
1.7C, 2.28C, 2.54C, 3.34C Cast Irons
1.8070 Steel
1.8154 Steel
1.8154 Steel
1.8159 Steel
1.8159 Steel
1.8159 Steel
1.8159 Steel
1.8159 Steel
1.8161 Steel
1.8161 Steel
1.8506 Steel
1.8507 Steel
1.8509 Steel
1.8515 Steel
1.8515 Steel
1.8519 Steel
1.8519 Steel
1.8521 Steel
1.8521 Steel
1.8523 Steel
1.8550 Steel
1.8550 Steel
1.8807 Steel
1.8814 Steel
1.8903 Steel
1.8905 Steel
1.8905 Steel
1.8905 Steel
1.8905 Steel
1.8918 Steel
1.8918 Steel
1.8918 Steel
1.8928 Steel
1.8931 Steel
1.8940 Steel
1.8983 Steel
1.95C-10.80Cr-3.80Mo Alloyed White Cast Iron
1.95C-10.80Cr-3.80Mo Alloyed White Cast Iron
1.96C-15.40Cr-2.20Mo Alloyed White Cast Iron
1.96C-15.40Cr-2.20Mo Alloyed White Cast Iron
1.98C-20.25Cr-2.14Mo Alloyed White Cast Iron
1.98C-20.25Cr-2.14Mo Alloyed White Cast Iron
1.98TC Steel
1.9N Steel
1/2 Cr Mo Steel
1/2 Cr Mo Steel
1/2 Cr Mo V Steel
1/2 Cr Steel
1/2 Cr Steel
1/2 Cr Steel
1/2 Cr Steel
1/2 Mo Steel
1/2 Mo Steel
1/2 Ni Cr Mo Steel
1/2 Ni Cr Mo Steel
1/2 Ni Cr Mo Steel
1/2 Ni Cr Mo Steel
1/2 Ni Cr Mo Steel
1/2 Ni Cr Mo Steel
1/2 Ni Steel
1/4 Mo Steel
1/4 Mo Steel
1/4 Mo Steel
1/4 Mo Steel
1/4 Mo Steel
10 CAD 8 Steel
10 CD 9-10 Steel
10 CD 9-10 Steel
10 ChSND/Ch.1 Steel
10 ChSND/Ch.2 Steel
10 CrMo 9.10 Steel
10 G 2 S1D/Ch.1 Steel
10 G 2 S1D/Ch.2 Steel
10 G 2S1 Steel
10 MnCrMo 5.5.4 Steel
10 MnCrMo 6.5.3 Steel
10 MnCrMo 6.5.4 Steel
10 MnCrNiMo 5.6.2.4 Steel
10 MnCrNiMo 6.6.4.1 Steel
10 MnCrNiMo 6.6.4.4 Steel
10 N 14 Steel
10 N 14 Steel
10 N 8 Steel
10 NC 12 Steel
10 NC 6 Steel
10 NC 6 Steel
10% Nickel Steel, 0.50% C
10% Nickel Steel, 0.80% C
10% Nickel Steel, 1.2% C
100 C 3 Steel
100 C 6 Steel
100 C 6 Steel
100 CD 7 Steel
100 CD 7 Steel
100 CV 6 Steel
100 WC 10 Steel
100 WC 40 Steel
100 WC 40 Steel
1006/1008 Steel
1008 Steel
100A2 Steel
100A2 Steel
100B2 Steel
100B2 Steel
100C2 Steel
100C2 Steel
100Cr2 Steel
100Cr2 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel
100Cr6 Steel - Dry Grind-Hardening Process
100Cr6 Steel - Wet Grind-Hardening Process
100CrMn6 Steel
100CrMn6 Steel
100CrMn6 Steel
100CrMnSi6-4 (100CrMn6) Steel
100CrMnSi6-4 (100CrMn6) Steel
100CrMo6 Steel
100CrMo7 Steel
100CrMo7-3 Steel
100CrMo7-3 Steel
100CrMo7-3 Steel
100CrMo7-3 Steel
1010 Mo Steel
1010 Mo-B Steel
1010 Mo-B Steel
1010 Steel
1010 Steel
1010 Steel
1019 Steel
1019 Steel
1021 + 1 Ni + 0.5 Cr Steel
1021 + 1 Ni + 1 Cr Steel
1021 + 1 Ni + 2 Cr Steel
1021 + 1Ni + 0.5Mo Steel
1021 + 1Ni + 0.75Si Steel
1021 + 1Ni + 2Si Steel
1021 Steel
1021 Steel
1021 Steel
1021+1Ni/1021+1N+0.75Si Steel
1021+1Ni/1021+1Ni+0.25Mo Steel
1021+1Ni/1021+1Ni+0.5Cr Steel
1021+1Ni/1021+1Ni+0.5Mo Steel
1021+1Ni/1021+1Ni+1Cr Steel
1021+1Ni/1021+1Ni+2Cr Steel
1021+1Ni/1021+1Ni+2Si Steel
1021+1Ni/1021+1Ni+B Steel
1021+Ni/1021+1Ni+Mn Steel
1021/1021 + 1 Ni Steel
1022AK Steel
1022M1 Steel
102Cr6 Steel
102Cr6 Steel
1030 Mod. Steel
1030 Steel
1030 Steel
1030 Steel
1034 Steel
1035 Mod. Steel
1035 Steel
1036 Steel
1036 Steel
1038 Steel
1038 Steel
1040 Steel
1040 Steel
1045 Steel
1045/1050 Steel
1045/1050+Cu Steel
1045/1050+Cu Steel
1045/1050+Cu Steel
1050 Steel
1050 Steel
1050 Steel
1055 Mod. Steel
105Cr2 Steel
105Cr4 Steel
105CrW6 Steel
105CrW6 Steel
1060 Mod./1065 Mod. Steel
1060 Steel
1060 Steel
1060 Steel
1060/10B60 Steel
1070 Steel
1078 Steel
1078 Steel
1078 Steel
1080 Steel
1080 Steel
1080 Steel
1080 Steel
1086/1095 Steel
1086/1095+0.25V Steel
1090 Steel
1095 + 0.25V Steel
1095 Steel
1095 Steel
1095 mod. Steel
10B22 Steel
10B36 Steel
10B36 Steel
10B60 Steel
10Cr Steel
10Cr Steel
10CrMo5-5 (P4), 10CrMo9-10 (P5A), X10CrMoVNb9-1 (P15E) Steels
10CrMo5-5, 10CrMo9-10, X10CrMoVNb9-1 Steels
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
10CrSiMoV-7 Steel
10CrSiNiCu Steel
10G Steel
10G2ANb Steel
10G2AV Steel
10G2AVNb Steel
10G2FB Steel
10GN2MFA Steel
10HA Steel
10HNAP Steel
10N3 Steel
10Ni-0.1C Steel
10Ni14 Steel
10Ni3MnCuAl Steel
10NiCr6 Steel
10NiCr6 Steel
10V45Nb Steel
11.20Cr Cast Iron
11.20Cr Steel
113 Steel
114 Steel
12 Cr Mo V Steel
12 CrMo 4.3 Steel
12 NC 15 Steel
12 ND 16 Steel
12% Cr Martensitic Steel
12%Cr USC Rotor Steel
12.0Cr-1Mo Steel
12.P2 Steel
120 NCD 5-02 Steel
1210 Steel
12Cr Ferritic Stainless Steel
12Cr Ferritic Stainless Steel
12Cr Ferritic Stainless Steel
12Cr Ferritic Stainless Steel
12Cr-1Mo-1W-V-Nb Steel
12Cr-1MoV Steel
12Cr1MoV Steel
12Cr1MoV Steel
12CrMo Steel
12CrMo Steel
12CrMo19-5 Steel
12CrMo4 Steel
12Ni19 Steel
12Ta, 13Ta, 4Ta, F82H, JLF1 Steels
13 Cr Steel
13 Cr Steel
13 Cr Steel
13 Cr Steel
13 Cr Steel
13 CrMo 4.4/Ch.1 Steel
13 CrMo 4.4/Ch.2 Steel
13 CrMo 4.4/Ch.3 Steel
13 MnCuNi 6.6.2 (N) Steel
13 MnCuNi 6.6.2 (V) Steel
13 MnNiCu 8.2.6 Steel
1320 Carburized to 0.4C Steel
1320 Carburized to 0.6C Steel
1320 Carburized to 1.0C Steel
1320 Steel
1321 Carburized to 0.8C Steel
1321 Carburized to 1.2C Steel
1335 Steel
1335 Steel
1340 Steel
1340 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
13CrMo44 Steel
13CrMo44 Steel
13HMF Steel
13HNMBA Steel
13MnSi6-5 Steel
13NiCr6 Steel
13NiCr6 Steel
13NiCr6, 16NiCrS4 Steels
13NiCr6, 16NiCrS4 Steels
14 Cr 2 MnMoB Steel
14 NC 11 Steel
14 NC 11 Steel
14 NC 12 Steel
14 NCD 4 Steel
140 C 10 Steel
144 Steel
145Cr6 Steel
145Cr6 Steel
145V33 Steel
14CrMoV6-9 Steel
14CrMoV6-9 Steel
14GN2M Steel
14HGN3M Steel
14HGS Steel
14HNMBCu Steel
14MoV6-3 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14MoV6-3 Steel
14Ni6 Steel
14NiCr10 Steel
14NiCr10 Steel
14NiCr14 Steel
14NiCr14 Steel
14NiCr14 Steel
14NiCr18 Steel
14NiCr18 Steel
14NiCrMo13-4 Steel
14NiCrMo13-4 Steel
15 Ch 1M 1F Steel
15 G 2N Nb Steel
15 GA 2A Nb Steel
15 GA Steel
15 GB Steel
15 MDV 4-05 Steel
15 MDV 4-05 Steel
15 MDV 4-05 Steel
15 MDV 4-05 Steel
15 Mo 3 Steel
15 NCDV 11 Steel
15 NCDV 11 Steel
15-2-1 LC White Cast Iron
15-7 PH Steel
150 Steel
15218 Steel
1524MoV Steel
1541 Steel
1541 Steel
1541 Steel
1566 Steel
1572 Steel
157C Steel
15B41 Steel
15Cr-15Mn-4Ni Steel
15Cr-15Mn-4Ni Steels
15Cr-25Ni-Al-Ti Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15Cr3 Steel
15CrMnMoV Steel
15CrMo Steel
15CrMo Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15CrNi6 Steel
15G2ANb Steel
15G2ANbT Steel
15G2ANbTB Steel
15G2AT Steel
15G2ATB Steel
15GA Steel
15H2MFA Steel
15H2MFA-A Steel
15H2MFA-A grade A Steel
15HM Steel
15Kh2NMFA Steel
15Kh2NMFA-A Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15Mo3 Steel
15NCuMNb (K32Nb) Steel
15NiCr13 Steel
15NiCuMoNb5 Steel
15NiCuMoNb5 Steel
16 MC 5 Steel
16 MC 5 Steel
16 NC 18 Steel
16 NC 6 Steel
16 NC 6 Steel
16 NCD 13 Steel
16 NCD 13 Steel
16CD4 Steel
16CD4 Steel
16CMnR Steel
16CMnR Steel
16CrMo4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrMo4 Steel
16CrNi4 Steel
16CrNi4 Steel
16CrNi4 Steel
16CrNi4 Steel
16GNM Steel
16MND5 Steel
16MND5 Steel
16MND5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5 Steel
16MnCr5, 16MnCrS5 Steels
16MnCr5, 16MnCrS5 Steels
16MnCrB5 Steel
16MnCrB5 Steel
16MnCrB5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16MnCrS5 Steel
16MnCrS5, 20MnCrS5 Steels
16MnCrS5, 20MnCrS5 Steels
16MnCrS5, 20MnCrS5 Steels
16NiCr11 Steel
16NiCr4 Steel
16NiCr4 Steel
16NiCrMo12 Steel
16NiCrMo12 Steel
16NiCrMo2 Steel
16NiCrS4 Steel
17 CrMoV 10 Steel
17 MV Az 6 Steel
17-7 PH Steel
17-7 PH Steel
17Cr-13Ni-5Mo Alloy
17Cr3 Steel
17Cr3 Steel
17Cr3 Steel
17CrMoV10 Steel
17CrMoV10 Steel
17CrNi6-6 Steel
17CrNi6-6 Steel
17CrNi6-6, 15CrNi6 Steels
17CrNi6-6, 15CrNi6 Steels
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrNiMo6 Steel
17CrS3 Steel
17G1S, 10G2S, 16G2AF, 35KhM, 35KhGSM, 50KhNM Steels
17Mn4 Steel
17Mn4 Steel
17MnB4 - 20MnB4 - 22MnB4 - 23MnB4 Steels
17MoV8-4 Steel
17MoV8-4 Steel
17NiCrMo6-4 Steel
17NiCrMo6-4 Steel
17NiCrMoS6-4 Steel
17NiCrMoS6-4 Steel
18 C 3 Steel
18 CD 4 Steel
18 CD 4 Steel
18 CDSV 5 Steel
18 CDSV 5 Steel
18 Cr Ni Steel
18 NCD 6 Steel
18 NCD-4 Steel
18-0-1 Steel
18-4-1 + 5Co Steel
18-4-1 Steel
18-4-1 Steel
18-8 Steel
18-8 Steel
18/8 CrNi Steel
183 Steel
18Cr-15Ni Stainless Steel
18Cr-2Mo Ferritic Stainless Steel
18Cr-2Mo Ferritic Stainless Steel
18Cr-2Mo-Ti Stabilized Ferritic Stainless Steel
18Cr-2Mo-Ti Stabilized Ferritic Stainless Steel
18Cr-4Ni-2.5Mo Steel
18Cr-8Ni Austenitic Stainless Steel
18Cr-9Ni Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMo4 Steel
18CrMoS4 Steel
18CrMoS4 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNi8 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel
18CrNiMo7-6 Steel Steel
18G2A Steel
18G2ANb Steel
18G2AV Steel
18H2N4MA Steel
18Kh2N4VA Steel
18MnCr4 Steel
18MnCr4 Steel
18Ni200 Steel
18Ni250 Steel
18Ni300 Steel
18Ni350 Steel
18NiCr5-4 Steel
18NiCr5-4 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo5 Steel
18NiCrMo7 Steel
18NiCrMo7 Steel
19 M Nb 6 Steel
1906 Menganese Steel I
1906 Menganese Steel II
19Mn5 Steel
19Mn5 Steel
19Mn5 Steel
19Mn5 Steel
1C Steel
1C-0.21Si-0.98Mn-0.63Cr Steel
1C-0.21Si-0.98Mn-0.63Cr Steel
1C-0.3Mo Steel
1C-1.5Ni-0.8Cr-0.26Mo Steel
1C-2.9Cr Steel
1C-2Mn Steel
1C-4Cr Steel
1C-5.7Cr Steel
1C-8.8Cr Steel
1CH13N3 Steel
1CMo Steel
1CNb Steel
1CSi Steel
1Cr Steel
1Cr, 2.5Cr, 4Cr Steels
1Cr-0.3Mo-0.3V PM Steel
1Cr-0.5Mo Steel
1Cr-0.5Mo-B Steel
1Cr-1Mo-0.2V Steel
1Cr0.5Mo Steel
1Cr0.5Mo Steel
1F Steel
1F Steel
1H16AN4M3 Steel
1K Steel
1K Steel
1M Steel
1M Steel
1N Steel
1N Steel
1Ni Steel
1Ni Steel
1OCrMoV Steel
2 1/2 Ni- 1/2 Mo Turbine Rotor Steel
2 1/2 Nickel Saw Steel
2 1/4% Cr - 1% Mo Steel
2 1/4Cr-1 Mo Steel
2 3/4 Nickel Forging Steel
2 Ni Cr Mo Steel
2 Ni Cr Mo Steel
2 Ni Cr Steel
2 Si Mn Steel
2 Si Mn Steel
2 Si Mn Steel
2 Si Mo Steel
2-1/2 Cr Mo V Steel
2-1/2 Ni Cr Mo Steel
2-1/2 Ni Cr Mo Steel
2-1/2 Nickel Saw Steel
2-1/2Ni-1/2Mo Turbine Rotor Steel
2-1/4 Cr Mo Steel
2-1/4Cr-1% Mo Steel
2-1/4Cr-1% Mo Steel
2-1/4Cr-1% Mo Steel
2-1/4Cr-1Mo Steel
2-1/4Cr-1Mo Steel
2-1/4Cr-1Mo Steel
2-1/4CrlMo Steel
2-3/4 Nickel Forging Steel
2-9-2 Steel
2.00C-V Steel
2.00Cr Cast Iron
2.04C-20.55Cr-0.61Mo Alloyed White Cast Iron
2.04C-20.55Cr-0.61Mo Alloyed White Cast Iron
2.05C-15.60Cr-0.81Mo Alloyed White Cast Iron
2.05C-15.60Cr-0.81Mo Alloyed White Cast Iron
2.08C-15.85Cr Alloyed White Cast Iron
2.08C-15.85Cr Alloyed White Cast Iron
2.08C-20.55Cr-0.01Mo Alloyed White Cast Iron
2.08C-20.55Cr-0.01Mo Alloyed White Cast Iron
2.08C-V Steel
2.13C-11.30Cr-1.41Mo Alloyed White Cast Iron
2.13C-11.3Cr-1.41Mo Alloyed White Cast Iron
2.16TC Steel
2.19C-11.65Cr-0.02Mo Alloyed White Cast Iron
2.19C-11.65Cr-0.02Mo Alloyed White Cast Iron
2.19C-V Steel
2.25 Cr-1Mo Steel
2.25Cr-1Mo I Steel
2.25Cr-1Mo II Steel
2.25Cr-1Mo Steel
2.25Cr-1Mo Steel
2.25Cr-1Mo Steel
2.25Cr-1Mo Steel
2.25Cr-1Mo Steel
2.25Cr-1Mo Steel
2.25Cr-1Mo, 2.25Cr-1Mo-V-Ti-B Steels
2.25Cr-1Mo, 2.25Cr-1Mo-V-Ti-B Steels
2.25Cr-1Mo-0.25V Steel
2.25Cr-1Mo-0.25V Weld, 2.25Cr-1Mo-0.25V Base Metal
2.25Cr-l.00Mo Steel
2.25Cr-lMo Steel
2.25Cr1Mo Steel
2.25Cr1Mo Steel
2.25Cr1Mo Steel
2.25Cr1Mo Steel
2.25Cr1Mo Steel
2.25Cr-1Mo Steel
2.35N Steel
2.3Mo-0.22C Steel
2.41C-12.15Cr-2.45Mo Alloyed White Cast Iron
2.41C-12.15Cr-2.45Mo Alloyed White Cast Iron
2.45C-19.82Cr-2.94Mo Alloyed White Cast Iron
2.45C-19.82Cr-2.94Mo Alloyed White Cast Iron
2.50C-2.50Si-0.85Mn Cast Iron
2.50C-2.50Si-0.85Mn Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.10Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.30Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-2.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-3.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-4.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-0.50Mo-5.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-1.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-2.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-3.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-4.00Ni Cast Iron
2.50C-2.50Si-0.85Mn-0.10P-1.00Mo-5.00Ni Cast Iron
2.50C-V Steel
2.54C-20.22Cr-1.52Mo Alloyed White Cast Iron
2.54C-20.22Cr-1.52Mo Alloyed White Cast Iron
2.55C-0.25Si-0.35Mn-11.80Cr-0.65W Steel I
2.55C-0.25Si-0.35Mn-11.80Cr-0.65W Steel II
2.55C-0.25Si-0.35Mn-11.80Cr-0.65W Steel III
2.55C-12.40Cr-1.25Mo Alloyed White Cast Iron
2.55C-12.40Cr-1.25Mo Alloyed White Cast Iron
2.5C, 3.0C, 3.5C Cast Irons
2.5Cr-1Mo Steel - Steel 11
2.5Cr-1Mo Steel - Steel 14
2.5Cr-1Mo Steel - Steel 15
2.5Cr-1Mo Steel - Steel 2
2.5Cr-1Mo Steel - Steel 3
2.5Cr-1Mo Steel - Steel 32
2.5Cr-1Mo Steel - Steel 4
2.5Cr-1Mo Steel - Steel 8
2.5Ni-Cr-Mo High Carbon Steel
2.5Ni-Cr-Mo High Carbon Steel
2.5Ni-Cr-Mo Medium Carbon Steel
2.5Ni-Cr-Mo Medium Carbon Steel
2.5Si Cast Iron
2.5TC-1Ni-0.1Mo Steel
2.5TC-1Ni-0.5Mo Steel
2.5TC-1Ni-1Mo Steel
2.5TC-2Ni-0.5Mo Steel
2.5TC-2Ni-1Mo Steel
2.5TC-3Ni-0.5Mo Steel
2.5TC-3Ni-1.0Mo Steel
2.5TC-4Ni-0.5Mo Steel
2.5TC-4Ni-1Mo Steel
2.5TC-5Ni-0.5Mo Steel
2.5TC-5Ni-1Mo Steel
2.60C-0.4Mn-1.4Si-B Malleable Iron
2.60C-0.4Mn-1.4Si-B Malleable Iron
2.60C-0.4Mn-1.4Si-B Malleable Iron
2.60C-15.20Cr-1.95Mo Alloyed White Cast Iron
2.60C-15.20Cr-1.95Mo Alloyed White Cast Iron
2.65C-12.65Cr-0.02Mo Alloyed White Cast Iron
2.65C-12.65Cr-0.02Mo Alloyed White Cast Iron
2.67C-14.95Cr Alloyed White Cast Iron
2.67C-14.95Cr Alloyed White Cast Iron
2.67C-15.20Cr-1.09Mo Alloyed White Cast Iron
2.67C-15.20Cr-1.09Mo Alloyed White Cast Iron
2.67C-20.75Cr-0.01Mo Alloyed White Cast Iron
2.67C-20.75Cr-0.01Mo Alloyed White Cast Iron
2.6C, 3.0C, 2.6C Cast Irons
2.6C, 3.0C, 2.6C Cast Irons
2.6C, 3.0C, 3.6 Cast Irons
2.6N Alloy
2.6Ni-0.4Mo Steel
2.72C-25.15Cr-2.52Mo Alloyed White Cast Iron
2.72C-25.15Cr-2.52Mo Alloyed White Cast Iron
2.73C-0.03Mn-1.25Si-0.015S White Iron
2.75C-0.13Mn-1.21Si-0.008S White Iron
2.7Ni-0.9Cr-0.25Mo-B Steel
2.7Ni-0.9Cr-0.5Mo-B Steel
2.84V, 3.70V, 6.78V, 8.73V Cast Irons
2.87C-25.50Cr-1.22Mo Alloyed White Cast Iron
2.87C-25.50Cr-1.22Mo Alloyed White Cast Iron
2.90C-0.60Si-0.70Mn-19.40Cr-2.10Mo-1.00Cu Cast Iron
2.92C-17.59Cr-1.05Nb, 2.96C-17.68Cr-2.71Nb Cast Irons
2.93C-0.60Si-0.78Mn-17.4Cr-0.04Mo White Cast Iron
2.93C-1.89Si-0.74Mn-0.218P-0.513Mo Iron
2.95C-25.82Cr-0.02Mo Alloyed White Cast Iron
2.95C-25.82Cr-0.02Mo Alloyed White Cast Iron
2.96C-0.52Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
2.96C-0.93Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
2.97C-2.00Si Grey Cast Iron
2.97C-2.00Si Grey Cast Iron
2.97C-2.02Si-0.82Mn-0.30P Cast Iron
2.9C-0.6Si-17.0Cr-Mn-Mo White Cast Iron
2.9C-0.6Si-17.0Cr-Mn-Mo White Cast Iron
2.9C-0.6Si-17.0Cr-Mn-Mo White Cast Iron
2.9C-0.7Mn-0.6Si-17.5Cr White Cast Iron (Mo Addition)
2.9C-0.7Mn-0.6Si-17.5Cr White Cast Iron (Mo Addition)
2.9C-0.7Mn-0.6Si-17.5Cr White Cast Iron (Mo Addition)
2.9C-0.8Mn-0.6Si-17.0Cr-1.5Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.0Cr-1.5Mo-Si-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.0Cr-1.5Mo-Si-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo-Cu White Cast Iron
2.9C-0.8Mn-0.6Si-17.5Cr-Ni-Mo-Cu White Cast Iron
2.9Mn-0.7Si Steel
2.9TC-0.5Mo Steel
20 CDV 5-08 Steel
20 CDV 5-08 Steel
20 CrMoV 13.5 Steel
20 NC 6 Steel
20 NC 6 Steel
20 NCD 10 Steel
20 NCD 10 Steel
20 NCD 2 Steel
20 NCD 2 Steel
20 NCD 7 Steel
20 NCD 7 Steel
20 NCD 8 Steel
20 ND 16 Steel
20 ND 16 Steel
20 ND 8 Steel
20 ND 8 Steel
20-2-1 LC White Cast Iron
2006 TUNGSTEN Steel
206 Steel
2083/2083 SUPRA ESR Steel
20Cr and 12 to 16Ni Stainless Steel
20Cr and 12 to 16Ni Stainless Steel
20Cr and 12 to 16Ni Stainless Steel
20CrMo2 Steel
20CrMo2 Steel
20CrMo5 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrMoV13-5 Steel
20CrNi4 Steel
20CrNi4 Steel
20CrNi4 Steel
20G2ANbY Steel
20G2AVY Steel
20G2AY Steel
20G2SMRA Steel
20GFL Steel
20H12M1F Steel
20H2N4A-T Steel
20H2N4A-T Steel
20H2N4A-T Steel
20H3MWF Steel
20Kh2N4A Steel
20M (K22M) Steel
20Mn2Cr, 20Mn2CrNb Steels
20Mn5 Steel
20MnB4 Steel
20MnB4 Steel
20MnB8 Steel
20MnB8 Steel
20MnB8 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5 Steel
20MnCr5, 20MnCrS5 Steels
20MnCrB5 Steel
20MnCrB5 Steel
20MnCrS5 Steel
20MnCrS5 Steel
20MnCrS5 Steel
20MnCrS5 Steel
20MnCrS5 Steel
20MnMo4 Steel
20MnMo55 Steel
20MnMoNi4-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
20MnMoNi5-5 Steel
:35:16
20Mo5 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr4 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCr5 Steel
20MoCrS4 Steel
20MoCrS4 Steel
20MoCrS4 Steel
20MoCrS4 Steel
20MoCrS4 Steel
20NiCr6 Steel
20NiCr6 Steel
20NiCrMo14-6 Steel
20NiCrMo14-6 Steel
20NiCrMo2 Steel
20NiCrMo2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2 Steel
20NiCrMo2-2, 20NiCrMoS2-2 Steels
20NiCrMo2-2, 20NiCrMoS2-2 Steels
20NiCrMo3 Steel
20NiCrMo3 Steel
20NiMoCr6 Steel
20NiMoCr6 Steel
20NiMoCr6-5 Steel
20NiMoCr6-5 Steel
20NiMoCrS6 Steel
20g Steel
20g Steel
21/4Cr-1Mo Steel
2162 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21CrMoV5-11 Steel
21HG2SB Steel
21HG2SB Steel
21Mn5 Steel
21Mn6AlX1 Steel
21Mn6AlX1 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
21NiCrMo2 Steel
22 N 8 Steel
22.59% Cr Cast Iron
22.59Cr Steel
2205 Duplex Stainless Steel
2205 Steel
2210 Steel
22CrMoH Steel
22MnB4 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnB5 Steel
22MnCrN5-X Steel
22MnCrNiMo Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
22NiMoCr3-7 Steel
2311 Steel
23110 Steel
2312 Steel
2315 Steel
2315 Steel
2316/4122 Steel
2330 Steel
2330 Steel
2330 Steel
2330 Steel
2330 Steel
2330 Steel
2340 Steel
2340 Steel
2340 Steel
2340 Steel
2340 Steel
2343 EFS/EFS SUPRA ESR Steel
2344 EFS/EFS SUPRA ESR Steel
2361/4112 EFS/EFS SUPRA ESR Steel
2363 Steel
2365 EFS Steel
2367 EFS/EFS SUPRA ESR Steel
23CrMoB3-3 Steel
23CrMoB3-3 Steel
23CrNi3Mo Carburised Steel
23MnB4 Steel
23MnNiCrMo5-3 Steel
23MnNiCrMo5-4 Steel
23MnNiCrMo5-4 Steel
24 CrMo Steel
24 CrNi 3 MoV Steel
24 CrNiMoV 8.5.7 Steel
24.0Ni-4.0Mn Steel
2410 Manganese Steel I
2410 Manganese Steel II
2436 Steel
24CrMo5 Steel
24CrMo5 Steel
24CrMo5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24CrMoV5-5 Steel
24Mn5 Steel
24Mn5 Steel
24Mn6 Steel
24Mn-18Cr-3Ni-0.62N Steel
25 CD 4 Steel
25 CD 4 Steel
25 M 6 Steel
25 M 6 Steel
25.7Cr-22.8Ni Austenitic Stainless Steel
2507 Steel
2510 SDSS Steel
2510 Steel
2512 (0.4 C) Carburized Steel
2512 (0.6 C) Carburized Steel
2512 (0.8 C) Carburized Steel
2512 (1.0 C) Carburized Steel
2512 (1.2 C) Carburized Steel
2512 Carburized to 0.4C Steel
2512 Carburized to 0.6C Steel
2512 Carburized to 0.8C Steel
2512 Carburized to 1.0C Steel
2512 Carburized to 1.2C Steel
2512 Steel
2512 Steel
2512 Steel
254 SMO Steel
2550 Steel
25Cr-3Mo-4Ni Ferritic Stainless Steel
25Cr-3Mo-4Ni Ferritic Stainless Steel
25Cr-3Mo-7Ni, 23Cr-6Ni Steels
25Cr-6.9Ni-3.8Mo-0.3N Steel
25Cr-7Ni-3Mo Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMo4 Steel
25CrMoS4 Steel
25CrMoS4 Steel
25HMCu Steel
25KhGM, 25KhGT Steels
25KhGT Steel
25MnCrSiVB6S Steel
25MnSiNiMo, 20CrMnSiNiMo1, 20CrMnSiNiMo Steels
25MoCr4 Steel
25MoCr4 Steel
25MoCr4 Steel
26Cr-1-4Mo-0-4Ni Alloy
26CrMo4 Steel
26G2S Steel
26MnSiVS7 Steel
26MnSiVS7 Steel
26NiCr6-4 Steel
26NiCr6-4 Steel
271 Steel
2714 Steel
272 Steel
273 Steel
2738/2738 HH Steel
275 Steel
2764 Steel
2767/2767 SUPRA ESR Steel
27MnCrB5 Steel
27MnCrB5 Steel
27MnCrB5-2 Steel
27MnCrB5-2 Steel
27MnCrV4 Steel
27MnCrV4 Steel
27MnSiVS6 Steel
27MnSiVS6 Steel
27MnSiVS6 Steel
27MnSiVS6 Steel
28 CDV 5-08 Steel
28 CDV 5-08 Steel
28 CrNi 7Mo Steel
28 NCD 6 Steel
28 NCD 6 Steel
280 Steel
281P Steel
2826 Steel
2842 Steel
287 Steel
28CrMoNiV4-9 Steel
28CrMoNiV4-9 Steel
28Mn6 Steel
28Mn6 Steel
28Mn6 Steel
28NCD6 Steel
28NbHC Steel
28NiCrMo7 Steel
28NiCrMo7 Steel
28NiCrMo7 Steel
28NiCrMo7-4 Steel
28NiCrMo7-4 Steel
29-4 Ferritic Stainless Steel
290 Steel
2908 Manganese Steel
2910 Steel
294 Steel
295 Steel
297 Steel
2990 Steel
29Cr-4Mo Ferritic Stainless Steel
29Cr-4Mo Ferritic Stainless Steel
29Cr-4Mo-2Ni Ferritic Stainless Steel
2C-5Cr-5Mo-5W-5V-5Co Steel
2CrMoNiWV Steel
2H 6D Steel
2H 6D Steel
2H 7C Steel
2H 7C Steel
2H 7C Steel
2H-50 Steel
2H-50 Steel
2H-Cr Steel
2H-Cr Steel
2H-Supper Steel
2H-Supper Steel
2H-Te Steel
2H-Te Steel
2H-Ultra Steel
2H-Ultra Steel
2HA Steel
2HA Steel
2HB Steel
2HB Steel
2HB Steel
2HB Steel
2HB Steel
2HB1 Steel
2M Steel
2M Steel
2Mn Steel
2Mn Steel
2Mo Cast Iron
2Ni-1.3Cr-0.5Mo Steel
2Ni-3Cr-0.7Mo, 3Cr-0.7Mo-0.15V, 3.5Ni-0.6Mo-0.15V Steels
2Si, 3Si Cast Irons
2Si, 3Si Cast Irons
3 1/4 Ni-Cr-Mo Steel
3 Cr Mo Steel
3 Cr Mo Steel
3 Cr Mo Steel
3 Ni Cr Mo Steel
3 Ni Cr Mo Steel
3 Ni Cr Steel
3 Ni Steel
3 Ni-Cr-Mo-V Steel
3%Si-0.45%C-X Steel
3-1/2 Ni Cr Mo Steel
3-1/2 Ni Mo Steel
3-1/2 Ni Steel
3-1/2 Ni Steel
3-1/2 Ni Steel
3-1/2 Si Cr Steel
3-1/2NiCrMoV Turbine Disk Steel
3-1/2NiCrMoV Turbine Disk Steel
3-1/4 Cr Mo Steel
3-1/4 Cr Mo Steel
3-1/4 Cr Mo V Steel
3-1/4 Ni Cr Steel
3-1/4Ni-Cr-Mo Steel
3.00C-1.85Si-0.73Mn-0.216P-0.249Mo Cast Iron
3.00Mn Cast Iron
3.04C-1.83Si-0.72Mn-0.212P-0.149Mo Cast Iron
3.06C-0.73Si, 3.11C-1.61Si, 3.04C-2.60Si, 3.09C-2.53Si, 3.09C-4.48Si Cast Irons
3.06C-1.79Si-0.57Mn-0.60Mo Cast Iron
3.12C-1.91Si-0.76Mn-0.21P-0.086Mo Cast Iron
3.14C-2.15Si-0.81Mn-0.219P Grey Cast Iron
3.14TC-2.15Si Steel
3.17C-2.0Si-0.75Mn-0.30Mo-0.60Cu Grey Cast Iron
3.1TC-0.09Mo Steel
3.25C-11.80Cr-2.60Mo Alloyed White Cast Iron
3.25C-11.80Cr-2.60Mo Alloyed White Cast Iron
3.25Si Steel
3.25Si Steel
3.29C-2.35Si-0.07Mn-1.90Mo-0.94Ni Cast Iron
3.2C-0.3Mn-2.36Si-4.82Ni-0.4Mo Alloyed Ductile Iron
3.30C-0.3Mn-2.6Si Ductile Iron
3.30C-0.3Mn-2.6Si Ductile Iron
3.30C-0.3Mn-2.6Si Ductile Iron
3.39C-11.95Cr-1.36Mo Alloyed White Cast Iron
3.39C-11.95Cr-1.36Mo Alloyed White Cast Iron
3.3C-0.3Mn-2.45Si-0.6Ni-0.5Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.46Si-1.17Ni-0.4Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.4Si-2.37Ni-0.5Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.57Si-0.7Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.58Si-0.4Mo Alloyed Ductile Iron
3.3C-0.3Mn-2.69Si-0.2Mo Ductile Cast Irons
3.3C-0.3Mn-2.6Si-0.2Mo Alloyed Ductile Iron
3.40C-19.85Cr-3.40Mo Alloyed White Cast Iron
3.40C-19.85Cr-3.40Mo Alloyed White Cast Iron
3.40C-2.69Si-0.52Mn Cast Iron I
3.40C-2.69Si-0.52Mn Cast Iron II
3.40C-2.69Si-0.52Mn Cast Iron III
3.45C-16.01Cr, 3.56C-15.74Cr-0.92Mo, 3.70C-15.93Cr-2.96Mo Cast Irons
3.4C-0.3Mn-2.47Si-0.5Mo Alloyed Ductile Iron
3.4C-0.3Mn-2.4Si-0.5Mo Ductile Iron (Ni Addition)
3.4C-0.3Mn-2.4Si-0.5Mo Ductile Iron (Ni Addition)
3.4C-0.3Mn-2.4Si-0.5Mo Ductile Iron (Ni Addition)
3.4C-0.3Mn-2.6Si Nonalloyed Ductile Iron
3.4NiCrMoV Rotor Steel
3.5% Chromium Magnet Steel
3.50Cr Cast Iron
3.51C-12.20Cr-0.02Mo Alloyed White Cast Iron
3.51C-12.20Cr-0.02Mo Alloyed White Cast Iron
3.51C-20.10Cr-1.37Mo Alloyed White Cast Iron
3.51C-20.10Cr-1.37Mo Alloyed White Cast Iron
3.52C-24.65Cr-2.67Mo Alloyed White Cast Iron
3.52C-24.65Cr-2.67Mo Alloyed White Cast Iron
3.56C-14.60Cr-0.47Mo Alloyed White Cast Iron
3.56C-14.60Cr-0.47Mo Alloyed White Cast Iron
3.58C-14.45Cr Alloyed White Cast Iron
3.58C-14.45Cr Alloyed White Cast Iron
3.58C-14.65Cr-0.52Mo Alloyed White Cast Iron
3.58C-14.65Cr-0.52Mo Alloyed White Cast Iron
3.5C-0.2Mn-2.71Si Nonalloyed Ductile Iron
3.5C-0.3Mn-2.69Si-0.4Mo Ductile Cast Iron
3.5C-0.3Mn-3.45Si Nonalloyed Ductile Iron
3.5Ni Steel
3.5Ni Steel
3.5Ni-Cr-Mo Steel
3.61C-15.92Cr-0.89V, 3.60C-16.11Cr-2.89V Cast Irons
3.62C-20.35Cr-0.01Mo Alloyed White Cast Iron
3.62C-20.35Cr-0.01Mo Alloyed White Cast Iron
3.62Mn-23.2Ni Steel
3.63C-1.75Si-0.53Mn-0.56P-0.10S Grey Cast Iron
3.66C-24.95Cr-1.53Mo Alloyed White Cast Iron
3.66C-24.95Cr-1.53Mo Alloyed White Cast Iron
3.68C-1.20Si-0.37Mn-0.28P-0.11S-2.03Ni Cast Iron
3.68C-9.70Cr, 3.45C-16.0Cr, 2.3C-25.5Cr Cast Irons
3.6C-0.2Mn-2.83Si Nonalloyed Ductile Iron
3.6C-0.3Mn-2.61Si Ductile Cast Iron
3.6C-0.3Mn-2.75Si Ductile Cast Iron
3.6C-0.3Mn-2.7Si Ductile Cast Iron
3.6C-0.3Mn-3.68Si Nonalloyed Ductile Iron
3.6Ni-0.5Mo Steel
3.6TC-1.75Si Steel
3.70C-2.30Si-0.25Mn Steel
3.70C-25.32Cr-0.02Mo Alloyed White Cast Iron
3.70C-25.32Cr-0.02Mo Alloyed White Cast Iron
3.72C-2.32Si-0.31Mn-0.50Cr-3.85Ni-1.03Cu Cast Iron
3.75C-2.40Si-0.33Mn-0.51Cr-1.41Mo-1.03Cu Cast Iron
3.78C-2.26Si-0.24Mn-0.89Cr-0.78Ni-1.50Cu Cast Iron
3.7C-0.4Mn-2.74Si-0.4Mo Ductile Cast Iron
3.7C-0.4Mn-2.75Si Ductile Cast Iron
3.7TC-2Ni Steel
3.81C-14.75Cr-2.50Mo Alloyed White Cast Iron
3.81C-14.75Cr-2.50Mo Alloyed White Cast Iron
3.83C-2.36Si-0.06Mn-2.00Mo-1.62Ni Cast Iron
3.8C-0.4Mn-2.31Si-0.3Mo Ductile Cast Iron
3.8C-0.4Mn-2.32Si Ductile Cast Iron
3.8Mn-0.7Si Steel
3.94C-23.45Cr-2.94Mo Alloyed White Cast Iron
3.94C-23.45Cr-2.94Mo Alloyed White Cast Iron
3.96C-14.80Cr-1.45Mo Alloyed White Cast Iron
3.96C-14.80Cr-1.45Mo Alloyed White Cast Iron
3.96C-17.55Cr-2.53Mo Alloyed White Cast Iron
3.96C-17.55Cr-2.53Mo Alloyed White Cast Iron
3/4 Cr Mo Steel
3/4 Cr Mo Steel
3/4 Cr Mo Steel
3/4 Cr Steel
3/4 Cr Steel
3/4 Ni Cr Mo Steel
3/4 Ni Cr Steel
30 C 5 Steel
30 CAD 6-12 Steel
30 CD 12 Steel
30 CD 12 Steel
30 CND 8 Steel
30 CND 8 Steel
30 CV 5 Steel
30 MS 6 Steel
30 NC 11 Steel
30 NC 11 Steel
30 NC 12 Steel
30 NCD 12 Steel
30 NCD 12 Steel
30 NCD 12 Steel
30 NCD 2 Steel
30 NCD 2 Steel
30 NCD 8 Steel
30 SC 6 Steel
30 SCD 6 Steel
301LN Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304L Stainless Steel
304L Stainless Steel
304LN Steel
308 Stainless Steel
308 Stainless Steel
308CRE Steel
30Cr (Alloy 90) Steel
30CrMnSiNi2 Steel
30CrMo4 Steel
30CrMo4 Steel
30CrMoNiV10-25-6-2 Steel
30CrMoNiV10-25-6-2 Steel
30CrMoNiV5-11 Steel
30CrMoNiV5-11 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrMoV9 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30CrNiMo8 Steel
30HGSNA Steel
30MiCrMo12 Steel
30Mn5 Steel
30Mn5 Steel
30Mn5 Steel
30MnB5 Steel
30MnVS6 (27MnSiVS6) Steel
30NC1 Steel
30NiCr-11 Steel
30NiCr-11 Steel
30NiCrMo12 Steel
30NiCrMo12 Steel
30NiCrMo2-2 Steel
30NiCrMo2-2 Steel
310 Stainless Steel
310 Stainless Steel
311 Steel
312 Steel
3120 Steel
3120 Steel
3135 Steel
3140 Steel
3140 Steel
3140 Steel
3140 Steel
3140 Steel
3140 Steel
3140 Steel
3140 Steel
316 Nb Steel
316 Stainless Steel
316 Stainless Steel
316 Stainless Steel
316 Stainless Steel
316 Stainless Steel
316 Stainless Steel
316 Stainless Steel
316, 316L, 316N Steels
316, 317 LMN, 254 SMO, 904L Steels
316L Stainless Steel
316L Stainless Steel
316L Stainless Steel
316L Stainless Steel
316L Stainless Steel
316L Stainless Steel
3190 Steel
3190 Steel
31CrMo12 Steel
31CrMo12 Steel
31CrMo12 Steel
31CrMoV9 Steel
31CrMoV9 Steel
31CrMoV9 Steel
31CrMoV9 Steel
31CrV2 Steel
31CrV3 Steel
31CrV3 Steel
31CrV3 Steel
32 C 4 Steel
32 C 4 Steel
32 CND 11 Steel
32 CND 11 Steel
32 NCD 15 Steel
3205 Manganese Steel I
3205 Manganese Steel II
321 Stainless Steel
3240 Steel
3240 Steel
32CrB4 Steel
32CrB4 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMo12 Steel
32CrMoV12-10 Steel
32MnCrMo6-4-3 Steel
32NiCrMo-14-5-X1* Steel
32NiCrMo-14-5-X1* Steel
3310 (0.4 C) Carburized Steel
3310 (0.6 C) Carburized Steel
3310 (0.8 C) Carburized Steel
3310 (1.0 C) Carburized Steel
3310 Carburized to 0.4C Steel
3310 Carburized to 0.6C Steel
3310 Carburized to 0.8C Steel
3310 Carburized to 1.0C Steel
3310 Steel
3310 Steel
3310 Steel
3330 Carburized Steel
3330 Steel
3330 Steel
3335 Steel
33MnCrB5-2 Steel
34 CrMo 4 Steel
34 CrNi 3Mo Steel
3410 Steel
3410 Steel
347 Stainless Steel
347 Stainless Steel
347 Stainless Steel
347 Stainless Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4 Steel
34Cr4, 34CrS4 Steels
34Cr4, 34CrS4 Steels
34CrAl6 Steel
34CrAlMo5 Steel
34CrAlMo5 Steel
34CrAlMo5 Steel
34CrAlNi7 Steel
34CrAlNi7 Steel
34CrAlNi7 Steel
34CrAlNi7-10 Steel
34CrAlNi7-10 Steel
34CrAlS5 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4 Steel
34CrMo4, 34CrMoS4 Steels
34CrMo4, 34CrMoS4 Steels
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrNiMo6 Steel
34CrS4 Steel
34CrS4 Steel
34GS Steel
35 CD 4 Steel
35 CD 4 Steel
35 M 5 Steel
35 M 5 Steel
35 M 6 Steel
35 NC 11 Steel
35 NC 15 Steel
35 NC 15 Steel
35 NC 15 Steel
35 NC 6 Steel
35 NC 6 Steel
35 NCD 16 Steel
35 NCD 16 Steel
35 NCD 16 Steel
35 NCD 5 Steel
35 NCD 5 Steel
35 NCDV 10 Steel
354 Steel
35CrNi5Si Steel
35CrNi5Si Steel
35HGSA Steel
35HGSA Steel
35MnCrMoV8-6-4-1 Steel
35NiCr18X1 Steel
35NiCr18X1 Steel
361 Steel
365 Steel
367 Steel
368 Steel
36Cr6 Steel
36Cr6 Steel
36CrMn5 Steel
36CrMn5 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36CrNiMo4 Steel
36HNM Steel
36Mn5 Steel
36NiCr6-4 Steel
36NiCr6-4 Steel
36NiCrMo16 Steel
36NiCrMo16 Steel
371 LMN, 316, 904 L, 254 SMO Steels
37Cr4 Steel
37Cr4 Steel
37Cr4 Steel
37Cr4, 37CrS4 Steels
37Cr4, 37CrS4 Steels
37CrS4 Steel
37MnB4 Steel
37MnB5 (40MnB4) Steel
37MnB5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi5 Steel
37MnSi7 Steel
37MnSi7 Steel
37Mo2 Steel
38 C 4 Steel
38 C 4 Steel
38Cr2 Steel
38Cr2 Steel
38Cr4 Steel
38Cr4 Steel
38CrMo, 42CrMo4, 42CrMo4-MA Steels
38H2MJUAT Steel
38KhGMA Steel
38KhGMA, 40KhGMA, 40KhGMRA Steels
38MnB5 Steel
38MnB5Nb Steel
38MnCrNi6-4-4 Steel
38MnSiV4S Steel
38MnSiVS5 Steel
38MnVS6 Steel
38Si6 Steel
38Si6 Steel
38Si7 Steel
39MnCrMo6-4-3 Steel
39NiCrMo3 Steel
39NiCrMo4 Steel
39NiCrMo4 Steel
3CR12Ti, 3CR12L Steels
3Cr-1Mo Steel
3Cr1.5Mo Steel
3Cr2MnNiMo Steel
3M50 BS-1 Steel
3M50BC-1 Steel
3M50BN-1 Steel
3Mn Steels
3Mn-1Cr Steel
3Mn-Si-Ni Steel
3Mn-Si-Ni Steel
3Mn20B Steel
3Mn5B Steel
3Mo Low Carbon Tool Steel
3Mo Low Carbon Tool Steel
3Mo Low Carbon Tool Steel
3Mo, SW Steels
3Ni-2Cr-0.7Mo Steel
3Ni-Cr Steel
3Ni-Cr Steel
3Ni-Cr-Mo Steel
3TC-0.15Mo Steel
3TC-0.25Mo Steel
3TC-2Si Steel
3TC-2Si Steel
3TC-2Si Steel
3U Steel
3U Steel
4 1/4 Ni - 1 1/2 Cr - 1/10 Mo Steel
4 1/4 Ni - 1 1/2 Cr - 1/3 Mo Steel
4 Ni Cr Mo Steel
4 Ni Cr Mo Steel
4 Ni Cr Mo Steel
4 Ni Cr Steel
4 Ni Cr Steel
4% Manganese Steel
4% Mn Steels I
4% Mn Steels II
4-1/4Ni-1-1/2Cr-1/10Mo Steel
4-1/4Ni-1-1/2Cr-1/3Mo Steel
4.08C-18.00Cr-1.14Mo Alloyed White Cast Iron
4.08C-18.00Cr-1.14Mo Alloyed White Cast Iron
4.10C-15.10Cr Alloyed White Cast Iron
4.10C-15.10Cr Alloyed White Cast Iron
4.10C-23.67Cr-1.32Mo Alloyed White Cast Iron
4.10C-23.67Cr-1.32Mo Alloyed White Cast Iron
4.13C-18.22Cr-0.05Mo Alloyed White Cast Iron
4.13C-18.22Cr-0.05Mo Alloyed White Cast Iron
4.23Cr-0.03C Steel
4.25Ni-Cr Steel
4.25Ni-Cr Steel
4.31C-24.80Cr-0.02Mo Alloyed White Cast Iron
4.31C-24.80Cr-0.02Mo Alloyed White Cast Iron
4.49% Mn Steel
40 CAD 6-12 Steel
40 CAD 6-12 Steel
40 CV 5 Steel
40 CV 5 Steel
40 NC 18 Steel
40 NCD 18 Steel
40 NCD 18 Steel
40 NCD 3 Steel
40 NCD 3 Steel
40 NDCV 18-11 Steel
40 WCDS 35-12 Steel
4024 Steel
4027 Steel
4027 Steel
403 Stainless Steel
403/410 Stainless Steel
403/410 Stainless Steel
403/410 Stainless Steel
4037 Steel
4037 Steel
4040 Steel
4042 Steel
4042 Steel
4047 Steel
4047 Steel
4047 Steel
405 Steel
4068 Steel
4068 Steel
40CrMnMo7 Steel
40CrMnNiMo8-6-4 Steel
40CrMnNiMo8-6-4 Steel
40KhGMA Steel
40KhGSTF Steel
40Mn4 Steel
40Mn4 Steel
40MnSiCrMoB4 Steel
40MnSiCrMoB4 Steel
40NiCrMo18-6 Steel
40NiCrMo18-6 Steel
40NiCrMo2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo2-2 Steel
40NiCrMo3 Steel
40NiCrMo7 Steel
40NiCrMo7 Steel
40NiCrMo7 Steel
40NiCrMo8-4 Steel
40WCrMoSi35-12 Steel
41 S 7 Steel
410 Steel
4105 Manganese Steel I
4105 Manganese Steel II
411 Steel
412 Steel
4130 Steel
4130 Steel
4130 Steel
4130 Steel
4130HW Steel
4137/4140 Steel
4140 Steel
4140 Steel
4140 Steel
4140 Steel
4140 Steel
4142 Steel
4150 Mod. Steel
4150 Steel
4150 mod. Steel
416 Stainless Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4 Steel
41Cr4, 41CrS4 Steels
41Cr4, 41CrS4 Steels
41CrAlMo7-10 Steel
41CrAlMo7-10 Steel
41CrMo4 Steel
41CrMo4 Steel
41CrS4 Steel
41CrS4 Steel
41MnSi6-5 Steel
41NiCrMo7-3-2 Steel
41Si7 Steel
41x40 Steel
41x40 Steel
42 C 4 Steel
42 C 4 Steel
42 MnV 7 Steel
42C Steel
42C Steel
42Cr4 Steel
42Cr4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4 Steel
42CrMo4, 42CrMoS4 Steels
42CrMo4, 42CrMoS4 Steels
42CrMo4-M, 42CrMo4, 38CrMnMo Steels
42CrV6 Steel
42CrV6 Steel
42D Steel
42D Steel
42Mn2V Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42MnV7 Steel
42SiCr Steel
430 Stainless Steel
4317 Steel
4317 Steel
4317/43B17 Steel
4330 Mod. (Si+V) Steel
4330 Modified (Si+V) Steel
4330 Steel
4330 Steel
4330 Steel
4340 + Si Steel
4340 Steel
4340 Steel
4340 Steel
4340 Steel
4340 Steel
4360 Steel
4360 Steel
4360 Steel
43B17 mod. Steel
43BV14 Steel
440A Stainless Steel
440A Stainless Steel
442 Stainless Steel
446 Stainless Steel
44MnSiV5-6 Steel
45 M 5 Steel
45 M 5 Steel
45 MS 6 Steel
45 MS 6 Steel
45 SC 6 Steel
45 SC 6 Steel
45 SCD 6 Steel
45 SCD 6 Steel
45 SCD 6 Steel
45 WC 20-04 Steel
45 WC 20-04 Steel
451 Steel
452 Steel
453 Steel
454 Steel
455 Steel
458 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrMoV6-7 Steel
45CrVMoW5-8 Steel
45CrVMoW5-8 Steel
45Mn5 Steel
45Mn5 Steel
45MnSi6 Steel
45MnSi6 Steel
45WCrV7-7 Steel
45WCrV7-7 Steel
4601 Steel
4615 Steel
4615 Steel
4615 Steel
4615/46B15 Steel
4626 Steel
4630 Steel
4630 Steel
4640 Steel
4640 Steel
4640 Steel
4640 Steel
4695 Steel
4695 Steel
46B15 Steel
46Cr2 Steel
46Cr2 Steel
46CrS2 Steel
46Si7 Steel
46Si7 Steel
46Si7 Steel
46Si7 Steel
46SiCrMo6-3 Steel
46SiCrMo6-3 Steel
4815 (1.0% C) Steel
4815 Carburized Steel
4815 Carburized to 1C Steel
4815 Steel
4815 Steel
4815 Steel
4815 Steel
4840 Steel
48Si7 Steel
49CrMo4 Steel
49CrMo4 Steel
4Cr5Mo2V, 4Cr5Mo2VNi, 4Cr5Mo2VCo Steels
4KhV2S Steel
4Mo-0.4C Steel
4Mo-1.0C Steel
4OCDVI3 Steel
5 1/4 Ni - 1/4 Mo-V Steel
5 Cr Mo Steel
5 Cr Mo Steel
5 Ni Mo Steel
5 Ni Steel
5% Nickel Steel, 0.50% C
5% Nickel Steel, 0.80% C
5% Nickel Steel, 1.2% C
5-1/4Ni-1/4Mo Steel
5-4-4-1 + 5Co Steel
5-4-4-1 + 5Co Steel
5-4-4-1 Steel
5.79Cr Steel
50 CD 4 Steel
50 CD 4 Steel
50 CV 4 Steel
50 CV 4 Steel
50 NC 2 Steel
50 NC 2 Steel
50 NCD 6 Steel
50 NCD 6 Steel
500 MPa-Class Steel
501 Steel
502 Steel
503 Steel
504 Steel
505 Steel
506 Steel
507 Steel
508 Steel
509 Steel
50CV4 Steel
50CrMnMoV, 45Cr3MnNiMoV Steels
50CrMnMoV, 45Cr3MnNiMoV Steels
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMo4 Steel
50CrMoV18-30-6 Steel I
50CrMoV18-30-6 Steel II
50CrNiMo Steel
50CrV2Si Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50CrV4 Steel
50MnV7 Steel
50MnV7 Steel
50SiCrMo6 Steel
5106 Manganese Steel I
5130 Steel
5130 Steel
5140 Steel
5140 Steel
5140 Steel
5140 Steel
5140 Steel
5140 Steel
5140 Steel
5150 Steel
5160 Steel
5160 Steel
5160 Steel
5160/51B60 Steel
51B60 Steel
51CrMoV4 Steel
51CrMoV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51CrV4 Steel
51Si7 Steel
51Si7 Steel
51Si7 Steel
51Si7 Steel
5210 Manganese Steel II
5210 Manganese Steel II
52100 Steel
52100 Steel
52100 Steel
52100 Steel
52100 Steel
52100 Steel
52CrMo4V Steel
52CrMo4V Steel
52CrMoV4 (51CrMoV4) Steel
52CrMoV4 (51CrMoV4) Steel
52CrMoV4 Steel
52CrMoV4 Steel
52E Steel
52MnCrB3 Steel
52MnCrB3 Steel
52SiCrNi5 Steel
52SiCrNi5 Steel
52SiCrNi5 Steel
52SiCrNi5 Steel
53MnSi4-X-1 Steel
53MnSi4-X-1 Steel
53MnSiX1 Steel
53MnSiX1 Steel
54SiCr6 Steel
54SiCr6 Steel
54SiCrV6 Steel
54SiCrV6 Steel
55 NCDV 7 Steel
55 NCDV 7-05 Steel
55 NCDV 7-05 Steel
55 S 7 Steel
55 S 7 Steel
551 Steel
552 Steel
55CNDV-4 Steel
55Cr3 Steel
55Cr3 Steel
55Cr3 Steel
55Cr3 Steel
55CrMo Steel
55NiCrMoV6 Steel
55NiCrMoV6 Steel
55NiCrMoV6 Steel
55Si3Mn2CrMoVNb Steel
55Si3Mn2CrMoVNb Steel
55Si7 Steel
55Si7 Steel
55Si7 Steel
55Si7 Steel
55SiMo8 Steel
56NiCrMoV7 Steel
56NiCrMoV7 Steel
56NiCrMoV7 Steel
56NiCrMoV7 Steel
56Si7 (55Si7) Steel
56Si7 Steel
56Si7 Steel
56SiCr7 Steel
58CrV Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
58CrV4 Steel
590 MPa Grade Galvannealed Sheet Steel
590-MPa Steel
590MPa Grade Steel
5Cr-0.5Mo Steel
5Cr-0.5Mo Steel
5Cr-0.5Mo Steel
5Cr0.5Mo Steel
5Cr0.5Mo Steel
5KhV2S Steel
5Mn Steel
5Ni Steel
6-5-2 Steel
6-6-2 Steel
6.27Cr Cast Iron
6.27Cr Steel
6.5% Cr Steel
60 NCD 11 Steel
60 NCD 11 Steel
60 SC 7 Steel
60 SC 7 Steel
60Cr3 Steel
60Nb Steel
60Nb, 30NbMo31 Steels
60NbMo31 Steel
60NiCrMo11-03 Steel
60Si7 Steel
60SiCr7 Steel
60SiCr7 Steel
60SiCr8 Steel
60SiCrV7 Steel
60SiCrV7 Steel
60SiCrV7 Steel
6135 Steel
6145 Steel
6145 Steel
6150 Steel
6150 Steel
6155 Steel
61CrSiV5 Steel
61CrSiV5 Steel
61CrSiV5 Steel
61CrSiV5 Steel
61SiCr7 (60SiCr7) Steel
61SiCr7 Steel
61SiCr7 Steel
63CrMnMo6 Steel
640 Steel
65Mn Steel
65Mn Steel
65Nb Steel
65Si7 Steel
65Si7 Steel
65Si7 Steel
65Si7 Steel
65SiCr7 Steel
65SiCr7 Steel
6F4 Steel
6F4 Tool Steel
6F5 Steel
6F5 Tool Steel
6KhV2S Steel
6Mn16 Steel
6NA Steel
6NA Steel
6NB Steel
6NB Steel
6NC Steel
6NC Steel
6ND Steel
6ND Steel
6NE Steel
6NE Steel
6NF Steel
6NF Steel
6NG Steel
6NG Steel
6Q Steel
6Q Steel
7% Cr Steel
7-1/2% Nickel Steel, 0.25% C
7-1/2% Nickel Steel, 0.50% C
7-1/2% Nickel Steel, 0.80% C
7-1/2% Nickel Steel, 1.2% C
7.6Ni-0.48C Steel
70 C 1 Steel
700 MC Steel
70MC5 Steel
718 Steel
718 Superalloy
718 Superalloy
71Si7 Steel
71Si7 Steel
724 Steel
728 Steel
730 Steel
731 Steel
78.P1 Steel
7C, 7NbMo, 7V Rail Steels
7CrMoVTiB10-10 (T/P24) Steel
7Nb Steel
7Nb Steel
7QA Steel
7QA Steel
7QB Steel
7QB Steel
7QC Steel
7QC Steel
7QD Steel
7QD Steel
8-10Cr Steels
80 DCV 42-16 Steel
80A2 Steel
80A2 Steel
80B2 Steel
80B2 Steel
80B20 Steel
80B20 Steel
80C2 Steel
80C2 Steel
80MnS5 Steel
80MoCrV42-16 Steel
80MoCrV42-16 Steel
80MoCrV42-16 Steel
819B Steel
81B40 Steel
81B40 Steel
826B Steel
8620 Steel
8620 Steel
8620 Steel
8620 Steel
8620/86B20 Steel
8630 Steel
8630 Steel
8630 Steel
8630 Steel
8640 & 8740 Steel
8640 Steel
8640, 8740 Steels
8645, 8745 Steels
8650/86B50 Steel
8660 Steel
8660 Steel
8660 Steel
8680/86B80 Steel
8695 Steel
8695 Steel
86B20 Steel
86B40 Steel
86B45 Steel
86B45 Steel
86B50 Steel
86B80 Steel
86CrMoV7 Steel
86CrMoV7 Steel
86CrMoV7 Steel
86CrMoV7 Steel
8745 Steel
8745 Steel
8A Steel
8A Steel
8B Steel
8B Steel
8Cr-2Mo Steel
8MnCrB3 Steel
8MnCrB3 Steel
8MnMoNi5-5 Steel
9 Cr Mo Steel
9 CrMo 4.5 Steel
9 Ni Steel
9% Nickel Low Carbon Steel
9% Nickel Steel
9% Nickel Steel
9% Nickel Steel
90 M 5 Steel
90 M 5 Steel
90 MV 8 Steel
90 MV 8 Steel
90MV8 Steel
90MnCrV8 Steel
90MnCrV8 Steel
90MnCrV8 Steel
90MnV8 Steel
90MnV8 Steel
90MnV8 Steel
911 Steel
9260 Steel
9260 Steel
9261 Steel
9262 Steel
9310 Steel
9315 Steel
9315 Steel
9395 Steel
9395 Steel
9420 Steel
9420 Steel
9440 Steel
9440 Steel
94B17 Steel
94B17 Steel
95 C 3 Steel
9860 Steel
9860 Steel
98B45 Steel
98B45 Steel
9Cr-1Mo Steel
9Cr-ODS Steel
9CrMoWV Steel
9CrMoWV Steel
9F-Free Machining Steel
9G Turbine Steel
9Ni Steel
9Ni Steel
9Ni Steel
9Ni-4Co Steel
9Ni-4Co Ultra-Strength Steel
9Ni-Mo Steel
9Ni-C Steel I
9Ni-C Steel II
A 1320 Steel
A 3120 Steel
A 3120 Steel
A 3140 Steel
A 4340 Steel
A 4620 Steel
A-2, S20C Steels
A-4, S50C Steels
A-4042 Steel
A-4140 Steel
A-4142 Steel
A-9, SK3 Steels
A1-3 Steel
A10 Steel
A10 Tool Steel
A2 Steel
A2 Steel
A2 Steel
A2 Tool Steel
A508 type RPV Steel
A533 Steel
A710M Steel
A731 Steel
A752 Steel
A8P66 Steel
A8P67 Steel
A8P68 Steel
A8P69 Steel
A8P70 Steel
A8P71 Steel
A8P72 Steel
A8P73 Steel
A8P74 Steel
A8P75 Steel
A9P48 Steel
A9P59 Steel
ABC III Steel
ADC3 Steel
ADI Cast Iron I
ADI Cast Iron II
ADS-4 Steel
AH36 Steel
AH36 Steel
AH36 Steel
AIRDI 150 Steel
AIRDI 150 Steel
AIRDI 150 Steel
AIRKOOL DIE Steel
AISI 01 Steel
AISI 1005 Steel
AISI 1005 Steel
AISI 1010 Steel
AISI 1010 Steel
AISI 1012 Steel
AISI 1020 Steel
AISI 1020 Steel
AISI 1020 Steel
AISI 1021 Steel
AISI 1021 Steel
AISI 1021B Steel
AISI 1023 Steel
AISI 1025 Steel
AISI 1025 Steel
AISI 1029 Steel
AISI 1034, 1090 Steels
AISI 1034, 1090 Steels
AISI 1036, 10B36 Steels
AISI 1038 Steel
AISI 1038, 0.35C-0.20Si-1.55Mn-0.28Mo Steel
AISI 1040 Steel
AISI 1040, 5140, 45CrMoV67 Steels
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045 Steel
AISI 1045, 5140, 4140, 4340 Steels
AISI 1045, 5140, 4140, 4340 Steels
AISI 1050 Steel
AISI 1050 Steel
AISI 1050 Steel
AISI 1055 Steel
AISI 1080 Steel
AISI 1080 Steel
AISI 1080 Steel
AISI 1080 Steel
AISI 1080 Steel
AISI 1080, 5140, 1034, 9216 Steels
AISI 1080, 5140, 1034, 9261 Steels
AISI 1090 Steel
AISI 1094 Steel
AISI 1095 Steel
AISI 1541 Steel
AISI 1541 Steel
AISI 1541 Steel
AISI 15B41 Steel
AISI 15B41 Steel
AISI 2205, 2304, 2507 Steels
AISI 300M Steel
AISI 300M Steel
AISI 304 Steel
AISI 304 Steel
AISI 304 Steel
AISI 304 Steel
AISI 304 Steel
AISI 304, 316 and X6CrNiMoTi Steels
AISI 304, 316 and X6CrNiMoTi17-12-2 Steels
AISI 310S, 310, 253 Steels
AISI 3140 Steel
AISI 3140 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 Steel
AISI 316 and AISI316L Steels
AISI 316L Steel
AISI 316L Steel
AISI 316L Steel
AISI 321 Stainless Steel
AISI 321 Stainless Steel
AISI 321 Stainless Steel
AISI 410 Steel
AISI 410 Steel
AISI 410 Steel
AISI 410 Steels
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4130 Steel
AISI 4135, 5140, 4050 Steels
AISI 4137 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140 Steel
AISI 4140, 4340 Steels
AISI 4140, 4340 Steels
AISI 416 Steel
AISI 420 Steel
AISI 420C Steel
AISI 420C Steel
AISI 431 Steel
AISI 4320 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340 Steel
AISI 4340* Steel
AISI 444 Steel
AISI 5140 Steel
AISI 5140, 8630 Steels
AISI 5150H Steel
AISI 52100 Steel
AISI 6150 Steel
AISI 6150 Steel
AISI 632 Steel
AISI 8630 Steel
AISI 8630 mod. Steel
AISI A10 Steel
AISI A2 (A2, A2F) Steel
AISI A2 Steel
AISI A2 Steel
AISI A2 Steel
AISI A514 Steel
AISI D2 (D2, D2F) Steel
AISI D2 Steel
AISI D2 Steel
AISI D2 Steel
AISI D4 Steel
AISI E52100 Steel
AISI H10 Steel
AISI H11 Steel
AISI H12 Steel
AISI H13 EFS Steel
AISI H13 Steel
AISI H13 Steel
AISI H13 Steel
AISI H13 Steel
AISI H13 Steel
AISI H13 Steel
AISI H13 Steel
AISI H21 Steel
AISI H22 Steel
AISI H25 Steel
AISI L2 Steel
AISI L2 Steel
AISI L6 Steel
AISI M2 Steels
AISI M4 Steel
AISI M4 Steel
AISI M4 Steel
AISI M42 Steel
AISI O1 Steel
AISI O1 Steel
AISI O1 Tool Steel
AISI O2 Steels
AISI P2 Steel
AISI P2 Steel
AISI P20 Steel
AISI P20 Steel
AISI S1 Steel
AISI S1 Steel
AISI S1 Steel
AISI S2 Steel
AISI S4 Steel
AISI S5 Steel
AISI S5 Tool Steel
AISI S6 Steel
AISI S7 Steel
AISI T1 Steel
AISI T1 Steel
AISI T1 Steel
AISI W1 Steels
AISI W210 Steel
AISI type 1080 Steel
AISI type 15B41 Steel
AISI ~403 Steel
AISI/SAE 4340 Steel
AL-6X Austenitic Stainless Steel
AL-6XN Steel
ALVA EXTRA Steel
AMS 6416 (200-M) Steel
AMS 6416 (300-M) Steel
AMS 6416 (300-M) Steel
AMS 6416 (300-M) Steel
AMS 6418 Steel
AMS 6418 Steel
AMS 6428 & 6434 Steel
AMS 6428 and 6434 Steel
ANTINIT N680 Steel
API 5CT L80 Steel
API 5CT L80 Steel
API 5CT L80 Steel
API 5L X-60 Steel
API 5L X80 Steel
API X-65 Steel
API X-70 Steel
API X-70 Steel
API X-70 Steel - Round-Robin Test
API X-80 Steel
API X70 Steel
API X70 Steel
API X80 Steel
API X80 Steel
API X80 Steel
AREA Steel
ARMAD Steel
ARMAD Steel
ARMOX 500 Steel
ASC 100.29 + 4%H45-0.6C, Astaloy85 Mo + 4%H45-0.6C, Astaloy CrA + 4%H45-0.6C, Astaloy CrM + 4%H45-0.6C Steels
ASC 100.29_0.6C, Astaloy85 Mo_0.6C, Astaloy CrA_0.6C, Astaloy CrM_0.6C Steels
ASP 2017 Steel
ASP 2023 Steel
ASP 2023 Steel
ASP 2030 Steel
ASP 2030 Steel
ASP 2053 Steel
ASP 2060 Steel
ASP 2060 Steel
ASSAB 8407 2M Steel
ASSAB 8407 SUPREME Steel
ASSAB 8407 Steel
ASSAB 88 Steel
ASSAB 88 Steel
ASSAB PM 23 SuperClean Steel
ASSAB SuperClean Steel
ASTM A710 Mod. Steel
ASTM A710 Steel
ASTM Grade 91 Steel
ASTM Grade 911 Steel
ASTMA302B Steel
ASTMA302B Steel
ATHA PNEU Steel
AUD11 Steel
Ac1, Ac3, Ar1, Ar3, Ms and Mf points of SAE Steels
Acicular Ferrite Pipe Steel
AerMet 100 Steel
Aerospace Steel
Airdi 150 Steel
Airsteel X200 Steel
Al killed Steel
Al killed Steel
Al-3 Steel
Al-Si Weathering Steel
Al-Si Weathering Steel
Al2O3 Inclusion
Alloy 625 Steel
Alloy 718
Alloy 718
Alloy 718 and Alloy 718Plus
Alloy 718 and Alloy 718Plus
Alloy 718Plus
Alloy 718Plus
Alloy 718Plus
Alloy 800
Alloy 800
Alloy 800
Alloy 800
Alloy 800
Alloy 800
Alloy 800 (Incoloy 800), Inconel 600 and 304 Stainless Steel
Alloy-White-Cast-Iron
Allvac 718Plus Alloy
Alnico Steels
Armor Steel
Astaloy CrA, Astaloy CrA+2Ni and Astaloy CrM Steels
Astaloy CrL+0.6C
Astaloy CrM Steel
Astaloy CrM Steel
Astaloy D 0.67%C Steel
Ausa 42CrMo4 Steel
Austenitic 308 Stainless Steel
Austenitic 308 Stainless Steel
Austenitic 308 Stainless Steel
Austenitic 308 Stainless Steel
Austenitic Cr-Mn-C-N Stainless Steel
Austenitic Cr-Mn-C-N Stainless Steel
Austenitic Cr-Ni-Mo Steel X5CrNiMo17-13
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steel
Austenitic Stainless Steels
Austenitic Steel
Austenitic Steel
Austenitic Steel
Austenitic Steel
Austenitic Steel
Austenitic Steel
Austenitic Steel
Avesta 654 SMO Steel
Avesta 654 SMO Steel with 5Mo5W
Avesta Sheffield 2205 Steel
B, Mo-B, Cr-B Steels
B-3 Steel
B-3 Steel
B18 Steel
B20 Steel
B30 Steel
B30H Steel
B360 Steel
B500B Steel
B500B Steel
B50A365 Steel
BA-160 Steel
BAS100 Steel
BATMAN II Steel
BHT80 Steel
BHW35 Steel
BHW35 Steel
BM Steel
BMWRS Steel
BMo2 and NoSi Steels
BN1 Steel
BOHLER K100 Steel
BOHLER K100 Steel
BOHLER K105 Steel
BOHLER K105 Steel
BOHLER K105 Steel
BOHLER K107 Steel
BOHLER K107 Steel
BOHLER K110 Steel
BOHLER K110 Steel
BOHLER K110 Steel
BOHLER K190 MICROCLEAN Steel
BOHLER K245 Steel
BOHLER K305 Steel
BOHLER K305 Steel
BOHLER K306 Steel
BOHLER K340 ISODUR Steel
BOHLER K340 ISODUR Steel
BOHLER K353 Steel
BOHLER K360 ISODUR Steel
BOHLER K390 MICROCLEAN Steel
BOHLER K455 Steel
BOHLER K455 Steel
BOHLER K460 Steel
BOHLER K460 Steel
BOHLER K490 MICROCLEAN Steel
BOHLER K600 Steel
BOHLER K600 Steel
BOHLER K605 Steel
BOHLER K605 Steel
BOHLER K700 Steel
BOHLER K720 Steel
BOHLER K720 Steel
BOHLER K890 MICROCLEAN Steel
BOHLER K990 Steel
BOHLER M200 Steel
BOHLER M238 VMR/VAR Steel
BOHLER M238 VMR/VAR Steel
BOHLER M300 ISOPLAST Steel
BOHLER M303 EXTRA Steel
BOHLER M310 ISOPLAST Steel
BOHLER M330 VMR Steel
BOHLER M333 ISOPLAST Steel
BOHLER M333 ISOPLAST Steel
BOHLER M340 ISOPLAST Steel
BOHLER N360 ISOEXTRA Steel
BOHLER S290 MICROCLEAN Steel
BOHLER S390 MICROCLEAN Steel
BOHLER S500 Steel
BOHLER S500 Steel
BOHLER S590 MICROCLEAN Steel
BOHLER S600 Steel
BOHLER S600 Steel
BOHLER S690 MICROCLEAN Steel
BOHLER S705 Steel
BOHLER S705 Steel
BOHLER S790 MICROCLEAN Steel
BOHLER W100 Steel
BOHLER W100 Steel
BOHLER W300 Steel
BOHLER W300 Steel
BOHLER W302 ISOBLOC Steel
BOHLER W302 Steel
BOHLER W303 Steel
BOHLER W320 Steel
BOHLER W320 Steel
BOHLER W321 Steel
BOHLER W321 Steel
BOHLER W360 ISO BLOC Steel
BOHLER W360 ISOBLOC Steel
BOHLER W400 VMR Steel
BOHLER W400 VMR Steel
BOHLER W403 VMR Steel
BOHLER W500 Steel
BOHLER W500 Steel
BR1500HS Steel
BR1500HS Steel
BR885 Steel
BR885 Steel
BRM1 Steel
BRM2 Steel
BRM2 Steel
BRU Steel
BRW1 Steel
BRW1 Steel
BS 11 Rail Steel
BS 11 Rail Steel
BS 708A37 Steel
BS 708A42 Steel
Bainidur 1300 Steel
Bainite and Martensite Start Temperatures
Bainitic Steel
Bainitic Steel
Bainitic Steel
Bainitic Steels
Bainitic Steels
Balder Steel
Base and Base-Mo Steels
Base-Cr-Mo-V and Base-Si-Cr-Mo-V Steels
Base-Mo, Base-V, Base-Mo-V, Base-Cr-Mo-V, Base-Si-Cr-Mo-V Steels
Base-V, Base-Mo-V Steels
BaseMoV Steel
Bearing Steel
Bearing Steel
Bethlehem 0.1% Cr Steel
BeyLos 2329 Steel
BeyLos 2340 Steel
BeyLos 2343 Steel
BeyLos 2344 Steel
BeyLos 2365M Steel
BeyLos 2367 Steel
BeyLos 2711 Steel
BeyLos 2714 Steel
Bohler 25CrMo4 Steel
Bohler B108 Steel
Bohler B108 Steel
Bohler B524 Steel
Bohler B524 Steel
Bohler B524 Steel
Bohler B524 Steel
Bohler CM193 Steel
Bohler CM193 Steel
Bohler D112 Steel
Bohler D112 Steel
Bohler D114 Steel
Bohler D114 Steel
Bohler D116 Steel
Bohler D116 Steel
Bohler D118 Steel
Bohler D118 Steel
Bohler D122 Steel
Bohler D122 Steel
Bohler D204 Steel
Bohler D204 Steel
Bohler D206 Steel
Bohler D206 Steel
Bohler D217 Steel
Bohler D217 Steel
Bohler D220 Steel
Bohler D220 Steel
Bohler D221 Steel
Bohler D221 Steel
Bohler D230 Steel
Bohler D230 Steel
Bohler D240 Steel
Bohler D240 Steel
Bohler D320 Steel
Bohler D320 Steel
Bohler D326 Steel
Bohler D326 Steel
Bohler D326 Steel
Bohler D334 Steel
Bohler D334 Steel
Bohler D402 Steel
Bohler D402 Steel
Bohler D500 Steel
Bohler D500 Steel
Bohler D608 Steel
Bohler D608 Steel
Bohler D612-SO Steel
Bohler D612-SO Steel
Bohler D612-SO Steel
Bohler D612-SO Steel
Bohler D902-SO Steel
Bohler D902-SO Steel
Bohler E-E103 Steel
Bohler E-E103 Steel
Bohler E101 Steel
Bohler E101 Steel
Bohler E200 Steel
Bohler E200 Steel
Bohler E200 Steel
Bohler E200 Steel
Bohler E230 Steel
Bohler E230 Steel
Bohler E410 Steel
Bohler E410 Steel
Bohler F550 Steel
Bohler F550 Steel
Bohler F554 Steel
Bohler F554 Steel
Bohler H700 SD Steel
Bohler H700 SD Steel
Bohler H700 Steel
Bohler H700 Steel
Bohler H700 Steel
Bohler H700 Steel
Bohler H710 Steel
Bohler H710 Steel
Bohler H730 Steel
Bohler H730 Steel
Bohler H732 Steel
Bohler H732 Steel
Bohler K100 Steel
Bohler K100 Steel
Bohler K103 Steel
Bohler K103 Steel
Bohler K105 So Steel
Bohler K105 So Steel
Bohler K105 Steel
Bohler K105 Steel
Bohler K105 Steel
Bohler K105 Steel
Bohler K107 So Steel
Bohler K107 So Steel
Bohler K110 Steel
Bohler K110 Steel
Bohler K200 Steel
Bohler K200 Steel
Bohler K243 Steel
Bohler K243 Steel
Bohler K243 Steel
Bohler K243 Steel
Bohler K245 Steel
Bohler K245 Steel
Bohler K305 Steel
Bohler K305 Steel
Bohler K306 Steel
Bohler K306 Steel
Bohler K306 Steel
Bohler K306 Steel
Bohler K316 SA Steel
Bohler K316 SA Steel
Bohler K327 Steel
Bohler K327 Steel
Bohler K332 Steel
Bohler K332 Steel
Bohler K340 ECOSTAR Steel
Bohler K340 Steel
Bohler K450 Steel
Bohler K450 Steel
Bohler K455 ISODUR Steel
Bohler K455 ISODUR Steel
Bohler K455 Steel
Bohler K455 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K460 Steel
Bohler K463 Steel
Bohler K463 Steel
Bohler K465 Steel
Bohler K465 Steel
Bohler K490 MICROCLEAN Steel
Bohler K490 MICROCLEAN Steel
Bohler K510 Steel
Bohler K510 Steel
Bohler K600 Steel
Bohler K600 Steel
Bohler K600 Steel
Bohler K603 Steel
Bohler K603 Steel
Bohler K603 Steel
Bohler K603 Steel
Bohler K604 Steel
Bohler K604 Steel
Bohler K605 Steel
Bohler K605 Steel
Bohler K605 Steel
Bohler K616 Steel
Bohler K616 Steel
Bohler K710 So Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K720 Steel
Bohler K746 Steel
Bohler K746 Steel
Bohler K990 Steel
Bohler K990 Steel
Bohler M200 Steel
Bohler M200 Steel
Bohler M200 Steel
Bohler M200-So Steel
Bohler M200-So Steel
Bohler M210 Steel
Bohler M210 Steel
Bohler M210 Steel
Bohler M210 Steel
Bohler M210-So Steel
Bohler M210-So Steel
Bohler M210-So Steel
Bohler M210-So Steel
Bohler M238 Steel
Bohler M238 Steel
Bohler M303 EXTRA Steel
Bohler M310 ISOPLAST Steel
Bohler M333 ISOPLAST Steel
Bohler M340 ISOPLAST Steel
Bohler M368 MICROCLEAN Steel
Bohler N310 Steel
Bohler N310 Steel
Bohler N320 Steel
Bohler N320 Steel
Bohler N320 Steel
Bohler N335 Steel
Bohler N335 Steel
Bohler N335 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N350 Steel
Bohler N351 SB Steel
Bohler N351 SB Steel
Bohler N352 Steel
Bohler N352 Steel
Bohler N400 Steel
Bohler N404 G+ Steel
Bohler N404 G+ Steel
Bohler N530 Steel
Bohler N530 Steel
Bohler N540 Steel
Bohler N540 Steel
Bohler N540 Steel
Bohler N545 Steel
Bohler N545 Steel
Bohler N555 Steel
Bohler N555 Steel
Bohler N685 EXTRA
Bohler N685 Steel
Bohler N685 Steel
Bohler N690 Steel
Bohler N690 Steel
Bohler N700 Steel
Bohler P435 Steel
Bohler P435 Steel
Bohler S200 Steel
Bohler S200 Steel
Bohler S200 Steel
Bohler S200 Steel
Bohler S300 Steel
Bohler S300 Steel
Bohler S305 Steel
Bohler S305 Steel
Bohler S400 Steel
Bohler S400 Steel
Bohler S400 Steel
Bohler S400 Steel
Bohler S401 Steel
Bohler S404 Steel
Bohler S404 Steel
Bohler S404 Steel
Bohler S406 Steel
Bohler S406 Steel
Bohler S500 Steel
Bohler S500 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S600 Steel
Bohler S601 Steel
Bohler S601 Steel
Bohler S604 Steel
Bohler S604 Steel
Bohler S607 Steel
Bohler S607 Steel
Bohler S607 Steel
Bohler S607 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S700 Steel
Bohler S705 Steel
Bohler S705 Steel
Bohler S903 Steel
Bohler S903 Steel
Bohler SK13 Steel
Bohler T502 Steel
Bohler T502 Steel
Bohler T504 Steel
Bohler T504 Steel
Bohler T506 Steel
Bohler T506 Steel
Bohler T550 Steel
Bohler T550 Steel
Bohler T550 Steel
Bohler T550 Steel
Bohler T551 Steel
Bohler T551 Steel
Bohler T552 Steel
Bohler T552 Steel
Bohler T554 Steel
Bohler T554 Steel
Bohler T560 Steel
Bohler T560 Steel
Bohler T560 Steel
Bohler T560 Steel
Bohler T562 Steel
Bohler T562 Steel
Bohler T565 Steel
Bohler T565 Steel
Bohler T602 Steel
Bohler T602 Steel
Bohler T608 Steel
Bohler T608 Steel
Bohler T622 Steel
Bohler T650 Steel
Bohler T650 Steel
Bohler T651 Steel
Bohler T651 Steel
Bohler T655 Steel
Bohler T655 Steel
Bohler V-V118 Steel
Bohler V-V118 Steel
Bohler V109 Steel
Bohler V109 Steel
Bohler V111 Steel
Bohler V111 Steel
Bohler V112 Steel
Bohler V112 Steel
Bohler V113 Steel
Bohler V113 Steel
Bohler V116 Steel
Bohler V116 Steel
Bohler V117 Steel
Bohler V117 Steel
Bohler V119 Steel
Bohler V119 Steel
Bohler V121 Steel
Bohler V121 Steel
Bohler V122 Steel
Bohler V122 Steel
Bohler V124 Steel
Bohler V124 Steel
Bohler V126 Steel
Bohler V126 Steel
Bohler V128 Steel
Bohler V128 Steel
Bohler V128 Steel
Bohler V128 Steel
Bohler V129 Steel
Bohler V129 Steel
Bohler V130 Steel
Bohler V130 Steel
Bohler V130 Steel
Bohler V130 Steel
Bohler V131 So Steel
Bohler V131 So Steel
Bohler V131 So Steel
Bohler V131 So Steel
Bohler V131 Steel
Bohler V131 Steel
Bohler V133 Steel
Bohler V133 Steel
Bohler V142 Steel
Bohler V142 Steel
Bohler V145 Steel
Bohler V145 Steel
Bohler V145 Steel
Bohler V145 Steel
Bohler V147 Steel
Bohler V147 Steel
Bohler V155 Steel
Bohler V155 Steel
Bohler V155 Steel
Bohler V155 Steel
Bohler V162 Steel
Bohler V162 Steel
Bohler V163 Steel
Bohler V163 Steel
Bohler V164 Steel
Bohler V164 Steel
Bohler V165 Steel
Bohler V165 Steel
Bohler V186 Steel
Bohler V186 Steel
Bohler V304 Steel
Bohler V304 Steel
Bohler V306 Steel
Bohler V306 Steel
Bohler V310 Steel
Bohler V310 Steel
Bohler V320 SX Steel
Bohler V320 SX Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V320 Steel
Bohler V330 Steel
Bohler V330 Steel
Bohler V330SH Steel
Bohler V340 Steel
Bohler V340 Steel
Bohler V350 Steel
Bohler V350 Steel
Bohler V359 Steel
Bohler V359 Steel
Bohler V612 Steel
Bohler V612 Steel
Bohler V762 Steel
Bohler V762 Steel
Bohler V913 Steel
Bohler V913 Steel
Bohler V930 Steel
Bohler V930 Steel
Bohler V945 Steel
Bohler V945 Steel
Bohler W100 Steel
Bohler W100 Steel
Bohler W104 Steel
Bohler W104 Steel
Bohler W108 Steel
Bohler W108 Steel
Bohler W108 mod. Steel
Bohler W108 mod. Steel
Bohler W2773 Steel
Bohler W2773 Steel
Bohler W300 Steel
Bohler W300 Steel
Bohler W300 Steel
Bohler W300 Steel
Bohler W302 ISOBLOC Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W302 Steel
Bohler W303 ISODISC Steel
Bohler W303 Steel
Bohler W304 Steel
Bohler W304 Steel
Bohler W304 Steel
Bohler W320 ISODISC Steel
Bohler W320 Steel
Bohler W320 Steel
Bohler W320 Steel
Bohler W320 Steel
Bohler W3202 Steel
Bohler W321 Steel
Bohler W321 Steel
Bohler W321 Steel
Bohler W322 Steel
Bohler W322 Steel
Bohler W326 Steel
Bohler W326 Steel
Bohler W329 Steel
Bohler W329 Steel
Bohler W333 Steel
Bohler W333 Steel
Bohler W335 Steel
Bohler W335 Steel
Bohler W337 Steel
Bohler W337 Steel
Bohler W338 Steel
Bohler W338 Steel
Bohler W350 ISOBLOC Steel
Bohler W360 Steel
Bohler W400 WMR Steel
Bohler W403 WMR Steel
Bohler W500 Steel
Bohler W500 Steel
Bohler W501 Steel
Bohler W501 Steel
Bohler W503 Steel
Bohler W503 Steel
Bohler W6735 Steel
Bohler W6735 Steel
Bohler W6735 Steel
Bohler W6735 Steel
Bohler W705 Steel
Bohler W705 Steel
Bohler W705 Steel
Bohler Z-B 975 Steel
Bohler Z-B975 Steel
Boron Bearing Steel
Boron Steels
Boron Steels I
Boron Steels II
Buderis 1730 Steel
Buderus 1730 Steel
Buderus 2067 Steel
Buderus 2080 Steel
Buderus 2085 Steel
Buderus 2085 Steel
Buderus 2311 ISO-BM Steel
Buderus 2312 Steel
Buderus 2313 Steel
Buderus 2316 ISO-B MOD Steel
Buderus 2323 ISO-B Steel
Buderus 2343 ISO-B MOD Steel
Buderus 2343 ISO-B MOD Steel
Buderus 2343 ISO-B Steel
Buderus 2344 ISO-B Steel
Buderus 2344 ISO-B Steel
Buderus 2360 ISO-B Steel
Buderus 2360 ISO-B Steel
Buderus 2365 ISO-B Steel
Buderus 2365 ISO-B Steel
Buderus 2367 ISO-B Steel
Buderus 2367 ISO-B Steel
Buderus 2436 ISO-B Steel
Buderus 2436 ISO-B Steel
Buderus 2510 Steel
Buderus 2550 Steel
Buderus 2601 Steel
Buderus 2606 ISO-B Steel
Buderus 2606 ISO-B Steel
Buderus 2678 Steel
Buderus 2711 ISO-B MOD Steel
Buderus 2711 ISO-B Steel
Buderus 2711 ISO-B Steel
Buderus 2711 Steel
Buderus 2714 ISO-B MOD Steel
Buderus 2714 ISO-B MoD Steel
Buderus 2714 ISO-B Steel
Buderus 2714 ISO-B Steel
Buderus 2738 ISO-BM Steel
Buderus 2738 Mod. TS Steel Thruhard Supreme Steel
Buderus 2738 Steel
Buderus 2739 ISO-B Steel
Buderus 2744 ISO-B Steel
Buderus 2744 ISO-B Steel
Buderus 2766 Steel
Buderus 2767 ISO-B Steel
Buderus 2767 ISO-B Steel
Buderus 2842 Steel
Buderus 7220 Steel
Buderus 9966 SUPER C Steel
Buderus 9966 SUPER C Steel
Buderus HIPERDIE Steel
Buderus Thruhard Diamond-HHH Steel
Buderus Thruhard Efficient Extrahard Steel
Buderus Thruhard Efficient Steel
Buderus Thruhard Supreme 2738mod.TS(HH) Steel
Buderus Thruhard Supreme 2738mod.TS(HHH) Steel
C 100 Steel
C 1080 Steel
C 1080 Steel
C 1080 Steel
C 45 Steel
C(0.02%)-Mn(1.30%) MIG Weld
C(0.04%)-Mn(0.85%)-Ni(2.56%) MMA Weld
C(0.04%)-Mn(0.98%) MIG Weld
C(0.04%)-Mn(1.20%)-Ni(1.10%) MMA Weld
C(0.04%)-Mn(1.29%)-Ni(3.58%) MMA Weld
C(0.04%)-Mn(1.60%) MIG Weld
C(0.04%)-Mn(1.67%)-Ni(2.48%) MMA Weld
C(0.05%)-Mn(0.68) MIG Weld
C(0.05%)-Mn(0.69%) MIG Weld
C(0.05%)-Mn(0.78%)-Ni(5.53%) MMA Weld
C(0.05%)-Mn(0.78%)-Ni(5.53%) MMA Weld
C(0.05%)-Mn(0.78%)-Ni(5.53%) MMA Weld
C(0.05%)-Mn(0.98%)-Ni(0.06%) MMA Weld
C(0.05%)-Mn(1.18%)-Ni(2.52%) MMA Weld
C(0.05%)-Mn(1.30%) MIG Weld
C(0.05%)-Mn(1.45%) TIG Weld
C(0.05%)-Mn(1.58%) MIG Weld
C(0.05%)-Mn(1.68%)-Ni(0.95%) MMA Weld
C(0.05%)-Mn(1.72%)-Ni(1.87%)-Mo(0.31%) MMA Weld
C(0.05%)-Mn(1.75%)-Ni(2.73%)-Mo(0.20%) MMA Weld
C(0.06%)-Mn(0.56%) MMA Weld
C(0.06%)-Mn(0.67%)-Ni(3.32%) MMA Weld
C(0.06%)-Mn(1.40%)-Ni(0.14%) SFCAW Weld
C(0.06%)-Mn(1.50%)-Ni(0.96%)-Mo(0.25%) MMA Weld
C(0.06%)-Mn(1.55%)-Ni(2.00%) SFCAW Weld
C(0.07%)-Mn(1.35%) MMA Weld
C(0.07%)-Mn(1.35%) MMA Weld
C(0.07%)-Mn(1.36%) MIG Weld
C(0.07%)-Mn(1.51%) MIG Weld
C(0.075)-Mn(1.26%)-Ni(2.25%) TIG Weld
C(0.08%)-Mn(0.96%)-Ni(0.90%) MMA Weld
C(0.08%)-Mn(0.97%)-Nb(0.02%) MMA Weld
C(0.08%)-Mn(1.25%) FCW Weld
C(0.08%)-Mn(1.33%)-Ni(0.73%) TIG Weld
C(0.08%)-Mn(1.41%) FCW Weld
C(0.08%)-Mn(1.48%) FCW Weld
C(0.08%)-Mn(1.53%) MIG Weld
C(0.08%)-Mn(1.53%) MIG Weld
C(0.089%)-Mn(1.43%)-Ti(0.028%) SA Weld
C(0.09%)-Mn(0.81%)-Si(0.11) MIG Weld
C(0.09%)-Mn(1.05%)-Nb(<0.01%) MMA Weld
C(0.09%)-Mn(1.10%)-Si(0.27%)-Ti(0.038%)-B(0.0027%) MIG Weld
C(0.09%)-Mn(1.32%)-Nb(<0.01%) MMA Weld
C(0.09%)-Mn(1.35%) SA Weld
C(0.09%)-Mn(1.61%)-Ni(1.99%) TIG Weld
C(0.09)-Mn(1.05%)-Ni(3.32%) TIG Weld
C(0.095%)-Mn(1.6%)-V(0.1%) TIG Weld
C(0.10%)-Mn(0.89%)-Ni(1.25%) TIG Weld
C(0.10%)-Mn(1.37%)-Nb(0.03%) MMA Weld
C(0.11%)-Mn(0.74%)-Si(0.09) MIG Weld
C(0.11%)-Mn(0.96%)-Si(0.22%)-Ti(0.029%)-B(0.0026%) MIG Weld
C(0.11%)-Mn(1.09%)-Si(0.40)-Ti(0.05%) MIG Weld
C(0.11%)-Mn(1.16%)-Si(0.29%)-Ti(0.043%)-B(0.0034%) MIG Weld
C(0.11%)-Mn(1.50%)-Mo(0.30%) TIG Weld
C(0.11%)-Mn(2.10%) TIG Weld
C(0.12%)-Mn(0.80%)-Si(0.25)-Ti(0.027%) MIG Weld
C-0.08 Steel
C-0.08 Steel
C-0.15 Steel
C-0.15 Steel
C-0.3 Steel
C-0.3 Steel
C-0.38 Steel
C-0.38 Steel
C-0.53 Steel
C-0.53 Steel
C-0.94 Steel
C-0.94 Steel
C-1.37 Steel
C-1.37 Steel
C-253 Steel
C-253 Steel
C-253 Steel
C-Mn Steel
C-Mn Steel
C-Mn Steel Steel
C-Mn Steel Steel
C-Mn Steel Steel
C-Mn Steel Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn Weld Steel
C-Mn-B Steel
C-Mn-B Steel
C-Mn-B Steel
C-Mn-Nb Steel
C-Mn-Nb Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C-Mn-Ni Weld Steel
C10 Steel
C10 Steel
C100S Steel
C100S Steel
C100W1 Steel
C100W1 Steel
C100W1 Steel
C100W1 Steel
C100W1 Steel
C10E2C Steel
C10E2C Steel
C110 Steel
C110 Steel
C125S Steel
C15E2C (Cq15) Steel
C15R Steel
C16 Steel
C17E2C Steel
C20 Steel
C22.8 Steel
C32 Steel
C35 Steel
C35 Steel
C35E Steel
C35E Steel
C35EC Steel
C35EC Steel
C35EC Steel
C35EC Steel
C35R Steel
C35R Steel
C35R Steel
C35R Steel
C35RC Steel
C35RC Steel
C36 Steel
C36 Steel
C38 Steel
C40D2 Steel
C40E Steel
C40R Steel
C42 Steel
C42 Steel
C43 Steel
C43 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel
C45 Steel + Microstructures
C45E Steel
C45E Steel
C45E Steel
C45E Steel
C45E Steel
C45E, C45R Steels
C45E, C45R Steels
C45EC (Cq45) Steel
C45EC (Cq45) Steel
C45EC Steel
C45EC Steel
C45R Steel
C45R Steel
C45RC Steel
C45RC Steel
C46 Steel
C46 Steel
C50E Steel
C50E Steel
C50R Steel
C53 Steel
C55 Steel
C55E Steel
C55E Steel
C55R (Cm55) Steel
C55R (Cm55) Steel
C55R Steel
C55R Steel
C55R Steel
C55S Steel
C60 Steel
C60 Steel
C60 Steel
C60 Steel
C60 Steel
C60 Steel
C60E Steel
C60R Steel
C60R Steel
C60R Steel
C60R Steel
C60S Steel
C60S Steel
C67S Steel
C70 Steel
C70W1 Steel
C70W1 Steel
C75S Steel
C75S Steel
C75S Steel
C75S Steel
C80U Steel
C80U Steel
C80U Steel
C80U Steel
C80U Steel
C90 Steel
C90S Steel
CALDIE Steel
CALDIE Steel
CALMAX Steel
CARBODUR 15NiCr13 Steel
CARBODUR 16MnCr5/16MnCrS5 Steel
CARBODUR 17Cr3 Steel
CARBODUR 17CrNi6-6 Steel
CARBODUR 18CrNi8 Steel
CARBODUR 18CrNiMo7-6 Steel
CARBODUR 20MnCr4/20MnCrS4 Steel
CARBODUR 20MnCr5/20MnCrS5 Steel
CARBODUR 20NiCrMo2-2/20NiCrMoS2-2 Steel
CARBODUR 20NiMoCrS6-5 Steel
CCS Steel
CD3MN Steel
CD3MN Cast Steel
CD3MN Steel
CD3MN Steel
CD3MN, CD3MWCuN Steels
CD3MWCuN Steel
CD3MWCuN Steel
CD3MWCuN Steel
CELMAX Super Clean Steel
CH16V Steel
CH5M Steel
CHAMPALOY Steel
CHRO-MOW Steel
CLAM Steel
CLC 1.2312 Steel
CLC 1.2312 Steel
CLC 1.2316 S Steel
CLC 1.2316 Steel
CLI-SAF 2507 Steel
CM167 Steel
CMR Steel
CMn Steel
CMn, CMnNb and MoNbTi Steels
CMnAl-TRIP Steel
CMnAlSi TRIP Steel
CMnB, CMnNbB, CMnMoB, CMnNbMoB Steels
COR-TEN Steel
CP-IH Steel
CP1100 Steel
CP800 Steel
CP800 Steel
CPM S110V Steel
CR7V-L Steel
CRESCENT SPECIAL Steel
CRONIDUR 30 Steel
CRONIDUR 30 Steel
CRUCIBLE DOUBLE SPECIAL Steel
CRUCIBLE DOUBLE SPECIAL Steel
CRV1 Steel
CRV3 Steel
CRV3 Steel
CS1 Steel
CS1 Steel
CSM 2 Steel
CSM High C Steel
CSM Low C Steel
CT182 Steel
CT198 Steel
CT198 Steel
CT198 Steel
CT781 Steel
CT781 Steel
CTC-08A Steel
CTC03-L Consumable Steel
CTC03-L Steel
CTC03-R Consumable Steel
CTC03-R Steel
Calculated TTT Diagrams Steel
Calculated and Experimental Diagrams of C-Mn-Nb Steels
Calmax Steel
Carbidic Nodular Cast Iron I
Carbidic Nodular Cast Iron II
Carbidic Nodular Cast Iron III
Carbidic Nodular Cast Iron IV
Carbidic Nodular Cast Iron V
Carbodur 6587 Steel
Carbodur 6758 Steel
Carbodur 7131/Carbodur 7139 Steel
Carbon Free Fe-15.0Co-10.0Mo Steel
Carbon Free Fe-15.0Co-10.0Mo Steel
Carbon Free Fe-15.0Co-10.0Mo Steel
Carbon Free Fe-15.0Co-20.0Mo Steel
Carbon Free Fe-15.0Co-20.0Mo Steel
Carbon Free Fe-15.0Co-20.0Mo Steel
Carbon Steel
Carbon Steel
Carbon Steel
Carbon Steel (Davenport and Bain, 1930)
Carbon Steel (Davenport and Bain, 1930) I
Carbon Steel (Davenport and Bain, 1930) II
Carbon Steel (Davenport and Bain, 1930) III
Carbon Steel (Davenport and Bain, 1930) IV
Carbon Steel (Davenport and Bain, 1930) V
Carbon Steel (Davenport and Bain, 1930) VI
Carbon Steel (Davenport and Bain, 1930) VII
Carbon Steel I
Carbon Steel II
Carbon Steels
Carbon Steels
Carburized 1320 (0.4% C) Steel
Carburized 1320 (0.6% C) Steel
Carburized 1320 (0.8% C) Steel
Carburized 1320 (1.0% C) Steel
Carburized 1320 (1.2% C) Steel
Carburized 1321 (0.8% C) Steel
Carburized 1321 (1.2% C) Steel
Carburized 13B21 (0.6% C) Steel
Carburized 13B21 (1.0% C) Steel
Carburized 13B21 (1.2% C) Steel
Carburized 2512 (0.4% C) Steel
Carburized 2512 (0.6% C) Steel
Carburized 2512 (0.8% C) Steel
Carburized 2512 (1.0% C) Steel
Carburized 2512 (1.2% C) Steel
Carburized 3310 (0.4% C) Steel
Carburized 3310 (0.6% C) Steel
Carburized 3310 (0.8% C) Steel
Carburized 3310 (0.8C) Steel
Carburized 3310 (1.0% C) Steel
Carburized Case of SAE 2512 Steel
Carburized Case of SAE 2512 Steel
Carmo Steel
Carpenter 20Nb-3 Stainless Steel
Carpenter 20Nb-3 Stainless Steel
Carpenter 440-XH Steel
Carpenter AerMet Steel
Carpenter AerMet Steel
Carpenter CarTech A6 Steel
Carpenter CarTech No. 484 Steel
Carpenter D3 Steel
Carpenter Extendo-Die Steel
Carpenter HS30 Steel
Carpenter M2 Steel
Carpenter Micro-Melt 440-XH Steel
Carpenter Micro-Melt HS30 Steel
Carpenter Micro-Melt M42 Steel
Carpenter Micro-Melt M42 Steel
Carpenter Micro-Melt M48 Steel
Carpenter Micro-Melt T15 Steel
Carpenter Micro-Melt T15 Steel
Carpenter No. 158 Steel
Carpenter No. 158 Steel
Carpenter No. 345 Steel
Carpenter No. 481 Steel
Carpenter No. 484 Steel
Carpenter No. 484 Steel
Carpenter No. 610 Steel
Carpenter No. 610 Steel
Carpenter No. 882 Steel
Carpenter No. 882 Steel
Carpenter No. 883 Steel
Carpenter No. 883 Steel
Carpenter No.158 Steel
Carpenter O1 Steel
Carpenter O1 Steel
Carpenter Pyrowear 675 Steel
Carpenter Pyrowear 675 Steel
Carpenter S2 Steel
Carpenter Solar Tool Steel
Carpenter Speed Star Steel
Carpenter VIM-VAR M-50 Steel
Carpenter Vega Steel
Cast X155CrVMo121 Steel
Ce Steel
Cf35 Steel
Cf35 Steel
Cf45 Steel
Cf45 Steel
Cf53 Steel
Cf53 Steel
Cf70 Steel
Cf70 Steel
Characteristic Shapes of Continuous TTT-Diagrams
Chemical Composition of Ferritic-Martensitic Steels, Ac1, Ac3, Ms and Mf Temperatures
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck15 Steel
Ck30 Steel
Ck30 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck35 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45 Steel
Ck45, 41Cr4, 45CrMoV67 Steels
Ck50 Steel
Ck55 Steel
Ck55 Steel
Ck55 Steel
Ck55 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck60 Steel
Ck75 Steel
Ck75 Steel
Ck85 Steel
Ck85 Steel
Ck85 Steel
Ck85 Steel
Cold Forging Steel
Compax Supreme Steel
Compax Supreme Steel
Continuous TTA-Diagram for 100Cr6
Corrodur 4418 Mod Steel
Corten Steel
Corten Steel
Corus Z8B21 Steel
Cr-0.5 Steel
Cr-0.5 Steel
Cr-1 Steel
Cr-1 Steel
Cr-2 Steel
Cr-2 Steel
Cr-4 Steel
Cr-4 Steel
Cr-Hard Cast Steel
Cr-Hard Cast Steel
Cr-Mo-V Rotor Steel
Cr-Mo-alloyed Steels
Cr-Ni-Mo, Cr-Mn-Si-Mo, Cr-Mo-V Steels
Cr-Ni-alloyed Steels
Cr-alloyed Steels
Cr12MoV Steel
Cr12MoV Steel
Cr12MoV Steel
Cr26Ni6Mo3Cu3 Steel
Cr7V-L Steel
CrMo70L Steel
CrMo80L Steel
CrMo80L Steel
CrMoZr Structural Steel
Croloy 1-1/4 Steel
Croloy 2-1/4 Steel
Croloy 3M Steel
Croloy 5 Steel
Croloy 7 Steel
Croloy 9M Steel
Cronidur 30 Steel
Cronidur 30 Steel
Cronifer1925 hMo - alloy 926
Crucible 440A Steel
Cryodur 1520 Steel
Cryodur 2002 Steel
Cryodur 2067 Steel
Cryodur 2080 Steel
Cryodur 2101 Steel
Cryodur 2210 Steel
Cryodur 2235 Steel
Cryodur 2242 Steel
Cryodur 2243 Steel
Cryodur 2249 Steel
Cryodur 2327 Steel
Cryodur 2362 Steel
Cryodur 2363 Steel
Cryodur 2379 Steel
Cryodur 2381 Steel
Cryodur 2436 Steel
Cryodur 2510 Steel
Cryodur 2516 Steel
Cryodur 2550 Steel
Cryodur 2721 Steel
Cryodur 2766 Steel
Cryodur 2767 Steel
Cryodur 2826 Steel
Cryodur 2833 Steel
Cryodur 2842 Steel
Cryodur 2990 Steel
Cu-3 Steel
Cu-3 Steel
Cu-Ni-Mo-Cb(Nb) Steel
C-Mn-Cr-B Steel
D Steel
D-6ac High Strength Steel
D-6ac Steel
D05651 Steel
D05651 Steel
D2 Steel
D2 Steel
D2 Tool Steel
D3 Steel
D32 Steel
D4 Steel
D4 Tool Steel
D6AC Steel
D6AC Steel
DAC-MAGIC Steel
DB590 Steel
DC04 Steel
DC04 Steel
DC11 Steel
DC11 Steel
DC11 Steel
DC11 Steel
DC53 Steel
DCMX Steel
DH31-EX Steel
DH36 Steel
DHA-HS1 Steel
DHA-Thermo Steel
DHA-World Steel
DHA1 Steel
DIEVAR SUPREME Steel
DIEVAR SUPREME Steel
DIEVAR Steel
DIEVAR Steel
DIEVAR Steel
DIEVAR Steel
DIMO 2311 Steel
DIMO 2312 Steel
DIMO 2312 Steel
DIMO 2738 XH Steel
DIMO 2738 XH Steel
DIMO 30H Steel
DIMO 30M Steel
DIMO P20 Steel
DMo5 Steel
DP 600 Steel
DP 600 Steel
DP 780 Steel
DP 800 Steel
DP Steel Steel
DP Steels I
DP Steels II
DP-1 Steel
DP-2 Steel
DP-3 Steel
DP-4 Steel
DP1400, DP1000, DP800 Steels
DP590 Steel
DP600 Steel
DP600 Steel
DP780 Steel
DRM3 Steel
DS213 Steel
DSS 2205 Steel
DT Steel
DT Steel
DURODI Steel
Deep Drawing Steel I
Deep Drawing Steel II
Deep Drawing Steel III
Deep Drawing Steel IV
Deep Drawing Steel V
Deep Hardening Steel
Deep Hardening Steel
Deep Hardening Steel
Dievar Steel
Docol Boron 02 Steel
Docol PHS 1500 Steel
Docol PHS 1800 Steel
Docol PHS 2000 Steel
Dominial BA Steel
Dominial C H W Steel
Dominial CH 16 V Steel
Dominial CH 160 W Steel
Dominial CH 16V Steel
Dominial CH 2 V Steel
Dominial CH 5 M Steel
Dominial CH Steel
Dominial CM 167 Steel
Dominial CR 7V Steel
Dominial DSW, PK Steels
Dominial Extra E, Extra Mo, C 2 Mo Steels
Dominial HMoD Steel
Dominial HWD Steel
Dominial KL Steel
Dominial KS 60, KS 80 Steels
Dominial KTW/KTW-Ni Steel
Dominial MA Steel
Dominial MAK Steel
Dominial MKSt Steel
Dominial N400 Steel
Dominial PD Steel
Dominial PWM Steel
Dominial RP Mo H Steel
Dominial RP Steel
Dominial RPU Steel
Dominial SN Steel
Dominial SP und RS Steels
Dominial SS 50, SS 60 Steels
Dominial UNI Steel
Dominial US Steel
Dominial USD Steel
Dominial USN Steel
Dominial W44 Steel
Dorrenberg P5M Steel
Dorrenberg R65 Steel
Dorrenberg WP5 Steel
Dorrenberg 1.2379 PLUS Steel
Dorrenberg 1.2379PLUS Steel
Dorrenberg 1.3343PLUS Steel
Dorrenberg A50 Steel
Dorrenberg AMO Steel
Dorrenberg AMO Steel
Dorrenberg CP10V Steel
Dorrenberg CP2M Steel
Dorrenberg CP2M Steel
Dorrenberg CP4M Steel
Dorrenberg CP72 Steel
Dorrenberg CP72PLUS Steel
Dorrenberg CPPK Steel
Dorrenberg CPPU Steel
Dorrenberg CPPU Steel
Dorrenberg CPR Steel
Dorrenberg CPR Steel
Dorrenberg CPW Steel
Dorrenberg DM05 Steel
Dorrenberg DM3 Steel
Dorrenberg DM3X Steel
Dorrenberg DM3X Steel
Dorrenberg DM51 Steel
Dorrenberg DMO5 Steel
Dorrenberg DMO5H Steel
Dorrenberg ECN4M Steel
Dorrenberg EMo5Co5 Steel
Dorrenberg EMo5Co5 Steel
Dorrenberg EMo9CoH Steel
Dorrenberg EPM2 Steel
Dorrenberg Extra Nr. 45 Steel
Dorrenberg GP4M Steel
Dorrenberg GX155CrVMo12-1 Steel
Dorrenberg HC16S Steel
Dorrenberg HC17M Steel
Dorrenberg HC17M Steel
Dorrenberg HC50 Steel
Dorrenberg HC50 Steel
Dorrenberg Hidalgo I Steel
Dorrenberg KHD Steel
Dorrenberg KHD Steel
Dorrenberg KHD Steel
Dorrenberg KHD Steel
Dorrenberg M4S Steel
Dorrenberg M4S Steel
Dorrenberg M4S Steel
Dorrenberg M4S Steel
Dorrenberg MCM Steel
Dorrenberg MCMN Steel
Dorrenberg MCMS Steel
Dorrenberg MS Steel
Dorrenberg NC50E Steel
Dorrenberg NCM Steel
Dorrenberg NCM Steel
Dorrenberg NCM Steel
Dorrenberg NCM Steel
Dorrenberg NCV Steel
Dorrenberg NCV Steel
Dorrenberg NCV Steel
Dorrenberg NCV Steel
Dorrenberg Ni50 Steel
Dorrenberg Ni50 Steel
Dorrenberg Ni50 Steel
Dorrenberg Ni50 Steel
Dorrenberg PMD M4 Steel
Dorrenberg PMD V4 Steel
Dorrenberg PMD23 Steel
Dorrenberg PMD2380 Steel
Dorrenberg PMD30 Steel
Dorrenberg PMD60 Steel
Dorrenberg PV4 Steel
Dorrenberg PV6 Steel
Dorrenberg R118 Steel
Dorrenberg R17WS Steel
Dorrenberg R17X Steel
Dorrenberg R18 Steel
Dorrenberg R18So Steel
Dorrenberg R45 Steel
Dorrenberg VNC4 Steel
Dorrenberg WP5V Steel
Dorrenberg WP7V Steel
Dorrenberg WR Special Steel
Dorrenberg Z1B Steel
Dorrenberg Z3C Steel
Dual Phase Sheet Steel
Dual Phase Steel
Dual-Phase Steel
Dual-Phase Steel
Ductile Gray Iron
Ductile Iron Steel
Ductile iron
Dupla Steel
Duplex Stainless Steel
Duplex Stainless Steel
Duplex Stainless Steel
Duplex Stainless Steel
Duplex Stainless Steel
Duracat Chipper Knife Steel
Duracat Chipper Knife Steel
Durapur 1219 Steel
Durapur 3505 Steel
Durapur 3520 Steel
E - 4342 Steel
E 3310 Steel
E 36 Steel
E1 Steel
E2 Steel
E3-1 (Base Metal) Steel
E3-2 (EB Weld in the Air) Steel
E3-4 (EB Weld in Vacuum) Steel
E355 Steel
E52100 Steel
E550 Steel
E595 Steel
E595 Steel
E599 Steel
E599 Steel
E602 Steel
E602 Steel
E911 Steel
E911 Steel
EB 12 Steel
EC100 Steel
EC100 Steel
EC60 Steel
ECMO100 Steel
ECMO100 Steel
ECN150 Steel
ECN200 Steel
ECN35 Steel
ECN35 Steel
ECN35 Steel
ECN35 Steel
EH36 Steel
ELI Ferritic Stainless Steel
ELMAX SUPERCLEAN 3 Steel
ELMAX SUPERCLEAN Steel
EM812 Steel
EN 15 Steel
EN14, EN16 Steels
EN19B Steel
ER70S-6 Steel
ES 100 K Steel
ES 106 K Steel
ES 120 K ESR Steel
ES 120 K Steel
ES 235 W Steel
ES 245 W ESR Steel
ES 245 W Steel
ES 265 W ESR Steel
ES 265 W Steel
ES 275 ESR Steel
ES 275 K ESR Steel
ES 370 G Steel
ES 4122 Steel
ES 50 S Steel
ES 50 SW Steel
ES 60 S Steel
ES 65 S Steel
ES 70 S Steel
ES Aktuell 1000 Steel
ES Aktuell S Steel
ES Aktuell Steel
ES Antikor S Steel
ES Antikor Steel
ES Maximum 500 Steel
ES ULW 65 Steel
EU20Si Steel
EU20SiNb Steel
EUROFER 97 Steel
EUROFER 97 Steel
EUROFER-97 Steel
EUROFER-97 Steel
EUROFER-97 Steel
EUROFER97/2 Steel
EUROFER97/2 Steel
EX-1 Steel
EX-1 Steel
EX-2 Steel
EX-2 Steel
EXTRA TOOL Steel
Effect of C on CCT diagram of steel
Effect of Cooling Times on Steel Transformation
Effect of Mn on CCT diagram of steel
Effect of Mo Alloying on the Transformation Behavior of a Low-Carbon Base Steel
Effect of Nb on the Transformation Behaviour of a C-Mn Steel
Effect of Near-Stoichiometric Additions of V
Effect of Si, Mn, deformation on continuous-cooling transformation
Effect of the C on the Isothermal Transformation Curve
Eglin Steel
Elmax Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 100 Steel
En 11 Steel
En 110 Steel
En 110 Steel
En 110 Steel
En 110 Steel
En 110 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 111 Steel
En 12 Steel
En 12 Steel
En 12 Steel
En 12 Steel
En 12 Steel
En 13 Steel
En 13 Steel
En 14 Steel
En 14 Steel
En 14 Steel
En 14 Steel
En 14B Steel
En 15 Steel
En 15 Steel
En 16 Steel
En 16 Steel
En 16 Steel
En 160 Steel
En 160 Steel
En 160 Steel
En 160 Steel
En 160 Steel
En 160 Steel
En 17 Steel
En 17 Steel
En 17 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 19 Steel
En 19 Steel
En 19 Steel
En 19 Steel
En 19 Steel
En 2 Steel
En 20 Steel
En 20 Steel
En 20 Steel
En 20 Steel
En 207 Case Steel
En 207 Core Steel
En 21 Steel
En 21 Steel
En 22 Steel
En 22 Steel
En 22 Steel
En 23 Steel
En 23 Steel
En 23 Steel
En 23 Steel
En 23 Steel
En 23 Steel
En 24 Steel
En 24 Steel
En 24 Steel
En 24 Steel
En 24 Steel
En 24 Steel
En 25 Steel
En 25 Steel
En 25 Steel
En 25 Steel
En 25 Steel
En 26 Steel
En 26 Steel
En 26 Steel
En 26 Steel
En 26 Steel
En 27 Steel
En 27 Steel
En 27 Steel
En 27 Steel
En 28 Steel
En 28 Steel
En 28 Steel
En 28 Steel
En 28 Steel
En 29 Steel
En 29 Steel
En 30 Steel
En 30 Steel
En 30 Steel
En 30A Steel
En 30B Steel
En 30B Steel
En 31 Steel
En 31 Steel
En 31 Steel
En 31 Steel
En 31 Steel
En 31 Steel
En 31 Steel
En 32 Steel
En 325 Steel
En 33 Case Steel
En 33 Core Steel
En 33 Steel
En 33 Steel
En 33 Steel
En 33 Steel
En 34 Steel
En 34 Steel
En 34 Steel
En 34 Steel
En 35 Case Steel
En 35 Core Steel
En 35 Core Steel
En 351 Steel
En 351 Steel
En 351 Steel
En 351 Steel
En 352 Steel
En 352 Steel
En 352 Steel
En 352 Steel
En 353 Core Steel
En 353 Steel
En 353 Steel
En 353 Steel
En 353 Steel
En 354 Steel
En 354 Steel
En 354 Steel
En 354 Steel
En 355 Steel
En 355 Steel
En 355 Steel
En 355 Steel
En 35A Core Steel
En 35B Core Steel
En 36 Core Steel
En 36 Core Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 36 Steel
En 361 Case Steel
En 361 Core Steel
En 362 Case Steel
En 362 Core Steel
En 363 Case Steel
En 363 Core Steel
En 37 Core Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39A Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 39B Steel
En 40 Steel
En 40B Steel
En 40C Steel
En 41 Steel
En 41 Steel
En 42
En 42
En 42
En 42 Steel
En 42 Steel
En 43 Steel
En 44 Steel
En 44 Steel
En 44 Steel
En 44 Steel
En 45 Steel
En 45 Steel
En 45 Steel
En 45 Steel
En 47 Steel
En 47 Steel
En 47 Steel
En 47 Steel
En 49 Steel
En 5 Steel
En 50 Steel
En 56 Steel
En 56 Steel
En 56 Steel
En 56 Steel
En 56A Steel
En 56A Steel
En 56AM Steel
En 56C Steel
En 56D Steel
En 59 Steel
En 8 Steel
En 8 Steel
En 8 Steel
En 8 Steel
En 9 Steel
EskyLos 2001 Steel
EskyLos 2002 Steel
EskyLos 2083 Steel
EskyLos 2083 Steel
EskyLos 2083 Steel
EskyLos 2340 DC Steel
EskyLos 2340 HDC Steel
EskyLos 2340 Steel
EskyLos 2343 DC Steel
EskyLos 2343 HDC Steel
EskyLos 2343 Steel
EskyLos 2344 HDC Steel
EskyLos 2344 Steel
EskyLos 2344 Steel
EskyLos 2367 Steel
EskyLos 4542 Steel
EskyLos HiMo Steel
EskyLos HiMo Steel
EskyLos OptiMo Steel
EskyLosS 6959 Steel
Eskylos 2365M Steel
Esshete 1250 Austenitic Steel
Eurofer97 Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steels with no V and V
Extremely-Low Carbon Bainitic Steel
Extremely-Low Carbon Bainitic Steel
Extremely-low Carbon Bainitic Steel
Extremely-low Carbon Bainitic Steel
F2 Steel
F2 Tool Steel
F82H (8Cr-2WVTa) Steel
F82H Steel
F82H mod. Steel
F82H mod. Steel
FAM Steel
FCD 700 Cast Iron
FCD 700 Cast Iron
FCD 700 Cast Iron
FCD40, FD60 Cast Irons
FDG (W) Steel
FH Steel
FH Steel
FH-1914 Steel
FI2N Steel
FIRD Steels
FL-4405 Steel
FL-4605 PM Steel
FL-4605 PM steel
FLC-4608 Steel
FND (W) Steel
FORMOLD Steel
FORMOLD Steel
FSS 436L Steel
FTW52A Steel
FTW52A Steel
FTW52B Steel
FTW52B Steel
FTW58 Steel
FTW58 Steel
FV520B Steel
FV520B Steel
FX-EXTRA Steel
Fe - 30.8Ni - 26.6Cr Alloy
Fe-0.031%Nb-0.07%C Steel
Fe-0.4C, Fe-2Al-0.4C Steels
Fe-1.43% C, Fe-1.49% C-4.90% Cu Steels
Fe-26Cr Ferritic Stainless Steel
Fe-28 wt% Cr-Mo Steel
Fe-30.8Ni-26.6Cr Alloy
Fe-8.50%Cr-0.05%C Steel
Fe-9.6Cr-0.33Hf Alloy
Fe-C Alloys
Fe-C Alloys
Fe-C Alloys
Fe-C Steels
Fe-C-C Alloy Steel
Fe-C-Cr Steel
Fe-C-Cr Steel
Fe-C-Cr-Mo Steel
Fe-C-Mo Steel
Fe-C-Ni-Cr-Mo-V Steel
Fe-Cr-C Steel
Fe-Mn Alloys
Fe-Mn-Ni Steel
Fe-Nb-C Alloy Steel
Fe-Nb-C Alloy Steel
Fe-Nb-C Alloy Steel
Fe-Ni Alloys
Fe-Ni Alloys
Fe-Ni Alloys
Fe-Ni Alloys
Fe-Ni-Cr Steel
Fe-Ni-Cr Steel
Fe-Ni-Mn Steel
Fe-Ni-Mn Steel
Fe-V-C Steel
FeMnN Steel
Feroxy 1.2311 Steel
Feroxy 1.2311 Steel
Feroxy 1.2738 Steel
Ferritic Cr-Mo-Ni Stainless Steel
Ferritic Stainless Steel
Ferritic Stainless Steel
Ferritic Steel I
Ferritic Steel II
Ferritic Steel III
Fe-9Ni-C Steels
Firmodur 1213 Steel
Firmodur 1249 Steel
Firmodur 6582 Steel
Firmodur 7220/Firmodur 7226 Steel
Firmodur 7225/Firmodur 7227 Steel
Formadur 2083/2083 Superclean Steel
Formadur 2085 Steel
Formadur 2162 Steel
Formadur 2311 Steel
Formadur 2312 Steel
Formadur 2316/2316 Superclean Steel
Formadur 2335 Steel
Formadur 2711 Steel
Formadur 2738 Steel
Formadur 2764 Steel
Formadur 2891 Steel
Formadur 320/320 Superclean Steel
Formadur 400/Formadur 400 Superclean Steel
Formvar Steel
Four CCT Diagrams of Steels
G 46 4 M G4Si1 Steel
G Mn3Ni1Mo 'Union MoNi' Steel
G Mn3Ni1Mo Steel
G Mn4Ni1,5CrMo Steel
G Mn4Ni2CrMo Steel
G4Si1 Steel
G91 Steel
GCr15 Steel
GEST80 VICTORY ESR Steel
GKH (W - YW) Steel
GKH (W - YW) Steel
GKP (W-YW) Steel
GL-E36 Steel
GO4 Steel
GO4 Steel
GOA Steel
GOA Steel
GP4M Steel
GS-15 Mn 4 Steel
GS-17 Cr Mo 5.5 Steel
GS-17 CrMoV 6.11/Ch.1 Steel
GS-17 CrMoV 6.11/Ch.2 Steel
GS-18 CrMo 9 10 Steel
GS-20 Mn 5 Steel
GS-22 Mo 4 Steel
GS-22CrMo5 Steel
GS-25CrMo4 Steel
GS-28Mn6 Steel
GS-30CrMo4 Steel
GS-45/Ch.1 Steel
GS-45/Ch.2 Steel
GS-50 Steel
GS-52/Ch.2 Steel
GS-60/Ch.1 Steel
GS-60/Ch.2 Steel
GS-60/Ch.3 Steel
GS-C25/Ch.1 Steel
GS-C25/Ch.2 Steel
GSF ESR Steel
GSF Steel
Garant K Steel
Grade 50 Steel
Grade 52 Steel
Grade 900 Steel
Grades 900 and 1100 Rail Steels
Grain Coarsened HAZ Steel
Grain refined HAZ Steel
Granada Steel
Graph-Air Steel
Gray Cast Iron I
Gray Cast Iron II
H.T.2 Steel
H11 Steel
H11 Tool Steel
H12 Steel
H12 Steel
H12 Tool Steel
H13 SLM Steel
H13 SLM Steel
H13 Steel
H13 Steel
H13 Steel
H13 Steel
H13 Steel
H13 Steel
H13 Steel
H13 Tool Steel
H14 Steel
H14 Tool Steel
H16 Steel
H16 Tool Steel
H21 Steel
H21 Steel
H21 Tool Steel
H5M Steel
HAL COMB SS TOOL Steel
HALCOMB 218 Steel
HALCOMB 218 Steel
HALVAN Steel
HCCI Cast Iron
HCCI Cast Iron
HCM12A Steel
HCT780T Steel
HCT780T Steel
HCe, LCe Steels
HCrLMo, HMoLCr, C-Mn Steels
HDB Steel
HFX 6926 Steel
HFX 6926 Steel
HFX 6928 Steel
HFX 6928 Steel
HFX 7783 Steel
HFX 7783 Steel
HFX 8090 Steel
HMoD Steel
HMoD Steel
HN5MVNb Steel
HN5MVNb Steel
HOTVAR Steel
HP1 Steel
HP1 Steel
HRHS Steel
HS 0-5-5+Ni1 Steel
HS 0-5-5+Ni2 Steel
HS 0-5-5+Ni3 Steel
HS1 Steel
HS18-0-1 Steel
HS220-27 Steel
HS6-5-2 Steel
HSF Steel
HSLA 100 Steel
HSLA 80 Steel
HSLA 80/10 Steel
HSLA Steel
HSLA Steel
HSLA Steel
HSLA Steel
HSLA Steel
HSLA Steel
HSLA Steel
HSLA Steel
HSLA Steel I
HSLA Steel II
HSLA Steel III
HSLA Steel IV
HSLA Steel Plate
HSLA Steel Plate
HSLA Steel Plate
HSLA Steel V
HSLA Steel VI
HSLA-100 Steel
HSLA-100 Steel
HSLA-100 Steel
HSLA-100 Steel
HSLA-100 Steel
HSLA-100 Steel
HSLA-100 Steel
HSLA-80 Steel
HSLA-80 Steel
HSLA-80 Steel I
HSLA-80 Steel II
HSLA-80 Steel III
HSLA-80 Steel IV
HSLA80 Steel
HSLA80 Steel
HSLA80 Steel
HSLA80 Steel
HSS Steel for Hot Rolling
HSS Work Roll Steel
HT 60 Steel
HT-100 Steel
HT-50 Steel
HT-50 Steel
HT-60 Steel
HT-60 Steel
HT-70 Steel
HT-80 Steel
HT-80 Steel
HT36 Steel
HT50, HT60 Steels
HT60 Steel
HT60 Steel
HT80 Steel
HTP Steel
HTR Steel
HTi, LTi, HTi-Mo and LTi-Mo Steels
HWD Steel
HY 85 Steel
HY 85 Steel
HY-180 Steel
HY-180 Steel
HY-80 Steel
HY-80 Steel
HY-TUF Steel
HY-TUF, 20CrMnSiNiMo1, 20CrMnSiNiMo2 Steels
HY80 2K Steel
HY80 7G Steel
HY80 7G Steel
HY80 7H Steel
HY80 7H Steel
HY80 K1 Steel
HY80 K1 Steel
HY80 K2 Steel
HY80 K3 Steel
HY80 K3 Steel
HY80 K4 Steel
HY80 K4 Steel
HY80 M1 Steel
HY80 M1 Steel
HY80 N1 Steel
HY80 N1 Steel
HY80 N2 Steel
HY80 N2 Steel
HY80 N3 Steel
HY80 N4 Steel
HY80 N4 Steel
HY80 NA Steel
HY80 NA Steel
HY80 NB Steel
HY80 NB Steel
HY80 NE38 Steel
HY80 NE38 Steel
HY80 NE38 Steel
HY80 NER38 Steel
HY80 NER38 Steel
HY80 NS63 Steel
HY80 NS63 Steel
HY80 Y1 Steel
HY80 Y1 Steel
HY80 Y4 Steel
HY80 Y4 Steel
HYCC Steel
Hardox 450 Steel
Hasco 1.2436 Steel
Her-Ten60 Steel
Her-Ten60 Steel
Hi-Chrome Work Rolls (Core)
Hi-Chrome Work Rolls (Shell)
Hi-Cr Iron
Hi-Z Steel
Hi-Z Steel
High Carbon Steel Wire Steel
High Chromium Cast Iron
High Cr White Cast Iron
High Nb Steel
High Nitrogen Stainless (HSN) Steels
High Stregth Bainitic Steel
High Strength Weld Metal
High and Low Si 0.1% C Steel
High-Carbon Krupp Steel I
High-Carbon Krupp Steel II
High-Tensile-Strength Hot-Rolled Steel Plate
High-Tensile-Strength Hot-Rolled Steel Plate
High-Tensile-Strength Hot-Rolled Steel Plate
Hot Stamping Steels
Hot Work Tool Steel
Hot Work Tool Steel
Hot-Rolled Dual Phase Steel
Hultgren (1947) Steel
Hultgren (1951) Steel
Hypereutectoid Carbon Steel
Hypereutectoid Carbon Steel
Hypereutectoid Carbon Steel
Hypereutectoid Plain Carbon Steels
Hypereutectoid Steel
Hypo-Eutectoid Nickel Steel
Hypo-Eutectoid Nickel Steel
Hypoeutectoid Steel
Hypothetical Steel
Hypothetical Steel
ICR 1.25 Al Steels
IF and IF-TiNb Steels
IF and MA Steels
Inconel 625 Steel
Industeel 1.2312 Steel
Industeel 1.2316S Steel
Industeel D2 Steel
Industeel D2 Steel
Influence of C on the CCT Diagram of Steel - (A) 0.06% C and (B) 0.17% C
Influence of Mn on the CCT Diagram of Steel with 0.44% C: (A) 0.66% Mn and (B) 2% Mn
Influence of Mo Addition on the Dynamic Precipitation Behavior of Nb
Influence of Mo or Cr on TTT
Influence of the Austenitizing Temperature (8 Diagrams)
Influence of the External Magnetic Field on TTT Diagram
Iron-Carbon Powder Steel
Isothermal TTA-Diagram
Isothermal TTA-Diagram for 34CrMo4
J-1 Steel
J-1 Steel
J-1 Steel
J-2 Steel
J-2 Steel
J-3 Steel
J-3 Steel
J-4 Steel
J-4 Steel
J-6 Steel
J-6 Steel
JG Steel
JIS-S55C, SUP9, SUP7 and SUP12 Steels
Jakutsk Steel
K2H-U Steel
K2H-U Steel
KATO Steel
KATO Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO1 Steel
KATO2 Steel
KATO2 Steel
KATO2 Steel
KATO3 Steel
KATO3 Steel
KATO3 Steel
KATO3 Steel
KETOS Steel
KETOS Steel
KEYLOS 2001 Steel
KIP 103V Steel
KIP 30CRV Steel
KL Steel
KO Steel
KO Steel
KQ (Hi-Z) Steel
KQ (Hi-Z) Steel
KS Steel
KS Steel
KSV Steel
KT 315 Steel
KT 355 Steel
KT Steel
KT Steel
KeyLos 1730 Steel
KeyLos 1730M Steel
KeyLos 2002 Steel
KeyLos 2083 Steel
KeyLos 2085 Steel
KeyLos 2311 Steel
KeyLos 2311 Steel
KeyLos 2312 Steel
KeyLos 2316 Steel
KeyLos 2738 Steel
KeyLos 2738MHH Steel
KeyLos 2738MSH Steel
KeyLos 6959 Steel
KeyLos 7225 Steel
KeyLos PLUS Steel
KeyLos UP Steel
Krupp 0.15C Steel
Krupp 0.15C Steel
Krupp 0.90C Steel
Krupp 0.90C Steel
L1 Steel
L1 Tool Steel
L125GHNM Steel
L17HMF Steel
L2 Steel
L2 Tool Steel
L210GHNM Steel
L21HMF Steel
L24N Steel
L24N Steel
L36TM Steel
L6 Steel
L6 Steel
L6 Steel
L6 Steel
L6 Steel
L6 Tool Steel
L6 Tool Steel
L7 Steel
L70GHNM Steel
LA 13Ta Steel
LA BELLE 89 Steel
LA BELLE SILICON #2 Steel
LA-Steel with Ce+Ta
LA-Steel with Ta+Hf
LA13Ta Steel
LA13Ta Steel
LH800 Steel
LM691 Steel
LM691 Steel
LMF Steel
LO CRO 46 MO Steel
LO CRO 46 MO Steel
LP-163 Steel
LP-163 Steel
LP-164 Steel
LP-164 Steel
LR-896 Steel
Large Forgings Component
Low Alloy Steel
Low Alloy Steel
Low C MnNiMoB Steel
Low C-2.25Cr-1.6W-V-Nb Steel
Low C-2.25Cr-1.6W-V-Nb Steel
Low C-2.25Cr-1.6W-V-Nb Steel
Low Carbon Steel
Low Carbon Steel
Low Carbon Steel
Low Carbon 2.4-4.15% Cr Steel
Low Carbon 3Mn-1Cr Steel
Low Carbon Bainitic Steels with Nb Steel
Low Carbon Low Alloy High Strength Steels
Low Carbon Nb Bearing Steels
Low Carbon Pipeline Steel
Low Carbon Pipeline Steel
Low Carbon Pipeline Steel
Low Carbon Pipeline Steel
Low Carbon Pipeline Steel
Low Carbon Pipeline Steel
Low Carbon Steel
Low Carbon Steel
Low Carbon Steel I
Low Carbon Steel II
Low Carbon Steel III
Low Carbon Steel with Boron
Low Nb Steel
Low Silicon Gray Iron
Low alloyed steel
Low-Carbon Bainitic Steel I
Low-Carbon Bainitic Steel II
Low-Carbon Krupp Steel
Low-Carbon Low-Alloy High-Strength Steel
Low-Carbon Low-Alloy High-Strength Steel
Low-Carbon Low-Alloy High-Strength Steel
Low-Carbon Low-Alloy High-Strength Steel
Low-Carbon Low-Alloy High-Strength Steel
Low-Carbon Low-Alloy High-Strength Steel
Low-Si Microalloyed Steel I
Low-Si Microalloyed Steel II
M-0, M-2, M-4 Steels I
M-0, M-2, M-4 Steels II
M-0, M-2, M-4 Steels III
M-0, M-2, M-4 Steels IV
M-Steel
M.T.3 Steel
M.T.7 Steel
M10 Steel
M10 Tool Steel
M11 Steel
M2 Mod Tool Steel
M2 Steel
M2 Steel
M2 Tool Steel
M2 mod. Steel
M268 Steel
M42 Steel
MA Steel
MANET-I Steel
MANET-II Steel
MANET-II Steel
MAX-EL 1-B Steel
MAX-EL 1-B Steel
MAX-EL 2-B Steel
MAX-EL 4 Steel
MAXEL 3-1/2 Steel
MAXEL 7 Steel
MBL Steel
MBW 1500 Steel
MBW 1500 Steel
MBW 1500 Steel
MCV Steel
MD Steel
MD Xtra Steel
MEK3 Steel
MEK4 Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MERILO Steel
MFR Steel
MIL A46100 Steel
MIL A46100 Steel
MIL A46100 Steel
MLQ Xtra Steel
MSG-0.22Ni Steel
MSG-0.23Mo Steel
MSG-0.27Cr Steel
MSG-0.37Mo Steel
MSG-0.38Ni Steel
MSG-0.44Cr Steel
MSG-0.58Ni Steel
MSG-0.66Mo Steel
MSG-0.86Cr Steel
MSG-0.89Mn Steel
MSG-1.10Mn Steel
MSG-1.42Mn Steel
MSG-1.52Mn Steel
MSG/Ch.1 Steel
MSG/Ch.2 Steel
MSW1200 Steel
MSW1200 Steel
MV11K Steel
MV11K Steel
Magnadie-RF Steel
Marker DCM, DCM-ESR Steel
Marker PHM Steel
Marker WM 28 Steel
Medium Carbon Steel
Medium Carbon Steels
Mf temperature of 1.2080, 1.2345, 1.2363, 1.2376, 1.2379, 1.2436, 1.2550, 1.2601, 1.2631, 1.2714, 1.4116, 1.5028, 1.6511, 1.6580, 1.6582, 1.6773, 1.7225 Steels
Micro-Alloyed Steel
Microalloyed Carbon Steel
Microalloyed Carbon Steel
Microalloyed Steel
Microalloyed Steel I
Microalloyed Steel I
Microalloyed Steel II
Microalloyed Steel II
Microalloyed Steel III
Microalloyed Steel IV
Microalloyed Steel V
Microalloyed Steel VI
Microalloyed Steel with Nb
Mn and Ni alloys
Mn-0 Steel
Mn-0 Steel
Mn-1.0 Steel
Mn-1.0 Steel
Mn-2.0 Steel
Mn-2.0 Steel
Mn-Cr-Mo-V Steel
Mn-C~Mo Dual Phase Steel
Mn-C~Mo Dual Phase Steel
Mn-Mo-Si-Cr Steel Steel
Mn-Mo-Si-Cr Steel Steel
Mn-Mo-Si-Cr Steel Steel
Mn-Mo-V-N Steel
Mn-Si-Al Steel
Mn-Si-Al Steel
MnCrCu1 Steel
MnCrNi Steel
MnNb High Strength Pipeline Steel
MnNiMoNb High Strength Pipeline Steel
Mn-Mo-Nb Microalloyed Steel
Mn-Mo-Nb Microalloyed Steel
Mo-0.5 Steel
Mo-0.5 Steel
Mo-1.0 Steel
Mo-1.0 Steel
Mo-1.6 Steel
Mo-1.6 Steel
Mo-Cu Gray Cast Iron
Mo-alloyed Steels
Mo22 Steel
Mo22 Steel
Mo-Nb-Cu-B Low Carbon Steel
Mo-Nb-Cu-B Low Carbon Steel
Multiphase Microalloyed Steel
N-11 Steel
N-A-XTRA 70 Steel
N-TuF33 Steel
N-TuF33 Steel
N-TuFCR130 Steel
N-TuFCR130 Steel
N-TuFCR196 Steel
N-TuFCR196 Steel
N400 Steel
NA Steel
NA Steel
NAK 80 Steel
NB Steel
NB Steel
NC Steel
NC Steel
ND Steel
ND Steel
NE 8442 Steel
NE 8630* Steel
NE 8744 Steel
NE 8749 Steel
NE 8949 (Approximately NE 9550) Steel
NE 8949 Steel
NE 8949 Steel
NE 9442 Steel
NE 9540 (NE 9537) Steel
NE 9540 Steel
NE 9642 Steel
NE 9642 Steel
NE 9650 Steel
NE 9650 Steel
NE 9650 Steel
NE Steel
NE Steel
NF Steel
NF Steel
NITRALLOY G (MODIFIED) Steel
NITRODUR 15CrMoV5-9 Steel
NITRODUR 15CrMoV5-9 Steel
NITRODUR 31CrMoV9 Steel
NITRODUR 34CrAlMo5 Steel
NITRODUR 34CrAlNi7 Steel
NITRODUR 41CrAlMo7 Steel
NK Steel
NK Steel
NK-HT 80 Steel
NK-HT 80 Steel
NM Steel
NM Steel
NM360 Steel
NOVONOX FT 13 Steel
NRIM 431L Steel
NRIM 431L Steel
NRIM 432M Steel
NRIM 432M Steel
NRIM 55 Steel
NRIM 55 Steel
NRIM A-3 Steel
NRIM A-3 Steel
NRIM B-3 Steel
NRIM B-3 Steel
NRIM37 Steel
NRIM37 Steel
NS 80 Steel
NS 80 Steel
NS-I, NS-II Rail Steels
NU-DIE V Steel
NVONOX F 17a Steel
NVONOX M 131 Steel
NVONOX M 171 H Steel
NVONOX T 13 Steel
NVONOX T 131 Steel
NVONOX T 17 Steel
NVONOX T 171 Steel
NVONOX TT 13 Steel
NVONOX TT 131 Steel
NY80 N3 Steel
NZ3 Steel
Namos Steel
Nanobainitic Steel Containing 0.6%C Steel
Nb HSLA Steels
Nb Microaloyed Steel
Nb Steel
Nb Steel
Nb Steel I
Nb Steel I
Nb Steel II
Nb Steel II
Nb Steel III
Nb Steels
Nb Microalloyed, Nb-Mo Microalloyed Steels
Nb-2 Steel
Nb-2 Steel
Nb-3 Steel
Nb-3 Steel
Nb-Ti Low-Carbon Line-Pipe Steel
Nb-Ti Low-Carbon Line-Pipe Steel
Nb-Ti Low-Carbon Line-Pipe Steel
Nb-Ti Low-Carbon Line-Pipe Steel
Nb-Ti Micro-alloyed Steel
Nb-V-alloyed C-Mn Steel
New TAF Steel
Ni steels
Ni-1.0 Steel
Ni-1.0 Steel
Ni-2.5 Steel
Ni-2.5 Steel
Ni-2.5 Steel
Ni-3.5 Steel
Ni-5 Steel
Ni-5 Steel
Ni-7 Steel
Ni-7 Steel
Ni-9 Steel
Ni-9 Steel
Ni-Al-Ti-Cb Steel
Ni-Cr Steel
Ni-Cr Steel
Ni-Cr-Mo Steel
Ni-Cr-Mo-V (Weld Metal) Steel
Ni-Cr-Mo-V-Cu-B Steel
Ni-Cr-Mo-V-Cu-B Steel
Ni-Cr-Si-V-0.40Mo Steel
Ni-Cr-Si-V-0.49Mo Steel
Ni-Cr-Si-V-0.58Mo Steel
Ni-Cr-Si-V-0.58Mo Steel
Ni-Hard 1 Steel I
Ni-Hard 1 Steel II
Ni-Hard 4 Steel I
Ni-Hard 4 Steel II
Ni-Mo Ductile Iron
Ni-Mo Ductile Iron
Ni-alloyed Steels
NiCrMoV I Steel
NiCrMoV II Steel
NiCrMoV III Steel
NiCrMoV IV Steel
NiCrVCu Steel
Nicrofer 3127 hMo - alloy 31
Nicrofer 4823 hMo - alloy G-3
Nicrofer3033 - alloy 33
Nicrofer4221 - alloy 825
Nicrofer4320 Ti Alloy
Nicrofer5120 CoTi - alloy C-263
Nicrofer5621 hMoW - alloy 22
Nicrofer5716 hMoW - alloy C-276
Nicrofer5923 hMo - alloy 59
Nicrofer6020 hMo - alloy 625
Nicrofer6616 hMo - alloy C-4
Niolox Steel
Niolox Steel
Nippon Steel
Nitinol Wire Steel
Nitralloy, 135 Mod. Steel
Nitrodur 8515 Steel
Nitrodur 8523 Steel
Nitrodur 8524 Steel
Nitrodur 8550 Steel
Non-Superhardening Steel
O.11C Steel
O.28C (A-2) Alloy and S20C Steel
O.81C Steel
O1 Steel
O1 Steel
O1 Steel
O1 Steel
O1 Steel
O1 Tool Steel
O2 Steel
O2 Tool Steel
OA2 Steel
OA2 Steel
OC100 Steel
OC100 Steel
OC80 Steel
OCHN3MFA Steel
OCR12 Steel
OCR12 Steel
OCR12 Steel
OCR12 Steel
OCR12EX Steel
OCR12EX Steel
OCR12EXL Steel
OCR12EXL Steel
OCR12EXL Steel
OCR12EXL Steel
OCR12SP Steel
OCR12SP Steel
OCR12VM Steel
OCR12VM Steel
OCR12VM Steel
OCR12VM Steel
OCR12VMS Steel
OCR12VMS Steel
OCR12VMS Steel
OCR6 Steel
OCR6 Steel
OCR8VMS Steel
OCR8VMS Steel
OCR8VMS Steel
OCR8VMS Steel
OCR8VMS Steel
OH237 Steel
OH237 Steel
OH237 Steel
OH237 Steel
OH238 Steel
OH238 Steel
OH239 Steel
OH239 Steel
OH239 Steel
OH239 Steel
OH239 Steel
OH246 Steel
OH246 Steel
OH248 Steel
OH248 Steel
OH252 Steel
OH252 Steel
OH253 Steel
OH253 Steel
OH255 Steel
OH257 Steel
OH257 Steel
OH258 Steel
OH259 Steel
OH259 Steel
OH260 Steel
OH490 Steel
OH490 Steel
OH842 Steel
OH842 Steel
OHV4 Steel
OHV4 Steel
OHV4 Steel
OHV5 Steel
OK 15.17 Steel
OK 48.08 Steel
OK 74.70 Steel
OK 75.75 Steel
OK Femax 33.30 MSG Steel
OK Femax 33.30 Steel
OK Femax 33.80 MSG Steel
OK Femax 33.80 Steel
OK Femax 38.65 MSG Steel
OK Femax 38.65 Steel
OPTIFER II (GeCe) Steel
OPTIFER III (TaCe) Steel
OPTIFER Ib (WTaY) Steel
OPTIFER-V (W,Ce) Steel
OPTIFER-VI (Ge,Ce) Steel
OPTIFER-VII (8.5 Cr, W) Steel
OPTIFER-X (W) Steel
OPTIMAR Steel
OPTIMAR-W Steel
ORVAR 2 Microdized Steel
ORVAR SUPREME Steel
ORVAR SUPREME Steel
ORVAR SUPREME Steel
ORVAR SUPREME and DIEVAR Steels
OSIKROSP Steel
OSIKROSP Steel
OSIKROSP Steel
OSIKROSP Steel
OSIKROSP Steel
OTV Steel
OTV Steel
OTV Steel
OTV Steel
OTV Steel
OTV Steel
OTV Steel
OTV1 Steel
OTV1 Steel
OTV1B Steel
OTVN Steel
OTVN Steel
OW, 0.1W, 1W Steels
OW1 Steel
OW4 Steel
OW4 Steel
OW4 Steel
OW4 Steel
OW4 Steel
OX 525 Steel
OvaX 200 Steel
OvaX 500 Steel
OvaX 600 Steel
OvaX 600 Steel
OvaX 800 Steel
Ovako 146S Steel
Ovako 157C Steel
Ovako 157C Steel
Ovako 225A Steel
Ovako 225A Steel
Ovako 253F Steel
Ovako 255G Steel
Ovako 256G Steel
Ovako 277 Steel
Ovako 277Q Steel
Ovako 280T Steel
Ovako 420G Steel
Ovako 477L Steel
Ovako 477L Steel
Ovako 477L Steel
Ovako 495B Steel
Ovako 528E and 528Q Steels
Ovako 5450 Steel
Ovako 593B Steel
Ovako 677Q Steel
Ovako 803J Steel
Ovako 803Q Steel
Ovako 803Q Steel
Ovako 824 Steel
Ovako 824B Steel
Ovako 825B Steel
Ovako 825B Steel
Ovako 826B Steel
Ovako 827B Steel
Ovako 831B Steel
Ovako 832K Steel
Ovako Hybrid Steels 55 and 60
Ovako Ovako356D and Ovako356Q Steels
Ovatec 277Q Steel
Ovatec 477 Steel
Ovatec 677 Steel
P19 NiCrMo 15.4 V Steel
P2 (Carburized Case) Steel
P2 (Carburized) Tool Steel
P2 Steel
P2 Tool Steel
P20 MOULD Steel
P20 Steel
P20 Steel
P20 Steel
P20 Tool Steel
P20+Ni Steel
P23/P24 Steel
P295GH Steel
P355NL1 Steel
P4 Steel
P4 Tool Steel
P460NH Steel
P460NH Steel
P500NH Steel
P91 Steel
P91 Steel
P91 Steel
P92 HTRG Steel
P92 Steel
P92 Steel
P92-2% W Steel
P980 Steel
PA Steel
PA Steel
PA Steel
PANACEA Steel
PB Steel
PB Steel
PC Steel
PC Steel
PC52 Steel
PD Steel
PD Steel
PD Steel
PEERLESS A Steel
PER1 Steel
PER1 Steel
PH15-5 Steel
PK Steel
PK324 Steel
PK330 Steel
PK335 Steel
PK335 Steel
PK335 Steel
PK339 Steel
PK339 Steel
PK348 Steel
PK348 Steel
PK348 Steel
PK3ML Steel
PK4 Steel
PK4EX Steel
PK4EX Steel
PK8 Steel
PM Steels
PM steel Astaloy CrM + 4%MA H46 (Mn-Si)
PM steel Astaloy85Mo + 4%MA H45 (Cr-Si)
PM steel Fe (ASC 100.29) + 4%MA H47 (Mn-Cr-Si)
PMS 25 Steel
PMS 25 Steel
PMS 35 Steel
PMS 35 Steel
PO209 Steel
PO209 Steel
PO731 Steel
PO731 Steel
PO731 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO733 Steel
PO735 Steel
PO735 Steel
PO766 Steel
PO768 Steel
PO768 Steel
PO768 Steel
PO795 Steel
PO795 Steel
PO85 Steel
PO85 Steel
PS 32 Steel
PS 55 Steel
PT181 Steel
PT181 Steel
PT759 Steel
PT759 Steel
PT759 Steel
PV3A Steel
PV3L Steel
PV3L Steel
PW812 Steel
PWM Steel
PWU Steel
Pearlite-free multiphase Steel I
Pearlite-free multiphase Steel II
Pearlite-free multiphase Steel III
Pearlite-free multiphase Steel IV
Pearlitic Malleable Cast Iron
Pearlitic Malleable Iron I
Pearlitic Malleable Iron II
Pearlitic Malleable Iron III
Pearlitic Malleable Iron IV
Pearlitic Malleable Iron V
Piano Wire Steel
Protac 550 Steel
Protac 600 Steel
Pyrowear Alloy 53
Q10 Steel
Q1100 Steel
Q235B Steel
Q420 FRE Steel
Q960E Steel
QP980 Steel
QRO 90 SUPREME Steel
Quench Aging of Fe-C Alloys
Quench Aging of Fe-C Alloys I
Quench Aging of Fe-C Alloys II
Quench Aging of Fe-C Alloys III
R+Mo+Nb Steel
R+Mo+Nb Steel
R+Nb+V Steel
R+Nb+V Steel
R.D.S. Steel
R260 Steel
R260 Steel
R410N15 Steel
R6110 Steel
R7 Steel
RA4W Steel
RAVNE23 Steel
RAVNE30 Steel
RAVNEX Steel
RB V0, RB V1, RB V2 Steels
RB370 Steel
RB390 Steel
REX 95 Steel
REX AA Steel
REX AA Steel
REX AAA Steel
REX CHAMPION Steel
REX M-2 Steel
REX M-2 Steel
REX M2 Steel
REX M2-5 Steel
REX MM Steel
REX MM Steel
REX MMM Steel
REX SUPERVAN Steel
REX VM Steel
REZISTAL 410* Steel
REZISTAL 420 Steel
REZISTAL 440A Steel
REZISTAL 440BM Steel
RF Steel
RIGOR Steel
RM10Co Steel
RM161a Steel
RM189 Steel
RM200 Steel
RNO-D Steel
RNO-D Steel
RNO-D Steel
RNO-MoV Steel
RNO-MoV Steel
ROLTEC SF Steel
ROLTEC SF Steel
ROP12 Steel
RP Steel
RPCo Steel
RPU Steel
RR ALTAIR 1.2340 MOD. Steel
RR ALTAIR 1.2340 MOD. Steel
RR ANTARES 1.2344 MOD. Steel
RR ANTARES 1.2344 MOD. Steel
RR ASTRO 1.2343 MOD. Steel
RR ASTRO 1.2343 MOD. Steel
RR SIRIO 1.2367 MOD. Steel
RR SIRIO 1.2367 MOD. Steel
RR VEGA 1.2738 MOD. Steel
RR VEGA 1.2738 MOD. Steel
RS Steel
RS Steel
RSB Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel
Rail Steel with 0.50% C
Rapidur 3343 Steel
Relationship between a TCP diagram and a TTT diagram
Retained Austenite vs. Ms and Mf
Rex M-2 Steel
Rodacciai 12NiCr3 Steel
Rodacciai 16MnCr5, 16MnCrS5 Steels
Rodacciai 16MnCr5, 16MnCrS5 Steels
Rodacciai 16NiCr11 Steel
Rodacciai 16NiCr11 Steel
Rodacciai 16NiCr4, 16NiCrS4 Steels
Rodacciai 16NiCr4, 16NiCrS4 Steels
Rodacciai 17NiCrMo6-4, 17NiCrMoS6-4 Steels
Rodacciai 17NiCrMo6-4, 17NiCrMoS6-4 Steels
Rodacciai 20CrNi4, 20CrNi4Pb Steels
Rodacciai 20MnCr5, 20MnCrS5 Steels
Rodacciai 20NiCrMo2-2, 20NiCrMoS2-2 Steels
Rodacciai 20NiCrMo2-2, 20NiCrMoS2-2 Steels
Rodacciai 50CrMo4 Steel
Rodacciai 50CrMo4 Steel
Rodacciai C35R Steel
Rodacciai C35R Steel
Rodacciai C50E Steel
Rodacciai C50E Steel
Rohling-RT6 Steel
Rohling-RTW 2H Steel
Rolled Stainless Steel and 18Cr-10Ni Weld Metal
Rolled Stainless Steel and 18Cr-10Ni Weld Metal
Rolled Stainless Steel and 18Cr-10Ni Weld Metal
Rolled Stainless Steel and 18Cr-10Ni Weld Metal
Rolled Stainless Steel and 18Cr-12Ni-2 to 3 Mo Weld Metal
Rolled Stainless Steel and 18Cr-12Ni-2.8Mo
Ruukki R4 Steel
S-1 Steel
S-1 Steel
S-2 Steel
S-2 Steel
S-3 Steel
S-3 Steel
S-4 Steel
S-4 Steel
S-5 Steel
S-5 Steel
S-6 Steel
S-6 Steel
S1 Steel
S1 Steel
S1 Tool Steel
S1100 QL Steel
S1100QL Steel
S1100QL Steel
S1100QL Steel
S1100QL Steel
S1100QL/2 Steel
S1100QL/3 Steel
S1100QL/4 Steel
S1100QL/5 Steel
S135 Steel
S2 Steel
S2 Tool Steel
S235 Steel
S235JR Steel
S243 Steel
S31254, S32654 Steels
S32760 and UR52N,SAF2507,29Cr-6Ni-2Mo-O.38N Steels
S355 Steel
S355 Steel
S355 Steel
S355 Steel
S355 Steel
S355 Steel
S355 Steel
S355 Steel
S355 Steel
S355GP Steel
S355J2 Steel
S355J2G3 Steel
S355J2G3 Steel
S355JR Steel
S355N Steel
S355N Steel
S355NL Steel
S369 Steel
S420ML Steel
S430GP Steel
S45C Steel
S45C Steel
S45C Steel
S460 Steel
S460 Steel
S460 Steel
S460M Steel
S460N Steel
S5 Steel
S5 Tool Steel
S50C Steel
S550M Steel
S550MC Steel
S6 Steel
S690 Steel
S690Q Steel
S690QL Steel
S690QL Steel
S690QL Steel
S690QL Steel
S690QL Steel
S690QL Steel
S7 Tool Steel
S7 Tool Steel
S700 Steel
S700M Steel
S890 Steel
S890Q Steel
S890QL Steel
S890QL Steel
S890QL Steel
S960MC Steel
S960MC Steel
S960Q Steel
S960Q Steel
S960QL Steel
S960QL Steel
S960QL Steel
S960QL/2 Steel
SA508 Gr.3 Steel
SA508 Steel
SA508 Steel
SA508 Steel
SA508 Steel
SA508Gr.4N Steel
SA508Gr.4N Steel
SA508Gr4 Steel
SA508Gr4 Steel
SA738 Gr.B Steel
SAE 1025* Steel
SAE 1030 Steel
SAE 1038 Steel
SAE 1038 Steel
SAE 1050 Steel
SAE 1050 Steel
SAE 1050 Steel
SAE 1050 Steel
SAE 1075 Steel
SAE 1092 Steel
SAE 1092 Steel
SAE 1092 Steel
SAE 1141 Steel
SAE 1320 Steel
SAE 1513 + Nb Steel
SAE 1513 Steel
SAE 15B41 Steel
SAE 2340 Steel
SAE 2340* Steel
SAE 2515 Steel
SAE 3140 Steel
SAE 3140 Steel
SAE 3140 Steel
SAE 3140 Steel
SAE 3240 Steel
SAE 3240 Steel
SAE 3310 Steel
SAE 3312 Steel
SAE 3312 Steel
SAE 3360 (Modified) Steel
SAE 3360 (Modified) Steel
SAE 3360 mod. Steel
SAE 3360 mod. Steel
SAE 4024 Steel
SAE 4047 Steel
SAE 4047 Steel
SAE 4130 Steel
SAE 4130 Steel
SAE 4130 Steel
SAE 4130 Steel
SAE 4130 Steel
SAE 4130* Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4140 Steel
SAE 4142 Steel
SAE 4142 Steel
SAE 4142 Steel
SAE 4142 Steel
SAE 4147 Steel
SAE 4150 (+Ni) Steel
SAE 4150 Steel
SAE 43100* Steel
SAE 4315 Steel
SAE 4330 Steel
SAE 4330 Steel
SAE 4330 Steel
SAE 4330 Steel
SAE 4337 Steel
SAE 4340 Steel
SAE 4340 Steel
SAE 4340 Steel
SAE 4340 Steel
SAE 4340* Steel
SAE 4340+Si Steel
SAE 4342 Steel
SAE 4360 mod. Steel
SAE 43BV14 Steel
SAE 4615 Steel
SAE 4640 Steel
SAE 4640 Steel
SAE 4640 Steel
SAE 4640 Steel
SAE 48100 (Carburized Case of SAE 4815) Steel
SAE 4815 Steel
SAE 4815 Steel
SAE 4815 Steel
SAE 51100 Steel
SAE 5140 Steel
SAE 5140 Steel
SAE 5140 Steel
SAE 5160 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 52100 Steel
SAE 6140 Steel
SAE 6150 Steel
SAE 6150 Steel
SAE 8620 Steel
SAE 8620 Steel
SAE 8620 Steel
SAE 8630 Steel
SAE 8640 Steel
SAE 86B40 Steel
SAE 9254 Steel
SAE 9260 Steel
SAE 9840 Steel
SAE T-1335 Steel
SAE X4130 Steel
SAE/AISI 4140-4142 Steels
SAE1020 Steel
SAE15B41H Steel
SAF 2205 Duplex Stainless Steel
SAF 2205 Duplex Stainless Steel
SAF 2507 Steel
SAF2205 Steel
SAF2207 Steel
SANCY2 Steel
SANDERSON EXTRA Steel
SANDERSON SPECIAL Steel
SBQ Nitriding Steel with 0.03% Ni
SBQ Nitriding Steel with 0.70% Ni
SBQ Nitriding Steel with 1.40% Ni
SBQ Nitriding Steel with 2.75% Ni
SCM 3 Steel
SCM 5 Steel
SCr 3 Steel
SCr3 Steel
SCr415 Steel
SCr415 Steel
SCr420 Steel
SCr420 Steel
SD 600 S Steel
SDC Steel
SG Iron
SH-CCT Welding Diagrams I
SH-CCT Welding Diagrams II
SHELLDIE Steel
SIS 2092 Steel
SK3, S43C, SCM 22, SNCM 21 Steels
SK5 Steel
SKD 11 Steel
SKD11 Steel
SKD61 Steel
SKD61 Steel
SKF ToughTech Steel
SKS 5 Steel
SKS 5 Steel
SLEIPNER Steel
SLEIPNER Steel
SLM 4340 Steel
SM - 2738 Steel
SM - 2738 Steel
SM41 Steel
SM41(A) Steel
SM41(B) Steel
SM41A Steel
SM41A Steel
SM41B Steel
SM41B Steel
SM50 BS-1 Steel
SM50A Steel
SM50A Steel
SM50B Steel
SM50B Steel
SM50B Steel
SM50BC-1 Steel
SM50BN-1 Steel
SM50Y Steel
SMR Steel
SMV3 Steel
SMV5W Steel
SN Steel
SNC22 Steel
SNCM 8 Steel
SNCM8 Steel
SNCM8 Steel
SOLAR Steel
SP28T Steel
SS Steel
SS Steel
SS400 Steel
SS55 Steel
ST52V Steel
STAVAX ESR Steel
STAVAX ESR Steel
STD61 Steel
STENTOR TOOL Steel
STF4M Steel
SUJ 2 Steel
SUJ 2 Steel
SUJ 2 Steel
SUJ 2 Steel
SUJ 2 Steel
SUJ2 I Steel
SUJ2 II Steel
SUJ2 Steel
SUJ2 Steel
SUJ2 Steel
SUJ2 Steel
SUJ3 Steel
SUP7 Steel
SUP7 Steel
SUPERPLAST 300 Steel
SUPERPLAST 350 Steel
SUPERPLAST 350 Steel
SUPERPLAST FX Steel
SUS 1 Steel
SUS 1 Steel
SUS 1, SUS 2, SUS 3 Steels
SUS 2 Steel
SUS 2 Steel
SUS 3 Steel
SUS 3 Steel
SUS304 Steel
SUS304L Steel
SVERKER SF Steel
SW538H Steel
SW538H Steel
SW718H Steel
SWG 2083 VICTORY ESR Steel
SWG 2085 Steel
SWG 2311 Steel
SWG 2312 Steel
SWG 2316 Steel
SWG 2316 VICTORY ESR Steel
SWG 2343 (SWG EX3) Steel
SWG 2343 VICTORY ESR (EX3 ESR) Steel
SWG 2344 (EX4) Steel
SWG 2344 VICTORY ESR (EX4 ESR) Steel
SWG 2347 Steel
SWG 2357 (AISI S7) Steel
SWG 2367 VICTORY ESR (EX7 ESR) Steel
SWG 2379 Steel
SWG 2711 Steel
SWG 2711mod Steel
SWG 2711mod Steel
SWG 2714 Steel
SWG 2738 / 2738H / 2738HH Steel
SWG 2767 Steel
SWG 738HH Steel
SWG CPM50 VICTORY ESR Steel
SWG CRMHP VICTORY ESR Steel
SWG EX1 VICTORY ESR Steel
SWG EX2 Steel
SWG GPM58 VICTORY ESR Steel
SWG OPTI N+ Steel
SWG XPM Steel
SWG XPM VICTORY ESR Steel
SWG - 2080 Steel
SWG - 2083 Steel
SWG - 2311 Steel
SWG - 2312 Steel
SWG - 2343 Steel
SWG - 2344 Steel
SWG - 2379 Steel
SWG - 2714 Steel
SWG - 2738 Steel
SWG - 2738 mod. Steel
SWG - 2767 Steel
SWRH82B Steel
SZMF Steel
Sandvik 253 MA Steel
Sandvik Nanoflex Steel
Sanicro 69 Steel
Semi-HSS Steel
Semi-HSS, Semi-HSS +N Steels
Si-0 Steel
Si-0 Steel
Si-0.2 Steel
Si-0.2 Steel
Si-0.5 Steel
Si-0.5 Steel
Si-1.0 Steel
Si-1.0 Steel
Si-1.6 Steel
Si-1.6 Steel
Si-CAL Steel
Si-Mn Steel
Si-Mn Steels
Si-Mn-Ti-B Steel
SiMn HT50 Steel
SiMn HT50 Steel
Sleipner Steel
Sleipner Steel
St 3 SU Steel
St 315 N Steel
St 355 E Z Steel
St 355 E/Ch.1 Steel
St 355 E/Ch.2 Steel
St 355 E/Ch.3 Steel
St 355 Steel
St 355 T/Ch.1 Steel
St 355 T/Ch.2 Steel
St 355 T/Ch.3 Steel
St 355 T/Ch.4 Steel
St 355 TM Steel
St 355/Ch.1 Steel
St 355/Ch.2 Steel
St 4 SU Steel
St 44-3 Steel
St 440 Steel
St 45/60 Steel
St 460 E/Ch.1 Steel
St 460 E/Ch.2 Steel
St 460 E/Ch.3 Steel
St 460 E/Ch.4 Steel
St 52-3 Steel
St 52-3 Steel
St 600/Ch.1 Steel
St 600/Ch.2 Steel
St 600/Ch.3 Steel
St 600/Ch.4 Steel
St2S Steel
St3S Steel
St460 E Steel
St52-3 Steel
St52-3 Steel
StE 355 Steel
StE 355 TM Steel
StE 460 Steel
StE 690 Steel
StE 690 Steel
StE355 Steel
StE47 Steel
StE47 Steel
StE47 Steel
StE47 Steel
StE70 Steel
Stainless 12 Steel (As Forged)
Stainless 12 Steel (As Forged)
Stainless Steel
Stainless Steel
Stainless Steel
Stainless Steels
Staminal Steel
Steel with 0.00% Mo
Steel with 0.15% Mo
Steel with 0.16% Cr
Steel with 0.30% Cr
Steel with 0.30% Mo
Steel with 0.33% Ni
Steel with 0.38% Mo
Steel with 0.4% C
Steel with 0.48% Cr
Steel with 0.50% Mo
Steel with 0.99% Si
Steel with 1.00% Ni
Steel with 1.50% Si
Steel with 2.00% Si
Steel with 2.50% Ni
Steel with 2.50% Ni
Steel with B an Ga
Steel with about 8% Cr and 2% Mo
Steels 8, 10, 11, 12, 13, 17
Strong Bainite Steel
Strong Bainitic Steel
Structural Fe-Cr Steel
Structural Steel
Sumitomo Cr-Mo Steel
Supercooled Austenite Pipe Steel
Superhardening Steel
Superplast 300 Steel
Superplast 400 Steel
Superten Steel
T-1 Steel
T-1 Steel
T-1 Steel
T/P24 Steel
T/P24 Steel
T/P91 Steel
T/P91 Steel
T1 Steel
T1 Steel
T1 Steel
T1 Tool Steel
T2 Steel
T2 Tool Steel
T23 Steel
T23 Steel
T23 Steel
T24 Steel
T4 Steel
T4 Tool Steel
T7 Steel
T7 Tool Steel
T8 Steel
T8 Tool Steel
T8, 4CrMoV Steels
T8, 6CrW2Si, 4CrMoV, CrMn, Cr12W Steels
T92 Steel
TA2 Steel
TBL PLUS Steel
TBL Steel
TD2 Steel
TD2 Steel
TD2-A Steel
TD2-A Steel
THRUS-WASHER Steel
THYRAPID 2990 Steel
THYRAPID 3343 Steel
THYRODUR 2381 Steel
THYRODUR 1520 Steel
THYRODUR 2002 Steel
THYRODUR 2067 Steel
THYRODUR 2080 Steel
THYRODUR 2101 Steel
THYRODUR 2235 Steel
THYRODUR 2242 Steel
THYRODUR 2243 Steel
THYRODUR 2249 Steel
THYRODUR 2363 Steel
THYRODUR 2363 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2379 Steel
THYRODUR 2436 Steel
THYRODUR 2510 Steel
THYRODUR 2516 Steel
THYRODUR 2550 Steel
THYRODUR 2550 Steel
THYRODUR 2721 Steel
THYRODUR 2766 Steel
THYRODUR 2767 Steel
THYRODUR 2826 Steel
THYRODUR 2833 Steel
THYRODUR 2842 Steel
THYRODUR 2842 Steel
THYRODUR 2842 Steel
THYRODUR 2990 Steel
THYRODUR2067 Steel
THYRODUR2210 Steel
THYROFORT 25CrMo4/25CrMoS4 Steel
THYROFORT 28Mn6 Steel
THYROFORT 30CrNiMo8 Steel
THYROFORT 34Cr4/34CrS Steel
THYROFORT 34CrMo4/34CrMoS4 Steel
THYROFORT 34CrNiMo6 Steel
THYROFORT 36CrNiMo4 Steel
THYROFORT 36NiCrMo16 Steel
THYROFORT 37Cr4/37CrS4 Steel
THYROFORT 37Cr4/37CrS4 Steel
THYROFORT 41Cr4/41CrS4 Steel
THYROFORT 42CrMo4/42CrMoS4 Steel
THYROFORT 46Cr2/46CrS2 Steel
THYROFORT 50CrMo4 Steel
THYROFORT C22E Steel
THYROFORT C45E Steel
THYROFORT C55E/C55R Steel
THYROFORT C60E/C60R Steel
THYROFORT Cf53 Steel
THYROFORT CrMoV9 Steel
THYROLL 2327 Steel
THYROLL 2362 Steel
THYROPLAST 2083/2083 SUPRA Steel
THYROPLAST 2083/2083 SUPRA Steel
THYROPLAST 2085 Steel
THYROPLAST 2162 Steel
THYROPLAST 2311 Steel
THYROPLAST 2312 Steel
THYROPLAST 2312 Steel
THYROPLAST 2312 Steel
THYROPLAST 2316/2316 SUPRA Steel
THYROPLAST 2711 Steel
THYROPLAST 2738 Steel
THYROPLAST 2738 Steel
THYROPLAST 2764 Steel
THYROPLAST 2764 Steel
THYROPLAST 2764 Steel
THYROPLAST 2891 Steel
THYROTHERM 2342 EFS Steel
THYROTHERM 2343 EFS/2343 EFS SUPRA Steel
THYROTHERM 2343 EFS/2343 EFS SUPRA Steel
THYROTHERM 2343 EFS/2343 EFS SUPRA Steel
THYROTHERM 2343 Steel
THYROTHERM 2344 EFS/2344 EFS SUPRA Steel
THYROTHERM 2344 EFS/2344 EFS SUPRA Steel
THYROTHERM 2344 Magnum Steel
THYROTHERM 2344 Steel
THYROTHERM 2365 EFS/2365 EFS SUPRA Steel
THYROTHERM 2367 EFS/2367 EFS SUPRA Steel
THYROTHERM 2714 Steel
THYROTHERM 2885 EFS/2885 EFS SUPRA EFS SUPRA Steel
THYROTHERM 2999 EFS SUPRA Steel
THYROTHERM E 38 K Steel
THYROTHERME 38K Steel
TIG1, TIG2 Steels
TOOLOX Steel
TORKA Steel
TORKA Steel
TOUGHTEC SF Steel
TOUGHTEC SF Steel
TQ1 Steel
TQ1 Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP Steel
TRIP780 Steel
TRIP800 Steel
TTA Diagram of Steel
TTT Diagram by Davenport, Bain and N. Kearny
TV4 Steel
Tempaloy A-1 Steel
Tenasteel Steel
Tenasteel Steel
Thermit Steel
Thermodur 2342 EFS Steel
Thermodur 2343 Steel
Thermodur 2343 Superclean/Thermodur 2343 EFS Steel
Thermodur 2343 Superclean/Thermodur 2343 EFS Steel
Thermodur 2344 Steel
Thermodur 2365 Superclean/Thermodur 2365 EFS Steel
Thermodur 2367 Superclean Steel
Thermodur 2367 Superclean/Thermodur 2367 EFS Steel
Thermodur 2714 Steel
Thermodur 2999 Superclean Steel
Thermodur E 38 K Superclean Steel
Thermodur E 40 K Superclean Steel
Thruhard Supreme High Hard Steel
Thyrapid 3207 Steel
Thyrapid 3247 Steel
Thyrodur 2101 Steel
Thyrodur 2362 Steel
Thyrodur 2379 Steel
Thyrodur 2379 Steel
Thyrodur 2379 Steel
Thyrodur 2379 Steel
Thyrodur 2690 Steel
Thyrodur 2842 Steel
Thyroplast 2162 Steel
Thyroplast 2312 Steel
Thyroplast 2316 Steel
Thyrotherm 2343 Steel
Thyrotherm 2343 Steel
Thyrotherm 2343 Steel
Thyrotherm 2344 ESR Magnum Steel
Thyrotherm 2344 Steel
Thyrotherm 2344 Steel
Thyrotherm 2365 Steel
Thyrotherm 2365 Steel
Thyrotherm 2367 Steel
Thyrotherm 2367 Steel
ThyssenKrupp C-276, C-2000 and 686 Alloys
Ti Bearing Steels
Ti Killed Steel
Ti Modified 316 Stainless Steel
Ti-3 Steel
Ti-3 Steel
Ti-47Al-2Cr-2Nb-1Mo
Ti-47Al-2Cr-2Nb-1Mo-0.2B
Ti-Mo, Ti-Mo-Nb Steels
Ti-Oxide Bearing Steel
Ti-Oxide Bearing Steel
Ticonal 600 Si-Mod. Steel
Ticonal Steel
Timken 4140 Steel
Timken 4140HW Steel
Tool Steel
Tool Steel
Toolox 33 Steel
Toolox 44 Steel
Type 304 Steel
Type 304 Steel
Type 308 Steel
Type 321 Steel
Type 347 Steel
Type 403 Steel
Type 403 Steel
Type 410 Steel
Type 410 Steel
Type 410 mod. Steel
Type 416 Steel
Type 420 Steel
Type 440A Steel
Type 440B Steel
Tyrapid 3343 Steel
Tyrapid 3343 Steel
Tyrodur 2762 Steel
Tyrodur 2762 Steel
Tyrodur 2762 Steel
Tyrotherm 2343 Steel
Tyrotherm 2344 Steel
U-1 Steel
U-1 Steel
U-2 Steel
U-2 Steel
U-3 Steel
U-3 Steel
U-3 Steel
U.I.C 860 grade A and THS 11 Steels
U16-Sh Steel
U50 Alloy
U71Mn Steel
U71Mn Steel
UCS Steel
UGINOX MA2 Steel
UGINOX MA3 Steel
UGINOX MA3 Steel
UGINOX MA4 Steel
UGINOX MA5M Steel
UH-1 Steel
UH-1 Steel
UH-2 Steel
UH-2 Steel
UH-3 Steel
UH-3 Steel
UH-4 Steel
UH-4 Steel
UH-5 Steel
UH-5 Steel
UH-6 Steel
UH-6 Steel
UH1 Steel
UHS Steel
UIC60 Steel
UIC60, 900A-type Rail Steel
UK15 Steel
ULC Weld Metal
ULCB Steel
ULCB Steel
ULCB Steel
UNIMAX Steel
UNS G41400, UNS G43400 Steels
UNS S31803 Steel
UNS S31803 Steel
UNS S32750 Steel
UNS-S32750 Steel
UR 2205 Steel
UR 2205Mo Steel
UR210CrW46 Steel
UR45N Alloy
UR52N Steel
URANUS 45N Mo Steel
URANUS 52N
US Steel
USD Steel
USD-H Steel
USIBOR 1500 Steel
USIBOR 1500P Steel
USIBOR 1500P Steel
USN Steel
USS Airsteel X 200 Steel
USS Cor-Ten Steel
USS Cor-Ten Steel Steel
USS Strux Steel
USS Strux Steel
USS T1 Steel
USS T1 Steel
UTOP2 Steel
UTOPMO1 Steel
UTOPMO2 Steel
UTOPMO4 Steel
UTOPMO4 Steel
UTOPMO5 Steel
UTOPMO5 Steel
UTOPMO6 Steel
UTOPMO6 Steel
UTOPMO7 Steel
UTOPMO7 Steel
UTOPMONI Steel
UTOPN Steel
UTOPN Steel
UTOPN Steel
UTOPN Steel
UTOPN Steel
UTOPNIN Steel
Uddeholm Balder Steel
Uddeholm Formvar Steel
Uddeholm Tyrax ESR Steel
Ugitech 2205 Steel
Ultra Fine Grained Steel
Ultra Low Carbon Steel
Ultra-Low Carbon
Ultra-Strength Steel I
Ultra-Strength Steel I
Ultra-Strength Steel I
Ultrahigh Strength Bainitic Steel
Ultrahigh Strength Bainitic Steel
Umbrella-Bone Steel
Union K 56 Steel
Union MoNi Steel
Union NiMoCr Steel
Union X90 Steel
Uranus 50 Duplex Stainless Steel
Uranus 50 Duplex Stainless Steel
Usibor 1500 Steel
Usibor 1500-AS Steel
Usinor-Sacillor S355N Steel
V 1080 Steel
V Steel
V-3 Steel
V-3 Steel
V-Mo-Ti Steel
V-Mo-Ti Steel
V-N Steel
V5 Steel
V6 Steel
VAN-80 HSLA Steel
VAN-80 Steel
VANADIS 10 SUPER CLEAN Steel
VANADIS 10 SUPER CLEAN Steel
VANADIS 23 Super Clean Steel
VANADIS 23 SuperClean Steel
VANADIS 30 Steel
VANADIS 4 EXTRA SuperClean Steel
VANADIS 4 Extra Steel
VANADIS 4 Extra Steel
VANADIS 4 Extra SuperClean Steel
VANADIS 4 Steel
VANADIS 4 Steel
VANADIS 6 SUPERCLEAN Steel
VANADIS 6 SUPERCLEAN Steel
VANADIS 6 Steel
VANADIS 8 Extra SuperClean Steel
VANADIS-6 SUPER CLEAN Steel
VANADIS-6 SUPER CLEAN Steel
VANCRON 40 Steel
VANCRON 40 Steel
VANCRON 40 Steel
VANCRON 40 Steel
VC140 Steel
VC140 Steel
VC140 Steel
VCM Nitriding Steel
VCM Nitriding Steel
VCMO125 Steel
VCMO125 Steel
VCMO135 Steel
VCMO135 Steel
VCMO140 Steel
VCMO150 Steel
VCMO150 Steel
VCMO150 Steel
VCMO150 Steel
VCMO230 Steel
VCMO230 Steel
VCMO230 Steel
VCNMO100 Steel
VCNMO100 Steel
VCNMO150 Steel
VCNMO150 Steel
VCV150 Steel
VCV150 Steel
VCV150 Steel
VCV150 Steel
VIDAR SUPERIOR Steel
VIDAR 1 ESR Steel
VIDAR SUPREME Steel
VIKING Steel
VM100 Steel
VM12-SHC Steel
VMB Steel
VMS135 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ197 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
VZ727 Steel
Vanadis 23 SuperClean Steel
Vanadis 30 SuperClean Steel
Vanadis 60 SuperClean Steel
Vanadis 8 SuperClean Steel
Vanadium and Titanium Microalloyed Steels
Vancron SuperClean Steel
Viking Steel
Viking Steel
VoestAlpine steel V1 Steel
W ST 3 Steel
W St 3sp/Ch.1 Steel
W St 3sp/Ch.2 Steel
W St 3sp/Ch.3 Steel
W1 Steel
W1 Steel
W1 Steel
W1 Tool Steel
W1 Tool Steel
W1 Tool Steel
W1.2311 Steel
W1.2311 Steel
W1.2714 Steel
W1.2714 Steel
W1.2738 Steel
W2 Steel
W2 Tool Steel
W370B Steel
W370C Steel
W370D Steel
W370H Steel
W4 Steel
W4 Tool Steel
W44 Steel
WEARTEC SF Steel
WEARTEC SF Steel
WELDOX 1300 Steel
WELL-TEN60 Steel
WELL-TEN60H Steel
WELL-TEN60R Steel
WELL-TEN62 Steel
WELL-TEN74(A) Steel
WELL-TEN74(B) Steel
WELL-TEN80(A) Steel
WELL-TEN80(B) Steel
WELL-TEN80C(A) Steel
WELL-TEN80C(B) Steel
WELL-TEN80S(41) Steel
WELL-TEN80S(43) Steel
WP1-0.10CB, WP1-0.13CB, WP1-0.08CBMo Steels
WP1-B, WP1-BMo Steels
WP2-0.2CrB, WP2-Mo Steels
WP2-Nb Steel
WP2-Ni, WP2-0.2CrBNiCu Steels
WP2-Ref Steel
WT-60 Steel
WT-60 Steel
WT-80 Steel
WT-80 Steel
WT-80 Steel
WT-80 Steel
WT-80C Steel
WT-80C Steel
WT60(A) Steel
Welten 80 Steel
Welten 80 Steel
Welten55C Steel
Welten55C Steel
White Iron Class III (28% Cr)
White Iron Class IIc
White Iron Class IIe
Wrought 316 Stainless Steel and 19-12-3 Weld Metal Steel
Wrought 4340 Steel
X 20 Cr 13 Steel
X 20 Cr 3 Steel
X-80 Steel
X100 Steel
X100 Steel
X100 Steel
X100 Steel
X100 Steel
X100 Steel
X102CrMo17 Steel
X102CrMo17 Steel
X105CrMo17 Steel
X10CrAl7 Steel
X10CrAl7 Steel
X10CrMoVNb9-1 (T/P91) Steel
X10CrMoVNb9-1 Steel
X10CrMoVNb91 (9% Cr-mod, P91/T91) Steel
X10CrNiNb18-9 Steel
X10CrWMoVNb9-2 (T/P92) Steel
X10CrWMoVNb9-2 Steel
X11CrMoWVNb9-1 Steel
X11CrMoWVNb9-1-1 Steel
X12CrCoWVNb12-2-2 (VM12-SHC) Steel
X12CrMo7 Steel
X12CrMo9-1 Steel
X12CrMo9-1 Steel
X13T6 Steel
X153CrMoV12 Steel
X155CrMoV12 Steel
X15TN Steel
X18CrNiMoVNb121 Steel
X20Cr13 Steel
X20CrMoV11-1 Steel
X20CrMoV12-1 Steel
X20CrMoV12-1 Steel
X20CrMoV12-1 Steel
X20CrMoV12-1 Steel
X20CrMoWV12-1 Steel
X20CrMoWV12-1 Steel
X210Cr12 Steel
X210Cr12 Steel
X210Cr12 Steel
X210Cr12 Steel
X210Cr12 Steel
X210Cr12 Steel
X210CrW12 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X22CrMoV12-1 Steel
X2CrNiMoN22-5-3 Steel
X30Cr13 Steel
X30WCrV5-3 Steel
X30WCrV5-3 Steel
X30WCrV9-3 Steel
X30WCrV9-3 Steel
X32CrMoV33 Steel
X37CrMoV5-1 Steel
X37CrMoV5-1 Steel
X37CrMoV5-1/BH11 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1 Steel
X38CrMoV5-1, X40CrMoV5-1, X38CrMoV5-3, X32CrMoV3-3 Steels
X38CrMoW5 Steel
X40 WCrV5 Steel
X40Cr13 Steel
X40Cr13 Steel
X40Cr13 Steel
X40Cr13 Steel
X40Cr14 Steel
X40CrMo15 Steel
X40CrMoV5-1 Steel
X40CrMoV5-1 Steel
X40CrMoV51 Steel
X40CrSiMo10-2 Steel
X45Cr13 Steel
X45Cr13 Steel
X45Cr13 and X30Cr13 Steels
X45CrMoV14 Steel
X45CrSi9-3 Steel
X45Mn2 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X45NiCrMo4 Steel
X52 Steel
X55CrMoCuCo13-2 Steel
X5CrNi18-9 Steel
X5CrNiCuNb16-4 Steel
X5CrNiCuNb16-4 Steel
X5CrNiMo17-13 Steel
X5CrNiMo17-13 Steel
X5CrNiMo17-13 Steel
X5CrNiMoCuNb14-5 Steel
X60 Pipeline Steel
X60 Pipeline Steel
X60 Pipeline Steel
X60 Pipeline Steel
X60 Steel
X60 Steel
X60 Steel
X60 TM Steel
X60Cr14MoV Steel
X60CrMoV and X45CrMoV1 Steels
X65 (0.047C-1.23Mn) Steel
X6Bø, X12M Steels
X70 Steel
X70 Steel
X70 Steel
X80 Steel
X80 Steel
X80 Steel
X80 Steel
X82WMoCrV6-5-4 Steel
X82WMoCrV6-5-4 Steel
X8CrNi25-4 Steel
X8Ni9 Steel
X90CrMoV18 Steel
XC 32 Steel
XC 38 Steel
XC 38 Steel
XC 38 Steel
XC 42 Steel
XC 42 Steel
XC 48 Steel
XC 55 Steel
XC 55 Steel
XC 70 Steel
XC 70 Steel
XC 80 Steel
XD15NW Steel
XD16N Steel
XD16N Steel
Xl2CrMo7 Steel
Y1 120 Steel
Y1 120 Steel
Y1 90 Steel
YA Steel
YA Steel
YB Steel
YB Steel
YC Steel
YC Steel
YD Steel
YD Steel
YE Steel
YE Steel
YF Steel
YF Steel
YG Steel
YG Steel
YND33 Steel
YND33 Steel
YUS 550 Steel
Z 10 N 5 Steel
Z 10 N 5 Steel
Z 10 N 9 Steel
Z 10 N 9 Steel
Z 100 CDV 5 Steel
Z 110 DKCWV 09-08-04-02-01 Steel
Z 12 C 13 Steel
Z 120 M 12 Steel
Z 130 WCV 12-04-04 Steel
Z 130 WDCV 06-05-04-04 Steel
Z 15 CD 5-05 Steel
Z 15 CD 5-05 Steel
Z 150 WKVC 12-05-05-04 Steel
Z 160 CDV 12 Steel
Z 165 WKVC 12-10-05-04 Steel
Z 20 CDNbV 11 Steel
Z 200 C 12 Steel
Z 30 C 13 Steel
Z 30 WCKV 09-03 Steel
Z 30 WCV 9 Steel
Z 38 CDV 5 Steel
Z 38 CDV 5 Steel
Z 38 CDWV 5 Steel
Z 38 CDWV 5 Steel
Z 40 C 14 Steel
Z 40 C 14 Steel
Z 40 CSD 10 Steel
Z 40 WCV 5 Steel
Z 60 WCV 18 Steel
Z 65 WDCV 06-05 Steel
Z 80 WCDX 12-04-02-02 Steel
Z 80 WCV 18-04-01 Steel
Z 80 WDCV 6 Steel
Z 80 WKCV 18-05-04-01 Steel
Z 80 WKCV 18-10-04-02 Steel
Z 80 WKCV 18-10-04-02 Steel
Z 85 DCWV 08-04-02-02 Steel
Z 85 WCV 18-04-02 Steel
Z 85 WDKCV 06-05-05-04-02 Steel
Z3CN20.09M Steel
Z8 Steel
Z8B21 Steel
Z8B24 Steel
Z8B25 Steel
Z8B26 Steel
Zeron100 Alloy